구상흑연주철의 피로수명을 지배하는 내재결함부 크기는 정량적 평가 (Quantitative Evaluation for the Internal Defect Size Governing the Fatigue Life in Ductile Irons)

  • 김진학;김민건
    • 대한기계학회논문집A
    • /
    • 제24권11호
    • /
    • pp.2742-2748
    • /
    • 2000
  • In this study, the quantitative evaluation was performed by examination for gatigue crack origin in two prepared ductile irons specimens which have different microstructures using rotary bending fatigue tester, Series A has mixed microstructure. ferrite plus pearlite, and series B has bainitic microstructure. Obtained main results are as follows. The scatterings of fatigue strength were observed on σ(sub)α-Ν diagram of both specimen series, and it is observed that scatterings of series A were more serious. It is reasonable to evaluate the size of mesocrack range by means of √A(원문참조), where A means the area of mesocrack range including globular graphite nodule. As a result of reconsideration for the fatigue data by introduction of K(sub)α-Ν diagram, the scattrings of fatigue life were, remarkably. reduced. Therefore, it is more reasonable to evaluate of mesocrack range on fatigue life by parameter K(sub)α rather than σ(sub)α.

구상흑연주철 극저사이클 피로파괴의 시뮬레이션 구현 (Simulation of Extremely Low Cycle Fatigue Fracture in Ductile Cast Iron)

  • 김민건;임복규
    • 대한기계학회논문집A
    • /
    • 제30권12호
    • /
    • pp.1573-1580
    • /
    • 2006
  • In this study, fatigue tests were carried out under push-pull loading condition using spheroidal graphite cast iron in order to clarify the internal fatigue fracture mechanism in an extremely low cycle fatigue regime. It is found that a successive observation of internal fatigue damage it is found that the fracture processes go through three stages, that is, the generation, growth and coalescence of microvoids originated from debonding of graphite-matrix interface. It is also found that the crack which is initiated from the void propagates by coalescence of neighboring cracks and the fatigue crack growth rate can be expressed in form of the Manson-Coffin rule type. In this paper, quantitative analyses of fatigue properties for realization of simulation about fatigue life evaluation are also presented.

구상흑연주철의 피로수명분포에 대한 통계적 해석 (A Statistical Analysis on Fatigue Life Distribution in Spheroidal Graphite Cast Iron)

  • 장성수;김상태
    • 대한기계학회논문집A
    • /
    • 제24권9호
    • /
    • pp.2353-2360
    • /
    • 2000
  • Statistical fatigue properties of metallic materials are increasingly required for reliability design purpose. In this study, static and fatigue tests were conducted and the normal, log-normal, two -parameter Weibull distributions at the 5% significance level are compared using the Kolmogorov-Smirnov goodness-of-fit test. Parameter estimation were compared with experimental results using the maximum likelihood method and least square method. It is found that two-parameter Weibull distribution and maximum likelihood method provide a good fit for static and fatigue life data. Therefore, it is applicable to the static and fatigue life analysis of the spheroidal graphite cast iron. The P-S-N curves were evaluated using log-normal distribution, which showed fatigue life behavior very well.

오스템퍼드 구상흑연주철의 기계적 성질 및 감쇠능에 미치는 서브제로처리의 영향 (Effect of Subzero Treatment on the Mechanical Properties and Damping Capacity of Austempered Ductile Cast Ironn)

  • 이광희;권민기;김창규;강창룡
    • 동력기계공학회지
    • /
    • 제11권4호
    • /
    • pp.86-91
    • /
    • 2007
  • This study was investigated to know the effect of subzero treatment in austempered ductile cast iron. Retained austenite transformed to martensite by subzero treatment. With decreasing subzero treatment temperature, more volume fraction of retained austenite transformed to martensite and transformed to martensite above 30% by subzero treatment temperature at $-196^{\circ}C$. With decreasing subzero treatment temperature, the value of strength and hardness increased but the value of elongation and impact value decreased. In case of subzero treatment at $-196^{\circ}C$, hardness value increased about 18% and impact value decreased by above 20%. We could find that subzero treated specimens had a little of effect on the tensile properties but had very much effect on the hardness and value of the impact.

  • PDF

오스템퍼드 구상흑연주철의 미세조직 및 기계적 성질에 미치는 서브제로처리의 영향 (Effect of Subzero Treatment on the Microstructure and Mechanical Properties of Austempered Ductile Cast Iron)

  • 이광희;강창룡
    • 동력기계공학회지
    • /
    • 제12권1호
    • /
    • pp.47-52
    • /
    • 2008
  • This study was investigated the effect of subzero treatment in austempered ductile cast iron. Retained austenite transformed to martensite by subzero treatment and strain. With decreasing subzero treatment temperature and increasing strain, retained austenite transformed more to martensite and transformed 30% above by subzero treatment at $-196^{\circ}C$. With decreasing subzero treatment temperature, the value of strength and ratio of increasing of strength, hardness and ratio of increasing of hardness increased but the value of elongation and ratio of decreasing of elongation decreased. With decreasing subzero treatment temperature, impact value and ratio of decreasing of impact value decreased. In case of subzero treatment at $-196^{\circ}C$, hardness value increased about 18% and impact value decreased above 20%. We could find that in subzero treated specimens had a little of effect on the tensile properties but had very much effect on the hardness and value of the impact.

  • PDF

피로한도의 정량평가법과 구상흑연주철에 대한 적용 (Quantitative Evaluation for Fatigue Limit and its Application to Spheroidal Graphite Cast Iron)

  • 김진학;김민건
    • 산업기술연구
    • /
    • 제18권
    • /
    • pp.203-208
    • /
    • 1998
  • Fatigue tests were performed to examine the 4 parameter method for specimens prepared by various heat treatment which resulted in different mechanical properties. Obtained main results are as follows. (1) Samples treated by austempering did not show the expected improvement of fatigue limit although hardness and strength increased. This is attributed to the fact that defect sensitivities of materials increase as increasing of hardness and tensile strength, it is also shown that the graphites acting as stress concentration place become larger by austempering heat treatment than by normal annealing. (2) It is very reasonable to predict the fatigue limit of ductile irons with 4 parameter method based on ${\sigma}_{TS}$, $H_v$, ${\Delta}K_{th}$ and ${\sqrt{area}}_{max}$. (3) The half-austempering treatment appeared to be more useful than the full-austempering method to improve the fatigue limit in the spheroidal graphite cast iron with multi defective material.

  • PDF

삽입금속을 사용한 구상흑연주철과 2024 알미늄합금의 마찰압접에 관한 연구 (Friction Welding of Spheroidal Graphite Cast iron and 2024 Aluminium Alloys using Insert Metal)

  • 김창규;김치옥;심성보;김광일
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2002년도 추계학술대회 논문집
    • /
    • pp.283-288
    • /
    • 2002
  • This study accompanied with the friction welding of a spheroidal graphite cast iron bar and 2024 Aluminium alloy bar with A1050 insert metal and investigated between conditions of friction welding faces and welded joint strength. This principal results of the experimental investigation could be summarized as follows: If the optimum friction welding is selected, the aspect of the spheroidal graphite cast iron and 2024 Aluminium could be welded with a pure Aluminium insert metal.