• 제목/요약/키워드: $PbO_2$

검색결과 2,067건 처리시간 0.023초

Ga$_2$O$_3$ 첨가에 따른 SiO$_2$-PbO-K$_2$O-Al$_2$O$_3$계 적외선 센서용 Glass fiber의 광학적 특성 (Optical properties of the glass fiber by adding Ga$_2$O$_3$ in the SiO$_2$-PbO-K$_2$O-Al$_2$O$_3$ system for Infrared sensor)

  • 윤상하;강월호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 춘계학술대회 논문집
    • /
    • pp.68-71
    • /
    • 1996
  • In the study, the thermal and optical properties of SiO$_2$-PbO-K$_2$O-Al$_2$O$_3$ g1asses were investigated. According to Ga$_2$O$_3$ addictions, the properties of bulk glass, transition temperature and softening temperature were increased, whereas thermal expansion coefficient was decreased; In the optical properties, refractive index was increased, and IR cut-off wavelength was enlarged from 4.64$\mu\textrm{m}$ to 5.22$\mu\textrm{m}$. But, the optical loss of fiber was decreased.

  • PDF

화학증착법에 의한 PbTiO3박막의 조성분석 및 전기적성질에 관한 연구 (Study on the Composition Analysis and Electrical Properties of Chemical Vapor Deposited PbTiO3 Thin Film)

  • 이혜용;윤순길;김호기
    • 한국세라믹학회지
    • /
    • 제26권5호
    • /
    • pp.670-676
    • /
    • 1989
  • The PbTiO3 is well known materials having remarkable ferroelectric, piezoelectric, and pyroelectric properties. PbTiO3 thin films with a perovskite structure were successfully fabricated on titanium substrate by chemical vapor deposition. These films were characterized according to composition, crystal structure, and electrical properties. Semi-quantitative compositional analysis of the deposited films was made by Auger Electron Spectroscopy(AES). The PbTiO3 film deposited on titanium substrate at the deposition temperature 75$0^{\circ}C$, the Ti(C2H5O)4 fraction 0.15, and O2 partial pressure 0.06atm, has a columnar structure and grows with(001) preferred orientation, and has stoichiometric composition. A clear dielectric transition and offset in the dc conductivity near the transition temperature(48$0^{\circ}C$) were observed in the deposited lead titanate film.

  • PDF

스퍼터링법에 의한 강유전성 $Pb_{1+x}$($Fe_{0.5}$$Nb_{0.5}$)$O_3$ 박막의 제조 및 전기적 특성에 관한 연구 (Preparation and Electrical Properties of the Ferroelectric $Pb_{1+x}$($Fe_{0.5}$$Nb_{0.5}$)$O_3$ Thin Films by Sputtering Method)

  • 장영일;김장엽;임대순;김병호
    • 한국세라믹학회지
    • /
    • 제35권3호
    • /
    • pp.294-302
    • /
    • 1998
  • $Pb_{1+x}$($Fe_{0.5}$$Nb_{0.5}$)$O_3$ films have been synthesized on Pt/Ti/$SiO_2$/Si substrates using rfmagnetron sputtering Concentration of Fe and Nb in the deposited films was adjusted to near stoichiometry through the control of target composition, Films deposited with adjusted to near stoichiometry showed better electrical properties such as dielectic and leakage characteristics. Crystallinity and dielectric constant increased with increasing excess PbO upto 9 mol% This study also showed that dielectric constant and leakage current characteristics improved by optimum content of $O_2$ flow during deposition.

  • PDF

BiPbSrCaCuO 초전도 벌크의 Magnetic Suspension (Magnetic Suspension Effect of BiPbSrCaCuO Superconducting Bulk)

  • 이상헌
    • 한국전기전자재료학회논문지
    • /
    • 제17권5호
    • /
    • pp.545-551
    • /
    • 2004
  • Magnetic suspension effect has been studied by using superconductor of BiPbSrCaCuO ceramics containing Ag$_2$O. Magnetic flux measurements of a toroidal magnet revealed a concave shaped field distribution with a null field along the axis of the torus at the point where the field reversed. The suspension effect was observed only for the Ag$_2$O doped and field cooled sample which is attributed to the enhanced flux pinning due to the field cooled condition. It has been cleared that Ag$_2$O acts as pinning center which plays an important role to the magnetic suspension effect. Magnetic repulsive force which affects a superconductor located in magnetic flux from toroidal magnet has been investigated. It has been concluded that the magnetic suspension effect arises from the interaction between the pinning effect and the diamagnetic effect.

PZ-PT-PMWS의 압전 및 전기기계적 특성 (The Piezoelectic and electromechanical Characteristics of PZ-PT-PMWS)

  • 홍종국;이종섭;채홍인;윤만순;정수현;임기조
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.403-406
    • /
    • 2000
  • The piezoelectric properties and the doping effect of N $b_2$ $O_{5}$ and Mn $O_2$for 0.95PbZ $r_{x}$ $Ti_{x}$ $O_3$+0.05Pb(M $n_{0.42}$ $W_{0.26}$S $b_{0.32}$) $O_3$ compositions have been investigated. In the composition of 0.95PbZ $r_{0.54}$ $Ti_{0.46}$ $O_3$+0.05Pb(M $n_{0.42}$ $W_{0.26}$S $b_{0.32}$) $O_3$the Values Of $k_{p}$ find and $\varepsilon$$_{33}$ $^{T}$ are maximized, but $Q_{m}$ Was minimized ( $k_{p}$ =0.51, $Q_{m}$ =1750). The grain size was suppressed and the uniformity of grain was improved with doping concentration of N $b_2$ $O_{5}$ for 0.95PbZ $r_{0.54}$ $Ti_{0.46}$ $O_3$+0.005Pb(M $n_{0.42}$ $W_{0.26}$S $b_{0.32}$) $O_3$sample. The values of $k_{p}$ increased and the values of $Q_{m}$ slightly decreased when 0.5 wt% of N $b_2$ $O_{5}$ is doped. And the values of $k_{p}$ was the same formation of the N $b_2$ $O_{5}$ dopant when 0.5 wt% of M $n_2$ $O_{5}$ is doped. But the values of $Q_{m}$ was deeply decreased when 0.5 wt% of Mn $O_2$is doped. As a experiment results under high electric field driving, this piezoelectric ceramics are very stable. Conclusively, piezoelectric ceramic compsiton investigated at this paper is suitable for application to high power piezoelectric devices.. devices..ices.. devices..

  • PDF

$Fe_{2}O_{3}$$Nb_{2}O_{5}$가 첨가된 0.57Pb$(Sc_{1/2}Nb_{1/2})O_3-0.49PbTiO_3$계 세라믹스의 유전 및 압전특성 (Dielectric & Piezoelectric Properties of 0.57Pb$(Sc_{1/2}Nb_{1/2})O_3-0.43PbTiO_3$ Ceramics with $Fe_{2}O_{3}$, $Nb_{2}O_{5}$ Additions)

  • 김창석;이능헌;지승한;김진수;이상훈;전석환
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 추계학술대회 논문집 학회본부 C
    • /
    • pp.974-977
    • /
    • 1999
  • PSN-PT 2성분계 압전세라믹스의 상도로부터 유전적, 압전적 특성이 양호한 MPB (Morphotropic phase boundary)부근의 조성을 선택하여 도너 도펀트인 $Nb_{2}O_{5}$와 억셉터 도펀트인 $Fe_{2}O_{3}$를 각각 $0{\sim}0.9wt%$ 첨가하여 유전 및 압전특성을 비교, 연구해보았다. 시편모두 $1250^{\circ}C$ 이상에서 이론밀도의 96%이상의 값을 얻을 수 있었고 상온, 1kHz에서 $Fe_{2}O_{3}$의 경우 0.1wt% 첨가된 시편에서 ${\varepsilon}_r$=2054의 최대 비유전율이 나타났으며, 0.7wt% 첨가된 시편에서는 $tan{\delta}$=0.49%의 최소 유전 손실값을 얻었다. $Fe_{2}O_{3}$가 0.1wt%, 0.3wt%로 첨가되었을 때 각각 $K_p$=58%, Qm=222의 값을 얻을 수 있었다.

  • PDF

Dielectric Properties in the Pb1-3x/2Lax[(Mg1/3Ta2/3)0.66Zr0.34]O3 Systems

  • Kim, Yeon Jung
    • Applied Science and Convergence Technology
    • /
    • 제26권4호
    • /
    • pp.70-73
    • /
    • 2017
  • The dielectric constant and loss of poling/non-poling was measured in the $Pb_{1-3x/2}La_x[(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ samples. The addition of $La^{3+}$ to the $Pb_{1-3x/2}La_x[(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ did not cause a large change in grain size. But the addition of $La^{3+}$ did show transition temperature, which shifted toward low temperature in the $Pb[(Mg_{1/3}Ta_{2/3})Zr]O_3$ systems. In addition, the dielectric and pyroelectric properties (${\varepsilon}{\sim}20000$, $p{\sim}0.03C/m^2K$) of this system using $La^{3+}$ have been greatly improved. Pyroelectrics $Pb_{0.97}La_{0.02}(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ system was found to have a relatively high ferroelectric FOMs ($F_V{\sim}0.035m^2/C$, $F_D{\sim}0.52{\times}10^{-4}Pa^{-1/2}$) at room temperature. Spontaneous polarization showed a value of $0.27{\sim}0.35C/m^2$ in the composition added to $La^{3+}$. The piezoelectric constant ($d_{33}=350{\sim}490pC/N$) and electromechanical coupling factor ($k_P=0.25{\sim}0.35$) are obtained in $Pb_{1-3x/2}La_x[(Mg_{1/3}Ta_{2/3})_{0.66}Zr_{0.34}]O_3$ compositions with $La^{3+}$ dopant.

PZT/BT 세라믹 후막의 구조적 특성에 관한 연구 (A study on the Structural Properties of PZT/BT thick film)

  • 이상헌;임성수;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2005년도 춘계학술대회 논문집
    • /
    • pp.57-59
    • /
    • 2005
  • Ploycrystalline $Pb(Zr_{0.5},Ti_{0.5})O_3$ and $BaTiO_3$ powder were prepared by sol-gel process. The alumina substrate were sintered at $1400^{\circ}C$ with bottom electrode of Pt for 2 hours. The Pb(Zr0.5,Ti0.5)O3 / BaTiO3 multilayered thick films with laminating times were fabricated on alumina substrate by screening printing method. The obtained thick films were sintered at $800^{\circ}C$ with upper electrode of Ag paste for 1 hour. Structural properties of Pb(Zr0.5,Ti0.5)O3 / BaTiO3 multilayered thick films were investigated. As a result of the Differential Thermal Analysis(DTA) of Pb(Zr0.5,Ti0.5)O3, exothermic peak was observed at around $650^{\circ}C$. The X-ray diffraction (XRD) patterns indicated that BaTi03 and Pb(Zr0.5,Ti0.5)O3 phases and porosities were formed in the interface of Pb(Zr0.5,Ti0.5)O3 / BaTiO3 multilayered thick films.

  • PDF