Abstract

In this study, the quantitative evaluation was performed by examination for gatigue crack origin in two prepared ductile irons specimens which have different microstructures using rotary bending fatigue tester, Series A has mixed microstructure. ferrite plus pearlite, and series B has bainitic microstructure. Obtained main results are as follows. The scatterings of fatigue strength were observed on σ(sub)α-Ν diagram of both specimen series, and it is observed that scatterings of series A were more serious. It is reasonable to evaluate the size of mesocrack range by means of √A(원문참조), where A means the area of mesocrack range including globular graphite nodule. As a result of reconsideration for the fatigue data by introduction of K(sub)α-Ν diagram, the scattrings of fatigue life were, remarkably. reduced. Therefore, it is more reasonable to evaluate of mesocrack range on fatigue life by parameter K(sub)α rather than σ(sub)α.

Keywords

References

  1. James, M. N. and Wenfong, L., 1999, 'Fatigue Crack Growth in Austempered and Grey Cast Irons-Stress Rratio Effects in Air and Mine Water,' Materials Science and Engineering, A265, pp. 129-139 https://doi.org/10.1016/S0921-5093(98)01140-X
  2. 박홍식, 진동규, 1993, '오스템퍼링 한 저합금구상흑연주철의 부식마멸특성 및 그 기구에 관한 연구,' 대한기계학회논문집 A권, 제17권 제6호, pp. 1404-1411
  3. 최석림, 윤기혁, 문원진, 강창룡, 김한군, 1998, 'ADI의 조직특성에 미치는 2단 오스테나이트화 처리조건의 영향,' 한국열처리공학회지, 제11권, 제1호, pp. 46-53
  4. Lampman Steven R., 1996, 'Fatigue and Fracture Properties of Cast Irons,' ASM Handbook, Vol. 19, pp. 665-679
  5. 강명순, 박홍식, 1988, '오스템퍼링한 저합금환상흑연주철의 기계적 성질에 관한 연구,' 대한기계학회논문집 A권, 제12권, 제6호, pp. 1296-1302
  6. 鈴木秀人, 植木忠司, 福本昌宏, 1991, 'FCD80 材の高溫疲勞限度に及ぼすプラスマ溶射アルミナ被膜の影響,' 日本機械學會論文集, 57-537A, pp. 1062-1066
  7. 鈴木秀人, 大藪優, 植木忠司, 國尾武, 1985, '鑄造用アルミウム合金AC4A材の片辰り引張度勞强度に及ぼす鑄物寸法, 熱處理の影響,' 日本機械學會論文集, 51-468A, pp. 1977-1982
  8. 中谷辛一郞, 鈴木秀人, 片平和俊, 濟膝一樹, 佐藤秀之, 1991, '表面改質Mg合金鑄物の輕量化設計法の構築と安全性保證,' 日本機械學會論文集, 63-616A, pp. 2673-2678
  9. 鈴木秀人, 國尾武, 1988, 'ミクロとクロの破壞力學,' 27-8, pp. 608-614
  10. 김민건, 김진학, 1999, '오스템퍼링처리한 구상흑연주철의 피로한도에 미치는 기지조직인자와 역학인자의 영향,' 대한기계학회논문집 A권, 제23권 제2호, pp. 287-293
  11. 村上敬宣, 遠藤正造, 1983, '疲勞强度に及ぼす微少缺陷の影響の評價法,' 日本機械學會論文集, 49-438A, pp. 127-135
  12. 村上敬宣, 1989, '微少缺陷と企佐物の影響,' 養賢堂, pp. 233-258