A Study on Properties of Early Strength Development of the Concrete (콘크리트의 조기강도 발현특성에 관한 연구)

  • Kang, Chang-Woon;Lee, Jae-Sam;Kim, Jung-Sik;Sung, Yong-Hwan;Ryu, Deug-Hyun
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.11a
    • /
    • pp.541-544
    • /
    • 2008
  • Recently, due to the increase of high-rise buildings construction, many researches for making harden of concrete earlier and remove of forms faster are being performed to reduce construction period. The purpose of this study is to analysis which mixing condition and curing temperature of early strength concrete. Porperties of concrete by the different factors, such as the type of active admixtures, mineral admixtures, curing temperature, the amount of binder, etc. Through the test of concrete using the different type of admixture, PC type was more excellent than PNS type admixture. The concrete Strength remarkably will be able to confirm that decreases from temperature below 12$^{\circ}C$.

  • PDF

Compressive Strength Generation Properties of Concrete using a Large Amount of Industrial Byproduct (산업부산물을 다량 사용한 콘크리트의 압축강도 발현 특성 검토)

  • Kim, Yong-Ro;Song, Young-Chan;Park, Jong-Ho;Jeong, Yong
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.2
    • /
    • pp.67-73
    • /
    • 2011
  • In this study, it was investigated compressive strength generation of concrete using high volume mineral admixture obtaining fundamental data for the application of concrete structure in construction field. For this, it was evaluated compressive strength with unit binder contents($310{\sim}410kg/m^3$), replacement ratio of mineral admixture(70~90%), unit water contents($140{\sim}150kg/m^3$) and curing temperature in the normal strength range. Also, after producing mock-up structure, hydration heat and compressive strength generation was evaluated to examine properties in the concrete member. In case of concrete using a large amount of industrial byproducts which was reviewed in this study, it is possible to secure compressive strength more than 24MPa at age 28days with about $13^{\circ}C$ ambient temperature of curing condition and that is considered to be applied to structure at construction site.

  • PDF

Characteristics of Natural Hydraulic Lime Mortar Mixed with Basalt Fiber (바잘트 섬유를 혼합한 천연수경성석회 모르타르의 특성)

  • Moon, Ki-Yeon;Cho, Jin-Sang;Cho, Kye-Hong;Hong, Chang-Woo
    • Resources Recycling
    • /
    • v.24 no.6
    • /
    • pp.61-68
    • /
    • 2015
  • In this study, the strength properties of NHL based mortar with blending basalt fiber were investigated. In the first step, it was evaluated that physical properties of NHL based mortar according to mixing method of four types of basalt fiber and then mixing method of one type was selected. As a result of assessment, it showed that the physical properties with mixing method of dry blending were better than that of wet blending and mixing method that basalt fiber pre-mixed with NHL for 5 min in a blender was selected and water and aggregate were finally added. Secondly, the investigation of blending fiber length on the compressive and flexural strength for basalt fiber reinforced NHL based mortars was carried out. The compressive strength was decreased with adding fiber, and the flexural strength was increased more than plain mortar. In the case of adding 6 mm fiber, the compressive and flexural strength were improved more than that of others.

An Experimental Study on the Early Strength Development Properties of Concrete According to Curing Condition and Used Materials (사용재료 및 양생조건에 따른 콘크리트의 조기강도발현 특성에 관한 실험적 연구)

  • Lee, Sang-Soo;Song, Ha-Young;Lee, Ji-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.20 no.6
    • /
    • pp.721-729
    • /
    • 2008
  • The purpose of this study is to investigate the engineering properties of concrete for the early strength development. As a result of reviewing it by establishing each experimental factor and level, the cement had more excellent quality performance in CHC and HESPC than OPC. This study has shown that the PC series admixture was more excellent in side of elapsed time (aging) and early strength development than PNS series admixture. In addition, there was much difference according to the curing temperature, but the early strength development showed the considerable vulnerability in curing temperature below $12^{\circ}C$. To satisfy the strength requirements of 5 MPa/18 hr this study has shown that it needed the curing temperature over $17^{\circ}C$ to the minimum in OPC, over $14^{\circ}C$ in CHC, and over $11^{\circ}C$ in HESPC. On the other hand, as to the strength properties according to W/C, the less W/C was, the more strength development was excellent. If this study is to be used in construction filed on a basis of this result, this researcher is considered as possible of the economic execution of construction by advancing the early strength and by the reduction of construction cost according to shortening construction duration.

A Study on the improvement of Strength delay according to Low Temperature of Cold Weather Concrete (한중콘크리트의 저온에 의한 강도지연 개선연구)

  • Lee, Sang-Soo
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.1
    • /
    • pp.51-59
    • /
    • 2012
  • The cold weather concrete poured in the winter season can cause the problem of the Due to recent high-rise building is made. In this research, the nominal mix of the early strength in concrete tried to be set through the mixing proportion experiment for each empirical variable and each component strength properties for the early strength improvement tries to be examined. In the cold weather concrete experiment, the cement and high early strength (type3) cement improving in OPC than OPC was excellent. The polycarboxylic acid based compound was exposed to be excellent in the intensity revelation properties. Because the using of the fly ash was disadvantageous it was excluded from this experiment. It showed the optimum temperature for the intensity revelation up over $12^{\circ}C$.

  • PDF

A Study on Strength Development and Drying Shrinkages of Recycled Concrete (재생콘크리트의 강도발현 및 건조수축 특성연구)

  • 이진용
    • Magazine of the Korea Concrete Institute
    • /
    • v.9 no.6
    • /
    • pp.217-223
    • /
    • 1997
  • 재생콘크리트의 압축강도와 휨강도는 재생골재의 혼입량이 증가할수록 감소하였으며 플라이애쉬를 혼화재로 사용할 때 그 양이 증가할수록 재생콘크리트의 조기 압축강도는 떨어졌다. 골재원에 따른 압축강도는 재생골재의 혼입량이 적을수록, 양생기간이 길어질수록 증가하엿으나, 전반적으로 비슷한 강도변화의 경향을 보여주고 있다. 재생콘크리트의 휨강도 발현은 보통 콘크리트와 비슷하나, 휨강도에 대한 압축강도비는 보통 콘크리트에 비하여 낮았다. 재생콘크리트의 건조수축은 재생골재의 혼입량이 증가할수록 증가하였으며 , 특히 재령2주와3주사이에 건조수축량이 보통 콘크리트에 비해 월등히 높았다.

A Study on the Initial Shear Strength Characteristics of Sudden Gelation Grout (순결형 그라우트의 초기 전단강도 특성에 대한 연구)

  • Heo, Hyung-Seok;Park, Inn-Joon
    • Journal of the Korean Geotechnical Society
    • /
    • v.36 no.9
    • /
    • pp.33-44
    • /
    • 2020
  • In order to analyze the shear strength characteristics of the grout with sudden gelation in the pre-hardening state, the viscosity of the mixture and the indoor vane shear test were performed. The grout was prepared according to the water-cement (w/c) ratio and the shear strength test was conducted. The plastic-state shear strength of grout was affected by the w/c ratio, so the lower the w/c ratio, the higher the initial shear strength was, and the longer the curing time was, the higher the shear strength was. The maximum shear strength occurred at the faster rotation angle as the higher shear strength was developed, and the lower shear strength occurred at the larger rotation angle. In addition, it was confirmed that the pre-hardening grout rapidly decreased in strength after the maximum shear strength was gained, and converged at a certain level after the rotation angle of the vane blade was about 70° to 90°.

An Experimental Study on Strength Properties of Concrete Using Blast-Furnace Slag Subjected to Freezing at Early Age (초기재령에서 동결을 받은 고로슬래그 콘크리트의 강도발현특성에 관한 실험적 연구)

  • Choi, Sung-Woo;Ban, Seong-Soo;Ryu, Deuk-Hyun;Choi, Bong-Joo
    • Journal of the Korea Concrete Institute
    • /
    • v.15 no.1
    • /
    • pp.43-51
    • /
    • 2003
  • Recently, to consider financial and constructive aspect usage of Admixture such as Blast-Furnace Slag and Fly-Ash, are increased. Also the use of cold-weather-concrete is increased. Blast-Furnace Slag, a by-product of steel industry, have many advantage to reduce the heat of hydration, increase in ultimate strength and etc. But it also reduces early-age strength, so it is prevented from using of Blast-Furnace Slag at cold-weather-concrete. In this study, for the purpose of increasing usage of Blast-Furnace Slag at cold-weather-concrete, it is investigated the strength properties of concrete subjected to frost damage for the cause of early age curing. The factors of this experience to give early frost damaged were Freezing temperature(-1, -10, $-15^{\circ}C$), Early curing age(0, 12, 24, 48hour), Freezing times(0, 12, 24, 48hour). According to this study, if early curing is carried out before haying frost damage, the strength of concrete used admixture, subjected to frost damage, is recovered. And that properties are considered, the effect of using admixture like blast-furnace-slag, is very high

Early Strength Development Properties of Concrete using Early Strength Improvement Type Cement (조기강도 개선형 시멘트를 사용한 콘크리트의 조기강도 발현 특성)

  • Park, Kyu-Yeon;Kim, Yong-Ro;Kim, Gyu-Yong
    • Journal of the Korea Institute of Building Construction
    • /
    • v.13 no.3
    • /
    • pp.227-234
    • /
    • 2013
  • In this research, early strength development performance of early strength improvement type ordinary cement which is economically feasible early strength cement(Type III), improved early strength ordinary cement(Type I), was estimated to derive minimum curing temperature and proper water to cement ratio according to cement for early strength development through examination of fresh concrete properties and compressive strength according to water to cement ratio curing $10^{\circ}C$, $15^{\circ}C$ and $20^{\circ}C$ to suggest fundamental data for practical use of early strength concrete.

An Experimental Study on the Properties of Early-Strength for high performance Concrete according to Mix Design (배합설계 조건에 따른 고성능 콘크리트의 조기강도 발현특성에 관한 연구)

  • Choi, Sumg-Woo;Yoo, Jong-Su;Beak, Chul-Woo;Kim, Jeong-Sik;Ryu, Deung-Hyun
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.231-232
    • /
    • 2009
  • In this study, the properties of early strength development for high performance concrete according to mix design were examined In particulara, we examined the mineral addmixture influence for mix design.

  • PDF