• Title/Summary/Keyword: 레진 주조

Search Result 26, Processing Time 0.021 seconds

Review on additive manufacturing of dental materials (치과용 재료의 적층가공에 대한 문헌고찰)

  • Won, Sun;Kang, Hyeon-Goo;Ko, Kyung-Ho;Huh, Yoon-Hyuk;Park, Chan-Jin;Cho, Lee-Ra
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.37 no.1
    • /
    • pp.1-15
    • /
    • 2021
  • Additive manufacturing (AM) for dental materials can produce more complex forms than conventional manufacturing methods. Compared to milling processing, AM consumes less equipment and materials, making sustainability an advantage. AM can be categorized into 7 types. Polymers made by vat polymerization are the most suitable material for AM due to superior mechanical properties and internal fit compared to conventional self-polymerizing methods. However, polymers are mainly used as provisional restoration due to their relatively low mechanical strength. Metal AM uses powder bed fusion methods and has higher fracture toughness and density than castings, but has higher residual stress, which requires research on post-processing methods to remove them. AM for ceramic use vat polymerization of materials mixed with ceramic powder and resin polymer. The ceramic materials for AM needs complex post-processing such as debinding of polymer and sintering. The low mechanical strength and volumetric accuracy of the products made by AM must be improved to be commercialized. AM requires more research to find the most suitable fabrication process conditions, as the mechanical properties and surface of any material will vary depending on the processing condition.

The Effect of Temporary Cement Cleaning Methods on the Retentive Strength of Cementation Type Implant Prostheses (임시 시멘트 제거방법이 시멘트 유지형 임플란트 보철물의 유지력에 미치는 영향)

  • Shin, Hwang-Kyu;Song, Young-Gyun;Shin, Soo-Yeon
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.27 no.2
    • /
    • pp.125-140
    • /
    • 2011
  • The remnant of temporary cement on the intaglio surface of cast restoration may have a negative effect on the retentive strength of permanent cement. This study was to evaluate the effect of temporary cement cleaning methods on the retentive strength of cementation type implant prostheses. Prefabricated implant abutments - height 5.5mm, diameter 4.5mm, 6 degree axial wall taper with chamfer margins were used. Forty copings-abutment specimens were divided into four groups(each n=10) according to the cleaning methods for temporary cement(Temp-$Bond^{(R)}$) as follows : no temporary cementation(the control group), orange solvent, ultrasonic cleaning, air borne-particle abrasion. After the application of temporary cement and the separation, the cleaning procedure was performed according to the protocol of each group. The specimens were cemented with $Premier^{(R)}$ Implant $Cement^{TM}$. After the permanent cementation, the specimens were subjected to thermocycling and pulled out from the specimens with a universal testing machine at a cross-head speed of 0.5mm/min. After the retentive strength test, all the specimens were cleaned using ultrasonic cleaning, abraded with air borne-particles, and steam-cleaned. Likewise, the specimens were temporarily cemented(Temp-$Bond^{(R)}$ NE), cleaned according to the protocol of each group, cemented with $Premier^{(R)}$ Implant $Cement^{TM}$ and subjected to thermocycling and measurement of their retentive strength. The mean of group with orange solvent were significantly lower than those of other groups(p<0.05). There was no significance between group with ultrasonic cleaning and group with air borne-particle abrasion. Group with ultrasonic cleaning and group with air-particle abrasion were no significance at control group. There was no significance between group cemented with Temp-$Bond^{(R)}$ and group cemented with Temp-$Bond^{(R)}$ NE. Within the limitation of this study, it can be concluded that the temporary cement cleaning method with only orange solvent may have a negative effect on the retentive strength of permanent cement. Ultrasonic cleaning and air borne-particle abrasion methods are recommended for the temporary cement cleaning method on cementation type implant prostheses.

Study of heat transfer to the implant-bone interface induced by grinding of occlusal surface of implant gold prosthesis (금 합금 보철물의 교합면 삭제로 인한 임플란트-골 계면으로의 열전달에 관한 연구)

  • Jo, Jae-Young;Kang, Sun-Nyo;Jeong, Chang-Mo;Yun, Mi-Jung;Huh, Jung-Bo;Jeon, Young-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.50 no.1
    • /
    • pp.29-35
    • /
    • 2012
  • Purpose: The purpose of this study was to analyze temperature change along the implant-bone interface induced by grinding the occlusal surface of implant gold prosthesis and to compare the temperature generated by grinding of prosthesis with different cooling methods. Materials and methods: The experimental gold prostheses were fabricated with dental gold alloy and castable abutment. The prostheses had 3 cylindrical protrusions on the occlusal surface with 1mm in height. Temperature was measured using 16 thermocouple wires attached to the implant fixture surface and the fixture was embedded in an acrylic resin block inside the $37^{\circ}C$ water bath. Cylinders were grinded for a period of 30 second with a low-speed handpiece with green stone point. One cylindrical protrusion was grinded without cooling, the second one was grinded with air blow, and the third one was grinded with water-spray. Results: The mean maximum temperature was measured more than $47^{\circ}C$ of the implant and the maximum temperature was measured at the cervical portion of the implant in the group without cooling. There was statistically significant difference between the group without cooling and the groups with cooling (P<.05). However, there was no significant difference at all portion of implant in the groups with cooling (P>.05). Conclusion: The results of this study support that the grinding of implant gold prosthesis without cooling may damage the peri-implant tissue. The continuous use of air blow and water-spray adjacent to prosthesis during the grinding of implant gold prosthesis may prove to be beneficial for cooling of the implant.

EFFECT OF VARIOUS RESIN CEMENTS TO THE SHEAR BOND STRENGTH IN THE ADHESION BRIDGE (접착성가공의치에서 세멘트 종류가 전단결합강도에 미치는 영향)

  • Lee, Cheong-Hee
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.34 no.4
    • /
    • pp.791-799
    • /
    • 1996
  • The purpose of this study was to compare the shear bond strength of adhesion bridge by various resin cements. One hundred and foully 1st premolars were used. The teeth were cut below 2mm from CEJ and the coronal portions were used. The coronal portions were embeded with the acrylic resin and trimmed with sic paper until the flat plane with ${\phi}$ 4mm above acrylic resin sticks in height 5mm were casted with nonprecious metal and the using surfaces were treated with sic paper from #200 to #1200 and polished with alminum oxide paste. And then, the using surfaces were sandblasted and treated with the electrochemical etching. The teeth were divided into three groups of fourty two each. In group I, teeth and specimens were cemented with Panavia 21 In group II, teeth and specimens were cemented with Superbond In group I, teeth and specimens were cemented with All-Bond & composite resin cement Each group was subdivided into three subgroups according to the storage period ; one-day storage, fifteen-day storage, and thirty-day storage. The special jig was made. Then, the specimen and jig were mounted to Instron Universal Testing Machine and the failure were measured. The results were as follows. 1. There was statisfically significant difference between the failure loads of group I and group II and III after one day storage(P<0.01), 2. There was statisfically significant difference between the failure loads of group II and group I and III and between group I and group III at fifteen day storage(P<0.01). 3. There was statisfically significant difference between the failure loads of group I and II and group III after thirty day storage(P<0.01). 4. There was statisfically significant difference between the failure loads of one day storage and fifteen and thirty days storages in group III (P<0.01).

  • PDF

A comparison of the fidelity of various zirconia-based all-ceramic crowns fabricated with CAD/CAM systems (수종의 CAD/CAM 시스템으로 제작한 지르코니아 기반 완전도재관의 적합도 비교)

  • Kim, Sung-Jun;Jo, Kwang-Hun;Lee, Kyu-Bok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.2
    • /
    • pp.148-155
    • /
    • 2009
  • Statement of problem: The interest in all-ceramic restorations has increased as more techniques have become available. With the introduction of machinable dental ceramics and CAD/CAM systems there is a need to evaluate the quality levels of these new fabrication techniques. Purpose: This study is to evaluate the crown fidelity(absolute marginal discrepancy and internal gap) of various zirconia-based all-ceramic crowns fabricated with different CAD/CAM(computer-assisted design/computer-assisted manufacturing) systems and conventional cast metal-ceramic crowns. Material and methods: A resin tooth of lower right second premolar was prepared. After an impression was taken, one metal master die was made. Then 40 impressions of metal master dies were taken for working dies. 10 crowns per each system were fabricated using 40 working dies. Metal-ceramic crowns were cast by using the conventional method, and Procera, Lava, and Cerec inLab crowns were fabricated with their own CAD/CAM manufactruing procedures. The vertical marginal discrepancies and internal gaps of each crown groups were measured on a metal master die without a luting agent. The results were statistically analyzed using the one-way ANOVA and Tukey's HSD test. Results: 1. Vertical marginal discrepancies were $50.6{\pm}13.9{\mu}m$ for metal-ceramic crowns, $62.3{\pm}15.7{\mu}m$ for Procera crowns, $45.3{\pm}7.9{\mu}m$ for Lava crowns, and $71.2{\pm}2.0{\mu}m$ for Cerec inLab crowns. 2. The Internal gaps were $52.6{\pm}10.1{\mu}m$ for metal-ceramic crowns, $161.7{\pm}18.5{\mu}m$ for Procera crowns, $63.0{\pm}10.2{\mu}m$ for Lava crowns, and $73.7{\pm}10.7{\mu}m$ for Cerec inLab crowns. Conclusion: 1. The vertical marginal discrepancies of, 4 crown groups were all within the clinically acceptable range($120{\mu}m$). 2. The internal gaps of LAVA, Cerec inlab, and metal-ceramic crowns were within clinically acceptable range except Procera crown($140{\mu}m$).

Removal Torque Values of Retaining Screws Tightened to Implant-Supported Prosthesis with Different Connection Systems by Various Tightening Technique (다른 연결 시스템을 갖는 임플랜트 상부 구조물에서 조임술식에 따른 지대주 나사의 풀림 토크값에 대한 연구)

  • Kim, Dong-Wook;Choi, Yu-Sung;Jo, In-Ho
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.27 no.4
    • /
    • pp.343-358
    • /
    • 2011
  • As implant treatment has become popular, lots of different shapes and materials of the implant upper component have been supplied. And there are also diverse reports about failures including loosening of the abutment screw which is one of the most common reason. Purpose : The purpose of this study is to find out how different screw tightening orders and methods influence on screw loosening according to the different connection systems. The upper component was fabricated by casting method. After fabricating master models that are precisely attached to the upper component, 5 experimental models each for the external connection system and internal connection system were fabricated using splinting impression technique. First, to find out the influence of the screw tightening order, screws were tightened in 3 orders; 1-2-3-4, 2-3-1-4, 2-4-3-1. After tightening, removal torque values (RTV) of each group was measured. And also to find out the influence of screw tightening method, a model with 2-3-1-4 screw tightening order was tightened with 30 Ncm at one time(1-step method) and the RTV was compared with the same order group (2-3-1-4) in the 2 step method. In the external connection system, RTV appeared significantly lower in group 2-3-1-4 than group 2-4-3-1 (p<0.05). And also in the internal connection system, the RTV of group 2-3-1-4 appeared significantly lower than that of group 2-4-3-1 and 1-2-3-4 (p<0.05). When comparing the tightening number of the screw without considering the screw tightening order, the first tightened screw appeared significantly higher RTV than the second one in the external connection system (p<0.05), however there was no significant difference from the first tightened screw to the last tightened screw in the internal connection system. And there was no statistically significant difference between the two screw tightening methods in both internal and external connection system. In the comparison of external and internal connection system, each RTV appeared 16.27 Ncm and 14.25 Ncm and appeared as a statistically significant difference (p<0.05). There was a significant difference in RTV measured according to the screw tightening order. The lowest RTV appeared in the groups started tightening from the middle. There was also a significant difference in RTV between the two connection system groups. A further study is needed to find out the influence factors in RTV and also a study is required related to the load condition.