• Title/Summary/Keyword: 치과용 레진 시멘트

Search Result 49, Processing Time 0.034 seconds

SHEAR BOND STRENGTH OF GIOMER AND SELF-ETCHING PRIMER ON THE DENTIN (Giomer와 자가 산부식 접착제의 상아질에 대한 전단 결합강도)

  • Yoon, Eun-Young;Lee, Nan-Young;Lee, Sang-Ho
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.37 no.4
    • /
    • pp.422-428
    • /
    • 2010
  • Giomer is fluoride-releasing, resin-based dental materials that comprise PRG(pre-reacted glass ionomer) filler. The purpose of this study was to evaluate the shear bond strength of Giomer using self-etching primer systems to bovine dentin. Bovine incisors were mounted in self-curing orthodontic resin and the facial surfaces were wet ground on SIC paper to expose the dentin. Total 100 samples were made and divided randomly into 4 groups, Giomer group(I), Composite resin group(II) and Compomer group(III), Giomer and single bottle adhesive group(IV). The shear bond strengths of 25 samples per each group were measured using universal testing machine. And data were analyzed statistically with One-way ANOVA and Scheffe test. Giomer group(I) showed the significantly higher bond strength than Compomer group(III)(p<0.05). There was no significant difference between Giomer group(I) and Composite resin group(II)(p>0.05). And there is no significant difference between gourp(I) and group(IV). Based on the results of present study, the use of Giomer as an esthetic restorative material for primary teeth might be justified. It is considered that more study about the fluoride releasing ability is needed to evaluate the anticariogenic effect of giomer.

The effect of cleaning methods on bond strength of zirconia after saliva contamination (타액으로 오염된 지르코니아 수복물의 접착강도에 세척 방법들이 미치는 영향)

  • Shim, Young-Bo;Choi, An-Na;Son, Sung-Ae;Jung, Kyoung-Hwa;Kwon, Yong Hoon;Park, Jeong-Kil
    • Korean Journal of Dental Materials
    • /
    • v.44 no.1
    • /
    • pp.61-68
    • /
    • 2017
  • This study evaluated the effects of various cleaning methods on the shear bond strength of zirconia ceramics after saliva contamination. Eighty zirconia disk specimens were divided into 8 groups. All groups were treated with one coat of MDP primer. All specimens (except the negative control) were contaminated with human saliva on the zirconia surface. The positive control went through the bonding procedure immediately after contamination without any cleaning procedure. With the exception of control groups, the remaining six groups were rinsed with water and either applied with MDP recoating (WATER+MDP) or without MDP recoating (WATER). While some were cleaned with a Ivoclean with MDP recoating (IVOCLEAN+MDP) or not applied with MDP recoating(IVOCLEAN), others were cleaned with a 1% NaOCl solution with MDP recoating (NaOCl+MDP) or without MDP recoating (NaOCl). The shear bond strength of all specimens were measured after being stored in distilled water at $37^{\circ}C$ for 24 hours. The data was analyzed statistically by an analysis of ANOVA, Tukey's post hoc test and Student's t-test was used to compare the shear bond strength according to the re-coating of MDP after the cleaning procedure. The positive control group showed the lowest shear bond strength value, and the WATER group and NaOCl group showed no significant difference when compared to the positive control group. The IVOCLEAN group showed significantly higher shear bond strength when compared to Water group and NaOCl group but not with the group of negative control. After rinsing with water or the NaOCl solution, the comparison of the single coating of MDP and re-coating of MDP showed different shear bond strengths but there was no significant difference to the negative control. After rinsing with Ivoclean, there was no significant difference to the negative control regardless of the recoating of MDP. In conclusion, the shear bond strength was affected by the cleansing procedure and Ivoclean was found to be effective regardless of the re-coating of MDP. When water or the NaOCl solution is used to remove surface contaminants, the re-coating of MDP provides a positive effect on cementation.

Retentive bond strength of fiber-reinforced composite posts cemented with different surface treatments (Fiber reinforced composite post의 표면 처리에 따른 접착 강도)

  • Roh, Hyunsik;Noh, Kwantae;Woo, Yi-Hyung;Pae, Ahran
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.52 no.2
    • /
    • pp.113-120
    • /
    • 2014
  • This study will evaluate the effectiveness of various pretreatments when fiber-reinforced composite (FRC) post is bonded to endodontically treated tooth with resin cement. Materials and methods: Canal shaping of FRC post (DT Light post, Size 3, Bisco Inc., Schaumburg, IL, USA) was performed on endodontically treated premolars at 1.5 cm from CEJ. Samples were divided into 6 groups of surface treatment after conventional washing and drying to the canal. Total of 24 FRC posts were randomly divided into 6 groups of surface treatment as follows: Group C: control - no surface treatment, Group A: airborne-particle abrasion (Cojet sand, 3M ESPE), Group S: silanization (Bis-silane, Bisco Inc.), Group M: universal primer (Monobond-plus primer, Ivoclar Vivadent Inc.), Group AS: silanization after airborne-particle abrasion, Group AM: universal primer treatment after airborne-particle abrasion. Pretreated fiber posts were cemented with resin-based luting material and photo-polymerized and cut to the thickness of 1 mm. Push-out test using a universal testing machine was performed. Bonding failure strength of post dislodgement was measured and the type of bonding failure was classified. Data were analyzed with Kruskal-Wallis test and multiple comparison groups were performed using Tukey HSD value of rank test (${\alpha}=0.05$). Results: Group AS showed significantly highest bonding strength. Group S, group AM, group A, and group M showed lower bonding strength in order. The control group showed the lowest bonding strength. Conclusion: Surface treatment with silane showed to be the most effective of the surface pretreatment methods for cementation of FRC post. Surface treatment with universal primer showed no significant difference compared with no surface treatment group as for bonding strength.

A STUDY ON THE BOND STRENGTHS BETWEEN GLASS IONOMER CEMENT BASES AND COMPOSITE RESINS (글래스 아이오노머 이장재와 복합레진간의 결합강도에 관한 연구)

  • Kim, Min-Hee;Kim, Shin;Jeong, Tae-Sung
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.26 no.3
    • /
    • pp.520-527
    • /
    • 1999
  • For the purpose of providing some suggestions in selection of filling materials used in 'sandwich technique', the bond strengths between glass ionomer cement bases and composite resins were investigated and compared. For lining materials, 'Vitrebond' and 'Ketac-fil' were used. Using these two as bases, 10 of each following resins were built up on the top ; Z-100 (light curing resin) Clear-fil (chemical curing resin), Bis-core (dual cure resin), Dyract (compomer), therfore 10 specimens of each group and total of 80 specimens were made. After storing specimens in $37^{\circ}C$ deionized water for 24 hours, the shear bond strengths were measured under universal testing machine with 50 kg of full load scale and 1mm/min of cross-head speed and obtained the results as follows : 1. Over Vitrebond base, Z-100 showed the lowest bond strength but the other three did not show any difference in bond strength. 2. Over Ketac-fil base, Clear-fil showed the highest bond strength followed by Dyract, Bis-core, and Z-100 showed the lowest bond strengths. 3. Whereas Clear-fil showed the similar bond strengths on the Vitrebond base as other resins, it showed the highest bond strength on Ketac-fil base, which showed some difference in bond strength by differing GIC bases. 4. The bond strengths between base materials and composite resin showed a stronger resin-dependence tendency in cases with Ketac-fil bases rather than with Vitrebond bases.

  • PDF

A STUDY ON THE COLOR STABILITY OF RESIN CEMENTS LUTED FOR PORCELAIN LAMINATE VENEER (도재라미네이트 접착용 레진시멘트의 색조 안정성에 관한 연구)

  • Kim, Young-Woon;Park, Ha-Ok;Vang, Mong-Sook;Yang, Hong-So;Park, Sang-Won
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.2
    • /
    • pp.191-202
    • /
    • 2007
  • Statement of problems: Long-term success of esthetic restorations, depends on various factors, especially on color stability of the restorations. The color stability is affected by resin cements beneath the porcelain laminate veneers. Purpose: The purpose of this study was to comprehend the color stability of resin cements by comparing with 4 different kinds of resin cements (Choice, Variolink II, Nexus 2, Rely-X). Material and methods: Porcelain laminate disk samples were luted with resin cements. After thermocycling of each 1000, 2000 and 3000 cycle, specimens were measured by spectrophotometers and the color differences were. Results: 1. After thermocycling of 1000, 2000 and 3000cycle, color difference, $({\Delta}E^*)$ of all specimens were incresed, but were not statiscally significant differences. 2. In the Choice of A1 shade and the Nexus 2 of A3 shade, color difference$({\Delta}E^*)$ after thermocycling of 3000cycle was $incre^*ased$ significantly than after thermocycling of 1000cycle. However, other groups did not show any statistically significant differences (P<0.05). 3. After thermocycling of 3000cycle, color difference$({\Delta}E^*)$ between A1 shade and A3 shade of Nexus 2 showed statistically significant difference. However no statistically significant differences were observed in other groups (P<0.05). 4. The mean of color difference$({\Delta}E^*)$ is 1.0-2.06 after 3000 thermocycling and the data were ranked in the ascending order of Variolink II, Nexus 2, Choice and Rely-X in A1 shade group and Choice, Rely-X, Variolink II and Nexus 2 in A3 shade group. Conclusion: Above results revealed that, after 3000 thermocycing, the color difference $({\Delta}E^*)$ of experimental resin cements was within clinically acceptable ranges. Color stability of 4 different resin cements was comparatively excellent.

REMINERALIZATION EFFECTS OF GLASS IONOMER RESTORATIONS ON ADJACENT INTERPOXIMAL-A MICROTOMOGRAPHIC STUDY (미세전산화 단층 촬영을 이용한 글라스 아이오노머 수복의 인접면 재광화 효과에 대한 연구)

  • Lee, Hyeok-Sang;Lee, Sang-Dae;Kim, Jung-Wook;Kim, Chong-Chul;Hahn, Se-Hyun;Jang, Ki-Taeg
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.31 no.3
    • /
    • pp.474-480
    • /
    • 2004
  • The purpose of this in vitro study was to compare the remineralizing effects of three glass ionomer cements (high filled glass ionomer cement, compomer, resin modified glass ionomer cement) with resin composite (control group) on incipient interproximal caries, and to assess long-term change of remineralization effect, in each material, evaluated by microtomography. Proximal restoration was simulated with tooth specimen and Glass Ionomer Cements. And each of these groups was placed into a closed container with artificial saliva at $37^{\circ}C$ and pH 7.0 for a time period of thirty days with constant circulation. At the end of thirty and sixty days, tomographic images were taken from these specimens with micro CT scanner. Materials used in this study were as follows. Group 1: Fuji IX GP (GC Corp., Tokyo, Japan) Group 2: Vitremer (3M ESPE, St. Paul, Minn., USA) Group 3: F2000 (3M ESPE, St. Paul, Minn., USA) Group 4: Z250 (3M ESPE, St. Paul, Minn., USA) Using density-measuring program, the micro-density of carious lesions on the specimens were measured. The mean density changes of each group were compared to the other groups to evaluate the effect of remineralization. The results were as follows: 1. The lesion density of all groups increased. 2. The mean density increase of Group 1, 2, 3 were higher than that of Group 4 every month(p<0.05). 3. There were significant differences of density increase among glass ionomer group(Group 1, 2, 3).

  • PDF

IMMOBILIZATION OF LOWER MANDIBULAR ALVEOLAR BONE FRACTURE USING RESIN-WIRE OPEN CAP SPLINT (하악 유전치부 치조골 골절시 resin-wire open cap splint를 이용한 고정)

  • Kwon, Joung-Hyun;Choi, Byung-Jai;Choi, Hyung-Jun;Kim, Seong-Oh;Son, Heung-Kyu;Lee, Jae-Ho
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.35 no.1
    • /
    • pp.175-180
    • /
    • 2008
  • Traumatic injuries to the primary dentition are commonly encountered problems in dental practice. It is found that 30% of the children had injuries to the primary dentition and 22% to the permanent dentition. The greatest incidence of trauma to the primary dentition occurs at the ages of 2 and 3 as children start to learn motor coordination. Because teeth and alveolar bone are traumatized simultaneously, alveolar bone fractures are likely to occur when multiple teeth are involved in injuries. Dental splints are indicated for the management of maxillofacial fractures. They enable anatomic reduction of fractured segments and help immobilization and maintenance of the fragments after reduction. They also act as a stabilizer during rehabilitation. Various types of dental splints are available. In this case, routine resin-wire splint technique could not be applied because of the child's uncooperative behavior. Oral sedation was not indicated because N.P.O. had not been preceded. Therefore, we decided to use open-cap acrylic splint instead. Stabilization using open cap acrylic splint requires minimum chair time with reduced discomfort to both patient and dentist. It is an effective means of splint for uncooperative children and especially useful when other means of fixation have been failed. Because trauma on the primary dentition can affect the underlying permanent tooth germ, it is important to monitor eruption process of the permanent dentition.

  • PDF

A Study on the Experience of Clinical Practice and the Performance Confidence (치위생과 학생의 임상실습 경험정도와 수행자신감에 관한 연구)

  • Lee, Yeong-Ae;Kim, Young-Sun
    • Journal of dental hygiene science
    • /
    • v.8 no.4
    • /
    • pp.353-359
    • /
    • 2008
  • To find out the relationship between the experience of clinical practice and the performance confidence, some 2nd and 3rd grade students in D health college who completed clinical practice in 2008. Sept. were surveyed. The results are as follows. 1. During the clinical practice of the dental hygiene students, the performance experience was highest in the basic prep. part among every part. As for the dental hygiene part, the students showed more than 70%, rather higher performance experience in the following parts: arrangement before and after treatment, suction, basic instruments setup, local anesthesia setup, extraction setup, resin filling setup, temporary filling setup, cements mixing, and ligation and removal setup. 2. As for performance confidence, those with performance experience showed higher performance confidence than those with only observation experience or with no experience in every treatment field except basic prep. (p < 0.001). 3. It was proven that the hygiene students have seldom had performance experience in other treatment parts except in assisting treatment part in clinical practice. In order to improve future performance experience on dental hygiene activities, subsequent research is needed to set more specific and objective criterion about the dental hygiene students' clinical practice.

  • PDF

A comparison of the fidelity of various zirconia-based all-ceramic crowns fabricated with CAD/CAM systems (수종의 CAD/CAM 시스템으로 제작한 지르코니아 기반 완전도재관의 적합도 비교)

  • Kim, Sung-Jun;Jo, Kwang-Hun;Lee, Kyu-Bok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.2
    • /
    • pp.148-155
    • /
    • 2009
  • Statement of problem: The interest in all-ceramic restorations has increased as more techniques have become available. With the introduction of machinable dental ceramics and CAD/CAM systems there is a need to evaluate the quality levels of these new fabrication techniques. Purpose: This study is to evaluate the crown fidelity(absolute marginal discrepancy and internal gap) of various zirconia-based all-ceramic crowns fabricated with different CAD/CAM(computer-assisted design/computer-assisted manufacturing) systems and conventional cast metal-ceramic crowns. Material and methods: A resin tooth of lower right second premolar was prepared. After an impression was taken, one metal master die was made. Then 40 impressions of metal master dies were taken for working dies. 10 crowns per each system were fabricated using 40 working dies. Metal-ceramic crowns were cast by using the conventional method, and Procera, Lava, and Cerec inLab crowns were fabricated with their own CAD/CAM manufactruing procedures. The vertical marginal discrepancies and internal gaps of each crown groups were measured on a metal master die without a luting agent. The results were statistically analyzed using the one-way ANOVA and Tukey's HSD test. Results: 1. Vertical marginal discrepancies were $50.6{\pm}13.9{\mu}m$ for metal-ceramic crowns, $62.3{\pm}15.7{\mu}m$ for Procera crowns, $45.3{\pm}7.9{\mu}m$ for Lava crowns, and $71.2{\pm}2.0{\mu}m$ for Cerec inLab crowns. 2. The Internal gaps were $52.6{\pm}10.1{\mu}m$ for metal-ceramic crowns, $161.7{\pm}18.5{\mu}m$ for Procera crowns, $63.0{\pm}10.2{\mu}m$ for Lava crowns, and $73.7{\pm}10.7{\mu}m$ for Cerec inLab crowns. Conclusion: 1. The vertical marginal discrepancies of, 4 crown groups were all within the clinically acceptable range($120{\mu}m$). 2. The internal gaps of LAVA, Cerec inlab, and metal-ceramic crowns were within clinically acceptable range except Procera crown($140{\mu}m$).