There has been increasing attention and research in various nanoparticle applications. Nanoparticles have been used for a variety of purposes in different departments including but not limited to cosmetics, food, machinery, and chemical. A highly sought-after field to use nanoparticles, especially natural or artificial silver nanoparticles (SNPs), is the utilization of their significant antimicrobial properties in daily items such as fabrics, indoor air filters, and, water filtration units where abundant bacterial and fungal growth are inevitable. These applications of SNPs, however, have enabled continuous human exposure and hence paved the way for potential SNP toxicity depending on exposure method and particle size. This potential toxicity has led to researches on safer antimicrobial solutions to be utilized in textile and filtration. In this context, products of natural origin have gained expanding interest due to their eco-friendly, cost-effective, and biologically safe properties along their promising antibacterial and antifungal activities. Natural product-applied fabrics and filters have been shown to be comparable to those that are SNP-treated in terms of ease production, material durability, and antimicrobial efficiency. This article summarizes and assesses the current state of in vitro and in vitro toxicity of SNPs and discusses the potential of natural products as an alternative.
Silver nanoparticles were prepared by chemical reduction-protection method using 1-decanoic acid and tri-n-octylphosphine as surfactants, and using $NaBH_4$ as a reducing agent. The silver nanoparticles were also studied for their formation, structure, morphology and size using UV-Visible spectroscopy, XRD, TEM and SEM. Further the viscosity of the silver paste and the surface resistance of the silver metal film produced by screen coating onto a PET film were investigated. Well dispersed and quasispherical silver nanoparticles with the size of 10-200 nm were obtained under the optimal molar ratio of $NaBH_4/AgNO_3=1:5$. The surface resistance of silver metal film coated on the PET film made with the silver nanoparticles under the optimal molar ratio showed a minal value of $41{\mu}{\Omega}/cm^2$.
Journal of the Korea Academia-Industrial cooperation Society
/
v.18
no.11
/
pp.88-93
/
2017
It is important to develop a simple method oftuning localized surface plasmon resonance(LSPR) properties, due to their numerous applications. In addition, the careful examination of the shape, size and combination of metal nanoparticles is useful for understanding the relation between the LSPR properties and metal nanostructures. This article describes the dependence of theLSPR properties on the arrays of metal nanoparticles obtained from a block copolymer(BCP) micellar thin film. Firstly, two different Au nanostructures, having a dot and ring shape, were fabricated using conventional block copolymer micelle lithography. Then, Ag was plated on the Au nanostructures through the silver mirror reaction technique to obtain Au/Ag bimetallic nanostructures. During the production of these metallic nanostructures, the processing factors, such as the pre-treatment by ethanol, silver mirror reaction time and removal or not of the BCP, were varied. Once the Au nanoparticles were synthesized, Ag was properly plated on the Au, providing two distinguishable characteristic plasmonic bands at around 525nm for Au and around 420nm for Ag, as confirmed bythe UV-vis measurements. However, when a small amount of Au seed nanoparticles, which accelerate the Ag plating speed,was formed by usinga block copolymer with a relatively highmolecular weight, all of the Au surfaces were fully covered by Ag during the silver mirror reaction, showing only the characteristic peak for Ag at around 420nm. The Ag plating technique on Au nanoparticles pre-synthesized from a block copolymer is useful to study the LSPR properties carefully.
Proceedings of the Korean Vacuum Society Conference
/
2012.08a
/
pp.383-383
/
2012
최근 나노 소재의 활용 가능성이 확대되어감에 따라 다양한 소재의 나노구조체에 대한 연구가 진행되어 왔다. 그 중 은(Silver)은 열전도율과 전기전도율이 가장 우수한 금속으로 다양한 형태의 은 나노 입자를 형성할 수 있고. 이를 탄소, 비석, 고분자 등의 기판에 다양한 방법으로 성장시키는 연구가 진행되었다. 기판으로 사용되는 재료 중 탄소 복합소재는 내열성, 화학적 안정성, 열전도성, 저열팽창성에 따른 치수 안정성, 유연성 등의 우수한 특징을 지니고 있으며 최근까지 방열 소재로서 활용되고 있다. 본 연구에서는 탄소섬유의 표면에 다양한 결정 구조를 가지는 Ag seed 입자를 형성하고 폴리올 공정을 통하여 와이어 형태의 나노구조체를 성장시켜 그 형상제어 특성을 FE-SEM을 통하여 확인하였다.
We report organically functionalized Ag nanoparticles spontaneously form two-dimensional (2D) novel superstructures at the air-water interface. Analysis of the superstructures suggests that the 2D assembly of Ag nanoparticles originates from a subtle interplay between characteristic inter-particle interactions that can be readily controlled by changing the sizes of nanoparticle metal core and surfactants. Such structures have potential uses in nanostructured functional materials, catalysis, and device applications.
Proceedings of the Korean Vacuum Society Conference
/
2016.02a
/
pp.346.1-346.1
/
2016
본 연구에서는 열처리(Thermal Dewetting Process)와 빗각 증착(Oblique angle deposition)을 이용하여 비주기 서브파장 구조물을 마이크로 렌즈 형태의 유리 기판 상부에 제작하였다. 먼저 $2{\times}2cm2$ 크기의 유리 기판에 기존 리소그래피 공정으로 원기둥 형태의 감광액을 형성한다. 이후 Hot-plate로 $180^{\circ}C$에서 90초간 열을 가해 지름이 $20{\mu}m$인 반구형태로 변형시킨 뒤 반응성이온식각 공정을 진행하여 마이크로 렌즈를 제작한다. 렌즈의 표면에 나방 눈 구조를 형성하기 위해 전자빔 증착으로 15nm의 은 박막을 쌓은 뒤 $500^{\circ}C$에서 1분간 열처리 공정을 진행하였다. 열이 가해졌을 때 은 박막은 표면자유에너지를 최소화하기 위해 나노 크기의 덩어리진 입자 형태로 변화한다. 여기서 형성되는 나노입자의 크기가 렌즈 표면 중심에서 가장자리로 갈수록 작아진다는 것을 주사전자현미경을 통해 확인하였다. 증착 각도가 증가할수록 열처리 공정 후의 은 나노입자의 크기가 점점 작아진다는 것을 검증하기 위해 은 박막의 증착 각도를 $0^{\circ}$, $35^{\circ}$, $55^{\circ}$, $70^{\circ}$로 증착 후 열처리 공정을 진행하여 확인하였다. 비스듬하게 증착되어 형성된 박막은 다공형태로 낮은 밀도를 가지는데 이는 박막 두께 감소를 일으킨다. 따라서 증착 각도가 증가할수록 열처리 공정 후의 은 나노입자의 크기는 점점 작아진다. 이후 은 나노입자를 마스크로 하여 다시 반응성이온식각 공정을 진행하였으며 식각 후 나머지 은 나노입자들은 HNO3용액에서 1분간 처리하여 제거하였다. 제작된 구조물의 평균 직경과 크기는 각각 ~220nm 및 ~250nm인 것으로 확인하였다. 위와 같은 공정을 통해 다양한 크기를 가진 비주기 서브파장 구조물을 제작할 수 있다. 구조물의 주기가 파장 길이보다 짧을 경우 분산이 최소화되며 넓은 파장 대역에서 무반사 효과를 얻을 수 있다. 이 공정은 마스크를 통한 리소그래피의 한계를 극복할 수 있으며 여러 곡면형 표면에 적용가능한 장점이 있다. 또한 프리즘, 렌즈, 광섬유와 같은 광소자의 광투과율을 향상시키는데 이용될 수 있다.
Proceedings of the Korean Vacuum Society Conference
/
2016.02a
/
pp.164.1-164.1
/
2016
본 연구에서 지지체로 사용된 단결정 형태의 수산화인회석(Hydroxyapatite)은 칼슘과 인산염으로 구성된 무기물이다. 염기 조건 (10 M NaOH)에서 수열합성법 (Hydrothermal method)을 이용하여 단결정 형태의 수산화인회석을 합성하였다. 합성된 단결정 수산화인회석의 표면에 이온 교환 반응을 통하여 은 원자를 도입하였으며, 아르곤 및 수소 기류 (96% Ar, 4% $H_2$) 조건에서 가열하는 온도를 조절하는 것으로 은 나노 입자를 생성시켰다. 합성된 샘플은 XRD 패턴 및 TEM 이미지 분석을 통하여, 수산화인회석의 합성 및 은 나노 입자가 형성된 것을 확인하였다. 합성된 샘플을 유기 반응 촉매로 사용하여 여러 가지 알코올 (1차, 2차 알코올)의 산화 반응에 응용하였으며, UV-Visble light 영역에서의 메틸렌 블루 분해 반응 실험에 광촉매로서 사용하였다.
Ag/polystyrene(PS) nanocomposites were prepared by in situ reduction of silver 2-ethylhexylcarbamate (Ag-CB) complex and follwing radical polymerization only by heating at 110 $^{\circ}C$. In contrast to this conventional heating method, the microwave irradiation afforded well-dispersed silver nanoparticles(NPs) in styrene monomer without polymerization. The synthesis of Ag NPs proceeded uniformly throughout the reaction vessel only under microwave irradiation, completing the reaction simultaneously in the whole reaction solution. Successive polymerization of the monomer containing the resultant NPs has successfully produced a hybrid of the silver NPs dispersed in PS matrix. Ag/PS (0.1/100) nanocomposites were prepared successfully by melt-mixing process using Ag/PS(4.0/100) as a master-batch. UV-VIS spectroscopy, TEM, and X-ray diffraction techniques were used to investigate the process of formation of Ag/PS nanocomposites.
Effects of silver nanoparticles on the polymerization rate and morphology of poly(vinyl acetate) (PVAc)/silver microspheres prepared by suspension polymerization of VAc were investigated. Scanning electron microscopy, transmission electron microscopy, X-ray diffraction and atomic absorption spectrometry were used to characterize the morphology and properties of the PVAc/silver microspheres. Due to the change of hydrophilicity of silver nanoparticles, appearance of the microspheres having golf ball-like convave surfaces was observed. Under controlled concentration of surfactant, PVAc/silver microspheres with various hollow structures were synthesized. In the case of silver nanoparticles modified by surfactant, the polymerization rate increased slightly. PVAc/silver microspheres with a conversion up to 80% were prepared via suspension polymerization.
The aim of this study was to develop a simple, environmentally friendly synthesis of silver nanoparticles (SNPs) without the use of chemical reducing agents by exploiting the extracellular synthesis of SNPs in a culture supernatant of Bacillus thuringiensis CH3. Addition of 5 mM $AgNO_3$ to the culture supernatant at a ratio of 1:1 caused a change in the maximum absorbance at 418 nm corresponding to the surface plasmon resonance of the SNPs. Synthesis of SNPs occurred within 8 hr and reached a maximum at 40-48 hr. The structural characteristics of the synthesized SNPs were investigated by various instrumental analysis. FESEM observations showed the formation of well-dispersed spherical SNPs, and the presence of silver was confirmed by EDS analysis. The X-ray diffraction spectrum indicated that the SNPs had a face-centered cubic crystal lattice. The average SNP size, calculated using DLS, was about 51.3 nm and ranged from 19 to 110 nm. The synthesized SNPs exhibited a broad spectrum of antimicrobial activity against a variety of pathogenic Gram-positive and Gram-negative bacteria and yeasts. The highest antimicrobial activity was observed against C. albicans, a human pathogenic yeast. The FESEM observations determined that the antimicrobial activity of the SNPs was due to destruction of the cell surface, cytoplasmic leakage, and finally cell lysis. This study suggests that B. thuringiensis CH3 is a potential candidate for efficient synthesis of SNPs, and that these SNPs have potential uses in a variety of pharmaceutical applications.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.