Failure and Flexural Behavior of Reinforced Concrete Beams Strengthened with CFRP Strips (탄소섬유판(CFRP Strip)으로 보강된 철근콘크리트 부재의 파괴거동 및 휨 거동 특성)

  • Lim, Dong Hwan;Park, Sung Hwan
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.28 no.2A
    • /
    • pp.289-295
    • /
    • 2008
  • The purpose of this study was to examine the flexural behavior of reinforced concrete beams strengthened with CFRP strips. A total of 12 rectangular beams were tested. Test variables in this study were the shapes, bonded length and the number of longitudinal layers of CFRP strips. From the experimental study, flexural capacity of the beams strengthened with CFRP strips significantly increased compared to the reinforced concrete beam without a CFRP strip. Maximum increase of ultimate strength was found about 120% more than the control beam. In this test, most of the strengthened beams failed suddenly due to the debonding of CFRP strips. It is also observed that the debonding of the strip was initiated in the flexural zone of the beam and propagated rapidly to the end of the beam. The ultimate tensile strains of CFRP strips in this test were occurred at the level of 36% of rupture tensile strength of the CFRP strip, and an analytical approach to compute the flexural strength of reinforced beams strengthened with CFRP strips based on the effective stresses was conducted.

Fracture Behaviour Analysis of the Crack at the Specimen with the Type of Mode I Composed of the Bonded Carbon Fiber Reinforced Plastic (접합된 CFRP로 구성된 Mode I형 시험편 크랙의 파괴 거동 해석)

  • Lee, Jung-Ho;Cho, Jae-Ung;Cheon, Seong-Sik;Kook, Jeong Han
    • Composites Research
    • /
    • v.28 no.6
    • /
    • pp.356-360
    • /
    • 2015
  • In this paper, the carbon fiber reinforced plastic is processed as the double cantilever beam in order to estimate the fracture behavior of composite and is carried out with the static analysis as the mode I. The specimen sizes are 25 mm, 30 mm, 35 mm and 40 mm. And the material property is used with carbon. As the analysis result of mode I, the adhesive part is detached latest by the small force at the specimen thickness of 25 mm. The largest force is happened at the specimen thickness of 40 mm. The defection of the adhesive interface is shown slowest at the displacement of 9.75 mm at the specimen thickness of 25 mm. And the defection is shown quickest at the displacement of 7.82 mm at the specimen thickness of 40 mm. This defection is due to the fracture of specimen. The result of this study on the defection of the adhesive interface and the reaction force due to this defection is thought to be contributed to the safe structural design of the carbon fiber reinforced plastic.

Strengthening Capacity of Bridge Deck Strengthened with Carbon Fiber Rod and Polymer Mortar (고강도 폴리머 모르타르 및 탄소섬유 봉(Rod)으로 보강된 교량 바닥판의 보강성능)

  • Sim Jongsung;Moon Do-Young;Ju Mm-Kwan
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.2 s.80
    • /
    • pp.213-220
    • /
    • 2004
  • This paper deals with an enhanced structural capacity of reinforced concrete bridge deck strengthened with carbon fiber rod (CFR) which is subjected to monotonic and cyclic loads. Strengthening variables considered in this test were evenly and unevenly strengthening type. To evaluate strengthening capacity for these two strengthening types, load-carrying capacity and crack and failure pattern from the failure test were analyzed and fatigue response were examined. According to the test results, all the strengthened specimens showed punching shear failure as a result of premature failure of bonding interface between mortar and concrete. In the case of strengthening capacity, it was observed that the strengthened specimens was more effective in strength, stiffness and fatigue endurance limit than the unstrengthened specimen. In addition, the unevenly strengthening method (CR-UE) was more effective than the evenly strengthening method (CR-E).

A COMPARATIVE STUDY OF BOND STRENGTH OF RECYCLED BRACKETS (재생 브라켓의 전단접착강도에 관한 비교 연구)

  • Shur, Cheong-Hoon;Choi, Eun-Ah
    • The korean journal of orthodontics
    • /
    • v.28 no.4 s.69
    • /
    • pp.641-657
    • /
    • 1998
  • This study was undertaken to compare the bond strength and the fracture site of new and recycled brackets according to the base design. 252 sound premolars extracted for orthodontic treatment were collected and Type I, Type II, Type III brackets were divided into four groups by recycling method Each bracket was then bonded to an extracted premolar. Instron Universal Testing Machine(model W) was used to measure the shear bond strength, and the surface of the recycled brackets were viewed in SEM For the analysis of the results, one way ANOVA and Scheffe's multiple range test was executed using the SPSSWIN program. 1. The shear bond strength showed statistically significant difference according to the bracket base design(p<0.001). Type III bracket(round indentation base, micro-etched) showed the highest bond strength, Type I bracket(foil-mesh base) was second, and Type II bracket(grooved integral base, micro-etched) was last. 2. The effect of recycling on the bond strength was different according to bracket type. The shear bond strength of Type I, Type II brackets showed the smallist reduction when treated for 1 minute in Big Jane(p<0.05), but the shear bond strength of Type III brackets showed no statistically significant difference according to recycling method(p>0.05). 3. In Type I, Type II brackets, frequent fracture site was bracket-resin interface, but in Type III brackets, about half of the resin was retained on the tooth surface frequently. 4. The shear bond strength was highest when about half of the resin was retained on the tooth surface(p<0.05). 5. The resin remnant on the bracket base after recycling had no effect on the shear bond strength.

  • PDF

An Investigation on the Behavior of Fracture Mechanics as the Type of Mode I at Specimen Bonded with Tapered Carbon Fiber Reinforced Plastic (경사진 CFRP로 접합된 시험편에서의 Mode 1 형 파괴역학적 거동에 관한 연구)

  • Lee, Jung-Ho;Cho, Jae-Ung;Cheon, Seong Sik
    • Composites Research
    • /
    • v.29 no.2
    • /
    • pp.85-89
    • /
    • 2016
  • This paper aims at estimating the fracture behavior at the bonded part of composite material. CFRP is manufactured as the type of TDCB. The static analysis of Mode 1 due to the configuartion factor of m is carried out. Four kinds of specimens have the configuartion factor(m) of 2, 2.5, 3 and 3.5. As the study result, the displacements at specimens are shown to be similar each other in these four cases. At m of 3.5, the reaction force becomes highest as 412 N and is shown to be improved as much as 14% by comparing m of 2. The data on defection of the bonded interface and reaction force are thought to be contributed to the structural design of CFRP and the safe design.

THE EXPRESSION OF OSTEONECTIN AND OSTEOCALCIN IN THE EXPERIMENTAL TOOTH MOVEMENT IN RAT (백서의 실험적 치아이동시 osteonectin 및 osteocalcin의 발현)

  • Bae, Sung-Real;Kim, Sang-Cheol
    • The korean journal of orthodontics
    • /
    • v.28 no.5 s.70
    • /
    • pp.699-716
    • /
    • 1998
  • This study was designed to evaluate the expression of non-collagenous protein in periodontal tissue during the experimental movement of rat incisors, by LSAB(labelled streptavidine biotin) immunohistochemical staining for osteonectin and osteocalcin. Twenty seven Sprague-Dawley rats were divided into a control group(3 rats) and 6 experimental groups(24 rats) where 75g of force was applied from helical springs across the maxillary incisors. Rats of experimental groups were sacrificed at 12 hours, 1, 4, 7, 14 and 28 days after force application, respectively. And the tissues of a control group and experimental groups were studied immunohistochemically and histologically. The results were as follows : 1. Until 28 days after force application, periodontal fibers had been strectched on tension side and compressed in pressure side of all the experimental groups, and the arrangement of periodontal fibers had not been recovered yet. 2. The expression of osteonectin in control group was rare in dentin, cementum and osteocyte, and was mild in odontoblasts and matrix of alveolar bone. 3. The expression of osteocalcin in control group was negative in gingiva, osteoblasts, osteocyte and cementum, and was rare in predentin, capillaries in pulp and periodontal ligament and the matrix of alveolar bone. 4. There was no difference in the expression of osteocalcin or osteonectin in dentin, cementum, pulp, odontoblasts, between of control and of experimental groups. 5. The expression of osteonectin in intermaxillary suture got the peak in 7-day and was declined after 14-day. The expression of osteocalcin remained in a same degree since it became mild in 14-day. 6. The expression of osteonectin in pressure side of periodontal ligament of experimental group was rare, which was similar to control group. But in tension side, it was increased until 14-day aftrer which it was declined. 7. The expression of osteocalcin in periodntal ligament was rare in 12-hour to 14-day, but became severe in 28-day, which was greater in tension side than in pressure side, and in the periodontal fiber next to alveolar bone than to tooth surface. 8. The expression of osteocalcin in alveolar bone was rare until 14-day in pressure side, but became moderate in 28-day. The expression of osteonectin was increased from 7-day by time dependency, which was greater in tension side than in pressure side.

  • PDF

Morphological, Protein and pectin alteration following Treatment with Surfactant in Epidermis of Mouse (Mouse 피부조직의 계면활성제에 의한 형태학적변화, 면역반응에서의 Protein 및 Lectin변화양상)

  • 최정숙
    • Journal of the Society of Cosmetic Scientists of Korea
    • /
    • v.23 no.2
    • /
    • pp.118-151
    • /
    • 1997
  • Allergic contact dermatitis is a common skin disease resulting from specific immumologic sensitization to topically applied various allergen. Purpose of this study was to investigate skin morphologic chganges by light microscopic, changes of protein band by SDS-PAGE in the skin treated on the surfactant. Furthermore, lectin histochemistry is used to know the chagnges of the terminal sugar of the glycoconjugate in the skin treated on the surfactant. The results were as follows : The 1 day of treated group was indicated the enlargement of capillary, the 3 days of treated group was showed that the cytoplasm was eosinophlic by the pyknotic of nucleus. The 6 days of treated group was observed hyperkeratinoid, increased of inflammation cells to epithelium. The 9 days of treated group was appeares that serum crust was sheded and formed a acanthosis. But dermis layer was cytoplasmic vaculation and enlargement of intercellular space. The 12 days treated group made up new epidermis layer of seven layer and of observed an decreased in quantity of inflammation cells. The mast cell of degranulated type was increased in treated surfactnat. It was secreating granules hold histamin, serotonin and heparin. Accordingly, protein band of electrophortic phase was observed a sudden changes since 3 days treated group. At observeation of the cell-surface glycoconjugates, LCA, PNA, SBA and WGA lectin positive cells but inducated lectin negative cells in Con-A. Furthermore, PNA and SBA showed stroger positive reaction as treated surfactant group.

  • PDF

The effect of denture adhesives on the retention of complete denture (의치 접착제가 총의치의 유지력에 미치는 영향에 관한 연구)

  • Yoon, Yu-Mi;Choi, Yu-Sung;Lee, Joon-Seok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.48 no.2
    • /
    • pp.87-93
    • /
    • 2010
  • Purpose: The purpose of this study was to compare the retention of the two denture adhesives with a silicone edentulous model and a resin denture base in vitro study. Material and methods: The experimental groups were used two denture adhesives and classified into 5 subgroups each. Subgroups were divided by the number of times the saliva sprayed. The control group was used synthetic saliva only. Dislodging tensile strengths were applied to the resin denture base using Instron in 3 directions ; vertical, lateral, and anterior-posterior. Results: The retention of two denture adhesives was increased significantly than saliva alone (P <.05). In each denture adhesives, the retention of saliva sprayed first was decreased than denture adhesive alone, but it didn't have significant differences. Whenever saliva sprayed repeated, the retention was decreased significantly than saliva sprayed first (P <.05). In each denture adhesives, vertical retentive force was highest than lateral and anterior-posterior retentive forces, and anterior-posterior retentive force was higher than lateral retentive force. This results were significantly different (P < .05). Significant differences of the retentive ability among two denture adhesives were not observed. Conclusion: From the results, use of the denture adhesives resulted in improved retentive ability of denture. Especially retentive force was highest in vertical direction.

Bond strength of orthodontic brackets bonded to enamel with a self-etching primer after bleaching and desensitizer application (미백과 탈감작제 도포 후 셀프 에칭 프라이머를 이용한 브라켓 접착 시 법랑질과 브라켓 간의 결합 강도)

  • Attar, Nuray;Korkmaz, Yonca;Kilical, Yasemin;Saglam-Aydinatay, Banu;Bicer, Ceren Ozge
    • The korean journal of orthodontics
    • /
    • v.40 no.5
    • /
    • pp.342-348
    • /
    • 2010
  • Objective: The aim of this study was to compare the shear bond strengths (SBS) of orthodontic brackets bonded to enamel with a self-etching primer after bleaching, desensitizer application and combined treatment. Methods: Forty-eight premolars were randomly divided into four groups, each with n = 12 premolar samples. The four groups were; Group1: 15% hydrogen-peroxide office bleaching agent (Illumin$\acute{e}$ Office-IO), Group 2: IO + BisBlock Oxalate Dentin-Desensitizer, Group 3: Bis Block Oxalate Dentin-Desensitizer, Group 4: No treatment (control). Twenty-four hours after bonding, the specimens were tested in SBS at a crosshead speed of 5 mm/min until the brackets debonded. The failure mode of the brackets was determined by a modified adhesive remnant index. Results: Bleaching, bleaching and desensitizer treatment, and desensitizer treatment alone all significantly reduced SBS of the orthodontic brackets ($p$ = 0.001). No statistically significant difference was found between Group 1, Group 2 and Group 3 (Group 1-Group 2, $p$ = 0.564; Group 1-Group 3, $p$ = 0.371; Group 2-Group 3, $p$ = 0.133). The predominant mode of failure for the treatment groups (Group1, Group 2 and Group 3) was at the enamel-adhesive interface leaving 100% of the adhesive on the bracket base. Conclusions: Bleaching and desensitizer treatment should be delayed until the completion of orthodontic treatment.

Reinforcement Effect of Reinforced Concrete Beams Strengthened with Grid-type Carbon Fiber Plastics (격자형 탄소섬유로 보강한 R/C보의 보강효과)

  • Jo, Byung-Wan;Tae, Ghi-Ho;Kwon, Oh-Hyuk
    • Journal of the Korea Concrete Institute
    • /
    • v.15 no.3
    • /
    • pp.377-385
    • /
    • 2003
  • Flexural characteristics of the R.C beams strengthened with newly-developed grid-type carbon fiber plastics(CFRP-GRIDS) were investigated. The tests were conducted under the four-points load to the failure to investigate the strengthening effects of CFRP-GRIDS on the beams. Results showed that initial cracks appeared in the boundary layers of fibers embedded in the newly-placed mortar concrete slowly progressed to the direction of supports and showed fracture of fiber plastics and brittle failure of concrete in compression in sequence after the yielding of steel reinforcement. Accordingly, the appropriate area of Grid-type carbon-fiber plastics in the strengthening design of deteriorated RC structures should be limited and given based on the ultimate strength design method to avoid the brittle failure of concrete structures.