• Title/Summary/Keyword: 순환 잔골재

Search Result 217, Processing Time 0.029 seconds

Proposal of Repair Method and Pop-out Phenomenon of Concrete Incorporating Electric Arc Furnace Oxidizing Slag Fine Aggregate (전기로 산화 슬래그 잔골재를 사용한 콘크리트의 팝아웃현상 및 보수공법 제안)

  • Lee, Gun-Cheol;Lee, Mun-Hwan;Lee, Sea-Hyun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.1
    • /
    • pp.65-71
    • /
    • 2007
  • Since pop-outs are occurred recently on concrete surface occasionally, it is needed to find out accurate causes and to suggest appropriate methods. On this study, it is investigated the occurrence mechanism of pop-outs caused by electric arc furnace Oxidizing slags as fine aggregate for concrete. As a result, it is investigated the cause of pop-outs that extremely small quantities of free CaO and free MgO in the electric furnace slag react with water to produce $Ca(OH)_2$ and $Mg(OH)_2$, so that their volumes are expanded and erupted about two times. As a resolution, it is needed to remove the potential cause of expansion by replacing the deteriorated concrete section up to the depth to secure the safe of structural element with repairing polymer mortar, especially more than 50MPa.

  • PDF

Fundamental Characteristics of Concrete According to Fineness Modulus and Replacement Ratio of Crushed Sand (부순모래의 조립률 및 치환률에 따른 콘크리트의 기초 특성)

  • Yun, Yong-Ho;Choi, Jong-Oh;Lee, Dong-Gyu;Jung, Yong-Wook
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.3
    • /
    • pp.244-251
    • /
    • 2015
  • The paper evaluates the effect of the physical property, fineness modulus (FM) and replacement ratio of crushed sand on the characteristics of concrete. This is intended to use crushed sand from Daegu-Kyungbuk region as the fine aggregate of concrete. The experimental result indicates that the replacement ratio of crushed sand needs to be less than 50% to satisfy the mixed gradation of both natural and crushed sand when their FMs are 2.0 and 3.2, respectively. The slump of concrete with crushed sand increased as the replacement ratio of crushed sand increased, while the workability of concrete with the replacement ratio of more than 75% was significantly reduced. The air content and bleeding rate of concrete was reduced as the replacement ratio increased. Furthermore, due to the enhancement of the concrete adhesive regardless of the FM of crushed sand, compressive strength of concrete tended to improve as the replacement ratio increased.

Effects of Incineration Waste Ash and Gypsum Substitution on the Properties of Blast Furnace Slag Mortar using Recycled Aggregate (소각장 애쉬 및 석고치환이 고로슬래그 미분말 기반 순환골재 모르타르의 물성에 미치는 영향)

  • Han, Min Cheol;Han, Dong Yeop;Lu, Liang Liang
    • Journal of the Korea Institute of Building Construction
    • /
    • v.15 no.2
    • /
    • pp.161-167
    • /
    • 2015
  • Nowadays, all the world face to the global warming problems due to the emission of $CO_2$. From the previous studies, recycled aggregates were used as an alkali activator in blast furnace slag to achieve zero-cement concrete, and favorable results of obtaining strength were achieved. In this study, gypsum and incineration waste ash were used as the additional alkali activation and effects of the gypsum and incineration waste ash to enhance the performance of the mortar were tested. Results showed that although the replacement ratio of 0.5% of incineration waste ash and 20% of anhydrous gypsum resulted in the low of mortar at the early age, while it improved the later strength and achieved the similar strength to that of conventional mortar (at 91 days).

Evaluation Method of Healing Performance of Self-Healing Materials Based on Equivalent Crack Width (등가균열폭에 기반한 자기치유 재료의 치유성능 평가 방법)

  • Lee, Woong-Jong;Kim, Hyung-Suk;Choi, Sung;Park, Byung-Sun;Lee, Kwang-Myong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.3
    • /
    • pp.383-388
    • /
    • 2021
  • In this study, constant head water permeability test was adopted to evaluate self-healing performance of mortars containing inorganic healing materials which consist of blast furnace slag, sodium sulfate and anhydrite. Clinker powder and sand replaced for a part of cement and fine aggregates. On constant head water permeability test for self-healing mortars, unit water flow rate of mortar specimens were measured according to crack width and healing period. As a result of evaluating the healing performance of self-healing mortar, it was confirmed that with the initial crack width of 0.3mm, the healing rate at healing period of 28 days increased by more than 30%p compared to plain mortar, greatly improving the healing performance. Furthermore, the coefficient(α) which was estimated from the relationship between crack width and unit water flow rate was used for calculating equivalent crack width. By analyzing the correlation of healing rate and equivalent crack width, the time and initial crack width attaining healing target crack width were predicted.

Recycling of the Waste Rock and Tailings from Yangyang Iron Mine (양양철광산 선광 부산물의 순환자원화)

  • Jung, Moon Young;An, Yong Hyeon;Kim, Young Hun
    • Resources Recycling
    • /
    • v.25 no.4
    • /
    • pp.23-31
    • /
    • 2016
  • It was found that there was no problem in recycling by-products (waste rock and tailings) from Yangyang iron mine themselves through matter conversion because they are not hazardous according to results of KSLT method. In case of using tailings as sub-materials of cement, it recommended the use of less than 3% tailings dosage not to exceed 0.6% of total alkali ($R_2O$) content based on standard quality of portland cement (KS L 5201). Non sintered eco-brick corresponding to class 1 quality of recycled clay brick (KS I 3013) can replace 15% of cement with tailings and 100% of general fine aggregate with waste rock from iron mine. As mentioned above, recycling the by-products (waste rock and tailings) as sub-materials of cement and non sintered eco-brick could gain both environmental and economic benefits, that is, reduction of scale and maintenance cost of tailing ponds, decrease of energy use and $CO_2$ emission.

Blast Furnace Slag Powder High Volume Substitution Mortar Quality Increase Due To Changes in Desulfurized Plaster Processing Method (탈황석고의 처리방법 변화에 의한 고로슬래그 미분말 다량 치환 모르타르의 품질향상)

  • Song, Yuan-Lou;Park, Yong-Jun;Kim, Sang-sup;Lee, Dong-Yun;Jang, Duk-Bae;Han, Min-Cheol
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2015.11a
    • /
    • pp.55-56
    • /
    • 2015
  • In this research the processing method of Desulfurized Plaster is changed to cyclotomy, 0.3mm sieve analysis and 500℃ heat exposure, and by changing the mix rate of the binding agent to 0~20%, it was applied to mortar that used natural aggregate and blast furnace slag for testing. The test results showed that the sieve analysis and high heat exposure of the flow and air volume increased according to the increase of mixing rate of FGD while the cyclotomy decreased. The setting time accelerated as the mixing rate of FGD increased, and the compression strength increased to its maximum when the mixing rate of FGD was right around 10%, and especially showed a high trend with cyclotomy and sieve analysis.

  • PDF

An Experimental Study on the Quality Variation by the Number of Production of Recycled Sand and Mechanics Properties of Mortar using Sand Flux Apparatus (샌드플럭스 장치를 이용한 순환모래의 생산횟수별 품질변화 및 모르타르의 역학특성에 관한 실험적 연구)

  • Lee, Sang-Soo;Song, Ha-Young;Kim, Joon-Seok;Kim, Jae-Hwan;Lee, Jong-Suk
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.1
    • /
    • pp.81-88
    • /
    • 2009
  • This study has shown the tendency to enhance Sand Flux, a device of separating screening the foreign matter, for the recycling of construction waste possible to improve the quality of wet type production system meaningfully as part of research. As a result of experiment on the basic material properties, this study had a tendency to improve the quality and performance significantly in case of absolute surface dried density, 0.08mm sieve throughput, volume of clay lumps, and content of organic foreign matter. In addition, as a result of examining the quality characteristics of mortar, this study has shown the tendency that the flow and compressive strength more increased than the mortar using RS-II by utilizing RS-VI recycled sand produced finally through the device Sand Flux. As for the shrinkage properties, this study has shown the character the generation rate of crack of mortar using RS-IV recycled sand produced finally through the device Sand Flux.

  • PDF

Fundamental Characteristics of Concrete for Nuclear Power Plant Using Crushed Sand (부순모래 사용에 따른 원전 구조물용 콘크리트의 기초적 특성)

  • Park, Sung-Hak;Kim, Kyung-Hwan;Choi, Byung-Keol;Choi, Yun-Wang
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.2
    • /
    • pp.168-176
    • /
    • 2017
  • This study, as a research for using crushed sand as a fine aggregate of concrete for nuclear structures, we improved the performance of impact crusher in the existing crushed sand production process and adjusted grain size to conform to ASTM C 33 The shape and grain size characteristics of a crushed sand were examined and concrete was prepared according to the substitution ratio of the sand to investigate the properties of fresh concrete and hardened concrete. The experimental results show that most of the concrete characteristics are equivalent to those of concrete using only heavy sand. However, when the substitution rate of steel sand exceeds 50%, the amount of air, compressive strength and tensile strength are somewhat reduced.

Evaluation of Self-Compaction Property of Section Enlargement Strengthening Concrete (단면확대 보강 적용을 위한 콘크리트의 자기충전 성능 평가)

  • Hwang, Yong-Ha;Yang, Keun-Hyeok;Song, Keum-Il;Song, Jin-Kyu
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.3
    • /
    • pp.235-242
    • /
    • 2019
  • The objective of this study is to modify the mixture proportions of concrete that were developed for section enlargement strengthening elements using a specially designed binder composed of 5% ultra-rapid hardening cement, 10% polymer, and 85% ordinary portland cement in order to assign the self-compaction property to such concrete. The self-compaction abilities of concrete were estimated by the performance criteria specified in JSCE and EFNARC provions. Test results showed that the increase in the unit binder content at the consistent water-to-bider ratio led to increase in viscosity of fresh concrete but did not exhibit the decrease in the fluidity due to a greater viscosity. The mixture proportioning of self-compaction section enlargement concrete could be considered at the following conditions: unit binder contents of $430kg/m^3{\sim}470kg/m^3$ and fine aggregate-to-total aggregate ratios of 40%~46% at the water-to-binder ratio of 38%.

Watertightness and Durability Properties of Ultra Rapid Hardening Grout using Bottom-ash (잔골재 대체재로서 바텀애쉬를 이용한 초속경 그라우트재의 수밀성 및 내구특성)

  • Lee, Gun-Cheol;Oh, Dong-Uk;Cho, Byoung-Young;Kim, Young-Geun;Cho, Chung-Ki
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.3
    • /
    • pp.102-109
    • /
    • 2011
  • In this study, in order to develop ultra rapid hardening mortar(URHM) for tunnel repairs using bottom ash of low recycle ratio and Admixture as Eco concept, watertightness and durability properties of URHM on temperature condition of construction field were performed. Test result, seepage quantity and water absorption coefficient regarding watertightness of URHM were as in the following : series II > series I. Seepage quantity for the standard condition were smaller than low temperatures. all specimens were satisfied below 20g as standards of seepage quantity on KS F 4042. Because of the decrease of unit cement content by to replacement of blast furnace slag, the neutrlization resistance for durability properties was reduced. The result of alkali resistance and acide resistance, compressive strengths for specimens soaked in calcium hydroxide solution of seriesI were lower than compressive strengths for specimens not soaked. On the other hand, the case of series II show that the deterioration of compressive strengths for specimens was not almost showed. Compressive strengths of specimens soaked were similar with specimens not soaked except series II-C in $5^{\circ}C$. Therefore, specimens using both blast furnace slag and bottom ash were good in alkali resistance and acide resistance.

  • PDF