Selenide Glass Optical Fiber Doped with $Pr^{3+}$ for U-Band Optical Amplifier

  • Chung, Woon-Jin;Seo, Hong-Seok;Park, Bong-Je;Ahn, Joon-Tae;Choi, Yong-Gyu
    • ETRI Journal
    • /
    • v.27 no.4
    • /
    • pp.411-417
    • /
    • 2005
  • $Pr^{3+}-doped$ selenide glass optical fiber, which guarantees single-mode propagation of above at least 1310 nm, has been successfully fabricated using a Ge-Ga-Sb-Se glass system. Thermal properties such as glass transition temperature and viscosity of the glasses have been analyzed to find optimum conditions for fiber drawing. Attenuation loss incorporating the effects of an electronic band gap transition, Rayleigh scattering, and multiphonon absorption has also been theoretically estimated for the Ge-Ga-Sb-Se fiber. A conventional double crucible technique has been applied to fabricate the selenide fiber. The background loss of the fiber was estimated to be approximately 0.64 dB/m at 1650 nm, which can be considered fairly good. When excited at approximately 1470 nm, $Pr^{3+}-doped$ selenide fiber resulted in amplified spontaneous emission and saturation behavior with increasing pump power in a U-band wavelength range of 1625 to 1675 nm.

  • PDF

THz Optical Properties of Pr3+-Doped Selenide Glasses (Pr3+ 도핑된 셀레나이드 유리의 테라헤르츠 광학 특성)

  • Kang, Seung Beom;Chung, Dong Chul;Kwak, Min Hwan
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.30 no.11
    • /
    • pp.745-750
    • /
    • 2017
  • Terahertz time-domain spectroscopy has been used to study the optical properties of $Pr^{3+}-doped$ selenide glasses. The complex refractive indexes of $Pr^{3+}-selenide$ glasses were measured in a frequency range from 0.3 to 1.5 THz. The real and imaginary refractive indexes increased with increasing frequency and $Pr^{3+}$ ion concentration. The obtained result indicated that the phonon modes of the $Pr^{3+}-doped$ selenide glasses shift to lower frequencies with the concentration of $Pr^{3+}$ ions. The theory of far-infrared absorption in amorphous materials was used to analyze the results. The measured data showed that the disorder-induced terahertz absorption increased with increasing $Pr^{3+}$ ion concentration.

$Pr^{3+}-and$ $Pr^{3+}/Er^{3+}$-Doped Selenide Glasses for Potential $1.6{\mu}m$ Optical Amplifier Materials

  • Choi, Yong-Gyu;Park, Bong-Je;Kim, Kyong-Hon;Heo, Jong
    • ETRI Journal
    • /
    • v.23 no.3
    • /
    • pp.97-105
    • /
    • 2001
  • $1.6\;{\mu}m$ emission originated from $Pr^{3+}:\;(^3F_3,\;^3F_4)\;{\longrightarrow}\;^3H_4$ transition in $Pr^{3+}-\;and\;Pr^{3+}/Er^{3+}$-doped selenide glasses was investigated under an optical pump of a conventional 1480 nm laser diode. The measured peak wavelength and fullwidth at half-maximum of the fluorescent emission are ~1650nm and 120nm, respectively. A moderate lifetime of the thermally coupled upper manifolds of ${\sim}212{\pm}10{\mu}s$ together with a high stimulated emission cross-section of ${\sim}(3{\pm}1){\times}10^{-20}\;cm^2$ promises to be useful for $1.6{\mu}m$ band fiber-optic amplifiers that can be pumped with an existing high-power 1480 nm laser diode. Codoping $Er^{3+}$ enhances the emission intensity by way of a nonradiative $Er^{3+}:\;^4I_{13/2}\;{\longrightarrow}\;Pr^{3+}:\;(^3F_3,\;^3F_4)$ energy transfer. The Dexter model based on the spectral overlap between donor emission and acceptor absorption describes well the energy transfer from $Er^{3+}$ to $Pr^{3+}$ in these glasses. Also discussed in this paper are major transmission loss mechanisms of a selenide glass optical fiber.

  • PDF

Determination of optical properties of Pr3+-doped selenide glasses of Ge-Sb-Se system using spectroscopic ellipsometry (분광타원법을 이용한 Pr 첨가 Ge-Sb-Se 계열 셀레나이드 유리의 굴절률 결정)

  • 신상균;김상준;김상열;최용규;박봉제;서홍석
    • Korean Journal of Optics and Photonics
    • /
    • v.14 no.6
    • /
    • pp.594-599
    • /
    • 2003
  • By using the spectroscopic ellipsometry, we have measured and analyzed the optical characteristics of P $r^3$$^{+}$-doped selenide glasses of Ge-Sb-Se system, a strong candidate material for U band fiber amplifiers. The ellipsometric spectra measured in the transparent wavelengths range of the material were all fitted to a model consisting of ambient/roughness/thin fil $m_strate structures to obtain simultaneously the optical properties such as refractive index, in terms of Sellmeier parameters and film structure of P $r^3$$^{+}$-doped selenide glasses. Repeated measurements on different positions in both polished faces rendered to verify positional dependence of measured spectre-ellipsometric data. Hence, the model made possible the analysis of the optical characteristics of the glasses. Even though surface roughness was mainly responsible for the position dependencies, the averaged refractive indexes were as precise as to reflect the minute compositional change tantamount to 1 mol%. The measured refractive indexes are useful for design of core and clad compositions of single-mode selenide optical fibers.