• Title/Summary/Keyword: 조강형 혼화제

Search Result 10, Processing Time 0.025 seconds

A Study on Properties of Concrete Correponding to Various High Early Strength Agents (조강형 혼화제 종류에 따른 콘크리트의 특성에 관한 연구)

  • Yoo, Seung-Yeup;Lee, Sang-Rae;Koo, Ja-Sul;Kang, Suck-Hwa
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2010.05a
    • /
    • pp.313-314
    • /
    • 2010
  • This study investigates properties of concrete corresponding to various high early strength agents. It was presented as reference data for reducing construction cost and improving quality of cold weather concrete through reduction of construction time.

  • PDF

An Experimental Study on Reduction of Working Period of Concrete using High Early Strength Binder (조강형 결합재를 사용한 콘크리트의 공기단축에 관한 실험적 연구)

  • Kim, Dong-Jin;Kim, Min-Jeong;Lee, Sang-Ho
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.11a
    • /
    • pp.513-516
    • /
    • 2008
  • Recently, a demand for reduction of construction cost by reducing construction period is increasing because of the slump of the construction business, the increasing price of raw-materials and the enforcement of after-sale system. As a method of reducing construction period, many construction companies usually apply a method of reducing curing period. But if they use an existing early strength cement or admixture, they spend a heavy cost on materials and there are many problems, such as a heat of hydration and a loss of workability. The purpose of this research is a reduction of construction cost by reducing construction period as a earlier removal time of form. To check up application of concrete using high early strength binder and admixture, comparative tests were carried out with concrete using an existing early strength cement or admixture such as tests of diurnal variation, setting time and compressive strength.

  • PDF

Effect of Cement Contents and Combinations of Accelerators on Strength Development of Concrete Cured at 10℃ (10℃ 양생조건에서 단위 시멘트량 변화 및 경화촉진제의 복합사용에 따른 강도발현 성능에 관한 연구)

  • Song, Young-Chan;Lee, Tea-Gyu;Kim, Yong-Ro;Seo, Chi-Ho
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.2
    • /
    • pp.94-99
    • /
    • 2018
  • The purpose of this study is to investigate the effect of combinations of different accelerators mixed on the early age strength development of concrete of 21 to 27MPa in the curing temperature of $10^{\circ}C$ compared with existing early strength agent. The present study was assessed the early strength development of combinations of three different accelerating admixtures with early strength type agent comparing to single accelerating admixture with early strength type agent. As a result of this study, the effect of $CaBr_2+NaSCN+DEA$ combination on strength development showed better than $CaBr_2$ or NaSCN alone with early strength type agent. Therefore, we observed that concrete using $CaBr_2+NaSCN+DEA$ combination with early strength agent was achieved 5MPa 12hours earlier than use of $CaBr_2$ or NaSCN alone.

A Study for Application of Polycarboxilic Type Admixture to Precast High-Strength Concrete Piles (프리캐스트 고강도 콘크리트(PHC) 파일에 조강형 폴리카본산(PC)계 혼화제의 적용에 관한 연구)

  • Yi, Seong Tae;Noh, Jae Ho;Park, Chul Ju;Heo, Hyung Seok
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.15 no.1
    • /
    • pp.263-270
    • /
    • 2011
  • In this study, the performance of Poly-Naphthalene Sulfonate (PNS) type-admixture used widely in South Korea and Polycarboxilic type-admixture(i.e., WF2000) developed in the J company of the domestic, for precast concrete products produced in the factories, was evaluated. With the 20% reduced usage of WF2000 compared to PNS type-admixture, workability was considerably improved due to high water-reducing ratio, accelerating effect of concrete setting and accelerant dispersant action, which the product has, under the high temperature. In addition, the development of initial and long-term strengths of PHC plies was predominant. For WF2000, it is also possible to correspond with the change of original materials and environmental conditions since the control of water-reducing and supporting forces is feasible. Accordingly, it was noted that WF2000 is superior for deterioration of production & workability and bad casting problems in summer and the solution of initial strength reduction problem due to the delay of setting in winter.

Compressive Strength Development Properties of Concrete using Sodium based Accelerating Admixtures (나트륨계 기반 조강형 혼화제를 사용한 콘크리트의 압축강도발현 특성)

  • Song, Yeong-Chan;Lee, Tae-Gyu;Kim, Yong-Ro;Seo, Chi-Ho
    • Journal of the Korea Institute of Building Construction
    • /
    • v.18 no.3
    • /
    • pp.259-266
    • /
    • 2018
  • In recent years, the early strength of concrete is important in order to shorten the time of form removal at the construction site. The purpose of this study is to analyze the moment of form removal as investigating the amount of cement contents and the physical properties and strength of the concrete according to types of admixture in the curing temperature of $10^{\circ}C$ for concrete of 21 to 27 MPa. As a result, it was found that compressive strength of concrete could not be secured 5 MPa by 36 hours even if the amount of cement contents were increased to $360kg/m^3$ with plain admixture. Also, it was confirmed that the strength improvement rate was excellent when using the accelerating agent with polycarboxylic acid type, and the moment of compressive strength of 5 MPa was estimated at 30 hours.

Experimental Study of Freezing Characteristics and Antifreezing Method of Liquid Additive for Early Strength (액상형 조강제의 동결특성 및 동결방지 방안에 관한 실험적 고찰)

  • Lee, Mun-Hwan;Ryu, Deug-Hyun
    • Journal of the Korea Concrete Institute
    • /
    • v.19 no.5
    • /
    • pp.647-653
    • /
    • 2007
  • In ready mixed concrete factory, in case of using the high molecular additive in winter especially the liquid additive for the early strength, it is required to check the stability. In this research, the freezing and gelling characteristics of the liquid additive for the early strength is reviewed, the material and mechanical solution are proposed to that the practical quality control method will be suggested. As the result, the Freezing temperature of the liquid additive for the early strength is $-11.8^{\circ}C$, and it is the lower than the temperature at which the strength is shown. By making with sodium silicate of $37{\pm}0.5%$ designed by $SiO_2\;and\;Na_2O$ in 0.31 of mol ratio, it minimizes the gelling at the lower temperature. On the other hand, facilities for storing and supplying the material should be set at $40^{\circ}C$ so the temperature distribution is well spreaded for practical operation.

Quality Improvement of High Volume Fly Ash Concrete due to Early Strength Gain Admixture (조강형 혼화제에 의한 플라이애시 다량 치환 콘크리트의 품질 향상)

  • Han, Cheon-Goo;Park, Jong-Ho;Lee, Joung-Ah
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.4
    • /
    • pp.117-124
    • /
    • 2009
  • The purpose of the study was to improve quality of high volume fly ash concrete. The study evaluated on the possibility of early quality improvement of high volume fly ash concrete with early strength gain admixture ('GA' below) developed by the preceding research. The study regarded applying naphthalene admixture ('NA' below) to mix proportion substituting FA 15 % to be plain. In the event of substituting FA 20, 25 and 30 %, the study compared engineering properties of concrete with plain by applying GA. Because of features of fresh concrete, fluidity falls down when GA is applied. Therefore, its use amount shall be increased. Only, in W/B 60 %, it was beneficial since slump loss was reduced about 35~70 mm than plain. The study could see that AE use should be increased proportionally since air content was reduced by coming from AE absorption operation of unburned coal content included in FA according to an increase in the amount of FA use. Reduction effect of bleeding could be anticipated since the amount of bleeding appeared at least in FA 20 %. Because of hardened concrete, time of setting appeared in the same level as plain when GA was applied. Therefore, it is judged that delay of setting can be reduced. In compressive strength, the study could check the same strength development as plain when GA was applied, having nothing to do with W/B and curing temperature. However, it is thought that we shall pay attention to GA use in the event of FA 30 % substitution. Freezing and melting resistance had less early value than plain. However, it is judged that there will be no problem of frost resistance since there is no a large difference between freezing and melting resistance and plain in overall. In accelerated neutralization, it was analyzed that a problem of weakening in neutralization appointed as a demerit when FA was applied in mass in proportion with GA use could be settled to some extent.

  • PDF

Compressive Strength and Fluidity of Low Temperature Curable Mortar Using High Early Strength Cement According to Types of Anti-freezer, Accelerator for Freeze Protection and Water Reducing Agent (조강형시멘트를 사용한 저온경화형 모르타르의 압축강도 및 유동특성에 미치는 방동제, 내한촉진제 및 감수제의 영향)

  • Park, Jung-Hoon;Ki, Kyoung-Kuk;Lee, Han-Seung;Kim, Hyeong-Cheol;Choi, Hyun-Kuk;Min, Tae-Beom
    • Journal of the Korea Institute of Building Construction
    • /
    • v.16 no.5
    • /
    • pp.405-412
    • /
    • 2016
  • In order to examine the possibility of practical use of concrete at low-temperature environment using high early strength cement with cold resistance admixture, an experimental study on workability, freezing temperature and compressive strength of the mortar with different types of anti-freezer, water reducing agent and accelerator for freeze protection at low-temperature were evaluated. Compressive strength was increased in use of anti-freezer, especially SN anti-freezer was higher than CN anti-freezer. 0min flow was increased, the 20min flow was decreased. And 20min flow was improved in use of FR, RT water reducing agent. CF, LS accelerator for freeze protection, regardless of the type of water reducing agent, compressive strength was increased.

Evalution of Practial Application of high early Strength Concrete using Early strength type material (조강형 재료를 사용한 초조강 콘크리트의 적용성 평가)

  • Yang, Hoon;Park, Kyu-Yeon;Lee, Sang-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2013.11a
    • /
    • pp.48-49
    • /
    • 2013
  • This test investigates early strength and durability of concrete using early strength type materials(cement, Polycarboxylate acid). The goal of this test is to secure the strength of 5.0 MPa in 12 hours early age and strength of 14 MPa for 24 hours correspondingly. This type of admixtures, concrete curing temperature, amount of binder and other concrete properties were confirmed by experimental factors. Comparing outcomes from two cases on using early strength type materials and common materials resulted in reducing of costs and shortening of the construction period, that determined the economical benefits of using early strength materials in construction.

  • PDF

Mix Proportions of Early-Strength Pavement Concrete Using Calcium Nitrate (질산칼슘 혼화재를 사용한 신속개방형 포장 콘크리트의 적정배합비 도출)

  • Won, Jong Pil;Lee, Si Won;Lee, Sang Woo;Park, Hae Geun
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.29 no.1A
    • /
    • pp.95-100
    • /
    • 2009
  • This study proposed mix proportions of early strength pavement concrete for large size area using calcium nitrate. Therefore, we used type III cement with calcium nitrate. Laboratory tests conducted to air content, slump loss test, setting time test, compressive strength test and flexural strength test. Our early strength pavement concrete mixture proportion proposed in this study for large size area attained the required compressive strength of 21 MPa and a flexural strength of 3.8 MPa, which allowed it to be opened to traffic within 8 hours. Based on test results, we suggested optimum mix proportions of early strength pavement concrete for large size area using calcium nitrate.