• Title/Summary/Keyword: 광물 탄산화

Search Result 119, Processing Time 0.028 seconds

Crystallographic and Spectroscopic Characterization of Talc proposed Mineral Carbonation after Heat Treatment (탄산염광물화용 활석의 열처리에 따른 결정학적 분광학적 특성변화)

  • Choi, Weon-Kyung;Cho, Tae-Hwan;Lee, Jae-Keun
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.17 no.1
    • /
    • pp.109-116
    • /
    • 2006
  • The heat treatment characteristics of natural talc sample was investigated in diverse analytical view point. The mass decrease comes to heat treatment was resulted by the continuous and the discontinuous process and the obtained result show very similar two step profiles with 8.9 % mass decrease. The dehydroxylation of -OH groups contained talc crystal was analyzed by spectroscopic method and the crystallographic variations was also observed after heat treatment. According to XPS result, the magnesium hydroxide($Mg(OH)_2$) of untreated talc powder changed to magnesium oxides(MgO) after heat treatment.

Preliminary Study on the Formation Environment of Serpentinite occurring in Ulsan Area (울산지역 사문암의 형성환경 해석을 위한 예비연구)

  • Koh, Sang-Mo;Park, Choong-Ku;Soh, Won-Ju
    • Journal of the Mineralogical Society of Korea
    • /
    • v.19 no.4 s.50
    • /
    • pp.325-336
    • /
    • 2006
  • Domestic serpentinite is one of the important industrial minerals utilizing in the iron manufacturing company such as POSCO in Korea. Serpentinite is distributed in the Ulsan Fe deposit, Andong, Hongseong-Cheongyang, and Gapyeong areas. This study tries to interpret the relationship among the formation of carbonate rocks, iron mineralization, and serpentinite alteration throughout the study of field occurrence, mineralogy, and chemical compositions. Serpentine is formed by the break-down of olivine and pyroxene of parent peridotite. The serpentinization is inferred to be formed by the hydrothermal fluid derived from intruded Cretaceous granite and the addition of meteoric water. Variation of major oxides such as $SiO_2,\;Fe_2O_3$, and MgO in serpentinized rocks are controlled by the degree of serpentinization and Fe mineralization. Variation of $Al_2O_3$ and CaO contents of altered rocks is dependent on the amount of the residual minerals such as calcite and homblende, and on the degree of chloritization. The presence of carbonate rocks reported in the sedimentary origin or igneous origin (carbonatite) provided a geological environment to form skarn type Fe deposit regardless of its origin. The geological processes of Ulsan Fe deposits are inferred to be formed as the order of the formation of carbonate rocks ${\to}$ the intrusion of Cretaceous granite ${\to}$ serpentinization ${\to}$ Fe mineralization by the interprelation of field occurrence and mineralogical characteristics.

Ettringite/Thaumasite Formation, Stability and Their Effect on Deterioration of Concrete (에트린자이트/사우마사이트의 형성 및 안정도와 콘크리트 성능저하에 미치는 영향)

  • 이효민;황진연
    • Journal of the Mineralogical Society of Korea
    • /
    • v.16 no.1
    • /
    • pp.75-90
    • /
    • 2003
  • Ettringite and thaumasite were observed in some concrete. The morphology and occurrence of these minerals were closely examined by performing SEM/EDAX analyses. We also experimentally induced the concrete deterioration using $Na_2SO_4$ solution with application of various environmental conditions. The stability of these minerals and deterioration characteristics under applied experimental conditions were determined. Abundant ettringite formed by“through solution reaction”occurred in many open spaces, and some microscopic ettringite formed by "tophochemical replacement" of calcium aluminate also occurred in cement paste. Severe cracking of cement paste causing premature deterioration was often associated with ettringite location. Under specific condition, ettringite was transformed to thaumasite, tricthloroaluminate, or decomposed. Thaumasite occurred with association of ettrinsite in concrete containing carbonate aggregate being subject to dedolomitization or in some concrete being subject to carbonation. Thaumasite appears to be formed under the similar condition to the general ettringite forming condition, but it formed solid solution with ettringite by substituting pre-existing ettringite. Ettringite can also be transformed to trichloroaluminate in the presence of abundant chlorides, but trichloroaluminate changed back to ettringite in late sulfate attack. It is considered that the substitution reaction direction solely depend on the concentration of chloride and sulfate ion.

The Extraction of Ca in Electric arc Furnace Slag for CO2 Sequestration (CO2고정화(固定化)를 위한 전기로제강(電氣爐製鋼)슬래그의 칼슘성분(成分) 침출(浸出))

  • Youn, Ki-Byoung
    • Resources Recycling
    • /
    • v.22 no.1
    • /
    • pp.64-71
    • /
    • 2013
  • Mineral carbonation has been proposed as a possible way for $CO_2$ sequestration. The electric arc furnace slags consist of calcium, magnesium and aluminum silicates in various combinations. If they could be used instead of natural mineral silicates for carbonation, considerable energy savings and $CO_2$ emissions reductions could be achieved. Indirect aqueous carbonation of the slags consists of two steps, extraction of calcium and carbonation. Acetic acid leaching of electric arc furnace slags had been already studied to extract Ca in them, but it was reported that the carbonation of the extracted $Ca^{2+}$ in the leached solution would suffer from too slow kinetics, even at high pressure of $CO_2$. In this work, to develop more efficient extraction of the electric arc furnace slags, hydrochloric acid leaching to separate calcium from them was studied, and the results were compared with the acetic acid ones. The phase boundary between $Ca^{2+}$ and $CaCO_3$ in the solution with pH was determined by thermodynamic calculations. Hydrochloric acid was more effective than acetic acid for the extraction of Ca in electric arc furnace slag, and there is a possibility to recycle an unreacted hydrochloric acid in the leached solution by electrolysis or evaporation.

The Mineral Carbonation Using Steelmaking Reduction Slag (제강 환원슬래그의 광물탄산화)

  • Ryu, Kyoung-Won;Choi, Sang-Hoon
    • Economic and Environmental Geology
    • /
    • v.50 no.1
    • /
    • pp.27-34
    • /
    • 2017
  • Mineral carbonation for the storage of carbon dioxide is a CCS option that provides an alternative for the more widely advocated method of geological storage in underground formation. Carbonation of magnesium- or calcium-based minerals, especially the carbonation of waste materials and industrial by-products is expanding, even though total amounts of the industrial waste are too small to substantially reduce the $CO_2$ emissions. The mineral carbonation was performed with steelmaking reduction slag as starting material. The steelmaking reduction slag dissolution experiments were conducted in the $H_2SO_4$ and $NH_4NO_3$ solution with concentration range of 0.3 to 1 M at $100^{\circ}C$ and $150^{\circ}C$. The hydrothermal treatment was performed to the starting material via a modified direct aqueous carbonation process at the same leaching temperature. The initial pH of the solution was adjusted to 12 and $CO_2$ partial pressure was 1MPa for the carbonation. The carbonation rate after extracting $Ca^^{2+}$ under $NH_4NO_3$ was higher than that under $H_2SO_4$ and the carbonation rates in 1M $NH_4NO_3$ solution at $150^{\circ}C$ was dramatically enhanced about 93%. In this condition well-faceted rhombohedral calcite, and rod or flower-shaped aragonite were appeared together in products. As the concentration of $H_2SO_4$ increased, the formation of gypsum was predominant and the carbonation rate decreased sharply. Therefore it is considered that the selection of the leaching solution which does not affect the starting material is important in the carbonation reaction.

Biomineralization Processes Using Fly Ash for Carbon Sequestration (석탄회를 이용하는 탄소 격리용 생광물화 작용)

  • Yul Roh;Moon, Ji-Won;Yungoo Song;Moon, Hi-Soo
    • Journal of the Mineralogical Society of Korea
    • /
    • v.16 no.2
    • /
    • pp.171-180
    • /
    • 2003
  • The objective of this study is to investigate biogeochemical processes to sequester $CO_2$and metals utilizing metal-rich fly ash (MRFA). Microbial conversion of $CO_2$into sparingly soluble carbonate minerals has been studied using MRFA under different $pCO_2$and different bicarbonate concentrations. Scaling from test tube to fermentation vessels (up to 4-L) using metal-reducing bacteria and MRFA has proved successful at sequestering carbon dioxide and metals. $CO_2$sequestration via precipitation processes using MRFA may complement the process of $CO_2$capture from fossil fuel plants while potentially stabilizing fly ash wastes.

In vitro CaCO3 Crystallization at Room Temperature and Atmospheric Pressure Using Recombinant Proteins GRP_BA and GG1234 (재조합단백질 GRP_BA 및 GG1234를 이용한, 상온상압조건에서의 In vitro 탄산칼슘 결정화)

  • Son, Chaeyeon;Song, Wooho;Choi, Hyunsuk;Choi, Yoo Seong
    • Korean Chemical Engineering Research
    • /
    • v.57 no.2
    • /
    • pp.205-209
    • /
    • 2019
  • The exquisite structure and attractive biological properties of biominerals have great potential and increased interest for use in a wide range of medical and industrial applications. Calcium carbonate biomineralization, mainly controlled by shell matrix proteins, has been used as a representative model to understand the biomineralization mechanism. In this study, in vitro calcium carbonate crystallization was carried out under room temperature and atmospheric pressure using recombinant shell matrix protein GRP_BA and artificial shell matrix protein GG1234. Both proteins inhibited the growth of typical rhombohedral calcite crystals in the calcium carbonate crystallization using $CaCl_2$ solution and $(NH_4)_2CO_3$ vapor, and spherulitic calcite crystals with rosette-like structures were synthesized in both the presence of GRP_BA and GG1234. These results might be caused by the properties of block-like domain structure and intrinsically disordered proteins. We expect that this study can contribute to enhance understanding of the calcium carbonate biomineralization controlled by shell matrix proteins.

Occurrence and Chemical Composition of Carbonate Mineral from Wallrock Alteration Zone of Janggun Pb-Zn Deposit (장군 연-아연 광상의 모암변질대내 탄산염 광물의 산상 및 화학조성)

  • Bong Chul Yoo
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.36 no.3
    • /
    • pp.167-183
    • /
    • 2023
  • The Janggun Pb-Zn deposit consists of Mn orebody, Pb-Zn orebody and Fe orebody. The Mn orebody composed of manganese carbonate orebody and manganese oxide orebody on the basis of their mineralogy and genesis. The geology of this deposit consists of Precambrian Weonnam formation, Yulri group, Paleozoic Jangsan formation, Dueumri formation, Janggum limestone formation, Dongsugok formation, Jaesan formation and Mesozoic Dongwhachi formation and Chungyang granite. This manganese carbonate orebody is hydrothermal replacement orebody formed by reaction of lead and zinc-bearing hydrothermal fluid and Paleozoic Janggum limestone formation. The wallrock alteration that is remarkably recognized with Pb-Zn mineralization at this hydrothermal replacement orebody consists of mainly rhodochrositization with minor of dolomitization, pyritization, sericitization and chloritization. Carbonates formed during wallrock alteration on the basis of paragenetic sequence are as followed : Ca-dolomite (Co type, wallrock) → ankerite and Ferroan ankerite (C1 type, early stage) → ankerite (C2 type) → sideroplesite (C3 type) → sideroplesite and pistomesite (C4 type, late stage). This means that Fe and Mn elements were enriched during evolution of hydrothermal fluid. Therefore, The substitution of elements during wallrock alteration beween dolomitic marble (Mg, Ca) and lead and zinc-bearing hydrothermal fluid (Fe, Mn) with paragenetic sequence is as followed : 1)Fe ↔ Mn and Mn ↔ Mg, Ca, Fe elements substitution (ankerite and Ferroan ankerite, C1 type, early stage), 2)Fe ↔ Mn, Mn ↔ Mg, Ca and Mg ↔ Ca elements substitution (ankerite, C2 type), 3)Fe ↔ Mn, Fe ↔ Ca and Mn ↔ Mg, Ca elements substitution (sideroplesite, C3 type), and 4)Fe ↔ Mg, Fe ↔ Mn and Mn ↔ Mg, Ca elements substitution (sideroplesite and pistomesite, C4 type, late stage)

Arsenic Removal Mechanism of the Residual Slag Generated after the Mineral Carbonation Process in Aqueous System (광물탄산화 공정 이후 발생하는 잔사슬래그의 수계 내 비소 제거 기작)

  • Kim, Kyeongtae;Latief, Ilham Abdul;Kim, Danu;Kim, Seonhee;Lee, Minhee
    • Economic and Environmental Geology
    • /
    • v.55 no.4
    • /
    • pp.377-388
    • /
    • 2022
  • Laboratory-scale experiments were performed to identify the As removal mechanism of the residual slag generated after the mineral carbonation process. The residual slags were manufactured from the steelmaking slag (blast oxygen furnace slag: BOF) through direct and indirect carbonation process. RDBOF (residual BOF after the direct carbonation) and RIBOF (residual BOF after the indirect carbonation) showed different physicochemical-structural characteristics compared with raw BOF such as chemical-mineralogical properties, the pH level of leachate and forming micropores on the surface of the slag. In batch experiment, 0.1 g of residual slag was added to 10 mL of As-solution (initial concentration: 203.6 mg/L) titrated at various pH levels. The RDBOF showed 99.3% of As removal efficiency at initial pH 1, while it sharply decreased with the increase of initial pH. As the initial pH of solution decreased, the dissolution of carbonate minerals covering the surface was accelerated, increasing the exposed area of Fe-oxide and promoting the adsorption of As-oxyanions on the RDBOF surface. Whereas, the As removal efficiency of RIBOF increased with the increase of initial pH levels, and it reached up to 70% at initial pH 10. Considering the PZC (point of zero charge) of the RIBOF (pH 4.5), it was hardly expected that the electrical adsorption of As-oxyanion on surface of the RIBOF at initial pH of 4-10. Nevertheless it was observed that As-oxyanion was linked to the Fe-oxide on the RIBOF surface by the cation bridge effect of divalent cations such as Ca2+, Mn2+, and Fe2+. The surface of RIBOF became stronger negatively charged, the cation bridge effect was more strictly enforced, and more As can be fixed on the RIBOF surface. However, the Ca-products start to precipitate on the surface at pH 10-11 or higher and they even prevent the surface adsorption of As-oxyanion by Fe-oxide. The TCLP test was performed to evaluate the stability of As fixed on the surface of the residual slag after the batch experiment. Results supported that RDBOF and RIBOF firmly fixed As over the wide pH levels, by considering their As desorption rate of less than 2%. From the results of this study, it was proved that both residual slags can be used as an eco-friendly and low-cost As remover with high As removal efficiency and high stability and they also overcome the pH increase in solution, which is the disadvantage of existing steelmaking slag as an As remover.

Phase equilibria between coexisting minerals in the talc ores and process of talc formation in the Daeheung Talc Deposits, Korea (대흥활석광상에 있어서 공존하는 광물의 상평형과 활석화 과정)

  • 이상헌
    • The Journal of the Petrological Society of Korea
    • /
    • v.3 no.2
    • /
    • pp.156-170
    • /
    • 1994
  • The talc ore deposits can be divided into chloritic and dolomitic ores according to mineral assemblages. The former is mainly composed of chlorite and talc accompanied with dolomite, muscovite and opaque mineral, and the latter of dolomite and talc with serpentine, calcite and magnesite in places. Talc was originated from chlorite and serpentine. Carbonate minerals were formed either directly from the introduced hydrothermal solution or secondarily as a by-product of steatitization of chlorite and serpentine. The process of talc formation may be governed by the chemical composition of the host rocks and the amount and/or chemical composition of the hydrothermal solution which may be different in places. However, the representative reactions producing talc from chlorite and serpentine are as follows : (1) chlorite+$Mg^{++}+Si^{4+}+H_2O$=talc, (2) chlorite+$Mg^{++}+Si^{4+}+Ca^{++}+CO_2+O_2+H_2O$=talc+ dolomite+ magnesite, and (3) serpentine +$Mg^{++}+Fe^{++}+Si^{4+}+Ca^{++}+CO_2+H_2O$=talc+dolomite. The reactions indicate that the carbonate minerals can be formed when the hydrothermal solution have high $fO_2$ and $fCO_2$. The steatitization might be proceeded by the hydrothermally metasomatic reaction between chlorite schist or chlorite gneiss intercalated in the granitic gneiss and hydrothermal solution accompanied to the wet granitization.

  • PDF