• 제목/요약/키워드: 용사 피막

검색결과 87건 처리시간 0.022초

상압 플라즈마 용사의 공정조건에 따른 세라믹 피막의 특성 (Effect of Processing Conditions for Atmospheric Plasma Spraying on Characteristics of Ceramic Coatings)

  • 주원태;최병룡;홍상희
    • 한국표면공학회지
    • /
    • 제26권4호
    • /
    • pp.192-202
    • /
    • 1993
  • The characteristics of the high-performance ceramic coatings fabricated on the optimum processings con-ditions for the atmospheric plasma spraying are evaluated by various material tests and analyses. The opti-mum processing parameters for the plasma spraying are determined by using the two-level orthogonal arrays of fractional factorial testing method as a statistical approach. Material tests for the coating specimens are carried out to evaluate microstructure, hardness, adhesion strength, and deposition efficiency. The properties of Al2O3-13%TiO2 coating are discussed with regard to the effective processings parameters. The decarburization effects of WC-12%Co coating is examined by XRD analysis in terms of the arc power and the secondary gas species. The hardness of Al2O2-13%TiO2 coating is increased with the arc power and shows the maximum value at around 40 lpm of Ar gas flowrate, which appears to be the most critical parame-ter on the deposition efficiency. For reducing the decarburization of WC-12%Co coating, the injection of inert He gas instead of reactive H2 gas as a secondary gas is more effective than the dropping of arc power to lessen the plasma enthalpy.

  • PDF

음향방출법에 의한 용사코팅 피막부식재의 파손 해석 (Failure Analysis of Corroded Coating Materials by Acoustic Emission)

  • 김귀식;현창해;홍용의;손창환
    • 한국해양공학회지
    • /
    • 제19권5호
    • /
    • pp.43-49
    • /
    • 2005
  • This paper is to investigate the effect of corrosion by acoustic emission method in tensile loading and the adhesiveness between substrate and coating layer. The powders used are Zn and Amdry625, respectively. They are coated on brass alloy substrate. AE signals of Zn and Amdry625 coating layer increase drastically in strain $2\%$. However, those of Zn specimen have more than those of Amdry625 specimen. When the specimens executed the corrosion test under $3.5\%$ NaCl solution for 500, 1000 hours, the salt solution penetrated into the surface of the substrate through the pores of the coating layer. As a result, corrosion production formed on the surface of the substrate. The adhesiveness between coating layers is weakened by the polarization and corrosion itself. The AE event, count, and energy of corroded coating specimens decrease, compared to specimens without corrosion. The results are summarized as follows : 1. In the tensile tests, the time that it took to start and develop the cracks and exfoliations between the surface of the substrates and the plasma spray coatings were different according to the type of plasma sprayed material, which are Zn and Amdry625. These phenomena were obvious at the strain rate 1 to $5\%$, and few available data were found after that stage. 2. The specimens with Zn coating showed the characteristics of crack, according to the changes of the tensile strength applied on the substrates while those with Amdry625 showed exfoliation as a result of low adaptation to the tensile strength. 3. The anti-corrosion specimens showed that the adhesive properties between the substrate and the plasma spray coating were strong in the order of Zn, Amdry. It showed that Corroded specimens cracked or exfoliated easily, even with the small energy, because those had a comparatively weakened adhesive property, due to corrosion. 4. Zn specimen showed no corrosion phenomena on the surface of the substrates, because they had the function of sacrifice anode however, Amdry625 specimen showed the corrosion, because it did not have that function.

$TiO_2$ 및 Ag 스퍼터링-$TiO_2$ 플라즈마 용사피막의 광전류 및 광분해 특성 (Photoelectrical Conductivity and Photodegradation Properties of $TiO_2$ and Ag Sputtered $TiO_2$ Plasma Spraying Coatings)

  • 강태구;장용호;박경채
    • Journal of Welding and Joining
    • /
    • 제27권2호
    • /
    • pp.38-43
    • /
    • 2009
  • In this study, we investigated photocatalytic ability of plasma sprayed $TiO_2$ and Ag sputtering $TiO_2$(Ag-$TiO_2$) coatings. A sputtering processes were adopted to coat the surface of $TiO_2$ with Ag(99.99%). Ag was sputtered at 10mA, 450V for $1{\sim}11$ seconds. $TiO_2$ and Ag-$TiO_2$ coatings were heat-treated at 250, 300, 350, $400^{\circ}C$ for $0{\sim}240$seconds. Photoelectrical conductivity was measured by four-point probe, and photodegradation was calculated by UV-V is spectrometer. Microstructure observation of $TiO_2$ and Ag-$TiO_2$ coatings were investigated by SEM. Crystal structure of $TiO_2$ and Ag-$TiO_2$ coatings were investigated by XRD. Qualitative analyses of $TiO_2$ and Ag-$TiO_2$ coatings were conducted by EDX. When $TiO_2$ coatings were heat-treated at $350^{\circ}C$ for 30 sec, photoelectrical conductivity and photodegradation were best. And in XRD analysis result, (101)/(110) relative intensity ratio of $TiO_2$(rutile) was comparably changed with photoelectrical conductivity. When Ag-$TiO_2$ coatings were heat-treated at $350^{\circ}C$ for 30 [sec] after sputtering Ag for 7 sec, Photoelectrical conductivity and photodegradation are best. Surface of coatings in such condition has very small and uniform Ag particles.

BSCCO 플라즈마 용사피막의 부분용융열처리 후 어닐링 시간에 따른 초전도 특성 (Characteristics of Plasma Sprayed BSCCO Superconductor Coatings with Annealing Time After Partial Melt Process)

  • 박정식;이선홍;박경채
    • 한국재료학회지
    • /
    • 제24권2호
    • /
    • pp.116-122
    • /
    • 2014
  • $Bi_2Sr_2CaCu_2O_x$(Bi-2212) and $Bi_2Sr_2Ca_2Cu_3O_y$(Bi-2223) high-Tc superconductors(HTS) have been manufactured by plasma spraying, partial melt process(PMP) and annealing treatment(AT). A Bi-2212/2223 HTS coating layer was synthesized through the peritectic reaction between a 0212 oxide coating layer and 2001 oxide coating layer by the PMP-AT process. The 2212 HTS layer consists of whiskers grown in the diffusion direction. The Bi-2223 phase and secondary phase in the Bi-2212 layer were observed. The secondary phase was distributed uniformly over the whole layer. As annealing time goes on, the Bi-2212 phase decreases with mis-orientation and irregular shape, but the Bi-2223 phase increases because a new Bi-2223 phase is formed inside the pre-existing Bi-2212 crystals, and because of the nucleation of a Bi-2223 phase at the edge of Bi-2212 crystals by diffusion of Ca and Cu-O bilayers. In this study the spray coated layer showed superconducting transitions with an onset Tc of about both 115 K, and 50 K. There were two steps. Step 1 at 115 K is due to the diamagnetism of the Bi-2223 phase and step 2 at 50 K is due to the diamagnetism of the Bi-2212 phase.

가열 롤에서 플라즈마 TiO2-NiCr 용사피막의 특성 (Characteristics of Plasma Sprayed TiO2-NiCr Conductive Heating Roll Coatings)

  • 강태구;진민석;고영봉;김태형;조상흠;박정식;김종철;박경채
    • Journal of Welding and Joining
    • /
    • 제25권4호
    • /
    • pp.28-34
    • /
    • 2007
  • The heating unit of direct heating method manufactured as the plasma spray coating of $TiO_2/NiCr$ conductive heating material on the surface of heating unit in order to improve the disadvantages of indirect heating method. $TiO_2$ and NiCr (80wt.%Ni-20wt.%Cr) that had the properties of conduction and heating was chosen for the conductive heating material. The compositions of the composite powders were studied $TiO_2-30wt.%NiCr\;and\;TiO_2-10wt.%NiCr$. As the heating temperature was increased, the hardness of heating layer was increased because of the fine microstructure and the decrease of porosity. The adhesion strength was decreased for coarsening and connection of voids in the insulation layer, and the electrical resistivity of heating layer was increased for fine crack formation and growth. In this study, the best efficient sprayed coatings with heating unit was concluded as the plasma sprayed $TiO_2-10wt.%NiCr$ coatings that was heat treated at $300^{\circ}C$.

전이금속을 첨가한 플라즈마 TiO2 복합 용사피막의 광전류 특성 (Photocurrent Characteristics of Plasma Sprayed TiO2 Composite Coatings according to Additive Transition Metal)

  • 고병천;고영봉;박경채
    • 한국표면공학회지
    • /
    • 제44권3호
    • /
    • pp.89-94
    • /
    • 2011
  • In this study, the photocurrent characteristics of plasma sprayed $TiO_2$ coatings have been investigated according to additive transition metal (Fe, Mn, Nb powder) and heat treatment conditions. The plasma sprayed $TiO_2$ coatings by heat treatment at $400^{\circ}C$ and 90 min had the higher photocurrent at ultraviolet light, no photocurrent at visible light. The photocurrent of plasma sprayed $TiO_2$ coatings added by Fe, Mn, Nb (named by plasma sprayed $TiO_2$ composite coatings) was lower than that of plasma sprayed $TiO_2$ coatings at ultraviolet light, as was low in intensity ratio of XRD(101)/(110). and the atomic percentage of oxygen by plasma sprayed $TiO_2$ composite coatings was higher than that by plasma sprayed $TiO_2$ coatings. The photocurrent of plasma sprayed $TiO_2$ composite coatings in heat treatment at $400^{\circ}C$ and 90 min was higher than that of plasma sprayed $TiO_2$ coatings in same heat treatment conditions at ultraviolet and visible light, as was high in oxygen affinity by heat treatment.

플라즈마 용사 BSCCO(Bismuth Strontium Calcium Copper Oxide) 초전도 피막의 접합 특성 (Joining Characteristics of Plasma Sprayed BSCCO Superconducting Coatings)

  • 박정식;조창은;고영봉;박광순;박경채
    • 한국표면공학회지
    • /
    • 제46권5호
    • /
    • pp.181-186
    • /
    • 2013
  • We performed plasma spraying for 2001 (Bi:Cu = 2:1), 0212 (Sr:Ca:Cu = 2:1:2) oxide powders. $Bi_2Sr_2CaCu_2Ox$ (2212) superconductor has been prepared by PMP-AT (partial melting process-annealing treatment). The 2212 phase is synthesized between Sr-Ca-Cu oxide coating layer (0212) and Bi-Cu oxide coating layer (2001) by movement of partial melted Bi on 2001 layer and the diffusion reaction (Cu, Sr, Ca) after PMP-AT. There are two different coating layers on joining process. The one is ABAB coating layers and the other is BAAB coating layers by arrangement of 2001 (A), 0212 (B) layers. We performed heat treatment these two different coating layers processes under same PMP-AT conditions. We obtained Bi-2212 superconducting layers at each experimental condition, and the result of MPMS, the critical temperature was showed about 78 K. But the microstructure images and result of EDS as each experimental variable were showed about the qualitatively different Bi-2212 superconducting phases. We also deduced the generation mechanism of Bi-2212 superconducting layer as a result of these experimental data, microstruc ture images, EDS data and phase diagram.