• Title/Summary/Keyword: 모합금

Search Result 202, Processing Time 0.035 seconds

A Study on the Fabrication of 2700 Series Al-alloy Sintered for Automobile Application (자동차 부품용 2700계열 Al소결체 제작에 관한 연구)

  • Lim, Tae-Whan;Jang, Tae-Suk
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.12 no.12
    • /
    • pp.5438-5442
    • /
    • 2011
  • In order to use as weight-reduced sintered parts for automobiles, mechanical properties of sintered compacts of 2712 Al-alloys containing 0, 10, 20, and 33% ceramics, respectively, were investigated in this study. (1)Regardless of ceramic contents, all sintered compacts possessed 4~7% pores. (2)After aging the compacts sintered for 12 minutes, tensile strength of the 2712 Al-alloys containing 0, 10, 20, and 33% ceramics was 165, 260, 256, and 166 N/$mm^2$, respectively, whereas those aged after sintering for 30 minutes exhibited the tensile strength of 186, 229, 219, and 202 N/$mm^2$, respectively. In addition, the 2712 sintered compact containing 10% ceramics showed the maximum elongation of about 3.6%, (3)After aging the 10% ceramic-containing sintered compacts reached a maximum apparent hardness ($H_RF$) of 97. (4)The minimum wear volume ($174{\times}10^{-3}mm^3$) was shown in the 10% ceramic-containing 2712 sintered compact after aging. From these results, the 2712 sintered compact containing 10% ceramics thought to be the most suitable one for the fabrication of aluminum engine part.

Preparation of Matte with Pyrite and Chalcopyrite as sulfur source and Leaching behaviour (황(黃) 원료(原料)로서 pyrite와 chalcopyrite를 사용(使用)한 matte 상(相)의 제조(製造) 및 침출특성(浸出特性))

  • Park, Kyung-Ho;Nam, Chul-Woo;Chang, Jong-Sin;Ahan, Sung-Chen;Kim, Hong-In
    • Resources Recycling
    • /
    • v.17 no.1
    • /
    • pp.51-58
    • /
    • 2008
  • Artificial mattes were prepared with adding pyrite or chalcopyrite as sulfur sources with Cu-Ni-Co-Fe alloy. The major phases identified by X-ray diffraction pattern were $(FeSi)_9S_8$, $CuFeS_2$, FeS, $Co_4S_3$, $Ni_3S_2$ and $Cu_2S$ for both mattes, and the matte prepared by adding chalcopyrite showed the higher peak of $Cu_2S$ due to high content of copper. Under optimum conditions, more than 95% copper, 90% nickel and 90% cobalt were extracted into leaching solution and sulfur concentration in the mattes did not much affect the leaching efficiency of the metals. The increase of the amount of pyrite or chalcopyrite added decreased pH in leaching solution and increased the concentration of iron ion dissolved in the leaching solution and the amount of residue.

An Experimental Study on the Evaluation of EMP Shielding Performance of Concrete Applied with ATMSM Using Zn-Al Alloy Wire (Zn-Al 합금 선재를 이용한 금속용사 공법 적용 콘크리트의 전자파 차폐 성능 평가에 관한 실험적 연구)

  • Choi, Hyun-Jun;Park, Jin-Ho;Min, Tae-Beom;Jang, Hyun-O;Lee, Han-Seung
    • Journal of the Korea Institute of Building Construction
    • /
    • v.19 no.3
    • /
    • pp.209-217
    • /
    • 2019
  • EMP (Electromagnetic Pulse) usually means High Power Electromagnetic Wave (HPEM). In the case of the shielding plate against the EMP, there is a possibility of deterioration of the electromagnetic wave shielding performance due to the skill of the constructor, bad construction, deformation of the shielding plate at the connection portion (joint portion). The inefficient use of space due to the separation distance is also pointed out as a problem. Therefore, this study aims to derive the optimum electromagnetic shielding condition by applying ATMSM to concrete as a part of securing electromagnetic wave shielding performance with reflection loss against concrete wall. Experimental parameters included concrete wall thickness and application of Zn-Al ATMSM. For the concrete wall, the wall thickness was 100 to 300mm, which is generally applied, and experimental parameters were set for the application of Zn-Al metal spraying method to evaluate electromagnetic shielding performance. Experimental results showed that as the thickness increases, the electromagnetic shielding performance increases due to the increase of absorption loss. In addition, after the application of Zn-Al ATMSM, the average shielding performance increased by 56.68 dB on average, which is considered to be increased by the reflection loss of the ATMSM. In addition, it is considered that the shielding performance will be better than that when the conductive mixed material and the ATMSM are simultaneously applied.

Fabrication of Porous Cu Layers on Cu Pillars through Formation of Brass Layers and Selective Zn Etching, and Cu-to-Cu Flip-chip Bonding (황동층의 형성과 선택적 아연 에칭을 통한 구리 필라 상 다공성 구리층의 제조와 구리-구리 플립칩 접합)

  • Wan-Geun Lee;Kwang-Seong Choi;Yong-Sung Eom;Jong-Hyun Lee
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.30 no.4
    • /
    • pp.98-104
    • /
    • 2023
  • The feasibility of an efficient process proposed for Cu-Cu flip-chip bonding was evaluated by forming a porous Cu layer on Cu pillar and conducting thermo-compression sinter-bonding after the infiltration of a reducing agent. The porous Cu layers on Cu pillars were manufactured through a three-step process of Zn plating-heat treatment-Zn selective etching. The average thickness of the formed porous Cu layer was approximately 2.3 ㎛. The flip-chip bonding was accomplished after infiltrating reducing solvent into porous Cu layer and pre-heating, and the layers were finally conducted into sintered joints through thermo-compression. With reduction behavior of Cu oxides and suppression of additional oxidation by the solvent, the porous Cu layer densified to thickness of approximately 1.1 ㎛ during the thermo-compression, and the Cu-Cu flip-chip bonding was eventually completed. As a result, a shear strength of approximately 11.2 MPa could be achieved after the bonding for 5 min under a pressure of 10 MPa at 300 ℃ in air. Because that was a result of partial bonding by only about 50% of the pillars, it was anticipated that a shear strength of 20 MPa or more could easily be obtained if all the pillars were induced to bond through process optimization.

Evaluation of Wear Characteristics of Low-alloy Steel Brake Discs for High Energy Capacity (고에너지용 저합금강 제동디스크의 마모 특성 평가)

  • Dong-gyu Lee;Kyung-il Kim;Gue-Serb Cho;Kyung-taek Kim
    • Journal of Advanced Navigation Technology
    • /
    • v.28 no.4
    • /
    • pp.532-537
    • /
    • 2024
  • In this study, wear characteristics and microstructure changes due to changes in alloy composition of Ni-Cr-Mo-V and Ni-Cr-Mo low-alloy steels used in brake discs for transportation system such as aircraft and high-speed trains. As a result of the hardness test, the hardness of C-Mo-V steel was the highest at 39.4±0.9HRc, and the hardness of Ni-Cr-Mo steel was the lowest at 32.4±0.6HRc. The friction coefficient tended to decrease as the vertical load increased. At a vertical load of 1 N, the friction coefficient of Ni-Cr-Mo steel was the highest at 0.842, and at a vertical load of 5 N, Mn-Cr-V steel was the highest at 0.696. Ni-Cr-Mo showed the largest wear scar width, depth, and wear amount, with a width of 711 ㎛, a depth of 8.24 ㎛, and a wear amount of 11 mg under a vertical load of 1 N, and a width of 1,017 ㎛, a depth of 19.17 ㎛, and a wear amount of 17 mg under a vertical load of 5 N. As a result of wear mechanism analysis, ploughing, delamination, and adhesion in all specimens, with plastic deformation being more prominently observed in Ni-Cr-Mo.

A Study on the Stress Distribution of Tooth/Implant Connected with Konus Telescope Denture Using 3-Dimensional Finite Element Method (이중관으로 연결된 자연치와 임플랜트의 악골 내응력분포에 관한 3차원 유한요소분석)

  • Lee, Su-Ok;Choi, Dae-Gyun;Kwon, Kung-Rock;Woo, Yi-Hyung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.46 no.4
    • /
    • pp.381-395
    • /
    • 2008
  • Purpoose: For decades dental implants have been used widely in the field of prosthetic dentistry. However there is confusion when establishing treatment plans in cases where some teeth are remained but an insufficient number of implants can be used due to limited anatomical status and ecomomical problems. Many clinicians have tried to connect natural teeth and implants, and it still has controversy. But, there have been few studies on mechanical analysis of connecting natural teeth and implants with konus telescopic removable partial dentures. The purpose of this study was to analyze the stress distribution of prosthesis, abutment and alveolar bone when teeth and implants were connected with the konus telescopic denture, by means of 3-dimensional finite element analysis. Material and methods: The assumption of this study was that there were 2 mandibular canine (11 mm in length, 4 mm in diameter) and 2 implants(10 mm in length, 4 mm in diameter) which are located in the second premolar region. The mandible, teeth, implants, abutments, and connectors are modeled, and analyzed with the commercial software, ANSYS Version 8.1(Swanson, Inc., USA). The control group used implants instead of natural teeth. 21038 elements, 23544 nodes were used in experimental group and 107595 elements, 21963 nodes were used in control group, Stress distribution was evaluated under 150 N vertical load on 3 experimental conditions - between teeth and implants (Load case 1), posterior to implants (Load case 2), between natural teeth (Load case 3). Results: 1. In all load cases, higher von mises stress value was observed in the experimental group. 2. Maximum von miss stress observed in all load cases and all locations were as follows ; a. 929.44 Mpa in the experimental group, 640.044 Mpa in the control group in outer crown and connector - The experimental group showed 1.45 times high value compared with the control group. b. 145,051 Mpa in the experimental group, 142.338 Mpa in the control group in abutment - The experimental group showed 1.02times high value compared with the control group. c. 32.489 Mpa in the experimental group, 25.765 Mpa in the control group in alveolar bone - The experimental group showed 1.26times higher value compared with the control group. 3. All maximum von mises stress was observed in load case 2, and maxim von mises stress in alveolar bone was 32.489 Mpa at which implant failure cannot occur. 4. If maximum von mises stress is compared between two groups, the value of the experimental group is 1.02 times higher than the control group in abutment, 1.26 times higher than the control group in alveolar bone. Conclusion: If natural teeth and implants are connected with the konus telescopic denture, maximum stress will be similar in abutment, 1.26 times higher in alveolar bone than the control group. With this result, there may be possible to make to avoid konus telescopic dentures where natural teeth and implants exist together.

The biofilm removal effect of MnO2-diatom microbubbler from the dental prosthetic surfaces: In vitro study (치과 보철 재료 표면에서 MnO2-diatom microbubbler의 세균막 제거 효과 연구: In vitro study)

  • Lee, Eun-Hyuk;Seo, Yongbeom;Kwon, Ho-Bum;Yim, Young-Jun;Kong, Hyunjoon;Kim, Myung-Joo
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.58 no.1
    • /
    • pp.14-22
    • /
    • 2020
  • Purpose: The aim of this study is to evaluate the effectiveness of MnO2-diatom microbubbler (DM) on the surface of prosthetic materials as a mouthwash by comparing the biofilm removal effect with those previously used as a mouthwash in dental clinic. Materials and methods: DM was fabricated by doping manganese dioxide nanosheets to the diatom cylinder surface. Scanning electron microscopy (SEM) was used to observe the morphology of DM and to analyze the composition of doped MnO2. Stereomicroscope was used to observe the reaction of DM in 3% hydrogen peroxide. Non-precious metal alloys, zirconia and resin specimens were prepared to evaluate the effect of biofilm removal on the surface of prosthetic materials. And then Streptococcus mutans and Porphyromonas gingivalis biofilms were formed on the specimens. When 3% hydrogen peroxide solution and DM were treated on the biofilms, the decontamination effect was compared with chlorhexidine gluconate and 3% hydrogen peroxide solution by crystal violet staining. Results: Manganese dioxide was found on the surface of the diatom cylinder, and it was found to produce bubble of oxygen gas when added to 3% hydrogen peroxide. For all materials used in the experiments, biofilms of the DM-treated groups got effectively removed compared to the groups used with chlorhexidine gluconate or 3% hydrogen peroxide alone. Conclusion: MnO2-diatom microbubbler can remove bacterial membranes on the surface of prosthetic materials more effectively than conventional mouthwashes.

핵융합로용 플라즈마 대향부품 개발을 위해 제작된 텅스텐/FM강 HIP 접합 목업의 수명 평가 해석

  • Lee, Dong-Won;Sin, Gyu-In;Kim, Seok-Gwon;Jin, Hyeong-Gon;Lee, Eo-Hwak;Yun, Jae-Seong;Mun, Se-Yeon;Hong, Bong-Geun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2014.02a
    • /
    • pp.452-452
    • /
    • 2014
  • 블랑켓 일차벽이나 디버터와 같은 핵융합로 플라즈마 대향부품은 플라즈마로부터 입사되는 중성자 및 입자들을 차폐하여 구조물을 보호하고, 발생열을 에너지로 변환하기 위해 냉각재를 활용한 열제거 기능을 담당한다. 특히, 고속중성자와 입사 열부하 및 여러 입자들로부터 블랑켓 및 내부 구조물을 보호하기 위해 차폐체와 구조물로 구성된다. 세계적으로 차폐체로서는 텅스텐 혹은 텅스텐 합금, 구조물용 재료로는 저방사화 Ferritic Martensitic (FM) 강이 유력한 후보재료로 개발, 연구 중에 있다. 국내에서는 국제핵융합로(ITER) 사업을 통해 고온등방가압(HIP, Hot Isostatic Pressing)을 이용한 이종금속간 접합기술과 한국형 저방사화 고온구조재료인 ARAA (Advanced Reduced Activation Alloy)가 개발되고 있으며, 이를 활용한 설계, 접합법 개발, 제작목업의 건전성 평가 등이 수행되고 있다. 한국원자력연구원에서는 핵융합 기초사업의 일환으로 전북대와 공동으로 수행 중인 건전성 평가체계 개발을 위해, 기 개발된 접합법을 활용한 $45mm(H){\times}45mm(W){\times}2mm(T)$의 W/FM강 목업을 제작한 바 있으며, 이를 국내 구축된 고열부하 시험 장비인 KoHLT-EB (Electron Beam)를 활용한 고열부하 인가 건전성 평가시험을 준비 중에 있다. 이종금속간 접합 특성은 기계적 평가를 위한 파괴시험을 통해 검증, 이를 활용한 목업이 제작되었으며, 제작된 목업에 대한 초음파를 이용한 접합면의 비파괴 검사를 통해 결함이 없음을 확인하였다. 최종적으로 실제 사용되는 핵융합 운전조건과 유사 혹은 가혹한 조건에서 고열부하를 인가하여, 그 건전성을 평가가 이루어질 것이다. 고열부하 시험을 위해서는 냉각조건, 인가 열부하, 수명평가를 통한 반복 고열부하 인가 횟수 등이 사전에 결정되어야 한다. 이를 위해 상업용 열수력, 구조해석 코드인 ANSYS-CFX와 -mechanical을 이용한 시험조건 모의 및 수명 평가가 수행되었다. 구축 장비의 냉각계통을 고려하여 냉각수의 온도 및 속도는 $25^{\circ}C$, 0.15 kg/sec로, 열부하는 0.5 및 $1.0MW/m^2$에 대해 모의를 수행하였다. 정상상태 시 텅스텐의 최대 온도는 각 열부하 조건에 따라 $285.3^{\circ}C$$546.8^{\circ}C$였으며, 이에 도달하는 시간을 구하기 위해 천이해석을 수행하였고, 이를 통해 30초에 최대온도 95 %이상의 정상상태 온도에 도달함을 확인하였다. 또한, 목업의 초기 온도에 도달하는 냉각시간도 동일한 천이해석을 통해 30초로 가능함을 확인하였고, 최종 시험 조건을 30초 가열, 30초 냉각으로 결정하였다. 결정된 반복 열부하 인가 조건에서 이종금속 접합체가 받는 다른 열팽창 정도에 따른 응력을 계산하여 목업의 수명을 도출하였고, 이를 시험해야 할 반복 횟수로 결정하였다. 각 열부하 조건에 따른 온도조건을 ANSYS-mechanical 코드를 활용하여 열팽창과 이에 따른 접합면의 응력분포로 계산하였다. 0.5 및 $1.0MW/m^2$에 대해, 목업이 받는 최대 응력은 334.3 MPa와 588.0 MPa 였으며, 이 때 텅스텐과 FM강이 받는 strain을 도출하여 물성치로 알려진 cycle to failure 값을 도출하였다. 열부하에서 예상되는 수명은 0.5 및 $1.0MW/m^2$에 대해, 100,000 사이클 이상과 2,655 사이클로 계산되었으며, 시간적 제약을 고려 최종 평가는 $1.0MW/m^2$에 대해, 3,000사이클 정도의 실험을 통해 그 수명까지 접합건전성이 유지되는 지 실험을 통해 평가할 예정이다.

  • PDF

Fatigue fracture of different dental implant system under cyclic loading (반복하중에 따른 수종 임플란트의 피로파절에 관한 연구)

  • Park, Won-Ju;Cho, In-Ho
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.4
    • /
    • pp.424-434
    • /
    • 2009
  • Statement of problem: Problems such as loosening and fractures of retained screws and fracture of implant fixture have been frequently reported in implant prosthesis. Purpose: Implant has weak mechanical properties against lateral loading compared to vertical occlusal loading, and therefore, stress analysis of implant fixture depending on its material and geometric features is needed. Material and methods: Total 28 of external hexed implants were divided into 7 of 4 groups; Group A (3i, FULL $OSSEOTITE^{(R)}$Implant), Group B (Nobelbiocare, $Br{\aa}nemark$ $System^{(R)}$Mk III Groovy RP), Group C (Neobiotec, $SinusQuick^{TM}$ EB), Group D (Osstem, US-II). The type III gold alloy prostheses were fabricated using adequate UCLA gold abutments. Fixture, abutment screw, and abutment were connected and cross-sectioned vertically. Hardness test was conducted using MXT-$\alpha$. For fatigue fracture test, with MTS 810, the specimens were loaded to the extent of 60-600 N until fracture occurred. The fracture pattern of abutment screw and fixture was observed under scanning electron microscope. A comparative study of stress distribution and fracture area of abutment screw and fixture was carried out through finite element analysis Results: 1. In Vicker's hardness test of abutment screw, the highest value was measured in group A and lowest value was measured in group D. 2. In all implant groups, implant fixture fractures occurred mainly at the 3-4th fixture thread valley where tensile stress was concentrated. When the fatigue life was compared, significant difference was found between the group A, B, C and D (P<.05). 3. The fracture patterns of group B and group D showed complex failure type, a fracture behavior including transverse and longitudinal failure patterns in both fixture and abutment screw. In Group A and C, however, the transverse failure of fixture was only observed. 4. The finite element analysis infers that a fatigue crack started at the fixture surface. Conclusion: The maximum tensile stress was found in the implant fixture at the level of cortical bone. The fatigue fracture occurred when the dead space of implant fixture coincides with jig surface where the maximum tensile stress was generated. To increase implant durability, prevention of surrounding bone resorption is important. However, if the bone resorption progresses to the level of dead space, the frequency of implant fracture would increase. Thus, proper management is needed.

Impact Resistance Reliability of Sn-1.2Ag-0.5Cu-0.4In Solder Joints (Sn-1.2Ag-0.5Cu-0.4In 조성 솔더 접합부의 내 충격 신뢰성 평가)

  • Yu, A-Mi;Lee, Chang-Woo;Kim, Jeong-Han;Kim, Mok-Soon;Lee, Jong-Hyun
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.226-226
    • /
    • 2008
  • 지난 10여년 동안 Sn-3.0Ag-0.5(wt%)Cu 합금은 대표 무연솔더 조성으로 다양한 전자제품의 실장 및 접합에 적용되어 왔으며, 그 신뢰성 역시 충분히 검증된 바 있다. 그러나 최근 Ag 가격의 급격한 상승과 솔더 접합부의 내 충격 신뢰성을 보다 향상시키고자 하는 업계의 동향은 Ag의 함량이 낮은 무연솔더 조성의 적용 확대를 유도하고 있다. 이에 따라 본 연구자들은 저 Ag 함유 무연슬더로 Sn-1.2Ag-0.5Cu-0.4In 조성을 제안한 바 있는데, 이는 Sn-3.0Ag-0.5Cu 조성 이상의 solderability를 가지면서도 그 금속원료 가격이 약 20% 가량 저렴한 특징을 가진다. 또한 열 싸이클링 (cycling) 테스트를 통한 슬더 조인트의 신뢰성을 평가한 결과, Sn-3.0Ag-0.5Cu에 크게 뒤떨어지지 않는 양호한 특성이 관찰되었다. 따라서 본 연구에서는 열 싸이클링 테스트와 더불어 최근 그 중요성이 지속적으로 커지고 있는 내 충격 신뢰성 평가 시험을 실시하여 개발된 4원계 무연솔더 조성의 기계적 특성을 기존 무연솔더 조성과 비교, 분석해 보았다. 각 솔더 조성은 솔더 볼 형태로 제조되어 CSP(Chip Scale Package) 상에 범핑 (bumping)되었으며, CSP를 PCB(Printed Circuit Board) 상에 실장하는 공정에서도 Sn-3.0Ag-0.5Cu 및 Sn-1.2Ag-0.5Cu-0.4In의 두 종류의 솔더 페이스트가 사용되었다. 본 연구에서의 내 충격 신뢰성 시험에는 자체 제작한 rod drop 시험기를 사용하였는데, 고정된 CSP 실장 board의 후면 부위를 일정한 높이에서 추를 반복적으로 자유 낙하시켜 급격한 충격을 주는 방식으로 실험을 실시하였다. 이 때 추의 무게는 30g, 낙하 높이는 10cm 였으며, 추의 낙하 시 측정된 board 의 휨 변위량은 약 0.7mm로 측정되었다. 사용된 CSP와 PCB 는 모두 daisy chain 방식으로 연결되어 있기 때문에 저항측정기를 사용한 간단한 실시간 저항 측정 방법으로 시험 이력에 따른 파단부의 발생 시점과 대략의 위치를 손쉽게 확인할 수 있었다. 솔더 조인트의 파단 기준 저항값으로 $1000\Omega$을 설정하였으며. 각 조건 당 5 개 이상의 샘플에 대해 평가를 실시한 후 그 평균값을 조사하였다. 시험 결과 제안된 Sn-1.2Ag-0.5Cu-0.4In 조성은 대표적인 저 Ag 함유 조성인 Sn-1.0Ag-0.5Cu에 비해서는 떨어지는 내 충격 신뢰성을 나타내었지만, 우수한 연성에 기인하여 Sn-3.0Ag-0.5Cu 조성에 비해서는 약 2 배 이상 우수한 신뢰성이 관찰되었다. 또한 CSP의 실장 시 Sn-3.0Ag-0.5Cu보다 Sn-1.2Ag-0.5Cu-0.4In 조성 솔더 페이스트를 적용한 경우에서 보다 우수한 내 충격 신뢰성을 나타내어 기본적으로 개발된 Sn-1.2Ag-0.5Cu-0.4In 솔더 페이스트가 Sn-3.0Ag-0.5Cu 조성의 기존 솔더 페이스트 보다 내 충격 신뢰성이 우수함을 검증할 수 있었다. 각 조성의 솔더 조인트를 $150^{\circ}C$ 에서 500시간 aging한 후 실시한 내 충격 신뢰성 평가에서는 모든 조성에서 그 신뢰성이 급감하는 경항을 나타내었으나, Sn-1.2Ag-0.5Cu-0.4In가 Sn-l.0Ag-0.5Cu보다도 그 상대적인 신뢰성이 우수한 것으로 관찰되었다. 이와 같이 aging 후 실시하는 충격시험은 가장 실제적인 상황과 유사한 조건이므로 상기의 실험 결과는 매우 고무적이었으며, 이에 대한 보다 면밀한 분석이 요청되었다. 마지막으로 파면 및 미세조직 관찰을 통하여 각 조성에서의 충격 파단 특성을 비교, 분석해 보았다.

  • PDF