Influence of Subsurface Layer on the Indentation Damage Behavior of YSZ Thermal Barrier Coating Layers Deposited by Electron Beam Physical Vapor Deposition (전자 빔 물리적 증착(EB-PVD)법으로 코팅된 YSZ 열차폐층의 압흔손상 거동에 대한 하부층의 영향)

  • Heo, Yong-Suk;Park, Sang-Hyun;Han, In-Sub;Woo, Sang-Kuk;Jung, Yeon-Gil;Paik, Un-Gyu;Lee, Kee-Sung
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.9
    • /
    • pp.549-555
    • /
    • 2008
  • The thermal barrier coating must withstand erosion when subjected to flowing gas and should also maintain good stability and mechanical properties while it must also protect the turbine component from high temperature, hot corrosion, creep, and oxidation during operation. In this study we investigated the influence of subsurface layer, $Al_2O_3$ or NiCrCoAIY bond coat layer, on the indentation damage behavior of YSZ thermal barrier coating layers deposited by electron beam physical vapor deposition (EB-PVD). The bond coat is deposited using different process such as air plasma spray (APS) or spray of high velocity oxygen fuel (HVOF) and the thickness is varied. Hertzian indentation technique is used to induce micro damages on the coated layer. The stress-strain behaviors are characterized by results of the indentation tests.

Annealing under low oxygen partial pressure for crystal growth of BaTiO$_3 $thin films prepared by coating-pyrolysis process (코딩-열분해법에 의해 제조한 BaTiO$_3 $ 박막의 결정 성장을 위한 낮은 산소 분압에서의 열처리)

  • Kim, Seung-Won
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.10 no.2
    • /
    • pp.111-115
    • /
    • 2000
  • $BaTIO_3$ thin films were prepared on (100) $BaTIO_3$ substrates by coating- pyrolysis process using metal-organic compounds of Ba and Ti. The amorphous films prefired at $450^{\circ}C$were crystallized above $700^{\circ}C$ under oxygen partial pressure of $2\times 10^{-4}$. The lattice parameters of the perpendicular axis for the $BaTIO_3$ thin films heat-treated below $800^{\circ}C$ were closer to a value of cubic $BaTIO_3$, whereas those above $800^{\circ}C$ were closer to a value of tetragonal BaTiG. The results of XRD P scan and pole-figure analyses indicated that BaTiO, thin films have an epitaxial relationship with the $SrTiO_3$ substrates. The $BaTIO_3$thin films annealed at$800^{\circ}C$ showed the surface with island-like grains about 0.4$mu \textrm{m}$ and the cross section of 0.8 $mu \textrm{m}$ thickness with granular grains.

  • PDF

Solidify Properties of Radioactive Waste using Paraffin Wax (파라핀 왁스를 이용한 방사성 폐기물의 고화 특성)

  • Lee, Han Chul;Chang, Yoon Ho
    • Applied Chemistry for Engineering
    • /
    • v.17 no.4
    • /
    • pp.391-396
    • /
    • 2006
  • When radioactive wastewater was solidified treatment by cement, the drying rate of cement and the volume reduction ratio was decreased because of boric acid component in the wastewater. In order to supplement the demerit, effects of paraffin wax investigated in this study. Paraffin wax has a hydrophobic properties and a low affinity with inorganic materials. When the radioactive wastewater was tested by a small of wax, the compressive strength of solidified waste are decreased Therefore boric acid in radioactive wastewater are first treated by alkali salt and coated by the stearic acid. During the solidification step, The amount of paraffin wax addition get the result that the compressive strength of solidification with cement was the same as that with paraffin wax. The leaching properties of radioactive waste solidified was the same CFL (cumulative fraction leached), PR (penetration rate), effective diffusivity if paraffin wax content in solidified waste was 20% or 25%.

A Study on the elastic properties of coated layers and the changes of microstructure in plasma spray coating of $Al_2$O$_3$-TiO$_2$ ceramics (Al$_2$O$_3$-TiO$_2$세라믹의 플라즈마 용사과정에서 미세구조의 변화와 용사코팅층의 탄성에 대한 연구)

  • 이형근;김대훈;황선효;안병국;김병희;서동수;안명구
    • Journal of Welding and Joining
    • /
    • v.14 no.6
    • /
    • pp.109-118
    • /
    • 1996
  • Al$_2$O$_3$-TiO$_2$powders of six different compositions were plasma-sprayed on Ti substrate. The spray powders and the spray coated layers were analysed and compared using SEM and X-RD. The elastic properties (specific elastic constant and damping coefficient) of the coated specimens were measured in order to select the optimum composition range of ceramics for use in a speaker diaphragm. A correlation between the microstructure and elastic properties was also investigated. When $Al_2$O$_3$powders with 0- 13% TiO$_2$were plasma sprayed, the coated layers were composed of metastable y-Al$_2$O$_3$with small amount of $\alpha$-Al$_2$O$_3$and the content of $\alpha$-Al$_2$O$_3$was increased with TiO$_2$content. Specific elastic constant was rapidly increased with 2 and 13% TiO$_2$addition to $Al_2$O$_3$. The internal damping was nearly unchanged with TiO$_2$content The specific elastic constant seemed to be dependent on the content of $\alpha$-Al$_2$O$_3$in the coated layer.

  • PDF

Preparation and Characteristics of Fouling Resistant Nanofiltration Membranes (내오염성 나노여과막의 제조 및 특성)

  • Kim, No-Won
    • Membrane Journal
    • /
    • v.17 no.1
    • /
    • pp.44-53
    • /
    • 2007
  • The primary objective of this study is to increase the extent of water flux and fouling resistance of nano-filtration or reverse osmosis membranes. This study was performed to investigate the effect of surface characteristics of silane coated membranes on modified fouling index. Commercial polyamide composite RO membrane (RE1812-LP) and NF membrane (ESNA4040-LF) were treated with silane coupling agents in ethanol at five different concentrations. The silane coupling reagent, aminopropylmethoxydiethoxysilane, contains one aminoalkyl and three alkoxy groups. The hydrophilic effect of aminoalkyl group of APMDES on the permeability and fouling resistance of the modified membrane was examined. The surfaces of the modified membranes were characterized by FE-SEM, contact angle analyzer, and zeta potentiometer in order to confirm successful sol-gel methods. The modified NF membranes showed significantly enhanced water flux and fouling resistance without a decrease in salt rejection in divalent ionic feed solution.

Effect of the Structure of the Smallest Poresize Layer on the Permeability of PES Microfiltration Membranes (최소 기공층 구조가 PES계 정밀여과막 투과 성능에 미치는 영향)

  • Kim, No-Won
    • Membrane Journal
    • /
    • v.19 no.1
    • /
    • pp.25-33
    • /
    • 2009
  • PES (polyethersulfone) membranes with highly enhanced their asymmetry were prepared by phase inversion process. The membranes were prepared by using PES/DMF (N,N-dimethylformamide)/TSA (p-toluenesulfonic acid)/PVP (polyvinylpyrrolidone) casting solution and water coagulant. The pre-coagulation of membrane surface which was induced by an addition of TSA as a demixing agent and PVP as a swelling polymer in the PES solution and humid exposure time, played a crucial role in determining morphological properties and the PWP (pure water permeation) performance. The PES solution was coated on polyester film under condition of 80% humidity for a while ($72{\sim}144$ sec) before immersing in a coagulation bath. The characterization of membranes was carried out by a capillary flow porometer, a FE-SEM and a permeation test apparatus. As the thickness of the smallest pore size layer (SPL) decreased, the asymmetry of membrane increased under conditions of 20 wt% of TSA and 10 wt% of PVP in 11 wt% of PES solution during longer humid contact time. As a result, the membranes showed a remarkable increase of PWP.

Fabrication of a Film Coated with Conducting Polymer Using One Atmospheric Pressure Plasma (대기압 플라즈마를 이용한 전도성 고분자 코팅 필름 제조)

  • Jung, Jin-Suk;Yang, In-Young;Myung, Sung-Woon;Choi, Ho-Suk;Kim, Jong-Hoon
    • Polymer(Korea)
    • /
    • v.31 no.4
    • /
    • pp.308-314
    • /
    • 2007
  • A composite film of polyurethane(PU)-graft-poly(acrylic acid) (PAAc)/polyaniline (PU-g-AAc/PANI) was successfully fabricated for the purpose of adding conductivity on the surface of a general purpose polymer and improving adhesive property between the general purpose polymer and conducting polymer layer. The results from ATR-FTIR and XPS analyses also supported the successful synthesis of the composite film by showing characteristic peaks for every step. A low surface resistivity of $2{\times}10^3\;ohm/sq$ proved the surface conductivity of synthesized PU-g-AAc/PANI film and the surface resistance decreased with increasing the amount of grafted AAc, which acted as a dopant for PANI film.

Preparation and Properties of Charged Microcapsule (하전 마이크로캡슐 입자의 제조와 성질)

  • Park, Soo-Min;Kim, Ye-Jeong;Kim, Hea-In;Kim, Chul-Am;Suh, Kyung-Soo
    • Proceedings of the Korean Society of Dyers and Finishers Conference
    • /
    • 2011.03a
    • /
    • pp.71-71
    • /
    • 2011
  • 전류를 흘렸을 때 양극과 음극에 따라 움직이는 미세한 나노입자를 이용하여 색, 글자, 그림 등을 표시하는 응용디스플레이 기술이 전기영동디스플레이(electrophoretic display)이다. 최근 전자종이 등 상품화가 진행되면서 전기영동디스플레이에 대한 관심증대와 함께 기술개발이 지속적으로 진행되고 있다. 본 연구에서는 분산중합을 이용하여 $TiO_2$ core 입자에 polystyrene을 shell로 코팅하여 마이크로캡슐형의 전기영동디스플레이에 적합한 입자를 제조하고 성능을 분석하였다. 먼저 분산제의 종류, 모노머의 농도, 개시제의 농도에 따라 제조된 대전복합입자의 크기 및 분포를 보면, 분산제의 종류를 달리 하였을때를 제외하고 대체로 균일하였다. 입경의 변화를 보면, 약 200-300nm의 $TiO_2$가 개질에 의해 400-500nm의 입경을 나타내는 것으로부터 200nm 두께의 shell층을 갖는다는 것을 확인 할 수 있었다. 또한 분산제의 종류에 따라서는 분산제를 사용하지 않는 경우가 오히려 제조된 입자의 분포가 균일함을 알 수 있었고 모노머의 농도에 따른 변화는 볼 수 없었으며 입경분포가 균일한 입자가 제조되었음을 알 수 있었다. 대전복합입자의 TGA 곡선으로부터 $300^{\circ}C$ 부근에서 polystrene shell에 의한 분해를 볼 수 있었고 $600^{\circ}C$ 이후에 잔류된 core의 $TiO_2$ 입자를 확인 할 수 있었다. 이 결과로부터 $TiO_2$ core-polystyrene shell형의 전자 종이용 대전복합입자의 제조를 확인 할 수 있었다. 또한 제조된 대전복합입자의 zeta potential을 보면, (+)전하를 띄며 64.8mV의 비교적 높은 zeta potential을 가지는 것을 확인 할 수 있었다. 그리고 $TiO_2$ 대전복합입자와 같은 방법으로 제조된 흑색 대전복합입자를 혼합하여 cell test를 측정한 결과, cell에 ${\pm}$10V의 저전압을 가했을 때에도 비교적 응답속도가 빠른 입자의 구동현상을 확인 할 수 있었다.

  • PDF

Properties of bulk-hetro junction polymer solar cells with P3HT:PCBM active layer (P3HT:PCBM의 고분자 유기박막태양전지의 특성연구)

  • Jang, Seong-Kyu;Choi, Jae-Young;Kim, Kun-Ho;Gong, Su-Cheol;Chang, Ho-Jung
    • Proceedings of the KAIS Fall Conference
    • /
    • 2010.11a
    • /
    • pp.488-490
    • /
    • 2010
  • 최근 심각한 환경오염 문제와 화석 에너지 고갈로 차세대 청정 에너지 개발에 대한 중요성이 증대되고 있다. 그중에서 태양정지는 공해가 적고, 자원이 무한적이며 반 영구적인 수명을 가지고 있어 미래에너지 문제를 해결할 수 있는 에너지원으로 기대되고 있다. 본 연구에서는 P3HT(regioregular poly(3-hexylthiophene))와 PCBM(fullerene derivative [6,6]-phenyl-C61-butyric acid methyl ester)을 전자 도너와 억셉터 물질을 하나의 브랜드로 광 활성층을 형성하는 BHJ(bulk hetero junction)구조를 갖는 고분자 유기 박막 태양전지를 각각 Toluene, Mono-Chlorobenzene, Dichlorobenzene에 $60^{\circ}C$, 200rpm으로 약 12시간동안 1wt%로 교반(Stirring)한 후에 중량비(1:1 wt%)로 혼합하여 스핀코팅(Spin-coating)으로 제작하였고, 완성된 소자의 광활성층 면적은 0.04cm2이며, $150^{\circ}C$에서 후속 열처리 공정을 통해 특성 향상이 측정 되었다. 태양전지 소자 구조는 Glass / ITO / PEDOT:PSS / P3HT : PCBM / Al이다. 전류-전압, FF(Fill Factor), 변환효율 측정을 위해 solar simulator를 AM1.5 조건(100 mW/cm2)으로 이용하였으며, 소자의 최대 전류밀도는 12mA/$cm^2$, 개방전압은 0.566V이고 F.F(Fill Factor)는 55.2%이고 변환효율은 3.7%이다. 후속 열처리후 더욱 좋은 성능을 갖게 되었고, 최대 효율은 Dichl orobenzene일 때 이다.

  • PDF

A Comparison of The One-side Water repellency in Polyester and Nylon/PU Fabrics by Low Temperature Plasma Treatment (저온 플라즈마를 이용한 Polyester, Nylon/PU 직물의 편면발수성 비교)

  • Ma, Jae-Hyuk;Son, Kung-Tai;Choi, Jin-Young;Koo, Kang
    • Proceedings of the Korean Society of Dyers and Finishers Conference
    • /
    • 2012.03a
    • /
    • pp.60-60
    • /
    • 2012
  • 최근 들어서 소비성향의 고급화 추세와 고기능성 및 쾌적성의 추구는 발수성의 개발로 이어져왔다. Polyester, Nylon 등 다양한 합성섬유소재의 발전으로 발수기능이 상품가치의 중요한 요소로 자리잡고 있다. 더 나아가 표면과 이면이 서로 다른 특성을 가지도록 유도하여 편면기능성을 부여하는 가공을 응용한다면 더욱 더 고부가가치를 기대할 수 있다. 본 연구에서는 불소계로 발수 처리된 Polyester직물 및 Nylon/PU 혼방직물에 저온 플라즈마를 출력 50W, 1, 3, 5, 7 분 처리하여 편발수성을 검토하였다. 불소계 발수제로 코팅처리한 Polyester직물의 경우 5분간 Plasma처리하면 접촉각이 미처리 시료의 $149^{\circ}$에서 처리 후, 앞면 $71.56^{\circ}$, 뒷면 $126.94^{\circ}$,Nylon/PU 혼방직물의 경우에는 $155.3^{\circ}$에서 앞면 $63.24^{\circ}$, 뒷면 $139.26^{\circ}$로 크게 편면 친수화 되었다. 그 결과로 볼 때 플라즈마처리에 의해 편면발수 가공으로 서의 효과를 얻을 수 있었다. SEM 관찰을 통해 Polyester직물 및 Nylon/PU혼방 직물에 플라즈마 처리한 후 처리시간에 따른 펴면의 발수가공 층이 파괴되는 것을 알 수 있었다. 이는 표면에서의 발수효과가 플라즈마처리에 의해 친수화가 진행된 결과와 일치한다.

  • PDF