• Title/Summary/Keyword: 고성능감수제

Search Result 72, Processing Time 0.029 seconds

A Study for Reducing the Slump Loss of Concrete Using High Range Water Reducing Admixture (고성능감수제(高性能減水劑)를 사용한 콘크리트의 유동성(流動性) 손실(損失)을 저감(低減)시키기 위한 연구(硏究))

  • Moon, Han Young;Kim, Ki Hyung
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.12 no.3
    • /
    • pp.81-90
    • /
    • 1992
  • This study gives results of 1aboratory investigations to minimize the slump loss of concrete using high range water reducing admixture (HRWR). Various factors influencing on the slump loss such as cement type, HRWR type and dosage time are investigated. The acquired results indicated that 30 minutes delayed dosage of HRWR is very effective on reducing the slump loss though this tendency makes a difference to some extent according to cement and HRWR type. For the most part, the more usage of HRWR increases, the higher the slump loss occurs and concrete using ordinary portland cement has the highest slump loss and concrete using fly ash 20% replacement cement with HRWR of naphthalene type has the good effect on reducing the slump loss.

  • PDF

The Fluidity of High Flowing Concrete According to the Component Ratio of Superplasticizer (고성능감수제 구성비율에 따른 고유동콘크리트의 유동특성)

  • Kim Moo-Han;Kim Yong-Ro;Kim Jae-Hwan;Ho Jang-Jong;Lee Tae-Hee
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.2 s.80
    • /
    • pp.147-154
    • /
    • 2004
  • It is the aim of this study to propose the fundamental data for the establishment of the application and qualify standard of the mixed type superplasticizer after investigating and comparing the fluidity of high flowing concrete according to the component ratio of superplasticizer such as naphthalene sulfonated and melamine sulfonated. The results of this study were shown as the followings; 1) The fluidity and adsorption ratio of cement-paste were improved according to the increasing of naphthalene sulfonated component ratio, and apparent viscosity of cement-paste was improved according to the Increasing of melamine sulfonated component ratio. 2) In case of using the granulated blast-furnace slag, the fluidity of cement-paste was considerably good and the adsorption ratio was decreased and in case of using fly-ash, the apparent viscosity and adsorption ratio of cement-paste were improved. 3) The dispersive capacity performance of concrete can be improved by means of the increasing of naphthalene sulfonated component ratio. Also the viscosity and early strength can be improved by means of the increasing of melamine sulfonated component ratio.

The Effect of the Amount of Polycarboxylate Superplasticizer on the Properties of Ultra-High Performance Fiber-Reinforced Concrete (폴리칼본산계 고성능감수제 사용량이 초고성능 섬유보강 콘크리트의 성질에 미치는 영향)

  • Kang, Su-Tae
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.38 no.1
    • /
    • pp.11-18
    • /
    • 2018
  • As the amount of polycarboxylate superplasticizer varied from 1.2% to 3.0% of the mass of binder, the change in the flowability & rheological properties, and strength of UHPFRC was investigated with experiments. The test results presented that the increase in the amount of superplasticizer was effective in improving the flowability up to 1.8%, but addition more than 1.8% was hardly beneficial for enhancing the flowability and rhelogical properties. Compressive strengths with different amounts of superplasticizer showed that the strength with 1.8% was slightly higher than that of 1.2%, but the amount more than 1.8% caused strength reduction, which was higher as the amount increased. The results in flexural strength according to the amount of superplasticizer showed a similar trend with the results in compressive strength. When the effect of compressive strength and fiber distribution characteristics on the flexural strength was analysed separately, it was found that high amount of superplasticizer caused an effect of fiber distribution in addition to the effect of compressive strength on flexural strength. This effect seems to be closely related to the results of flowability or rheological properties.

Performance Comparision of The $\beta$-NSF Based Superplasticizers Used in Domestic Area (국내에서 유통되고 있는 $\beta$-NSF계 고성능감수제의 성능 비교)

  • 조헌영;노재성;홍성수;이기준
    • Magazine of the Korea Concrete Institute
    • /
    • v.3 no.4
    • /
    • pp.125-132
    • /
    • 1991
  • $\beta$-NSF 계통의 콘크리트용 고성능감수계를 독자적으로 제조하여(제품C)국내에서 유통되고 있는 $\beta$-NSF계 고성능감수제들과 콘크리트의 유동화특성 및 고강도콘크리트의 특성을 비교검토한 결과는 다음과 같다. 가. $\beta$-NSF계 고성능감수제중에서 M제품과 C제품의 유동화성능 및 고강도성능이 다른 감수제에 비하여 전반적으로 좋게 나타났다. 나. $\beta$-NSF계 고성능감수제를 첨가한 모든 콘크리트는 감수제를 사용하지 않은 일반 콘크리트에 비하여 흐름도의 경시변화가 크며, 동결융해에 대한 저항성이 현저히 떨어지는 것으로 나타났다.

A study on the Effects of Superplasticizres on the Engineering Properties of Plain Concrete(II) (고성능감수제가 콘크리트의 공학적 특성에 미치는 영향(II))

  • 박승범
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.28 no.2
    • /
    • pp.74-86
    • /
    • 1986
  • 유동화콘크리트의 공학적 특성에서 시간-의존거동을 확인하기 위하여,나프타렌 설폰산염 폴리머 고축합물인 Rheobuild 1000과 메라민 설폰산염 고축합물인 NP-20의 고성능감수제를 사용한 유동화콘크리트와 보통콘크리트를 제조하여 비교.고찰을 행하였으며, 고성능감수제의 종류 및 함량이 콘크리트의 공학적 특성에 미치는 영향을 구명하기 위하여 재령 3일, 14일, 28일, 60일, 90일, 180일의 압축강도를 측정, 조기 및 장기압축강도를 조사하였고, 인장강도 및 탄성 변형에 미치는 영향을 조사하였다. 또한 습윤 및 에어콘디션의 양생조건하에서 시간의 경과에 따른 건조수축 및 크리이프 변형을 조사.분석함으로써 유동화콘크리트의 시간-의존거동을 확인하였다. 실험결과, 사용 고성능 감수제의 종류에 따라 차이는 있으나, 고성능 감수제의 사용은 일반적으로 워커빌리티 성능을 개선하고 압축 및 인장도를 크게 향상시키며, 탄성계수는 보통의 콘크리트에 비하여 높게 나타났다. 또한 건조수축 및 크리프 변형의 감소에 매우 양호한 결과를 나타내어 앞으로 건설용 용도로써 효과적인 것으로 판단되었다.

  • PDF

A Study on the Flow Loss of Cement-Based Composites Using High Range Water Reducing Admixture (고성능감수제를 사용한 시멘트복합체의 유동성 손실에 대한 연구)

  • 문한영;김기형
    • Magazine of the Korea Concrete Institute
    • /
    • v.4 no.2
    • /
    • pp.119-126
    • /
    • 1992
  • 고강도 시멘트 복합체의 유동성 손실을 감소시키기 위한 연구의 일환으로 시멘트계 입자에 대한 고성능감수제의 흡착특성, 현탄액 속에서의 응집특성을 관찰하여 시멘트풀과 모르터의 유동성과 관련시켜 고찰하였다. 본 연구결과 알루미네이트계 화합물이 많이 함유된 보통포틀랜드 시멘트의 흡착률이 가장 크며, 시멘트풀 및 모르처의 유동성 손실이 작았으며 나프탈린계 고성능 감수제가 유동성 손실면에서 얼마간 유리하였다.

Strength of CNT Cement Composites with Different Types of Surfactants and Doses (분산제의 종류 및 사용량에 따른 CNT 보강 시멘트 복합체의 강도변화)

  • Ha, Sung-Jin;Kang, Su-Tae;Lee, Jong-Han
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.2
    • /
    • pp.99-107
    • /
    • 2015
  • This study was aimed to investigate the difference in strength of Carbon Nanotube (CNT) reinforced cement mortars with different types of surfactants and doses. In the experimental program, CTAB, SDBS and TX10 which were common surfactants adopted to improve CNTs dispersion in fabricating CNT composites in many industrial fields were included and superplasticizer which was revealed to be effective to disperse CNTs especially in CNT reinforced cementitious composites were added as well. Superplasticizer presented less strength reduction in cement mortar and more strength gain by adding CNTs among four types of surfactants. Higher dosage of superplasticizer caused lower strength of cement mortar. Adding CNTs of 0.4 wt.% or less to cement didn't show strength enhancement by adding CNTs but 0.8 wt.% of CNTs resulted in strengthening effect after all. Finally, a combination of 0.1 wt.% of CNTs, superplasticizer and sonication treatment could lead to strength improvement by adding CNTs in cement mortar.