  • This study is aimed to obtain the critical crack lengthes of the concrete gravity dam and to investigate variation of the effective stress intensity factors at the crack tips of multiple cracks. Applied loads are dynamic load composed of blast vibration and hydrodynamic pressure which can be considered in case of the blast work at near construction site, in addition to static load composed of hydrostatic pressure, crack pressure, and gravity load of the dam. The critical crack lengthes were calculated according to the crack locations, directions, and magnitudes of blast vibration. Also variation of the effective stress intensity factors with respect to the multiple crack shapes and distances between the crack tips was investigated.

  • PDF

Zr-2.5Nb 합금의 하중방향에 따른 지연수소균열

  • 권상철;김영석
    • Proceedings of the Korean Nuclear Society Conference
    • /
    • 1997.05b
    • /
    • pp.153-158
    • /
    • 1997
  • Zr-2.5%Nb 합금에서 응력방향에 따른 DHC특성의 차이를 알아보고자 하였다. 판상의 CT시편을 이용하여 수소를 200 ppm 주입하고 응력을 압력관의 길이 방향으로 가하고 notch를 윈주방향으로 한 경우와 원주방향으로 응력을 가하고 notch를 길이 방향으로 한 경우의 균열전파속도를 측정하여 본 결과 길이 방향으로 응력을 가하였을 때 균열전파속도가 1/100 정도 감소하였으며, 균열발생을 위한 임계응력확대계수도 커짐을 알 수 있었다. 그리고 균열전파 방향도 원주방향으로 응력을 가하였을 때는 균열이 precrack을 따라 그대로 진행되었으나, 응력을 길이 방향으로 가하였을 때는 precrack을 따라 균열이 전파되지 못하고 균열분리 현상을 보였다 이것은 원래 모재가 보유하고 있는 집합조직과, 응력에의하여 수소화물이 재배열할 때 기존의 a상에서의 특정 방향 관계를 유지하여 석출함으로써 균열이 수소화물을 따라 전파됨이 원인인 것으로 생각된다. 응력을 원주방향으로 가하였을 때 균열주위에 수소화물이 길게 석출하지만, 응력을 길이 방향으로 기하였을 때는 수소화물이 20$\mu\textrm{m}$ 정도의 작은 크기로 분리된 균열과 같은 방향으로 분포하고 있음을 관찰하였다. 이로부터 집합조직을 개량함으로써 DHC저항성에 대한 효과를 얻을 수 있음을 확인 할 수 있었고 DHCV model에서 방향성을 수소화물의 재배열인자로부터 고려할 필요성이 있음을 알게 되었다.

  • PDF

Crack Resistance Behavior Using Digital Image Correlation and Crack Tip Opening Angle on Particulate Reinforced Composite (디지털 화상관련법 및 균열선단열림각도를 이용한 입자강화 복합재료의 균열저항거동)

  • Na, Seong Hyeon;Lee, Jeong Won;Kim, Jae Hoon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.40 no.12
    • /
    • pp.1021-1026
    • /
    • 2016
  • In this study, crack resistance is evaluated by the crack tip opening angle (CTOA) using a wedge splitting test (WST) on a viscoelastic particulate reinforced composite based on an HTPB binder. Generally, CTOA, as a function of crack extension, is used in order to determinate fracture resistance and has a steady state relative angle. Digital image correlation (DIC) is used to measure the crack tip opening displacement (CTOD) and crack extension for the critical crack tip opening angle (CTOAc). In these results, the CTOAc value of a particulate reinforced composite tends to approach a constant angle after a small amount of crack extension. The CTOAc value increases with decreasing temperature, from $50^{\circ}C$ to $-40^{\circ}C$. These CTOAc values may be used to measure fracture mechanics parameters for particulate reinforced composite.

Investigation of Cracking Condition during Press Forming of Extruded Aluminum Sheets (알루미늄 압출판재의 프레스성형 중 파열조건에 대한 조사)

  • Chu, Seok Jae;Park, Chang Gu;Cho, Eun Hwa
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.38 no.3
    • /
    • pp.251-258
    • /
    • 2014
  • Sunroof tracks are manufactured by press-forming extruded aluminum sheets. During press forming, cracking occurs along the sharply bent edge. The final positions of the punch and die were measured on the section, and their relation to cracking was investigated. Finite element simulation of bending to the final position was done to find the critical strains. Three-point bending tests with different material orientations, hardnesses, bending edge lengths, and bending radii were carried out in the laboratory, and finite element simulation of the three-point bending tests was performed to find the critical strains.

A Study on Fracture Bahavior of Composite Material Subjected to Simultaneous Deformation Mode (연립변형모드 구성된 복합재료의 파괴역학적 거동에 관한 연구)

  • 김상철
    • Magazine of the Korea Concrete Institute
    • /
    • v.9 no.3
    • /
    • pp.179-187
    • /
    • 1997
  • 콘크리트는 여러 구성 성분들이 불규칙적인 배열을 이루어 형성된 복합재료이지만, 과거에는 이 재료를 하나의 단종재료로 간주하여 해석하였기 때문에, LEFM에서 사용되는 파괴인성계수만으로는 콘크리트의 파괴역학적 접근이 어렵다는 것 이외에는 파괴인성계수들의 크기의존성에 대한 이유라든가, 실험을 통해서 관측된 구조물 두께 방향으로의 서로 다른 깊이의 균열 진행 현상에 대해서는 설명하기가 어려웠다. 따라서 본 연구는 콘크리트를 하나의 복합재료로써 각각의 구성요소들이 차지하고 있는 체적비 및 배열상의 효과를 고려하여 복합재료의 파괴거동을 해석하고, 구성재료의 수와 파괴인성계수와의 상관관계를 분석하였다. 각각의 구성요소들을 연립변형모드( SD mode)로 배열시킨 조건에서 복합재료역학개념에 입각하여 해석한 결과, 일반적으로 실험이나 비선형파괴역학 해석과 같이 하중-변위곡선 상단부에서 비선형 거동이 관측되었다. 또한 임계응력확대계수( $K_IC$)나 파괴에너지($G_r$)는 구성원의 수나 보의 크기에 대해서 거의 무관한 값을 나타내지만, 임계군열선단개구변위 ($CTOD_c$)는 크기에 영향을 받음을 보여 주었다. 균열의 진행속도는 균열이 진행될수록 감소하며, 파괴인성이 작은 구성원에서부터 균열이 발생되어 결과적으로 보의 두께 방향으로 서로 다른 크기의 균열길이가 생성됨이 관측되었다.

A study of mixed-mode interlaminar fracture toughness of graphite/epoxy composite (炭素纖維强化 複合材料의 혼합모우드 層間破壞靭性値에 대한 硏究)

  • 윤성호;홍창선
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.10 no.2
    • /
    • pp.198-207
    • /
    • 1986
  • This study investigates interlaminar fracture characteristics of Graphite/Epoxy composite (HFG Graphite/Epoxy) under mode I (opening mode), mode II (sliding mode) and mixed mode loading conditions. The effects on interlaminar fracture toughness due to different fiber orientations on the crack surface are also investigated. The antisymmetric test fixture proposed by M. Arcan is used for this test. Both critical stress intensity foctors and critical energy release rates were determined and several mixed mode fracture criteria were compared to the experimental data. Also fracture surfaces were investigaed to obtain informations on the fracture behaviors of Graphite/Epoxy composite by means of a scanning electron microscope(SEM).

Prediction of Fatigue Life in 2 Ply Rubber/Cord Laminate (2층 고무/코드 적층판의 피로 수명 예측)

  • 임동진;이윤기;윤희석;김민호
    • Composites Research
    • /
    • v.16 no.3
    • /
    • pp.9-17
    • /
    • 2003
  • In order to simulate the crack connection between cords and the interply crack growth in the belt-layer of real tire, 2 ply rubber/cord laminate specimens with exposed edges were tested in 4~11mm displacement control. Measurement of the crack connection is evaluated when crack reaches the half of the length between 45$^{\circ}$ aligned cords, and the amount of the crack growth is measured by the steel probe method. 2 dimensional analytic modeling was performed to simulate the crack connection between cords at the exposed edges. Also, the theoretical life of the specimens was calculated from the crack connection life between cords(critical value) and from the critical value to the final failure by the use of Tearing energy(T); the strain energy release per unit area of one fracture surface of a crack. Then, theoretical life was compared with those of experiments. The life prediction up to the critical value has about 20% error compared to experimental life, and up to the final failure about 65% error. Therefore, total theoretical life has about 45% error compared to the experimental life, which is conceivable in the case of rubber.

Fatigue Crack Growth Equation considered the Effect of Stress Ratio (응력비의 영향을 고려한 표면피로균열의 균열성장식)

  • 강용구;김대석
    • Journal of Ocean Engineering and Technology
    • /
    • v.12 no.1
    • /
    • pp.39-49
    • /
    • 1998
  • In this work, fatigue tests by axial loading were carried out to investigate the effect of stress ratio on the growth behaviors of surface fatigue crack for SM45C steel and Al 2024-T4 alloy. The growth behaviors of surface crack have been monitored during fatigue process by measuring system attached CCTV and monitor. When the growth rates of surface crack were investigate by the concept of LEFM based on Newman-Raju's .DELTA.K, the dependence of stress ratio appears both SM45C steel and Al 2024-T4 alloy. Therefore, modified stress intensity factor range, .DELTA.K' [=(1+R)/sup n/.DELTA.K] are intorduced to eliminate the dependence of stress ratio. Using .DELTA.K', it is found that the dependence of stress ratio disappears both SM45C steel and Al 2024-T4 alloy.

  • PDF

A Study on Fracture Characteristics of Woven Carbon Fiber Reinforced Composite Material (직물탄소 섬유강화 복합재료의 파괴특성에 관한 연구)

  • 김광수;김상태
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.16 no.3
    • /
    • pp.497-505
    • /
    • 1992
  • 본 연구에서는 최근에 개발된 직물 탄소섬유강화 복합재료의 파괴인성치를 정 량적으로 결정하고 파괴거동을 조사하고자 한다. 본 연구의 목적은 이 재료에 선형 탄성파괴역학의 적용여부를 알아보고, R곡선을 이용하여 균열의 생성점 및 불안정 파 괴점의 파괴인성치를 정확히 구하며, 주사형 전자현미경을 통해 파단면 및 균열 성장 시점을 관찰하여 파괴거동을 조사하는데 있다.

Image Processing Algorithm for Crack Detection of Sewer with low resolution (저해상도 하수관거의 균열 탐지를 위한 영상처리 알고리즘)

  • Son, Byung Jik;Jeon, Joon Ryong;Heo, Gwang Hee
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.2
    • /
    • pp.590-599
    • /
    • 2017
  • In South Korea, sewage pipeline exploration devices have been developed using high resolution digital cameras of 2 mega-pixels or more. On the other hand, most devices are less than 300 kilo-pixels. Moreover, because 100 kilo-pixels devices are used widely, the environment for image processing is very poor. In this study, very low resolution ($240{\times}320$ = 76,800 pixels) images were adapted when it is difficult to detect cracks. Considering that the images of sewers in South Korea have very low resolution, this study selected low resolution images to be investigated. An automatic crack detection technique was studied using digital image processing technology for low resolution images of sewage pipelines. The authors developed a program to automatically detect cracks as 6 steps based on the MATLAB functions. In this study, the second step covers an algorithm developed to find the optimal threshold value, and the fifth step deals with an algorithm to determine cracks. In step 2, Otsu's threshold for images with a white caption was higher than that for an image without caption. Therefore, the optimal threshold was found by decreasing the Otsu threshold by 0.01 from the beginning. Step 5 presents an algorithm that detects cracks by judging that the length is 10 mm (40 pixels) or more and the width is 1 mm (4 pixels) or more. As a result, the crack detection performance was good despite the very low-resolution images.