This study aimed to evaluate of the hardened properties (mortar consistency, setting time, absorption properties, drying shrinkage, and bond strength) of the basalt powder sludge mortar recycling a basalt powder sludge occurred during the manufacture process of basalt stone as a replacing material for the sea-sand used to cement filling compound for surface preparation. The hardened mortar made of the basalt powder sludge showed an enhanced performance or similar with the properties of normal mortar used to cement filling compound for surface preparation. But, the drying shrinkage was increased more than a normal cement mortar in the hardened mortar made of the basalt powder sludge since curing 8 - 9days. And the bond strength is low in the hardened mortar used the basalt powder sludge. On the whole, properties of the hardened mortar used the basalt powder sludge correspond to the required minimum quality criterion in the KS F 4716 'cement filling compound for surface preparation'.
When $Al_2(SO_4)_3$ as an accelerator was added to $\beta$-hemihydrate gypsum, the setting time, mobility and compressive strength properties of $\beta$-hemihydrate gypsum were examined with the adding of two types grounded gypsum crushed by ball mill. By 15wt% adding of 7% $Al_2(SO_4)_3$ dilute solution, the setting time of $\beta$-hemihydrate gypsum was sharply accelerated than that of non-added $\beta$-hemihydrate gypsum. When ground phospho gypsum(PG) and chemical gypsum(CG) were added to $\beta$-hemihydrate gypsum, the initial and final setting time of $\beta$-hemihydrate gypsum were accelerated markedly with the increasing of grinding time and added amount of ground phospho gypsum. Especially, this trend largely presented when ground phospho gypsum was added to $\beta$-hemihydrate gypsum. The compressive strength of $\beta$-hemihydrate gypsum added by ground phospho and chemical gypsum was largely increased at initial curing time such as 1, 3 days. Particularly, the compressive strength of $\beta$-hemihydrate gypsum added by ground phospho gypsum was increased by 15~20% than that of ground chemical gypsum.
In this paper, setting and strength performances of concrete containing saccharic type super retarding agents are investigated under various kinds and contents of super retarding agents. According to test results, as super retarding agents contents increase, slump shows to be increased, while air contents decrease about 1∼2%. Setting time shows to be retarded considerably with increase of super retarding agents. It takes 20 days after mixing to reach final setting in case of concrete containing gluconic acid more than 0.3%. And 10 days after mixing in case of enhancing sucrose, white and brown sugar. Compressive strength of concrete containing super retarding agents is lower than that of plain concrete at early age. However, it keeps up with and exceeds the compressive strength of plain concrete at later age. White sugar md brown sugar shows positive performances in delaying setting time and strength compared to existing super retarding agents. n further investigations on durability are conducted, it is thought that application of white sugar as super retarding agent is available.
Journal of the Korea Institute of Building Construction
/
v.15
no.1
/
pp.25-33
/
2015
In this study, initial crack index was evaluated by FEM analysis to find the crack propagation from hydration heat in precast concrete. As results, as the usage of hardening accelerator increased, initial compressive strength increased and setting time was shortened. Additionally, as amounts of hardening accelerators increased, the central temperature of concrete increased and the time to reach the highest temperature was shortened. It was demonstrated that the hardening accelerators accelerated the hydration reaction of cement, and caused the increase of hydration heat within the short period of time. Furthermore, the crack index for evaluating the heat level was performed by FEM. As results, there was no problem about the cracks, despite of the growth of initial high hydration heat. This is because of the increased tensile strength that is large enough to sustain the thermally induced-stress.
Proceedings of the Korean Institute of Building Construction Conference
/
2018.11a
/
pp.89-90
/
2018
In recent years, harmful substances and fine dust in the air are caused by respiratory and cardiovascular diseases through various mechanisms when they are introduced into the human body through respiration, thereby exacerbating human health and causing cancer by prolonged exposure do. In order to prevent such fine dust from being introduced into the room and to improve indoor air quality, improvement of air quality has attracted attention. Among indoor air pollutants, fine dust and CO2 are pollutants that are directly affected by indoor number and activity. The purpose of this study is to evaluate the basic performance of cement matrix using photosynthetic bacteria as a basic study of fine dust and CO2 adsorption type matrix to suppress indoor air pollution and improve air quality.
Proceedings of the Korea Concrete Institute Conference
/
2002.05a
/
pp.323-328
/
2002
Rapid set accelerators are widely used in tunnel construction, however quality criteria of and dosage are not well established. The density and solid content of admixtures, setting time and compressive strength of paste and mortar with admixtures were investigated to establish the quality criteria. While the early strength of mortar with sodium-silicate, sodium-aluminate and calcium aluminate type admixtures that have high alkali content are very high, but long-term strength are low. Aggregates of shotcrete has to be carefully selected. Sodium-silicate type admixture need longer setting time than the others.
Park, Nam-Kyu;Lee, Jong-Kyu;Chu, Yong-Sik;Song, Hun
Proceedings of the Korea Concrete Institute Conference
/
2008.11a
/
pp.545-548
/
2008
In this study aluminium sulfate, Ca(OH)$_2$, K-R Slag and $Na_2SO_4$ were used as active admixtures and their concentration 1, 3, 5, 7 weight percent in cement. The physical properties of active admixtures cement mortar were investigated by flow test and compressive strength. It was found that the resulting active admixtures exhibited the higher compressive strength than OPC mortar up. From the test results, cement mortars added active admixture have a good fundamental property.
Journal of the Korean Recycled Construction Resources Institute
/
v.8
no.1
/
pp.105-111
/
2020
The present study examined the effect of the silica-based accelerating agents on the setting time and compressive strength gain of biomimetic glycocalix coating materials that has been developed for protecting the substrate of concrete exposed to chemical and microbiological attacks. The accelerating agent contents varied from 10mL/L to 40mL/L in the mixtures of glycocalix coating materials determined for shotcrete and lining techniques. Test results showed that the setting time of coating materials containing accelerating agents was affected by the contents of the bacteria carrier. When the accelerating agent content was 40mL/L, the final setting time was 80 minutes for shotcrete mixtures and 318 minutes for lining mixtures. Meanwhile, the compressive strength gain of coating materials with accelerating agents tended to be lower than that of counterpart materials without accelerating agents.
When hot weather concrete is utilized, the cooling methods of cooling pipe, liquid nitrogen, ice, etc., are used to prevent the poor consistency and cold joint due to high temperature. These methods, however, spike the production cost and energy consumption, and make quality control difficult. Among these methods is one that involves the use of a retarder. Although economical, retarder is caused difficulty of retarded hardening and setting time control due to inaccurate weighing and poor working condition. Therefore, how to make a tablet for hot weather concrete, as with the existing pharmacy and foods, is discussed in this study, including the following items: mortar setting time, flow test by elapsed time, physical and mechanical properties of concrete. As a result, gluconic acid is superior to lignosulfonic acid and the possibility of using them for such purpose without quality degradation was confirmed in this study, when retarder is tabletting.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.