Roll Force Prediction of High-Strength Steel Using Foil Rolling Theory in Cold Skin Pass Rolling (고강도강의 냉간 조질 압연 시 호일 압연이론을 이용한 압연하중의 예측)

  • Song, Gil Ho;Jung, Jae Chook
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.37 no.2
    • /
    • pp.271-277
    • /
    • 2013
  • Skin pass rolling is a very important process for applying a certain elongation to a strip in the cold rolling and annealing processes, which play an important role in preventing the stretching of the yield point when the material is processed. The exact prediction of the rolling force is essential for obtaining a given elongation with the steel grade and strip size. Unlike hot rolling and cold rolling, skin pass rolling is used to apply an elongation of within 2% to the strip. Under a small reduction, it is difficult to predict the rolling force because the elastic deformation behavior of the rolls is complicated and a model for predicting the rolling force has not yet been established. Nevertheless, the exact prediction of the rolling force in skin pass rolling has gained increasing importance in recent times with the rapid development of high-strength steels for use in automobiles. In this study, the possibility of predicting the rolling force in skin pass rolling for producing various steel grades was examined using foil rolling theory, which is known to have similar elastic deformation behavior of rolls in the roll bite. It was found that a noncircular arc model is more accurate than a circular model in predicting the roll force of high-strength steel below TS 980 MPa in skin pass rolling.

Prediction of Sink Phenomenon during Forging Process and Improvement of LPI Fuel Filter Housing Forging Product (LPI 차량용 연료필터 상부 하우징 냉간 단조 성형 공정에서 sink 현상 예측 및 개선)

  • Kim, Jun-Young;Park, Sang-Min;Hong, Seokmoo
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.6
    • /
    • pp.395-399
    • /
    • 2017
  • The LPI fuel filter housings used in automobiles were made from conventional die castings but have recently been developed by cold forging to improve the weight and durability. On the other hand, a sink may develop at the core of the forged product due to the resulting T-shape, which not only reduces the aesthetics, but also increases the post-processing cost of the product. Therefore, this research focused on methods to predict and mitigate sink development and progression during the T-shape forging process. Finite element analysis of the forging process was first performed to determine the optimal initial workpiece devoid of burrs and underfills. An accurate sink prediction was then obtained via metal flow analysis, which was a result of the finite element simulation. Through finite element analysis, it was confirmed that sink development is a product of the differences in nodal velocities arising from the T-shaped forging process. Consequently, a pad was inserted beneath the sink to minimize these velocity differences. The results yielded significant improvement with regard to the sink defect. This method was practically applied to an industrial site to validate the sink improvement.

Evaluation of Mechanical Properties and Fatigue Behavior of STS 304L due to Plastic Working (소성가공에 따른 STS 304L 재료의 기계적 특성 및 피로평가)

  • Shim, Hyun-Bo;Kim, Young-Kyun;Suh, Chang-Min
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.41 no.7
    • /
    • pp.635-643
    • /
    • 2017
  • The purpose of this study is to investigate the influence of the cold reduction rate and an ultrasonic fatigue test (UFT) on the fatigue behaviors of STS 304L. The tensile strength, yield strength, hardness value and fatigue limit in the UFT fatigue test linearly increased as thickness decreased from 1.5 mm to 1.1 mm, as the cold reduction rate of STS 304L increased. As a result of the UFT fatigue test (R = -1) of four specimens, the fatigue limit of the S-N curve formed a knee point in the region of $10^6$, and the 2nd fatigue limit caused by giga cycle fatigue did not appeared. In the case of t = 1.1 mm, the highest fatigue limit was 345 MPa, which was 64.3% higher than the original material (t = 1.5 mm). As a result of the UFT fatigue test of STS 304L, many small surface cracks occurred, grown, coalesced while tearing.

A Study on the Electrical Discharge Machining Tap by using Cu Electrodes of the Cold-Work Tool Steel (냉간 금형용 공구강의 Cu 전극을 이용한 방전 탭에 관한 연구)

  • Lee, Eun-Ju;Park, In-Soo;Kim, Hu-Kwon;Wang, Duck-Hyun;Chung, Han-Shik;Lee, Kwang-Sung
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.15 no.5
    • /
    • pp.131-136
    • /
    • 2016
  • Currently, an EDM tapping procedure has comprised some parts of the engraving discharge process for the press die. Usually, tapping has been used in cases where we are unable to mechanically machine using steelwork processes due to an increase in the hardness of a material after heat treatment in relation to a design change or missing process. Here, we analyze the influence of discharge tap shape on discharge time, discharge current, and the number of repetition conditions when a cold-work tool steel (STD11) has been treated with a discharge tapped by a screw-shaped cu electrode. The most important influence on processing condition has been determined to be the number of discharge repetitions. As this number increases, the angle reduction of a thread closes to an angle of the electrode via a power generation reduction. The optimal combination of conditions has been determined to be three discharge repetitions, $180{\mu}s$ of discharge time (same as existing regulations), and 25.4A of peak current. A 0.2749db advantage has emerged after comparing between this combination of optimal conditions and the SN rate of existing regulations.

Electron Discharge Machining (EDM) and Hole EDM of Cold Heat-treated Tool Steel Molds (STD11) by using Cu Electrodes (냉간 금형용 공구강의 Cu 전극을 이용한 방전 홀에 관한 연구)

  • Park, In-Soo;Lee, Eun-Ju;Kim, Hwa-Jeong;Wang, Deok-Hyun
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.17 no.4
    • /
    • pp.76-82
    • /
    • 2018
  • 3D formed Electrical Discharge Machining (EDM) and hole EDM were conducted for die and mold manufacturing with electrodes which were made by mechanical machining and wire EDM. It is difficult to machine the hardened material after heat treatment and quenching with traditional machining. The only method of machining hardened material is die-sinking EDM. In this research, hole EDM was conducted for heat-treated cold-worked tool steel (SKD11) for use as a die material. The EDM surfaces were analyzed by pulse-on time and peak current of EDM current, according to the machining conditions of EDM. The EDM surface profiles were affected by the peak current. The contribution of each factor is peak current (91.63%) and pulse-on time (0.93%). The best surface roughness was obtained with a $130{\mu}s$ pulse-on time and a 14.2 A peak current. With uniform EDM processing, the surface deteriorated with increasing pulse-on time and peak current. The thickness of the solidified layer induced by EDM was increased as the peak current, crater shapes, and erupted shapes of EDM surfaces were increased. Therefore, microcracking gaps induced by surface tension were increased.

Finite element analysis of unconstrained axisymmetric piercing (구속이 없는 축대칭 피어싱 공정의 유한요소해석)

  • 양동열;유요한;이종수
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.10 no.6
    • /
    • pp.876-888
    • /
    • 1986
  • The Study is concerned with the analysis of unconstrained axisymmetric piercing as a nonsteady forging process by the rigid-plastic finite element method. In the numerical analysis of axisymmetric piercing, the initial velocity field is generated by assuming the material as a linear viscous material to begin with in order to facilitate the input handling and to ensure better convergencey. The strain-hardening effect for nonsteady deformation and the friction of the die-material interial interface are considered in the formulation. Rigid body treatment is also incorporated in the developed program. The experiments are carried out for aluminum alloy specimens (A1204) with different specimen heights. It is shown that the experimental results are in excellent agreement with the finite element simulations is deformed configuration. For load prediction the theoretical prediction shows excellent agreement with th eexperimental laod in the initial stage of loading before fracture of the specimen is not initiated. Distribution of stresses, strains and strain rates has been found for the given cases in computation. On this basis several fracture criteria are introduced in order to check the fracture initiation. It is found that maximum shear criterion is capable of good fracture prediciton.

The Influence of Extrusion Ratio on Microstructure and Thermoelectric Properties of Rapidly Solidified N-type $Bi_2Te_{2.75}Se_{0.15}$ (급속응고된 N-type $Bi_2Te_{2.75}Se_{0.15}$ 열전재료의 미세조직과 열전특성에 미치는 압출비의 영향)

  • 이상일;홍순직;손현택;천병선;이윤석
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2001.11a
    • /
    • pp.30-30
    • /
    • 2001
  • $Bi_2Te_3$계 열전재료는 200~400K 정도의 저온에서 네어지 변환효율이 가장 높은 재료로써 열전냉각, 바런재로 등에 응요하기 위하여ㅠ 제조법 및 특서에 관한 많은 연구가 진행되어 왔다. $Bi_2Te_3$계 화합물은 rhombohedral의 결정 구조를 가지는 층상 화 ;물로 결정대칭성으로 인해 연전기적으로 큰 이방성을 나타낸다. 현재는 일반향용고법에 의해서 입자를 a축 방향으로 성장시켜 큰 결정립을 가진 다결정재료를 사용하고 있으나, c면이 매우 취약하기 때문에 가공서이 나쁘다. 따라서 이와같은 단점을 개선하기 위하여 기계적 강도를 높일 수 있는 가공공정 및 합금설계에 대한 연구가 활발히 진행되고 있다. 측히 열간 압출법으로 제조된 열전재료는 결정립의 미세화와 높은 이방성으로 성능지수와 기계적 강도를 향상시킬 수 있다는 연구결과가 보고되고 있다 또한 Schultz드의 연구결과에 의하면 $Bi_2Te_3$ 계 열전재료는 소성변형에 의하여 발생한 점결함에 의하여 캐리어 농도가 변화되며 이로 인하여 재료의 전기적 성질이 결정된다고 하였다. 따라서 상당히 큰 소성가공량과 열전측성과의 관계를 규명하는 것은 매우 중요하다. 이에 본 연구에서는 압출변수 중 소성가공량에 중요한 변수로 작요아는 압출비를 변화시켜 최적의 열간 소성가공량을 검토하고, 이에 따른 열전측성과 압출비와의 상관관계에 대하여 연구하는 것을 목적으로 하였다. 연구에 사용된 N형의 조성은$Bi_2Te_{2.75}Se_{0.15}$로서 순도 99.99를 사용하였고, dopant로 0.1wt%의 $SbI_3$를 사용하였다. $Bi_2Te_{2.75}Se_{0.15}$ 분말은 가스분사법(Gas atomization Process)를 이용하여, 용탕제조시 아르곤가스로 산화를 방지하였고, 냉매로는 질소가스를 이용하였다. 제조된 분말을 기ㅖ적 분급법을 이용하여 분급하였고, 냉매로는 질소가스를 이용하였다. 제조된 분말을 기계적 분급ㅂ법을 이용하여 분급하였고, 압출에 이용된 분말은 250$\mu\textrm{m}$이하의 크기를 사용하였다. 또한 분말제조과정 중 형성되는 표면산화층을 제거하기 위하여 36$0^{\circ}C$에서 4시간동안 수소 환원처리를 행하였다. 제조된 분말은 열간 압출을 위하여 Aㅣcan에 넣고 냉간성형체를 만들고, 진공처리를 한 후 밀봉하여 탈가스처리를 하였다. 압출다이는 압출비가 각각 28:1과 16:1인 평다이(9$0^{\circ}C$)를 사용하여 각각 내경이 9, 12cm이고, 길이가 50, 30cm인 압출재를 제조하였다. 열간압출한 후의 미세조직을 광학현미경으로 압출방향에 평행한 방향과 수직방향으로 관찰하였고, 열간 압출재 이방성을 검토하기 위하여 X선 회절분석을 실실하여 결정방위를 확인하였다. 전기 비저항 및 Seebeck 계수 측정을 위하여 각각 2$\times$2$\times$10$mm^3$ 그리고 5$\times$5$\times$10$mm^3$ 크기의 시편을 준비하였다.준비하였다.

  • PDF

The Effect of Extrusion Temperature on Microstructure and Thermoelectric Properties of Rapidly Solidified P-type $P-type Bi_{0.5}Sb_{1.5}Te_3$ alloy (급속응고된 $P-type Bi_{0.5}Sb_{1.5}Te_3$ 합금 열전재료의 미세조직과 열전특성에 미치는 압출 온도의 효과)

  • 이영우;천병선;홍순직;손현택
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2001.11a
    • /
    • pp.28-28
    • /
    • 2001
  • $Bi_2Te_3$계 열전반도체 재료는 200 ~ 400K 정도의 저온에서 에너지 변환 효율이 가장 높은 재료로서 열전냉각 및 발전재료로 제조볍 및 특성에 관한 많은 연구가 진행되어 왔다. 전자냉각 모듈의 제조에는 P형 및 N형 $Bi_2Te_3$계 단결정이 주로 사용되고 있으나. $Bi_2Te_3$ 단결정은 C축에 수직한 벽개면을 따라 균열이 쉽게 전파하기 때문에 소자 가공사 수윤 저하가 가장 큰 문제점으로 지적되고 있다. 이에 따라 최근 열전재료의 가공방법에 따른 회수율 증가 및 열전특성 향상에 관한 열간압출, 단조와 같은 연구가 활발히 이루어지고 있다. 본 연구는 가스분사법(gas atomizer)을 이용하여 용질원자 편석의 감소, 고용도의 증가,균일고용체 형성, 결정립미세화 둥 급속응고의 장점을 이용하여 화학적으로 균질한$Bi_2Te_3$계 열전재료 분말을 제조하고, 제조된 분발을 압출가공하여 기계적성질, 소자의 가공성 및 열전 성능 지수율 향상시키는데 연구 목적이 있다. 본 설험에서는 99.9%이상의 고순도 Bi. Te. Se. Sb를 이용하여, 고주파 유도로에서 Ar 분위기로 용융하고, 가스분사법를 이용하여 균질한 $Bi_2Te_3$계 열전재료 분만을 제조하였다. 분말표면의 산화막을 제거하기 위하여 수소분위기에서 환원처리를 행하였고, 된 분말을 Al 캔 주입하여 냉간성형 한 후 진공중에서 압출온도를 변화시켜 열간압출 가공을 행하였다. 압출 온도변화에 따른 압출재의 미세조직 및 열전특성에 중요한 영향을 미치는 C면 배향에 대한 결정방위 해석, 압출재의 압축강도 등을 분석하였으며, 압출온도에 따삼 미세조직 변화와 결정방위의 변화에 따른 열전특성의 관계를 해석하였다성시켰고 이들이 산인 HNO3에서 녹았기 때문이다. 본 연구에서 개발된 새로운 에칭 용액인 90H2O2 - 10HNO3 (vol%)의 에칭 원리가 똑같이 적용 가능한 다른 종류의 초경 합금에서도 사용이 가능할 것으로 판단된다.로 판단된다.멸과정은 다음과 같다. 출발물질인 123 분말이 211과 액상으로 분해될 때 산소가스가 배출되며, 이로 인해 액상에서 구형의 기공이 생성된다. 이들 중 일부는 액상으로 채워져 소멸되나, 나머지는 그대로 남는다. 특히, 시편 중앙에 서는 수십-수백 마이크론 크기의 커다란 기공이 다수 관찰된는데, 이는 기공의 합체로 만들어진 것이다. 포정반응 열처리 시 기공 소멸로 만들어진 액상포켓들은 주변 211 입자와 반응하여 123 영역으로 변한다. 이곳은 다른 지역과 비교하여 211 밀도 가 낮기 때문에, 미반응 액상이 남거나 211 밀도가 낮은 123 영역이 된다. 액상으로 채워지지 못한 구형의 기공들 중 다수가 123 결정 내로 포획되며, 그 형상은 액상/ 기공/고상 계면에너지에 의해 결정된다.단의 경우, 파단면이 매끄럽고 파변상의 결정립도 매우 미세하였으며, 산확물 의 용집도 찾아보기 어려웠 나, 접합부 파단의 경우에는 파변의 굴곡이 비교척 심하고 연성 입계파괴의 형태를 보였£며, 결정립도 모채부 파단의 경우에 비해 조대하였다. 조대하였다. 셋째, 주상기간 중 총 에너지 유입률 지수와 $Dst_{min}$ 사이에 높은 상관관계가 확인되었다. 특히 환전류를 구성하는 주요 입자의 에너지 영역(75~l13keV)에서 가장 높은(0.80) 상관계수를 기록했다. 넷째, 회복기 중에 일어나는 입자들의 유입은 자기폭풍의 지속시간을 연장시키는 경향을 보이며 큰 자기폭풍일수록 현저했다. 주상에서 관측된 이러한 특성은 서브스톰 확장기 활동이 자기폭풍의

  • PDF

Fabrication of copper thin foils with 36 microns by cold rolling (냉간 압연 공정에 의한 두께 $36{\mu}m$ 동극박 제조 공정 해석)

  • Lee, S.H.;Kim, B.M.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.05a
    • /
    • pp.413-416
    • /
    • 2007
  • In general, by means of the electrodepositing technique, a copper foil sample was prepared with a high purity and a high density. But the mechanical properties of the electrodepositing copper foil was lower than it's the rolling copper foil. However, the production of copper foil with approximately 36 microns thick in rolling process was very difficult. This paper describes the outline of the high accuracy cold rolling in 6 high mill which was developed for the purpose of rolling very thin accurate gauge copper foil(36 micron thick), and give several rolling characteristic of 600 mm wide copper foil. a) Large strain can be accumulated pass by pass in industrial multi-pass rolling processing to overcome large critical strain for thickness accuracy through optimization of rolling schedule. b) Also, permissible tension for rolling 0.45 $\sim$ 0.036 mm thick copper strip stably in accordance with the each pass work had been established by FEM simulation results. c) During the plate rolling process, considerable values of the forces of material pressure on the tool occur. These pressures cause the elastic deformation of the roll, thus changing the shape of the deformation region. A numerical simulation of roll deflection during cold rolling is presented in the paper. d) The proposed pass schedule can roll very thin copper foil of 36 micron thickness to a tolerance of ${\pm}1$ microns. The validity of simulated results was verified into rolling experiments on the copper foil.

  • PDF

Evaluation of water-Soluble Lubricant for Cold Forging and Optimization of Coating Process (냉간단조용 수용성 윤활제의 평가 및 윤활 처리 공정의 최적화)

  • Lim, W.J.;Lee, I.S.;Je, J.S.;Ko, D.C.;Kim, B.M.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.05a
    • /
    • pp.149-154
    • /
    • 2007
  • The zinc prosphate film treatments used to lubricating treatment of mostly cold forging processes. But there are several problems happened to lubricating treatment process such as happening harmful environment on person, complex lubrication processing occurring in energy and time consumption, eco-destructive and chemical by-product generation, the needs of waste disposal etc. As a result, a water-soluble lubricant was developed to replace the perfect or some of the zinc prosphate film in the world. In order to solve these problems, this study evaluated the performance of the typical water-soluble. In this study, for these requirement inquiry of two part. First, about possibility of replace zinc phosphate lubricant, quantitatively evaluation developed of water-soluble lubricant for cold forging vs zinc phosphate lubricant. Second, About optimization of coating Process use to equipment with practicable automatic coating Process. The performance evaluation of these lubricants was conducted using the double cup extrusion test and spike forging test. With the use of the commercial FE code DEFORM, friction factor calibration curves, i.e. cup height ratio vs. punch stroke and spike height vs. punch stroke, were established for different friction factor values. By matching the cup height ratio and the punch stroke and spike height vs. punch stroke from experiment to that obtained from FE simulations, the friction factor of the lubricants was determined. Survey of comparative analysis use to SEM that sprayed lubricant surface structure of grain shape and characteristic of lubricant performance based on grain shape and deformed lubricant surface expansion. As a result, developed lubricant were found to perform comparable to or better than zinc phosphate. And thought this result, innovatively cope with generated problem of existing lubrication process.

  • PDF