• Title/Summary/Keyword: $Ti/WO_3$

Search Result 153, Processing Time 0.038 seconds

Development of Ultra-Thin TiO2 Coated WO3 Inverse Opal Photoelectrode for Dye-Sensitized Solar Cells (염료감응형 태양전지로의 응용을 위한 얇은 TiO2가 코팅 된 WO3 역오팔 광전극의 개발)

  • Arunachalam, Maheswari;Kwag, Seoui;Lee, Inho;Kim, Chung Soo;Lee, Sang-Kwon;Kang, Soon Hyung
    • Korean Journal of Materials Research
    • /
    • v.29 no.8
    • /
    • pp.491-496
    • /
    • 2019
  • In this study, we prepare pure $WO_3$ inverse opal(IO) film with a thickness of approximately $3{\mu}m$ by electrodeposition, and an ultra-thin $TiO_2$ layer having a thickness of 2 nm is deposited on $WO_3$ IO film by atomic layer deposition. Both sets of photoelectrochemical properties are evaluated after developing dye-sensitized solar cells(DSSCs). In addition, morphological, crystalline and optical properties of the developed films are evaluated through field-emission scanning electron microscopy(FE-SEM), High-resolution transmission electron microscopy(HR-TEM), X-ray diffraction(XRD) and UV/visible/infrared spectrophotometry. In particular, pure $WO_3$ IO based DSSCs show low $V_{OC}$, $J_{SC}$ and fill factor of 0.25 V, $0.89mA/cm^2$ and 18.9 %, achieving an efficiency of 0.04 %, whereas the $TiO_2/WO_3$ IO based DSSCs exhibit $V_{OC}$, $J_{SC}$ and fill factor of 0.57 V, $1.18mA/cm^2$ and 50.1 %, revealing an overall conversion efficiency of 0.34 %, probably attributable to the high dye adsorption and suppressed charge recombination reaction.

Highly Ordered Mesoporous Metal Oxides as Catalysts for Dehydrogenation of Cyclohexanol (메조기공을 갖는 다양한 금속 산화물 촉매를 이용한 사이클로헥사놀의 탈수소화 반응)

  • Lee, Eunok;Jin, Mingshi;Kim, Ji Man
    • Korean Chemical Engineering Research
    • /
    • v.51 no.4
    • /
    • pp.518-522
    • /
    • 2013
  • Cyclohexanone is important intermediate for the manufacture of caprolactam which is monomer of nylron. Cyclohexanone is generally produced by dehydrogenation reaction of cyclohexanol. In this study, highly mesoporous metal oxides such as meso-$WO_3$, meso-$TiO_2$, meso-$Fe_2O_3$, meso-CuO, meso-$SnO_2$ and meso-NiO were synthesized using mesoporous silica KIT-6 as a hard template via nano-replication method for dehydrogenation of cyclohexanol. The overall conversion of cyclohexanol followed a general order: meso-$WO_3$ >> meso-$Fe_2O_3$ > meso-$SnO_2$ > meso-$TiO_2$ > meso-NiO > meso-CuO. In particular, meso-$WO_3$ significantly showed higher activity than the other mesoporous metal oxides. Therefore, the meso-$WO_3$ has wide range of application possibilities for dehydrogenation of cyclohexanol.

Characteristic Evaluation of SCR catalyst using Aluminum dross (알루미늄 폐드로스를 활용한 SCR 탈질촉매 제조 및 특성평가)

  • Bae, Min A;Kim, Hong Dae;Lee, Man Sig
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.14 no.10
    • /
    • pp.4672-4678
    • /
    • 2013
  • Aluminum dross is formation at the surface of the molten metal as the latter reacts with the furnace atmosphere and it was an unavoidable by-product of the aluminum production process. However aluminum dross was usually landfilled or disposed without treatment, causing much environmental damage. The purpose of this study is to investigate the possibility of ceramic catalyst support using recycled Al dross. The recycled Al dross was made into SCR catalyst by mixing with $WO_3$, $V_2O_5$ and $TiO_2$. The $V_2O_5-WO_3/TiO_2-Al_2O_3$ SCR catalyst was observed with XRF, XRD and BET. $V_2O_5-WO_3/TiO_2-Al_2O_3$ SCR strength was measured by Universal Testing Machine(UTM). As the added $Al_2O_3$, streagth is increased. And the NOx removal activity was observed by MR(Micro-Reactor). The temperatures ranging from $350^{\circ}C$ and $400^{\circ}C$, $V_2O_5-WO_3/TiO_2-Al_2O_3$ SCR catalyst De-NOx performance result of showed excellent activity over 90% at application condition.

Effects of CuO and ${B_2}{O_3}$Additions on Microwave Dielectric Properties of $PbWO_4$-$TiO_2$Ceramic (CuO ${B_2}{O_3}$첨가에 따른 $PbWO_4$-$TiO_2$세라믹스의 마이크로파 유전특성)

  • 최병훈;이경호
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.11
    • /
    • pp.1046-1054
    • /
    • 2001
  • Effects of B$_2$O$_3$and CuO addition on the microwave dielectric properties of the PbWO$_4$-TiO$_2$ceramics were investigated in order to use this material as an LTCC material for fabrication of a multilayered RF passive components module. We found that PbWO$_4$could be used as an LTCC material because of its low sintering temperature (8$50^{\circ}C$) and fairy good microwave dielectric properties($\varepsilon$$_{r}$=21.5, Q$\times$f$_{0}$=37200 GHz and $\tau$$_{f}$ =-31 ppm/$^{\circ}C$). In order to stabilize $\tau$$_{f}$ of PbWO$_4$, TiO$_2$was added to the PbWO$_4$and the mixture was sintered at 8$50^{\circ}C$. A near zero $\tau$$_{f}$ value (+0.2 ppm/$^{\circ}C$) was obtained with 8.7 mol% TiO$_2$addition. $\varepsilon$r and Q$\times$f$_{0}$ values were 22.3 and 21400 GHz, respectively. It was believed that the decrement of Q$\times$f$_{0}$ value with TiO$_2$addition was resulted from increasing grain boundary. In order to improve Q$\times$f$_{0}$, various amounts of B$_2$O$_3$and CuO were added to the 0.913PbWO$_4$-0.087TiO$_2$mixture. The optimum amount of CuO was 0.05 wt%. At this addition, the 0.913PbWO$_4$-0.087TiO$_2$ceramic showed $\varepsilon$$_{r}$=23.5, $\tau$$_{f}$ =-2.2ppm/$^{\circ}C$, and Q$\times$f$_{0}$=32900 GHz after sintered at 8$50^{\circ}C$. In case of B$_2$O$_3$addition, the optimum amount range was 1.0~2.5 wt% at which we could obtain following results; $\varepsilon$$_{r}$=20.3~22.1, Q$\times$f$_{0}$=48700~54700 GHz, and $\tau$$_{f}$ =+2.4~+8.2ppm/$^{\circ}C$.

  • PDF

Effect of ACF and WO3 from ACF/WO3/TiO2 Composite Catalysts on the Photocatalytic Degradation of MO Under Visible Light

  • Meng, Ze-Da;Song, Da-Ye;Zhu, Lei;Park, Chong-Yeon;Choi, Jong-Geun;Oh, Won-Chun
    • Journal of the Korean Ceramic Society
    • /
    • v.48 no.4
    • /
    • pp.282-287
    • /
    • 2011
  • ACF and $WO_3$ modified $TiO_2$ composites (ACF/$WO_3$/$TiO_2$) were prepared using a sol-gel method. The composites were characterized by Brunauer.Emmett.Teller (BET) surface area measurements, X-ray diffraction (XRD), energy dispersive X-ray (EDX) analysis and scanning electron microscope (SEM) analysis. A methyl orange (MO) solution under visible light irradiation was used to determine the photocatalytic activity. The degradation of the MO was determined using UV/Vis spectrophotometry. An increase in photocatalytic activity was observed and attributed to an increase of the photo-absorption effect by the $WO_3$ and the cooperative effect of the ACF.

The interfacial properties of th eanneled SiO$_{2}$/TiW structure (열처리된 SiO$_{2}$/TiW 구조의 계면 특성)

  • 이재성;박형호;이정희;이용현
    • Journal of the Korean Institute of Telematics and Electronics A
    • /
    • v.33A no.3
    • /
    • pp.117-125
    • /
    • 1996
  • The variation of the interfacial and the electrical properties of SiO$_{2}$TiW layers as a function of anneal temperature was extensively investigated. During the deposition of SiO$_{2}$ on TiW chemical bonds such as SiO$_{2}$, TiW, WO$_{3}$, WO$_{2}$ TiO$_{2}$ Ti$_{2}$O$_{5}$ has been created at the SiO$_{2}$/TiW interface. At the anneal temperature of 300$^{\circ}C$, WO$_{3}$ and TiO$_{2}$ bonds started to break due to the reduction phenomena of W and Ti and simultaneously the metallic W and Ti bonds started to create. Above 500$^{\circ}C$, a part of Si-O bonds was broken and consequently Ti/W silicide was formed. Form the current-voltage characteristics of Al/Sico$_{2}$(220$\AA$)/TiW antifuse structure, it was found that the breakdown voltage of antifuse device wzas decreased with increasing annealing temperature for SiO$_{2}$(220$\AA$)/TiW layer. When r, the insulating property of antifuse device of the deterioration of intermetallic SiO$_{2}$ film, caused by the influw of Ti and W.W.

  • PDF

NO REDUCTION PROPERTY OF Pt-V2O5-WO3/TiO2 CATALYST SUPPORTED ON PRD-66 CERAMIC FILTER

  • Kim, Young-Ae;Choi, Joo-Hong;Bak, Young-Cheol
    • Environmental Engineering Research
    • /
    • v.10 no.5
    • /
    • pp.239-246
    • /
    • 2005
  • The effect of Pt addition over $V_2O_5-WO_3/TiO_2$ catalyst supported on PRO-66 was investigated for NO reduction in order to develop the catalytic filter working at low temperature. Catalytic filters, $Pt-V_2O_5-WO_3/TiO_2/PRD$, were prepared by co-impregnation of Pt, V, and W precursors on $TiO_2$-coated ceramic filter named PRD (PRD-66). Titania was coated onto the pore surface of the ceramic filter using a vacuum aided-dip coating method. The Pt-loaded catalytic filter shifted the optimum working temperature from $260-320^{\circ}C$(for the catalytic filter without Pt addition) to $190-240^{\circ}C$, reducing 700 ppm NO to achieve the $N_x$ slip concentration($N_x\;=\;NO+N_2O+NO_2+NH_3$) less than 20 ppm at the face velocity of 2 cm/s. $Pt-V_2O_5-WO_3/TiO_2$ supported on PRD showed the similar catalytic activity for NO reduction with that supported on SiC filter as reported in a previous study, which implies the ceramic filter itself has no considerable interaction for the catalytic activity.

Photochemical hydrogen production from coupled semiconductor systems : CdS-WO3/RuO2, CdS-TiO2 (혼합반도체 시스템에서의 광화학적 수소제조 : CdS-WO3/RuO2, CdS-TiO2)

  • Suh, J.K.;Heo, G.S.
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.4 no.2
    • /
    • pp.5-15
    • /
    • 1993
  • Hydrogen production in visible light with the following semiconductor systems, $CdS-WO_3$, $CdS-TiO_2$, have been investigated in the presence of redox catalyst (Pt, $RuO_2$). MeOH, EtOH, isopropanol, sulfide/sulfite mixture, lactic acid were used as sacrifical reagents. The optimal condition for $H_2$ evolution was found to be in qgueous lactic acid media for $CdS-WO_3/RuO_2$. The photochemical efficiency for this system was 1.05 % and the $H_2$ evolution rate was 26.5ml/min. at $6.07{\times}10^{-5}$ einstein/sec photon rate

  • PDF

Thermal Deactivation of Plate-type V2O5-WO3/TiO2 SCR Catalyst (Plate-type V2O5-WO3/TiO2 SCR 촉매의 열적 비활성화 특성)

  • Cha, Jin-Sun;Park, Jin-Woo;Jeong, Bora;Kim, Hong-Dae;Park, Sam-Sik;Shin, Min-Chul
    • Applied Chemistry for Engineering
    • /
    • v.28 no.5
    • /
    • pp.576-580
    • /
    • 2017
  • In the present paper, the thermal deactivation characteristics of plate-type commercial $V_2O_5-WO_3/TiO_2$ SCR catalyst were investigated. For this purpose, the plate-type catalyst was calcined at different temperatures ranging from $500^{\circ}C$ to $800^{\circ}C$ for 3 hours. Structural and morphological changes were characterized byXRD, specific surface area, porosity, SEM-EDS and also NOx conversion with ammonia according to the calcine temperature. The NOx conversion decreased with increasing calcine temperature, especially when the catalysts were calcined at temperatures above $700^{\circ}C$. This is because the crystal phase of $TiO_2$ changed from anatase to rutile, and the $TiO_2$ grain growth and $CaWO_4$ crystal phase were formed, which reduced the specific surface area and pore volume. In addition, $V_2O_5$, which is a catalytically active material, was sublimated or vaporized over $700^{\circ}C$, and a metal mesh used as a support of the catalyst occurred intergranular corrosion and oxidation due to the formation of Cr carbide.