Effect of MnO2 Addition on Dielectric and Piezoelectric Properties of 0.985[Li0.04(Na0.545K0.46)0.96(Nb0.81Ta0.15Sb0.04)]O3 Ceramics (MnO2 첨가가 0.985[Li0.04(Na0.545K0.46)0.96(Nb0.81Ta0.15Sb0.04)]O3+0.015KNbO3 세라믹스의 유전 및 압전 특성에 미치는 영향)

  • Kim, YouSeok;Yoo, JuHyun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.6
    • /
    • pp.361-366
    • /
    • 2014
  • $MnO_2$-doped $0.985[Li_{0.04}(Na_{0.545}K_{0.46})_{0.96}(Nb_{0.81}Ta_{0.15}Sb_{0.04})]O_3+0.015KNbO_3(0.985LNKNTS+0.015KNbO_3)$ lead-free ceramics were fabricated by conventional solid state method to develop excellent dielectric and piezoelectric properties. The result of X-ray diffraction patterns obviously indicated that all of the specimen has pure perovskite structure without secondary phase. In addition, orthorhombic phase and coexistance region of orthorhombic-tetragonal phase (MPB) were observed with amount of $MnO_2$. The optimal values of ${\rho}$=4.70 $g/cm^3$, $d_{33}=238$ pC/N, $k_P=0.46$, $Q_m=121$, ${\varepsilon}_r=849$, and $T_C=225^{\circ}C$ were obtained at 0.01 mol% $MnO_2$ doped $0.985LNKNTS+0.015KNbO_3$ ceramics sintered at $990^{\circ}C$ for 5 h, respectively. Hence, it was indicated that the suitable amount of $MnO_2$ could improve the electrical properties of $0.985[Li_{0.04}(Na_{0.545}K_{0.46})_{0.96}(Nb_{0.81}Ta_{0.15}Sb_{0.04})]O_3+0.015KNbO_3$ ceramics.

Temperature Characteristics of Elastic Surface Wave (탄성표면파의 온도특성)

  • 김종상
    • Journal of the Korean Institute of Telematics and Electronics
    • /
    • v.10 no.3
    • /
    • pp.53-60
    • /
    • 1973
  • Calculations of the temperature coefficients of the elastic surface wave velocity and delay time were performed for the propagation along the X axis of rotated Y cut plane of the LiNbO3 and LiTaO3. Measurements of the temperature dependence of delay time of the elastic surface wave were also performed for the propagation along the X axis of a 130" rotated Y cut plane of the LiNb03 at the temperature range from liquid He to room temperature. Experimental value 70$\times$10-6/$^{\circ}C$ of the temperature coefficient of the delay time of the elastic surface wave agrees well with the calculated value 72.7$\times$10-a/$^{\circ}C$. The temperature coefficient of delay time of elastic surface wave propagating along the X axis of a 130$^{\circ}$ rotated Y cut plane o( the LiNbO3 is approximately 16$\times$10-6/$^{\circ}C$ at the near temperature of liquid He.d He.

  • PDF

Pyroelectric Infrared Sensors using (Pb,La)TiO3/LiTaO3/(Pb,La)TiO3 Multilayer Ferroelectric Thin Films ((Pb,La)TiO3/LiTaO3/(Pb,La)TiO3 다층 강유전 박막을 이용한 초전형 적외선 센서)

  • Sung, Se-Kyoung;Lee, Du-Hyun;Choi, Hyek-Hwan;Lee, Myoung-Kyo;Kwon, Tae-Ha
    • Journal of Sensor Science and Technology
    • /
    • v.11 no.4
    • /
    • pp.247-253
    • /
    • 2002
  • For fabrication of the pyroelectric IR sensor $(Pb,La)TiO_3(PLT)$/$LiTaO_3$/(LTO)/PLT ferroelectric thin films was deposited by rf magnetron sputtering followed by rapid thermal annealing and the crystallinity as a function of annealing temperature and time was investigated. Permittivity and dielectric loss factor of ferroelectric thin films as a function of c-axis preffered orientation was measured. Also pyroelectric coefficient of ferroelectric thin films with largest c-axis preffered orientation was measured and obtain figure of merit of voltage response($F_V$) and detectivity($F_D$). In this case $F_V$, $F_D$ was $5.63{\times}10^{-10}\;C{\cdot}cm/J$, $1.98{\times}10^{-8}\;C{\cdot}cm/J$, respectively.

Piezoelectric and Dielectric Properties of Low Temperature Sintering (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics Doped with CuO (CuO 첨가된 저온소결 (Na,K,Li)(Nb,Sb,Ta)O3계 세라믹스의 압전 및 유전 특성)

  • Lee, Gwang-Min;Yoo, Ju-Hyun;Lee, Jie-Young
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.28 no.4
    • /
    • pp.229-233
    • /
    • 2015
  • In this paper, in order to develop outstanding Pb-free piezoelectric composition ceramics, the $(Na_{0.525}K_{0.443}Li_{0.037})(Nb_{0.883}Sb_{0.08}Ta_{0.037})O_3+0.3wt%Bi_2O_3+0.4wt%Fe_2O_3+xwt%CuO$ (x= 0~0.8 wt%)(abbreviated as NKL-NST) lead-free piezoelectric ceramics have been synthesized using the ordinary solid state reaction method. The effects of CuO-doping on the structure and electrical properties of the NKL-NST ceramics were systematically studied. The results show that the ceramics exhibit a pure perovskite structure with orthorhombic phase at room temperature, and secondary phase was found in the ceramics. The 0.4 wt%CuO added ceramics sintered at $950^{\circ}C$ showed the optimum properties of piezoelectric constant($d_{33}$), planar piezoelectric coupling coefficient(kp) and mechanical quality factor(Qm) : $d_{33}=213$[pC/N], kp= 0.43, Qm= 423,respectively.

Effect of $Na_2O$ Addition on Piezoelectric Properties in $(Na_{0.5}K_{0.5})NbO_3-LiTaO_3$ Ceramics ($Na_2O$ 첨가에 따른 $(Na_{0.5}K_{0.5})NbO_3-LiTaO_3$ 세라믹스의 압전특성)

  • Kim, Min-Soo;Oh, Suk;Lee, Dae-Su;Park, Eon-Cheol;Jeong, Soon-Jong;Song, Jae-Sung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.315-316
    • /
    • 2006
  • Dense $0.95(Na_{0.5}K_{0.5})NbO_3-0.05LiTaO_3$ (NKN-LT) ceramics were developed by conventional sintering process. Sintering temperature was lowered by adding $Na_2O$ as a sintering aid. The electrical properties of NKN-LT ceramics were investigated as a function of $Na_2O$ concentration. When the sample sintered at $1000^{\circ}C$ for 4h with the addition of 1 mol% $Na_2O$, electromechanical coupling factor ($k_p$) and piezoelectric coefficient ($d_{33}$) of NKN-LT ceramics were found to reach the highest values of 0.43 and 190 pC/N, respectively.

  • PDF

Dielectric and Piezoelectric Properties of (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics as a Function of CuO Addition (CuO 첨가에 따른 (Na,K,Li)(Nb,Sb,Ta)O3 세라믹스의 유전 및 압전 특성)

  • Lee, KabSoo;Kim, YouSeok;Yoo, JuHyun;Mah, Sukbum
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.10
    • /
    • pp.630-634
    • /
    • 2014
  • $(Na_{0.525}K_{0.4425}Li_{0.0375})(Nb_{0.9975}Sb_{0.065}Ta_{0.0375})O_3+0.3 wt%CoO$ ceramics were fabricated as a function of CuO addition by traditional solid state sintering process in order to develop excellent lead-free piezoelectric ceramics composition. The addition of CuO in the LNKNTS composition ceramics can effectively enhance the densification of the ceramics, resulting in the oxygen vacancies as hardening effect. The excellent piezoelectric properties of electromechanical coupling factor($k{\small}_P$) of 0.378, piezoelectric constant($d_{33}$) of 152 pC/N were obtained from the 1.0 mol% CuO doped LNKNTS ceramics sintered at $1,020^{\circ}C$ for 3 h.

Microstructure and Piezoelectric Properties of Low Temperature Sintering (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics (저온소결 (Na,K,Li)(Nb,Sb,Ta)O3계 세라믹스의 미세구조 및 압전특성)

  • Lee, Kab-Soo;Yoo, Ju-Hyun;Lee, Jie-Young
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.29 no.4
    • /
    • pp.205-209
    • /
    • 2016
  • In this paper, piezoelectric ceramics with the composition of $(Na_{0.525}K_{0.4425}Li_{0.0375})(Nb_{0.8975}Sb_{0.065}Ta_{0.0375})O_3+0.3wt%\;CoO+x\;CuO$ ($0.005{\leq}x{\leq}0.025$) (abbreviated to NKL-NST) were fabricated for ultrasonic sensor application. The effects of CuO addition and sintering on the microstructure and the piezoelectric properties of the NKL-NST ceramics were systematically studied. Excellent piezoelectric properties such as electromchanical coupling $factor(k_p)=0.415$, piezoelectric constant $(d_{33})=166pC/N$ and piezoelectric figure of merit $d_{{33}*}g_{33}=5.47pm^2/N$ were obtained from the 2.5 mol% CuO doped NKL-NST+0.3 wt%CoO ceramics sintered at $1,000^{\circ}C$ for 3 h.

Development of an SH-SAW Sensor for Protein Measurement (단백질 측정용 SH-SAW 센서 개발)

  • 권용준;김재호;고광락;노용래
    • The Journal of the Acoustical Society of Korea
    • /
    • v.23 no.1
    • /
    • pp.1-7
    • /
    • 2004
  • We developed SH-SAW sensors to detect protein molecules in liquid solutions applying a particular antibody thin film on the delay line of transverse SAW devices. The antibody investigated was human-immune-globulin G (HigG) to hold the antigens (anti-HigG) in the protein solution. We fabricated the sensor generating 100 MHz with the piezoelectric single crystal LiTaO₃. We measured the frequency change of the sensor by adding the anti-body concentration on SAM (self assembled monolayer) deposited on the Au layer. The sensor showed stable response to the mass loading effects of the anti-HigG molecules with the sensitivity up to 10.8 ng/ml/Hz at noise level 400 Hz below.

A study on the enhancement of refractive index in Ti:LiTaO$_{3}$ optical waveguides by Zn-vapor diffusion (Zn-Vapor확산에 의한 Ti:LiTaO$_{3}$ 광도파로의 굴절률 증가에 관한 연구)

  • 정홍식;정영식
    • Electrical & Electronic Materials
    • /
    • v.9 no.3
    • /
    • pp.298-303
    • /
    • 1996
  • A double diffusion technique is developed to enhance the effective mode index of optical waveguides in $LiTaO_3$. It consists of Zn diffusion from the vapor phase at relatively low temperatures (750->$800^{\circ}C$), into waveguides initially produced by Ti indiffusion at higher temperature (1150->$1200^{\circ}C$). Both X- and Z-cut substrates are investigated. A model that combines profiles of both diffusion is formulated to calculate the expected effective index values for planar waveguides. Good agreement is found between experimental results and model predictions which assume that the initial Ti profile is not affected by the lower temperature Zn diffusion. Effective index enhancements as high as 0.005 and 0.003 are obtained by this method for the fundamental extraordinary and ordinary modes, respectively.

  • PDF