Evaluation of SO2 Absorption Efficiency for Calcined Oyster Shell Slurry Using a Simulated Spray Type-flue Gas Desulfurization (FGD) System: A Comparative Study with Limestone Slurry (모사 Spray Type 배연탈황설비를 이용한 소성패각 슬러리의 SO2 흡수능 평가: 석회석과의 비교연구)

  • Kim, Seok-Hwi;Hong, Bum-Uh;Lee, Jin-Won;Cha, Wang-Seok;Kim, Kangjoo;Moon, Bo-Kyung
    • Economic and Environmental Geology
    • /
    • v.52 no.2
    • /
    • pp.119-128
    • /
    • 2019
  • About 300,000 tones of oyster shell are annually produced in Korea and, thus, a massive recycling plan is required. Many desulfurizing studies using oyster shells with chemical composition of $CaCO_3$ have been performed so far; however, most of them have focused on dry desulfurization. This study investigates the possibility of using oyster shells for wet desulfurization after calcination. For this, a simulated wet desulfurization facility of spray type was devised and compared the SOx-stripping characteristics of calcined oyster shell with those of limestone. The calcined oyster shell slurry indicate a better desulfurizability than the slurries of raw shell or limestone because the oyster shell transformed to a more reactive phase ($Ca(OH)_2$) by the calcination and hydration. Because of this reason, when the calcined oyster shell slurries were used, the reaction residue showed the higher gypsum ($CaSO_4{\cdot}2H_2O$) contents than any other cases. In the continuous desulfurization experiments, calcined oyster shell slurry showed a wider pH variation than limestone or raw oyster shell slurries, another clear indication of high reactivity of calcined oyster shells for $SO_2$ absorption. Our study also shows that the efficiency of wet desulfurization can be improved by the use of calcined oyster shells.

Effect of limestone addition on mechanical properties of ceramic tiles with fly ash (플라이애시가 첨가된 도자타일 성능에 석회석 함량이 미치는 효과)

  • Lee, Jin-Wook;Han, Kyu-Sung;Hwang, Kwang-Taek;Kim, Jin-Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.28 no.6
    • /
    • pp.256-262
    • /
    • 2018
  • A great amount of fly ash, which is a waste from a thermal power plant, has not been appropriately recycled until now. Landfill of flay ash causes environmental pollution and enormous economic costs. In this study, manufacturing of architectural ceramic tile was investigated replacing fly ash with clay raw material. The properties of porcelain tile was analyzed after manufacturing porcelain tile with mineral based glaze and fast firing process. In particular, the effect of the fly ash addition on the properties of ceramic tile was investigated by increasing the amount of limestone addition. Porcelain tile with fly ash showed excellent bending strength, water absorption, warping and abrasion resistance. However, a significant decrease in durability was observed through the autoclave test. Addition of limestone increased the water absorption, twisting and hydration expansion of the ceramic tile, but it was confirmed that the durability of the ceramic tile with fly ash was greatly improved. In conclusion, recycled architectural ceramic tiles, which can meet domestic construction standards, could be manufactured with the addition of fly ash and limestone.

Manufacturing Properties and Hardening Characteristic of CO2 Reactive Hardening Cement (이산화탄소 반응경화 시멘트 제조 및 경화특성 연구)

  • Ki-Yeon Moon;Byung-Ryeol Kim;Seung-Han Lee;Moon-Kwan Choi;Kye-Hong Cho;Jin-Sang Cho
    • Resources Recycling
    • /
    • v.31 no.6
    • /
    • pp.52-59
    • /
    • 2022
  • Calcium silicate based cement (CSC) is a low-carbon cement that emits less CO2 by up to 70% compared to ordinary Portland cement during its manufacture. Most developed countries have commercialized CSC, whereas Korea is still investigating the manufacturing characteristics and basic properties of CSC. This paper provides a review of methods for manufacturing CSC using domestic raw materials and discusses the possibility of CSC localization based on an evaluation of the basic physical properties of manufactured CSC. The experimental results of this study indicate that the primary mineral components of CSC were CS, C3S2 C2S, and unreacted SiO2. This suggests the possibility of manufacturing CSC using domestic raw materials that exhibit mineral compositions similar to that of theoretical CSC. The compressive strength of CSC mortar is less than 1MPa at the age of 7 d under wet curing. This implies that hydration does not affect the property development of CSC mortar. Meanwhile, during carbonation curing, the compressive strength is 56 MPa or higher after 7 d, which indicates excellent early strength development. Furthermore, results of Thermogravimetric Analysis Differential scanning calorimetry (TG/DSC) show that a significant amount of CaCO3 is formed, which is consistent with the results of previous studies. This implies that carbonation is associated significantly with the properties of CSC.

Research on manufacturing secondary construction products using in-situ carbonation technology (In-situ 탄산화 기술이 적용된 콘크리트 2차제품 제조 연구)

  • Hye-Jin Yu;Sung-Kwan Seo;Woo-Sung Yum
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.33 no.6
    • /
    • pp.226-233
    • /
    • 2023
  • In this study, the basic physical properties and microstructure of concrete interlocking blocks with amount of different CO2 gas injection were analyzed according to determine the applicability of In-situ carbonation technology to construction secondary products. The amount of carbon dioxide gas injection was selected as 0, 0.1, 0.3, 0.5, 0.7 wt.% compared to cement amount. A lab-scale press equipment was designed to apply developed carbonation technology to real construction site. And mixer for stable CO2 gas injection was designed. Using the designed devices, CO2 gas injected samples were created and physical property of samples were performed. As a result of the physical property test, as the CO2 injection amount increased to 0.3 %, it showed higher strength behavior compared to the original mix. And more than 0.5 % samples showed lower strength behavior than original sample, but they satisfied the standard of concrete interlocking block. This results were determined that CO2 injection contributed to the creation of hydrates such as C-S-H. Therefore, the possibility of applying carbonation technology, which injects CO2 during mixing, to various secondary construction products was confirmed.

Effect of Spray and Immersion Treatment of Mono-Ammonium Phosphate Solution on Properties of Recycled Fine Aggregate (일인산 암모늄 수용액 분사 및 침지처리가 순환잔골재의 물성 변화에 미치는 영향)

  • Seong-Jun Kwon;Seong-Ho Kim;Chan-Woo Park;Chul-Woo Chung
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.12 no.3
    • /
    • pp.314-321
    • /
    • 2024
  • Due to the depletion of natural aggregate resources, the use of recycled aggregates became an urgent issue. Microcracks generated during production of recycled aggregate and cement paste attached to the surface of aggregate have been the biggest obstacles to promote the use of recycled aggregate. To alleviate such problem, this study attempted the spray and immersion treatment of recycled fine aggregate using mono-ammonium phosphate solution, which is known to be effective for reducing the pH of recycled aggregate. The changes in physical properties before and after treatment were observed, and the compressive strength of mortar specimen was evaluated. According to the experimental results, the absorption capacity of the recycled fine aggregate increased with reduction in pH after mono-ammunium phosphate treatment. Calcium hydroxide and ettringite was removed, and skeletal density of recycled fine aggregate increased due to the formation of hydroxyapatite. Despite the increase in absorption capacity, the compressive strength of the mortar increased and it seems to be associated with the increase in adhesion strength at the interface between cement paste and recycled fine aggregate. When the concentration of ammonium monophosphate aqueous solution was excessive (immersion: 15% and 20%, spraying 20%), the compressive strength of the mortar decreased, which seemed to be related to the increase in the absorption capacity caused by the the excessive dissolution of the hydration products such as portlandite and ettringite.

Studies on the Physical and Chemical Denatures of Cocoon Bave Sericin throughout Silk Filature Processes (제사과정 전후에서의 견사세리신의 물리화학적 성질변화에 관한 연구)

  • 남중희
    • Journal of Sericultural and Entomological Science
    • /
    • v.16 no.1
    • /
    • pp.21-48
    • /
    • 1974
  • The studies were carried out to disclose the physical and chemical properties of sericin fraction obtained from silk cocoon shells and its characteristics of swelling and solubility. The following results were obtained. 1. The physical and chemical properties of sericin fraction. 1) In contrast to the easy water soluble sericin, the hard soluble sericin contains fewer amino acids include of polar side radical while the hard soluble amino acid sach as alanine and leucine were detected. 2) The easy soluble amino acids were found mainly on the outer part of the fibroin, but the hard soluble amino acids were located in the near parts to the fibroin. 3) The swelling and solubility of the sericin could be hardly assayed by the analysis of the amino acid composition, and could be considered to tee closely related to the compound of the sericin crystal and secondary structure. 4) The X-ray patterns of the cocoon filament were ring shape, but they disappeared by the degumming treatment. 5) The sericin of tussah silkworm (A. pernyi), showed stronger circular patterns in the meridian than the regular silkworm (Bombyx mori). 6) There was no pattern difference between Fraction A and B. 7) X-ray diffraction patterns of the Sericin 1, ll and 111 were similar except interference of 8.85A (side chain spacing). 8) The amino acids above 150 in molecular weight such as Cys. Tyr. Phe. His. and Arg. were not found quantitatively by the 60 minutes-hydrolysis (6N-HCI). 9) The X-ray Pattern of 4.6A had a tendency to disappear with hot-water, ether, and alcohol treatment. 10) The partial hydrolysis of sericin showed a cirucular interference (2A) on the meridian. 11) The sericin pellet after hydrolysis was considered to be peptides composed with specific amino acids. 12) The decomposing temperature of Sericin 111 was higher than that of Sericin I and II. 13) Thermogram of the inner portioned sericin of the cocoon shell had double endothermic peaks at 165$^{\circ}C$, and 245$^{\circ}C$, and its decomposing temperature was higher than that of other portioned sericin. 14) The infrared spectroscopic properties among sericin I, II, III and sericin extracted from each layer portion of the cocoon shell were similar. II. The characteristics of seriein swelling and solubility related with silk processing. 1) Fifteen minutes was required to dehydrate the free moisture of cocoon shells with centrifugal force controlled at 13${\times}$10$^4$ dyne/g at 3,000 R.P.M. B) It took 30 minutes for the sericin to show positive reaction with the Folin-Ciocaltue reagent at room temperature. 3) The measurable wave length of the visible radiation was 500-750m${\mu}$, and the highest absorbance was observed at the wave length of 650m${\mu}$. 4) The colorimetric analysis should be conducted at 650mu for low concentration (10$\mu\textrm{g}$/$m\ell$), and at 500m${\mu}$ for the higher concentration to obtain an exact analysis. 5) The absorbing curves of sericin and egg albumin at different wave lengths were similar, but the absorbance of the former was slightly higher than that of the latter. 6) The quantity of the sericin measured by the colorimetric analysis, turned out to be less than by the Kjeldahl method. 7) Both temperature and duration in the cocoon cooking process has much effect on the swelling and solubility of the cocoon shells, but the temperature was more influential than the duration of the treatment. 8) The factorial relation between the temperature and the duration of treatment of the cocoon cooking to check for siricin swelling and solubility showed that the treatment duration should be gradually increased to reach optimum swelling and solubility of sericin with low temperature(70$^{\circ}C$) . High temperature, however, showed more sharp increase. 9) The more increased temperature in the drying of fresh cocoons, the less the sericin swelling and solubility were obtained. 10) In a specific cooking duration, the heavier the cocoon shell is, the less the swelling and solubility were obtained. 11) It was considered that there are differences in swelling or solubility between the filaments of each cocoon layer. 12) Sericin swelling or solubility in the cocoon filament was decreased by the wax extraction.. 13) The ionic surface active agent accelerated the swelling and solubility of the sericin at the range of pH 6-7. 14) In the same conditions as above, the cation agent was absorbed into the sericin. 15) In case of the increase of Ca ang Mg in the reeling water, its pH value drifted toward the acidity. 16) A buffering action was observed between the sericin and the water hardness constituents in the reeling water. 17) The effect of calcium on the swelling and solubility of the sericin was more moderate than that of magnecium. 18) The solute of the water hardness constituents increased the electric conductivity in the reeling water.

  • PDF

A Review on the Recycling of the Concrete Waste Generate from the Decommissioning of Nuclear Power Plants (원전 해체 콘크리트 폐기물의 재활용에 대한 고찰)

  • Jeon, Ji-Hun;Lee, Woo-Chun;Lee, Sang-Woo;Kim, Soon-Oh
    • Economic and Environmental Geology
    • /
    • v.54 no.2
    • /
    • pp.285-297
    • /
    • 2021
  • Globally, nuclear-decommissioning facilities have been increased in number, and thereby hundreds of thousands of wastes, such as concrete, soil, and metal, have been generated. For this reason, there have been numerous efforts and researches on the development of technology for volume reduction and recycling of solid radioactive wastes, and this study reviewed and examined thoroughly such previous studies. The waste concrete powder is rehydrated by other processes such as grinding and sintering, and the processes rendered aluminate (C3A), C4AF, C3S, and ��-C2S, which are the significant compounds controlling the hydration reaction of concrete and the compressive strength of the solidified matrix. The review of the previous studies confirmed that waste concretes could be used as recycling cement, but there remain problems with the decreasing strength of solidified matrix due to mingling with aggregates. There have been further efforts to improve the performance of recycling concrete via mixing with reactive agents using industrial by-products, such as blast furnace slag and fly ash. As a result, the compressive strength of the solidified matrix was proved to be enhanced. On the contrary, there have been few kinds of researches on manufacturing recycled concretes using soil wastes. Illite and zeolite in soil waste show the high adsorption capacity on radioactive nuclides, and they can be recycled as solidification agents. If the soil wastes are recycled as much as possible, the volume of wastes generated from the decommissioning of nuclear power plants (NPPs) is not only significantly reduced, but collateral benefits also are received because radioactive wastes are safely disposed of by solidification agents made from such soil wastes. Thus, it is required to study the production of non-sintered cement using clay minerals in soil wastes. This paper reviewed related domestic and foreign researches to consider the sustainable recycling of concrete waste from NPPs as recycling cement and utilizing clay minerals in soil waste to produce unsintered cement.