Development of the Water-borne Separation Media Polymer for a Moving Historic Sites (자기분산형 수용성 에폭시를 이용한 유구 이전용 박리제의 개발)

  • Han, Won-Sik;Hong, Tae-Kee;Lim, Sung-Jin;Wi, Koang-Chul
    • Journal of Conservation Science
    • /
    • v.25 no.2
    • /
    • pp.171-178
    • /
    • 2009
  • When we considered the superior ability of the semi-water soluble urethane 1st transcription and final epoxy products, the stability for moving historic sites depend on physical properties and the peel off state of separation media. In this paper, we synthesised three type of water-borne epoxy solution without using a surfactant, and investigated the peel off state, physical properties, and the state between urethane surface and epoxy surface after exfoliation. The life time of water-borne separation media is over the 60 days. When it is used the 30% solution of water-borne separation media, it made good separation of urethane pre-products surface and epoxy final product surface and no color change. The separation tension pressure is about 15~50 kg/$cm^2$ and there is no surface whitewash phenomenon. We suggest that this water-borne epoxy will be best material as separation media of low viscosity type.

  • PDF

A Study on the Characteristics and Cleanliness of Fluidic Strip Process of Environment-Friendly Aqueous Stripper (친환경 수계 박리액의 유동박리 공정 특성 및 청정성 연구)

  • Lee, Ki-Seong;Lee, Jaeone;Kim, Young Sung
    • Clean Technology
    • /
    • v.24 no.3
    • /
    • pp.175-182
    • /
    • 2018
  • In this research, we investigated the cleanliness by optimizing the water content of the aqueous stripper in fluidic strip process. The stripping properties of the photoresist with optimized aqueous stripper were compared with the commercial organic stripper. The stripping performance was evaluated by electrical and optical characteristics on the surface of the transparent electrode that compare with stripped the transparent electrode surface and the rare surface before patterning by the photoresist. As a result of the photoresist stripping process of the organic stripper and the aqueous stripper optimized for water content, the aqueous stripper exhibited better electrical and optical characteristics than the organic stripper. In the case of the fluidic strip process with organic stripper, the photoresist dissolves in the stripper solution during stripping which can cause re-adsorption by contamination. Whereas that the aqueous stripper under development seems to decrease the photoresist dissolution in the stripper solution. Because the cyclodextrin contained in the stripper captures organic photoresist into hall of cyclodextrin which stripped through swelling and tearing. The photoresist residue captured by the cyclodextrin can be filtered. After the fluidic stripping process by different chemical stripping mechanism, the cleanliness of the organic stripper and aqueous stripper was compared and analyzed.

Effect of Antistripping Agent on the Enhancement of Resistance to Moisture Damage of Asphalt Mixture (아스팔트 혼합물의 내수분손상 향상에 대한 박리방지제의 효과)

  • Lee, Eun-Kyoung;Choi, Sei-Young
    • Journal of Adhesion and Interface
    • /
    • v.10 no.4
    • /
    • pp.182-190
    • /
    • 2009
  • In this work, effect of antistrip additives to reduce moisture damage of asphalt mixture were studied. Asphalt antistripping agents were prepared by condensation of formaldehyde with tetraethylene pentamine (TEPA), triethylenetetramine (TETA) and bis(hexamethylene)-triamine (BHMT), respectively. And also the metal type antistripping agent was prepatred by neutralization of stearic acid or palmitic acid with metal hydroxide. Mechanical characteristics of the asphalt mixture added antistripping agent were evaluated with Marshall stability, submerging residuals and coating rate. It was found that antistripping agent prepared in this study reduced moisture damages of asphalt mixtures. In particular, asphalt mixtures added BHMT and C/S (Calcium stearate hydroxide) antistripping agent showed highest submerging and coating rate. Because BHMT and C/S type antistripping agent was to improve bonding between asphalt and aggregate owing to increase of amine concentration and role of metal surfactant.

  • PDF

The Effects of Surface Coating Material for Aluminum Form on Surface Quality of the Concrete (알루미늄 거푸집 표면코팅재가 콘크리트 표면품질에 미치는 영향)

  • Han, Cheon-Goo;Park, Jae-Soon
    • Journal of the Korea Institute of Building Construction
    • /
    • v.10 no.3
    • /
    • pp.57-64
    • /
    • 2010
  • This study is to analyze the effects of aluminum form surface coating material on surface quality of concrete. When observing the surface quality of concrete affected by the change of aluminum form surface coating material, in general, as the number of use of the coating material increased, the surface quality of concrete decreased and good surface quality was shown in plywood (hereinafter PW). For epoxy (hereinafter EP) resin, when applying form remover, good surface quality was shown. For the surface roughness of concrete by the application form oil of form remover and the number of use of the coating material, as the number of use increased, highest surface roughness value was shown which meant the leveling was bad, but the surface roughness value in EP and PW was the lowest. Just for EP, when applying form remover, surface roughness value was low. For the number of void for concrete by the application of form remover and the number of use of the coating material, In general, the number of void which was generated when applying form oil the remover decreased.

Study on the Peel off Style Low Viscosity Epoxy and Separation Media for a Moving Historic Sites (유구 이전 전용 저점도형 에폭시와 박리제에 관한 연구)

  • Han, Won-Sik;Hong, Tae-Kee;Park, Gi-Jung;Lim, Sung-Jin;Wi, Koang-Chul
    • Journal of Conservation Science
    • /
    • v.24
    • /
    • pp.37-42
    • /
    • 2008
  • Stability of the moving historic sites have something to do with the degree of easiness of work as well as physical property of polymer product. These agents should be able to use without the effect of outer environments like water or low temperature and must have stability during progress of working the peel off Urethane pre-product from Epoxy surface. So, we synthesized low viscosity epoxy resin and hardener with best physical quality and separation media for the moving of historical sites. These products have very good tension strength, adhesion strength, low viscosity and various physical properties that the users want. Particularly, separation media products have good separation of Urethane pre-products surface and Epoxy final product surface.

  • PDF

Effect of Urea on the Exfoliation of Juvenile Abalone, Haliotis discus Reeve (농업용 요소비료를 이용한 까막전복, Haliotis discus Reeve 마취 및 박리효과)

  • 한석중;김봉래;원승환;김재우
    • Journal of Aquaculture
    • /
    • v.16 no.4
    • /
    • pp.223-228
    • /
    • 2003
  • An exfoliation, the detachment of juvenile abalones from a culture substrate, is essential for selection and population density control in abalone culture. Physical instruments and anesthetics are currently available for the exfoliation but the latter is regarded as more effective in reducing physical damage to the animals. In the present study, urea ($Co(NH_2)_2$), a chemical fertilizer, was selected as a anesthetic, and its optimal concentration and sea water temperature for exfoliation of Haliotis discus were determined in order to develop an exfoliation technique which is more economical and effective. A 97% cumulated exfoliation rate was observed within 3 min at all temperatures observed when the concentration rate of urea was 9∼15%. This range of urea concentration can be ideal for both exfoliation and recovery. Also it was found that the higher concentration of urea and temperature the higher exfoliation rate, however, these conditions reduced the recovery rates of the animals tested. These results could indicate that urea is a good tool for exfoliation of various species of young abalones, and urea could substitute for all techniques and anesthetics methods currently available for abalone exfoliation.

농업용 요소비료에 의한 시볼트전복, Haliotis gigantea의 마취 박리 효과

  • 한석중;원승환
    • Proceedings of the Korean Society of Fisheries Technology Conference
    • /
    • 2003.05a
    • /
    • pp.181-182
    • /
    • 2003
  • 생물에게 물리적인 손상(physical damage)이나 stress를 주지 않기 위한 마취제로서의 역할은 매우 중요하다. 특히 전복은 어류와는 달리 부착기질과 은신처를 이용하여 부착생활을 하기 때문에 무게측정(weighting), 표지(tagging), 선별(selection), 밀도 조절 등을 위해서 박리작업은 반드시 필요하다. 따라서 본 연구는 요소비료(CO(NH$_2$)$_2$)를 마취제로 이용하여 요소비료의 농도와 수온 등 물리적 요인이 시볼트 전복 Haliotis gigantea의 박리율과 회복율에 미치는 영향을 조사함으로서 경제적이며 효과적인 박리 기술을 개발하고자 하였다. (중략)

  • PDF

Exfoliation of abalone, Haliotis discus hannai by commercial exfoliating reagents (시판 전복박리제의 박리 효과)

  • Kim, Wi-Sik;Kang, Min-Ho;Kim, Jong-Oh;Lee, Si-Woo;Kim, Jung;Hwang, Doo-Jin;Oh, Myung-Joo
    • Journal of fish pathology
    • /
    • v.26 no.2
    • /
    • pp.117-121
    • /
    • 2013
  • Three commercial exfoliating reagents, product A (main components: citric acid and vitamin C), B (herb) and C (nicotinamide), were used to study their exfoliation effect on abalone, Haliotis discus hannai from the substrate. The exfoliating reagents A, B, C and oxytetracycline (OTC, control) of 6-31.25 g/L and 12-37.5 g/L exfoliated 81.2-84.8% and 90.3-95% of abalone, respectively. Post-treatment recovery time for the abalone was similar for all the reagents except product C. Recovery period for the abalone immersed in OTC for 5-20 second was slightly shorter than the reagents A, B and C; however, no mortality was observed in any group except with the reagents B (concentration: 20 g/L, immersion time: 5 sec) and C (12 g/L, 10 and 20 sec) that showed negligible mortality of 3.3%. Higher concentration and longer treatment with the reagents resulted in longer recovery time of the detached abalone. Although abalone exposed to the reagents needs slightly longer time to recover than that to OTC, the exfoliation effect is much similar. These results indicate that the commercial exfoliating reagents can replace OTC to detach abalone, though they need to be cautiously handled.

A study on the adhesion of HTPB liner and PCP propellant (HTPB 라이너와 PCP 추진제와의 접착에 관한 연구)

  • 홍명표;서태석;임유진
    • Journal of the Korean Society of Propulsion Engineers
    • /
    • v.5 no.3
    • /
    • pp.60-70
    • /
    • 2001
  • The study of compatible liner with ADP-505 propellant based PCP was performed. HTPB/DDl was chosen as a binder of liner in order to prohibit migration of nitroester plasticizer from propellant. The possible formulations for liner were screened by peel test of EPDM insulation/liner, propellant/liner and insulation/liner/propellant. Also, the adhesion tests including tension and shear were conducted. The adhesion of liner and propellant fumed out to be very good. The peel value was shown 1.5∼1.8 daN/cm, tensile force was 5.5∼6.0bar and shear force was 4.2∼5.0bar. In the samples of insulation/liner/propellant, they also have shown good adhesion properties. The peel, tensile and shear strength were 1.8 daN/cm, 5.0∼6.0bar and 4.5∼5.0bar, respectively.

  • PDF

Adhesive and Removable Characteristics of UV Curable Adhesive (자외선 경화형 점착제의 접착 및 재박리 특성)

  • Kim, In Beom;Lee, Myung Cheon
    • Korean Chemical Engineering Research
    • /
    • v.46 no.1
    • /
    • pp.76-81
    • /
    • 2008
  • UV curable pressure sensitive adhesive (PSA) was made by blending the di-functional or hexa-functional urethane-acrylate oligomer with synthesized acrylic PSA. The change of adhesive property and removability were investigated at various oligomer contents under each oligomer. As the content of oligomer increased, the peel strength was increased before UV irradiation, but it was decreased after UV irradiation. Also, it was observed that the peel strength increased with decrease of storage modulus (G'), and that loss factor (tan ${\delta}$) of the adhesive material affected the adhesive properties and removability.