Characteristics of Rock Phase and Phenomena of Exfoliation, Breakout and Cracks Developed on the Rocks Constituting the Soongryemoon (숭례문의 육축을 이루는 석재의 암상 특징과 박리, 박락 및 균열현상)

  • Lee, Sang Hun
    • Journal of Conservation Science
    • /
    • v.11 no.1 s.14
    • /
    • pp.1-14
    • /
    • 2002
  • After the construction (1398 year at first, secondarily reconstructed at 1448 year), the Soongryemoon (South Gate) had been preserved to late 19c without large damages. The present shape of the gate have been kept after the repairments of two times (1953, 1963). However, the rocks constituting the walls of the gate have been strongly weathered, exfoliated and cracked due to severe changes in the environment as traffic increase, air pollution and the subway which may seem also to cause the structural unstability. The rocks composed of the walls of the gate are almost of granites. On the rocks such deteriorations as onion structure, surface exfoliation, cracks, and edge breakout are developed. These deteriorations may be caused genetically by strong weathering, differential load due to possibly structural unstability, impact and unknown reasons. For the establishment of conservation plan, the factors of these deterioration phenomena and structural unstability must be quantitatively analyzed and diagnosed in detail.

  • PDF

Element Mobility during the Weathering of Granitic Gneiss in the Yoogoo Area, Korea. (유구지역 화강암질 편마암의 풍화작용에 따른 원소의 거동)

  • 이석훈;김수진
    • Journal of the Mineralogical Society of Korea
    • /
    • v.14 no.1
    • /
    • pp.39-51
    • /
    • 2001
  • 공주군 유구면 일대의 화강암질 편마암의 풍화작용에 따른 원소의 거동과 pH와 이차광물과의 관계를 XRF, ICP-AES, ICP-MS를 이용한 원소분석결과를 통하여 검토하였다. 이 지역의 암석은 pH6 내외의 산성환경, 침철석, 아나타제와 같은 다양한 이차광물을 생성하면서 심각한 화학조성의 변화를 초래했다. 주원소의 화학조성을 이용한 풍화지수는 토양층에서 79~88로 모암 중의 사장석이 용해되고 흑운모가 변질되어 캐올리광물의 생성이 활발한 방향으로 풍화작용이 진행되었다. 지표층으로 가면서 Al에 대한 주 원소의 거동은 Si, Ca, Na, K, P가 감소하고 Fe, Ti, Mn이 증가하는 경향을 보이며 pH가 낮은 풍화단면에서 주 원소의 변화량이 더 크다. 이 풍화대에서 Mg은 거의 일정하다. Li, As 모든 전이원소는 pH가 감소함에 따라 증가하며 특히 이들 원소는 Fe의 함량과 비례해서 증가해 침철석과 공침하였거나 표면에 흡착되어 있는 것으로 보인다. Ga은 Fe와 비례하기는 하지만 변화량은 전 풍화단면에서 일정하다. Zr, Mo, Sn, Cd은 pH에 변화에 상관없이 일정한 반면에 Rb, Sr, Ba, Y, Pb, Th, U 등은 감소하는 경향을 보인다. 특히 Rb 과 Sr은 Ca에 비례해서 감소한다. 희토류원소는 전 풍화단면에서 감소하는 경향을 보이는데 $Al_2$$O_3$에 대한 상대적인 변화량을 보면 경희토류원소는 사프롤라이트(saprolite)하부와 상부에서 부화되어 있고 중부 사프롤라이트와 토양층에서 감소하는 반면에 중희토류원소는 사프롤라이트 하부와 상부에서 감소하고 중부사프롤라이트 및 토양층에서 부화되는 경향을 보인다. 전반적으로 희토류원소의 원자번호가 클수록 손실율이 커진다. 이 풍화단면에서 원소의 거동은 각 풍화층의 pH와 생성된 이차광물의 조성에 지배를 받았다.

  • PDF

Mineralogical Study of the Granite Weathering in the Seoul Area: Water-Rock Interaction in the Namsan Granite (남산 화강암의 풍화 및 광물-물 반응에 관한 연구)

  • Lee, Soo-Jae;Kim, Soo-Jin
    • Journal of the Mineralogical Society of Korea
    • /
    • v.7 no.1
    • /
    • pp.40-48
    • /
    • 1994
  • The weathering of the Namsan granite was studied in terms of sorption process. The Namsan granite consists mainly of quartz, alkali feldspar, plagioclase (${Ab_{85}An_{15}}-Ab_{100}$ and biotite with small amounts of sericite, magnetite and ilmenite. The kinetic factors for altering the granite body are the proton and hydroxyl ions derived from the reaction of water and mineral. There are two different types of pH variation curves for rocks of different mineral assemblages. when powdered granite was dispersed in distilled water under ambient condition. The sorption-process proceeds by three steps for fresh granite; (1) the initial rapid pH-rise to 10 by the uptake of proton by negatively charged mineral surfaces, (2) the gradual pH-down, and (3) the stable pH tail between 7.1-7.5. For somewhat weathered granites, the sorption proceeds; (1) the initial rapid pH-down to 4.8, (2) the slight pH-rise and slow ph-down, and (3) the stable pH tail between 5.0-5.3. The reaction rate is controlled by the density of adsorbable sites, the solubility of the mineral, pH of the system and formation of amorphous gel and gibbsite. Amorphous gel floates on the surface of the solution while stirring the powdered granite and then is transformed into gibbsite in an hour or so. The pH saturation values for -325 mesh fresh granite from 5 m depth is about pH 10 when rock/water ratio is over 10g/200 ml.

  • PDF

Estimation of Excavation Difficulty in Rock Mass (토공작업시 암반 굴착난이도 판정기준)

  • 유병옥;김경석
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2003.06b
    • /
    • pp.85-115
    • /
    • 2003
  • 토공작업시 굴착난이도(토층, 리핑암, 발파암)를 판정하는 기준으로는 암반의 강도, 풍화정도, 불연속면 간격과 같은 여러 가지 암반의 공학적 특성 및 지반의 탄성파 속도 등이 사용된다. 그러나 실제 토공 작업시의 굴착난이도 평가는 탄성파 탐사와 같은 암석ㆍ암반의 정량적인 판단기준에 근거하지 않고 단지 현장 기술자들의 육안관찰에 의존하여 굴착난이도를 구분하고 있는 실정이다. 본 논문은 실내시험 및 현장시험, 현장굴착난이도 평가 및 탄성파탐사 등을 실시하여 여러 암석에 대한 강도특성을 파악한 것을 근거로 현장에서 사용할 수 있는 암반굴착난이도 평가법의 Checklist를 제안하였다.

  • PDF

Interpretation of Physical Weathering and Deterioration Mechanism for Thermal Altered Pelitic Rocks: Ulju Cheonjeon-ri Petroglyph (열변질 이질암의 물리적 풍화작용과 손상메커니즘 해석: 울주 천전리 각석)

  • Chan Hee Lee;Yu Gun Chun
    • Economic and Environmental Geology
    • /
    • v.56 no.6
    • /
    • pp.629-646
    • /
    • 2023
  • Host rock of Cheonjeon-ri petroglyph is shale belonging to the Daegu Formation of Cretaceous Gyeongsang Supergroup. The rocks were hornfelsified by thermal alteration, and shows high density and hardness. The petroglyph forms weathered zone with certain depth, and has difference in mineral and chemical composition from the unweathered zone. As the physical deterioration evaluations, most of cracks on the surface appear parallel to the bedding, and are concentrated in the upper part with relatively low density. Breakout parts are occurred in the upper and lower parts of the petroglyph, accounting for 6.0% of the total area and occurs to have been created by the wedging action of cracks crossing. The first exfoliation parts occupying the surface were 23.8% of the total area, the second exfoliations covered with 9.3%, and the exfoliation parts with three or more times were calculated as 3.4%. It is interpreted that this is not due to natural weathering, and the thermal shock caused by the cremation custom here in the past. As the ultrasonic properties, the petroglyph indicates highly strength in the horizontal direction parallel to bedding, and the area with little physical damage recorded mean of 4,684 m/s, but the area with severe cracks and exfoliations showed difference from 2,597 to 3,382 m/s on average. Physical deterioration to the Cheonjeon-ri petroglyph occurred to influence by repeated weathering, which caused the rock surface to become more severe than the inside and the binding force of minerals to weaken. Therefore, it can be understood that when greater stress occurs in the weathered zone than in the unweathered zone, the relatively weathered surface loses its support and exfoliation occurs.

Variation of Physical and Microstructural Properties of Limestone caused by Artificial Freezing and Thawing (인공 동결-융해 풍화에 따른 석회암의 물성 및 미세구조 변화 분석)

  • Park, Jihwan;Park, Hyeong-Dong
    • Tunnel and Underground Space
    • /
    • v.25 no.5
    • /
    • pp.435-449
    • /
    • 2015
  • Physical and microstructural properties of Pungchon and Maggol limestone were investigated quantitatively during 50 cycles of artificial freezing and thawing test. There were decrease in dry weight and P,S-wave velocity, and increase in absorption rate in both rock types. Porosity, pore volume, equivalent diameter, throat thickness and pore orientation were analyzed using X-ray computed tomography images. Porosity increased, and initiation and expansion of pores were investigated as weathering progresses. Physical and microstructural variation in Maggol limestone was larger than that of Pungchon limestone because Maggol limestone has more pores and microcracks at initial state. As this study analyzes physical and microstructural properties of rock specimens comprehensively, it can be applied to further rock weathering study and can be used as fundamental data of construction and resource development in cold regions.

Study on Material Characterization of Earthen Wall of Buddhist Mural Paintings in Joseon Dynasty (조선시대 사찰벽화 토벽체의 재질특성 연구)

  • Lee, Hwa Soo
    • Journal of Conservation Science
    • /
    • v.32 no.1
    • /
    • pp.75-88
    • /
    • 2016
  • In this study, 5 mural paintings in the Buddhist temples of Joseon era were researched for component analysis on the soil contained in the walls. The results of particle size analysis showed that the ratio of particle contents were different in each layer. In the finishing layer, the distribution of the middle sand fraction is higher than that of the middle layer. The results of XRD analysis showed that quartz, feldspar, and clay mineral are the main components of sand, suggesting similar mineral composition to that of ordinary soil component. It seems weathered rocks were used for construction of the walls. The main chemical components detected from EDX analysis were Si, Al, Fe, and K. Also the SEM images showed sand or clay sized minerals. In conclusion, the walls of the buddhist mural paintings in Joseon Dynasty had been constructed by using the loess, and had been produced by using mixture of clay and sand particles of different sizes for each layer. This study identified the characteristics of the materials and the manufacturing technologies used on the walls of mural paintings of Buddhist temples in Joseon era.

The Preliminary Study for Genetic Environment of the Gem fields in the Pailling Area, Cambodia (캄보디아 빠일링지역의 보석광상의 성인에 대한 예비연구)

  • 김인준
    • Economic and Environmental Geology
    • /
    • v.36 no.4
    • /
    • pp.269-274
    • /
    • 2003
  • This study, one of the projects for investigation of the precious metal deposits of the Circum-Pacific Ocean coon-tries, was performed in a gem field of Pailling, Cambodia, in which there are numbers of undeveloped mineral resources. The gem fields in the Pailling area are typically distributed in the laterite, lying on of weathered basalts. The gem grade of corundum is low in the surface soil horizon(less than 1 m in depth), but is higher in the subsurface. Occurrence and genetic environment of the precious stone are not concerned in the soils. A Precious stone that is already made from at the least upper part of volcanic rocks is produced in large quantities to undergoing to weathering of the rocks. A precious stone is made from upper part of the formation under the high temperature when volcano is vomiting or after vomiting. and/or made from between the formation under the high temperature when other volcano is vomiting. Volcanic rocks including precious stone are a little different from other volcanic rocks when volcano is vomiting, but chemical composition of rocks is not far different from other volcanic rocks.

Physical and Chemical Variation of Sedimentary Rocks due to Weathering (풍화에 의한 퇴적암의 물리-화학적 변화)

  • Kim, Young-Su;Heo, No-Young;Jeong, Woo-Seob;Rui, Da-Hu;Lee, Jea-Ho
    • Journal of the Korean GEO-environmental Society
    • /
    • v.3 no.2
    • /
    • pp.49-60
    • /
    • 2002
  • A study on mineral composition and chemical component governing of weathering process is necessary to know the weathering characteristics of sedimentary rocks. In this study, a mineral and chemical component analysis, and physical and engineering characteristic tests were conducted to find out the characteristics of sedimentary rocks in Daegu, according to the weathering degree of sedimentary rock. Test results show that the mineral composition of rock, such as Albite (Ab), Muscovite (Ms), Magenetite (Mt) and the chemical composition of $A_2O_3$, CaO, $Na_2O$, $K_2O$, MgO and so on are closely related to the weathering. Based on the test results, we illustrated the quantitative application of weathering decision for the sedimentary rocks.

  • PDF

Developmental Characteristics and Weathering Processes of Tafoni at Golgulsa Temple, Gyeongju, South Korea (경주 골굴사 타포니의 발달 특성과 풍화 과정)

  • Shin, Jae Ryul;Choo, Chang Oh;Lee, Jin Kook;Park, Kyung Geun
    • Journal of the Korean association of regional geographers
    • /
    • v.23 no.1
    • /
    • pp.168-177
    • /
    • 2017
  • In order to reveal formation factors and developmental processes of tafoni this study was conducted with petrological analysis including microscopic observation, measurement of water content and water analysis at Golgulsa temple in Gyeongju, South Korea. The direction of the entrance to tafoni at Golgulsa temple tends to coincide with the direction of slope, and this is thought to be related to the direction of wind flow and water supply. Tafoni's initial developmental processes is judged to have grown as a result of a breakaway of rock fragments along with beddings and cracks in rock. Then, tafoni have been enlarged along at the spots that sufficiently accommodate water supply depending on the direction of wind. The results of water analysis of the stagnant water in gnamma implies that a high meltage of Na and Cl compared to other inland areas can be from the adjacent shore. The effects of such saline substances on rock weathering and development of taponi are currently under way through electronic microscopy and geochemical analysis.