Evaluation of Shear Performance of Reinforced Concrete Beams for Varying Reinforcement Details of Web Opening (유공부 보강상세에 따른 철근콘크리트 유공 보의 전단 성능 평가)

  • Kim, Min-Jun;Lee, Bum-Sik;Kim, Dong-Whan;Kim, Hyeong-Gook;Lee, Yong-Jun;Kim, Kil-Hee
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.22 no.4
    • /
    • pp.19-26
    • /
    • 2018
  • This study evaluates the shear performance of reinforced concrete members with web opening reinforcement. A total of 4 reinforced concrete members with or without openings were cast then tested. The main variables investigated were with or without of web openings and with or without of web opening reinforcement, respectively. The proposed web opening reinforcement was a rectangle and rhombus-shaped spiral considering of construct ability. Test result showed that the proposed web reinforcement had improved shear capacity and ductility of the specimens. It was found that the web opening reinforcement proposed in this study had a positive effect on the shear strength and crack control of RC beams with web openings. In addition, it was confirmed that the analytical results by the current design codes underestimates the test results of the specimens with the proposed web opening reinforcement.

Concrete Shear Strength of FRP Reinforced Concrete Beam (FRP 보강근을 사용한 콘크리트 보의 콘크리트 전단강도)

  • Cho, Jae Min;Jang, Hee Suk;Kim, Myung Sik;Kim, Chung Ho
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.29 no.3A
    • /
    • pp.259-266
    • /
    • 2009
  • This study is to develop equations that consider the elastic modulus ratio of FRP bar and steel reinforcement, shear span to depth ratio, and flexural reinforcement ratio of FRP bar, to determine concrete shear strength of FRP reinforced concrete beams without shear reinforcement. As experimental parameters, 2 types of FRP bar, 3 types of shear span to depth ratio, and 3 types of flexural reinforcement were used. Experimental results for two of shear span to depth ratio were quoted from previous study to evaluate effect of shear span to depth ratio in more detail. Shear strength correction factors needed for evaluating concrete shear strength were proposed from regression analysis using above experimental results. Equations suggested from this study and other codes were examined and compared with 31 experimental results available in the literature. From this comparison, it could be known that the equation suggested from this study gives the most approaching result to experimental results.

Improvement and Evaluation of Structural Performance of Reinforced Concrete Beam using High Ductile Fiber-Reinforced Mortar with Ground Granulated Blast Furnace Slag (고로슬래그미분말을 혼입한 고인성섬유 복합모르타르를 이용한 철근콘크리트 보의 구조성능 평가 및 개선)

  • Ha, Gee-Joo;Lee, Dong-Ryul
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.14 no.6
    • /
    • pp.142-152
    • /
    • 2010
  • In this study, eleven reinforced concrete beams, without stirrup, using high ductile fiber-reinforced mortar with ground granulated blast furnace slag(SHF Series, SHFSC Series) and standard specimens without or with stirrup(SSS, BSS) were constructed and tested under monotonic loading. Experimental programs were carried out to improve and evaluate the shear performance of such test specimens, such as the load-displacement, the failure mode, the maximum strength, and shear strength. All the specimens were modeled in scale-down size. Test results showed that test specimens(SHF Series, SHFSC Series) was increased respectively the shear strength carrying capacity by 26%, 20% and the ductility capacity by 5.27, 5.75 times in comparison with the standard specimen without stirrup(SSS). And the specimens(SHF Series, SHFSC Series) showed enough ductile behavior and stable flexural failure.

Experimental Study for Shear Strength of Fiber-Reinforced-Polymer Reinforced Concrete Beams (GFRP 보강근 콘크리트 보의 전단성능에 대한 실험적 고찰)

  • Park, Jong-Sup;Park, Young-Hwan;You, Young-Jun
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.11a
    • /
    • pp.57-60
    • /
    • 2008
  • Compared with a steel-reinforced section with equal areas of longitudinal reinforcement, a cross section using FRP flexural reinforcement after cracking has a smaller depth to the neutral axis because of the lower axial stiffness. The compression region of the cross section is reduced, and the crack widths are wider. As a result, the shear resistance provided by both aggregate interlock and compressed concrete is smaller. Research on the shear capacity of flexural members without shear reinforcement has indicated that the concrete shear strength is influenced by the stiffness of the flexural reinforcement. In this research, experimental observations were made for the shear strength of FRP reinforced concrete beam and validity of existing predicting equations were examined. Test results showed that shear strength decreased as shear-span increased.

  • PDF

Behaviour of Lightweight Concrete Slab Reinforced with GFRP Bars under Concentrated Load (집중하중을 받는 GFRP 보강근 경량콘크리트 슬래브의 거동)

  • Son, Byung-Lak;Kim, Chung-Ho;Jang, Heui-Suk
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.4
    • /
    • pp.57-66
    • /
    • 2015
  • This paper is a preliminary study to apply the lightweight concrete slabs reinforced with GFRP (glass fiber reinforced polymer) bars to the bridge deck slabs or some other concrete structures. So, some different behaviors between the conventional steel reinforced concrete slab and the lightweight concrete slab reinforced with GFRP bars were investigated. For this purpose, a number of slabs were constructed and then the three point bending test and numerical analysis for these slabs were performed. The flexural test results showed that the lightweight concrete slabs reinforced with GFRP bars were failed by the shear failure due to the over-reinforced design. The weight and failure load of the GFRP bar reinforced lightweight concrete slabs were 72% and 58% of the steel reinforced concrete slab with the same dimensions, respectively. Results of the numerical analysis for these slabs using a commercial program, midas FEA, showed that the load-deflection curve could be simulated well until the shear failure of the slabs, but the applied loads and the deflections continuously increased even beyond the shear failure loads.

Effects of Shear Reinforcements on the Reinforced High-Strength Lightweight Concrete Beams (고강도 경량 철근콘크리트보의 전단보강 효과)

  • Shin, Sung-Woo;Lee, Kwang-Soo;Ahn, Jong-Mun;Choi, Myung-Shin
    • Magazine of the Korea Concrete Institute
    • /
    • v.11 no.1
    • /
    • pp.89-97
    • /
    • 1999
  • In this study, fifteen reinforced high-strength lightweight concrete(HLC)beams were tested to investigate shear behavior of specimens according to shear reinforcement ratio. Test variables are shear span to effective depth ratio(a/d=2.5, 3.5, 4.5) and shear reinforcement ratio(0~1.0${\rho}_{v,ACI}$). Concrete compressive strength and tensile steel reinforcement ratio are constantly 439kg/$cm^2$ and 0.0203, respectively. Test results for the HLC beams showed that ACI code equation underestimates the shear strength of concrete($V_c$), and overestimates the shear strength of shear reinforcements($V_s$). It is revealed that the effectivenesses of shear reinforcements of reinforced HLC beams are lower than those of normal weight concrete beams. Then, the shear strengths of shear reinforcements are increased in proportion not to first degree of shear reinforcement ration but to square root of them.

A Study on the Basic Development Length of GFRP Rebar With Ribs (이형 GFRP 보강근의 기본정착길이에 대한 연구)

  • Moon, Do Young
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.30 no.5A
    • /
    • pp.485-493
    • /
    • 2010
  • GFRP rebar with ribs resemble those of deformed steel rebar was developed in 2005. It was reported that ribs of the GFRP rebar were sheared off due to the lower shear strength of polymer. In this study, the basic development length of the GFRP rebar was investigated through pull-out tests, models specified in ACI440.1R-03 and -06, and empirical model derived by Cosenza et al. (2002). As a results of pull-out tests, the critical embeddment length, which is defined as the length when failure mode is changed from pull-out to bar fracture, was 20 times of bar diameter for GFRP rebar and was 15 times for steel rebar. It is believed that the basic development of the GFRP rebar is 21 times of bar diameter, which is determined from the application of average bond strength into the model equation specified in ACI440.1R-03. Compared to the model equation in ACI440.1R-06, that in ACI440.1R-03 is recommendable for design purpose. The Cosenza et al.'s model underestimates the basic development length of the GFRP rebar.

Evaluation of Structural Performance of Flat Plate-Column Interior Connections with Folded Bend Shear Reinforcement (밴드형 전단보강근으로 보강된 무량판 슬래브 내부접합부의 구조 거동 평가)

  • Lee, Bum-Sik;Park, Seong-Sik;Park, Ji-Young;Bang, Jong-Dae;Jun, Myoung-Hoon;Cho, Gun-Hee
    • Land and Housing Review
    • /
    • v.4 no.4
    • /
    • pp.371-382
    • /
    • 2013
  • This study performs an experimental investigation to evaluate the behavior of RC flat plate interior joints specimens. Three 60 percent scale Flat Plate interior specimens assemblies representing a portion of a Flat Plate Apartment Structural System subjected to simulated seismic loading (unbalanced moments) under constant axial load were tested, including one specimens with ordinary shear reinforcement and two specimens with folded bend type shear reinforcement. Test results are shown that (1) the design code KBC 2009 is accurate estimate the behavior of specimens. (2) Two types shear reinforcement have a similar structural behavior, but construction work of rebar with folded bend type shear reinforcement is easier than that of ordinary shear reinforcement. (3) In moderate seismic region, RC Flat Plate interior joint with folded bend type shear reinforcement is apply to structural design of Flat Plate.

The Combined Effect of Concrete Environment and High Temperature on Interlaminar Shear Strength of FRP Reinforcement (콘크리트 환경과 고온의 복합환경이 FRP 보강근의 계면전단성능에 미치는 영향)

  • Moon, Do-Young;Oh, Hong-Seob
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.6
    • /
    • pp.749-756
    • /
    • 2011
  • Most experimental studies on durability of FRP reinforcements subjected to high temperature have focused on the effect of high temperature only on tensile properties. But FRP reinforcement used in newly constructed concrete structure is first degraded by moisture and alkaline environment of concrete. When the structure is subjected to fire, the degraded FRP reinforcement is exposed to high temperature. Therefore, the effects of concrete environment and high temperature should be simultaneously considered for evaluation of FRP reinforcement damaged by fire. In this study, FRP reinforcements submerged in simulated solutions of pH 12.3 and 7 for extended period of time were subjected to temperatures of $60^{\circ}C$, $100^{\circ}C$, $150^{\circ}C$, and $300^{\circ}C$ to be examined. In order to investigate the effect of the high temperature, interlaminar shear strengths were measured and compared to those of control ones. The experimental results demonstrated that the combined effect of concrete environment and high temperature on properties of FRP reinforcement was more significant than the effect of high temperature or concrete environment solely.

Evaluation on the Horizontal Shear Strength of Precast Concrete Slab with the Inverted-Rib-Plus (리브플러스 PC슬래브의 수평전단강도 평가)

  • Park, Keum Sung;Lee, Sang Sup;Choi, Yun Cheul
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.15 no.6
    • /
    • pp.156-165
    • /
    • 2011
  • This study investigates the horizontal shear behavior of an interface between precast concrete (PC) and topping concrete(RC), and evaluates the horizontal based on the investigations by the experimental. Horizontal shear strength in connected surface is determined by the roughness an interface and the shear reinforcement or not. In this study, the main experimental parameters are the shear reinforcement types in the shape of loop-type and lattice-type, rebar spacing. A total of four specimens were shear strength tested and manufactured. As a result, the horizontal shear strength of reinforced connected surface was found to be controlled by deformation in vertical direction. Comparison of reinforcement shape, the mean initial crack load loop type specimens, the average maximum load and the junction of the average in terms of initial stiffness, respectively 33.7%, 45.9% and 55.2% were large enough. Evaluation results for shear strength equation of existing standard domestic, the loop-type reinforced 2.32 to 4.23 times, lattice-type reinforced 1.65 to 3.06 times appears to be higher. Behavior of interface or strength of structural design criteria was fairly safe side. It does not have any problems in the applied field is considered.