THE EFFECTS OF SALIVARY CONTAMINATION OF ACID-ETCHED ENAMEL ON BRACKET BOND STRENGTH (산부식 후 타액오염이 교정용 접착제의 결합강도에 미치는 영향)

  • Kim, Hyun-Deog;Kim, Jong-Sung;Kim, Jong-Ghee
    • The korean journal of orthodontics
    • /
    • v.26 no.3
    • /
    • pp.309-316
    • /
    • 1996
  • The purpose of this study was to determine the effect of salivary contamination of etched enamel on shear bond strength of a bracket adhered to etched enamel. Eighty extracted human permanent premolars were used in this study. These samples were divided into two groups. Buccal surface of samples were etched in vitro with 38% phosphoric acid for 15 seconds and 60 seconds. Each group was divided into four subgroups. Etched enamel surfaces were contaminated with saliva for 0, 1, 20, 60 seconds, washed and dried. Test surfaces were examined using scanning electron microscope(SEM). The shear bond strength of each sample was determined with a universal testing instrument(Instron Co. Model 4201). Results were as follows; 1. Salivary contamination for 1, 20, 60 seconds did not affect shear bond strength when compared with the uncontaminated enamel group. 2 There was no significant difference(P>.05) in shear bond strength between 15 sec. and 60 sec. etching in uncontaminated enamel groups. 3. When samples were examined using SEM, organic materials coated enamel surface masked the etched pattern partially.

  • PDF

THE EFFECTS OF MECHANICAL AND THERMAL FATIGUE ON THE SHEAR BOND STRENGTH OF ORTHODONTIC ADHESIVES (기계적 및 열적 피로가 교정용 접착제의 결합강도에 미치는 영향)

  • Shin, Wan-Cheal;Kim, Jong-sung;Kim, Jong-Ghee
    • The korean journal of orthodontics
    • /
    • v.26 no.2 s.55
    • /
    • pp.175-186
    • /
    • 1996
  • The purpose of this study was to examine the effects of mechanical and thermal fatigue on the shear bond strength(SBS) of stainless steel mesh brackets bonded to human premolar teeth with 3 no-mix adhesives. The stainless steel mesh bracket was Ormesh(Ormco, .022 slot) and three types of no-mix adhesives were Ortho-one(Bisco), $Monolok^2$(RMO), $System\;1^+$(Ormco). The $10^6$ loadcycles of $17.4{\times}10^2sin2{\pi}ftlg{\cdot}cm$ and the 1,000 thermocycles of 15 second dwell time in each bath of $5^{\circ}C\;and\;55^{\circ}C$ were acturated as mechanical and thermal fatigue stress, and SBS were measured after each fatigue test. The fracture sites were analyzed by stereoscope and scanning electron microscope. The results obtained were summarized as follows; 1. Before thermocycles, $Monolok^2$ showed the highest Knoop hardness number(KHN, $64.03kg/mm^2$) and $System\;1^+$ showed the lowest value($31.60kg/mm^2$). After thermocycling, $Monolok^2$ also showed the highest KHN($38.03kg/mm^2$) and $system\;1^+$ showed the minimum($20.87kg/mm^2$). The KHN of Ortho-one, $Monolok^2,\;System\;1^+$ significantly decreased after thermocycling (P<0.01). 2. In static shear bond test, three adhesives had no significant differences in the SBS(P>0.01). 3. After thermocycling test, $Monolok^2$ showed the maximum SBS($19.34{\pm}2.75MPa$) and Ortho-one showed the minimum SBS($13.66{\pm}2.23MPa$). The SBS of Ortho-one(P<0.01) and $System\;1^+$(P<0.05) significantly decreased after $10^3$ thermocycles. 4. The SBS of three adhesives after $10^6$ loadcycles were similar and were not significantly decreased compared with static group(P>0.01). 5. The failure sites were usually bracket/resin interface in all groups irrespective of experimental conditions.

  • PDF

Effects of direct and indirect bonding techniques on bond strength and microleakage after thermocycling (직접 부착법과 간접 부착법이 열순환 후 부착강도와 미세누출에 미치는 영향에 대한 연구)

  • Ozturk, Firat;Babacan, Hasan;Nalcaci, Ruhi;Kustarci, Alper
    • The korean journal of orthodontics
    • /
    • v.39 no.6
    • /
    • pp.393-401
    • /
    • 2009
  • Objective: The purpose of this study was to compare the shear bond strength (SBS) of brackets and microleakage of a tooth-adhesive-bracket complex bonded with a direct and an indirect bonding technique after thermocycling. Methods: Fifty non-carious human premolars were divided into two equal groups. In the direct bonding group a light-cured adhesive and a primer (Transbond XT) was used. In the indirect-bonding group, a light-cured adhesive (Transbond XT) and chemical-cured primer (Sondhi Rapid Set) were used. After polymerization, the teeth were kept in distilled water for 24 hours and thereafter subjected to thermal cycling (500 cycles). For the microleakage evaluation, 10 teeth from each group were further sealed with nail varnish, stained with 0.5% basic fuchsin for 24 hours, and examined under a stereomicroscope. Fifteen teeth from each group were used for SBS testing with the universal testing machine and adhesive remnant index (ARI) evaluation. Data were analyzed using the Mann-Whitney U test, Chi-square test, and Fisher's exact test. Results: There were no statistical differences on SBS and microleakage between the two bonding techniques. The indirect bonding group had a significantly lower ARI score. Bracket failures were obtained between enamel-resin interfaces. Conclusions: The type of bonding technique did not significantly affect the amount of microleakage and SBS.

Effect of Different Types of Bonding Agent and Application Methods on Shear Bond Strength of Orthodontic Bracket (Bonding agent의 종류 및 적용 방법에 따른 교정용 브라켓의 전단결합강도에 관한 연구)

  • Lee, Jaehee;Kim, Jongsoo
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.44 no.4
    • /
    • pp.419-426
    • /
    • 2017
  • Attachment of the orthodontic bracket conducted during the window opening procedure can result in failure due to various adverse conditions such as blood or saliva contamination, or other wet conditions. For the success of the bracket attachment, reduction of total operation time is crucial. The purpose of this literature is to evaluate the differences between the final resultant shear bond strength of the conventional method of using phosphoric acid and self-etching primer, and that of the operation time-reduced method in which the curing step is omitted subsequent to the primer application. A total of 40 human maxillary incisors were prepared. Group I(control group) and II were etched with 37% phosphoric acid and Group III and IV were conditioned with self-etching primer. Attachment of the group I and III was conducted by manufacturer's instructions. The operation time of Group II and IV was reduced by eliminating the curing step after the primer application. The resultant shear bond strength of each group was measured and an adhesive remnant index (ARI) was recorded. The mean shear bond strength of group I, II, III, and IV were 14.16 MPa, 8.33 MPa, 8.29 MPa, and 6.48 MPa respectively. Significant differences could only be found between the control group and the experimental groups (p < 0.05). The ARI indicated no significant difference among all groups.

A photoelastic study on the initial stress distribution of the upper anterior teeth retraction using combination loop archwire and sliding mechanics (Combination loon archwire와 활주역학을 이용한 상악전치의 후방 견인시 나타나는 초기 응력 분포에 관한 광탄성학적 연구)

  • Yim, Kang-Soon;Lee, Jin-Woo;Cha, Kyung-Suk
    • The korean journal of orthodontics
    • /
    • v.34 no.4 s.105
    • /
    • pp.303-312
    • /
    • 2004
  • An unfavorable tipping movement can occur during the retraction of anterior teeth because orthodontic force is loaded by brackets positioned far from the center of resistance. To avoid this unfavorable movement, a compensating curved wire or lingual root torque wire is used. The purpose of this study is to investigate, using photoelastic material, the distribution of initial stress associated with the retraction of the incisors according to the degree of the compensating curve, to model changes associated with tooth ud alveolar bone structure. The following results were obtained by analysis of the polarizing plate of the effects of initial stress resulting from retraction of the anterior teeth: 1. When the incisors were retracted using combination archwire or sliding mechanics, the maximal polarizing pattern of the apical area decreased as the degree of the compensating owe increased from 0 to 15 to 30. 2. When the incisors were retracted by the combination archwire or sliding mechanics, the maximal polarizing pattern of the canine and premolar area increased as the degree of the compensating curve increased from 0to 15to 30. 3. A lower degree of polarizing patterns were associated with the combination archwire technique than the sliding mechanics technique at a given force. The above results indicate that there is no significant difference between the combination loop archwire technique and sliding mechanics, for the retraction of maxillary anterior teeth with decreased lingual tipping tendency by a compensating curve on the arch wire. However, the use of sliding mechanics is more effective for the prevention of lingual inclination of the anterior teeth, because the hook used in sliding mechanics is closer to the center of resistance of the maxillary anterior teeth.

Effects of conventional and self-etching adhesive systems on bond strength of orthodontic attachments bonded to erupted and unerupted teeth (치아 맹출 유무에 대한 자가부식 접착제에 의한 교정용 부착장치의 접착강도)

  • Nur, Metin;Uysal, Tancan;Yesilyurt, Cemal;Bayram, Mehmet
    • The korean journal of orthodontics
    • /
    • v.40 no.4
    • /
    • pp.267-275
    • /
    • 2010
  • Objective: The aim of this study was to evaluate and compare the shear bond strength (SBS) and failure-mode of orthodontic buttons bonded to erupted and unerupted teeth with conventional and self-etching adhesive systems. Methods: Eighty-four erupted and 84 unerupted, human third-molar teeth were used. For both groups, the buccal surfaces of each tooth were assigned one of the following type of adhesive systems (n = 12). A, Conventional systems: 1, Transbond XT (3M Unitek, Monrovia, CA, USA); 2, Prime & Bond NT (Dentsply/Caulk, Milford, USA); 3, Single Bond (3M ESPE, Minnesota, USA); and B, Self-etching adhesives; 4, Clearfil SE Bond (Kuraray, Okayama, Japan); 5, Transbond Plus (3M Unitek, Monrovia, CA, USA); 6, Clearfil S3 (Kuraray, Tokyo, Japan); 7, G Bond (GC, Tokyo, Japan). The SBSs of the attachments and the adhesive remnant index (ARI) scores were recorded. Data were analyzed with analysis of variance (ANOVA), independent-sample t-test and chi-square tests. Results: When the SBSs of erupted and unerupted teeth were compared, only the Clearfil-SE Bond and G-Bond were significantly different. Bond strengths of all adhesive systems were higher in unerupted teeth than erupted teeth, except the Single-Bond system. Conclusions: When using conventional adhesives, bonding to erupted and unerupted teeth may not be significantly different. However, clinicians need to take into consideration the types of self-etching systems before usage.

The effect of using laser for ceramic bracket bonding of porcelain surfaces (세라믹 브라켓 부착 시 레이저를 이용한 포세린 표면처리 효과)

  • An, Kyung-Mi;Sohn, Dong-Seok
    • The korean journal of orthodontics
    • /
    • v.38 no.4
    • /
    • pp.275-282
    • /
    • 2008
  • Objective: The purpose of this study was to investigate the effect of using laser for ceramic bracket bonding of porcelain surfaces and to compare it with conventional treatment of porcelain surfaces. Methods: Ninety feldspathic porcelain specimens were divided into 9 groups of 10, with each group having different surface treatments performed. Surface treatment groups were orthophosphoric acid, orthophosphoric acid with silane, hydrofluoric acid, hydrofluoric acid with silane, sandblasted, sandblasted with silane, laser etched, laser etched with silane, and glazed surface served as a control group. In the laser etched groups, the specimens were irradiated with 2-watt superpulse carbon dioxide ($CO_2$) laser for 20 seconds. Ceramic brackets were bonded with light-cure composite resin and all specimens were stored in water at $37^{\circ}C$ for 24 hours. Shear bond strength was determined in megapascals (MPa) by shear test at 1 mm/minute crosshead speed and the failure pattern was assessed. For statistical analysis, one-way ANOVA and tukey test were used. Results: Statistical analysis showed significant differences between the groups. The HFA + S group showed the highest mean shear bond strength ($13.92{\pm}1.94\;MPa$). This was followed by SB + S ($10.16\;{\pm}\;1.27\;MPa$), HFA ($10.09\;{\pm}\;1.07\;MPa$), L + S ($8.25\;{\pm}\;1.24\;MPa$), L ($7.86\;{\pm}\;0.96\;MPa$), OFA + S ($7.22\;{\pm}\;1.09\;MPa$), SB ($3.41\;{\pm}\;0.37\;MPa$), OFA ($2.81\;{\pm}\;0.37\;MPa$), G ($2.46\;{\pm}\;1.36\;MPa$), Bond failure patterns of HFA and silane groups, except L + S, were cohesive modes in porcelain while adhesive failure was observed in the control group and the rest of the groups. Conclusions : A 2-watt superpulse $CO_2$ laser etching of porcelain surfaces can provide a satisfactory result for porcelain surface treatment for ceramic bracket bonding. Laser irradiation may be an alternative conditioning method for the treatment of porcelain surfaces.