Cell Properties for SOFC Using Synthesized Powder of Electrolyte LSGM System and Cathode LSM System (LSGM 전해질과 LSM 양극의 합성분말을 이용한 SOFC 단위전지의 특성)

  • Lee, Mi-Jai;Nam, Jeong-Hee;Choi, Byung-Hyun
    • Journal of the Korean Ceramic Society
    • /
    • v.39 no.4
    • /
    • pp.359-366
    • /
    • 2002
  • The purpose of this study is to investigate the properties of LSGM electrolyte and LSM cathode. The unit cell based on the optimum conditions and processing for high performance was fabricated and measured. The single phase of $LaGaO_3$ was obtained on sintering at $1500^{\circ}$ for 6h with composition of $(La_{0.85}Sr_{0.15})(Ga_{0.8}Mg_{0.2})O_{3-\delta}와 (La_{0.8}Sr_{0.2})(Ga_{0.8}Mg_{0.2})O_{3-\delta}$ and $(La_{0.85}Sr_{0.15})(Ga_{0.8}Mg_{0.2})O_{3-\delta}$. The grain size of the sintered body was about $10∼30{\mu}m$ and electrical conductivity was 0.13 S/cm measured at $800^{\circ}$. The single phase of $LaMnO_3$ structure in $(La1-xSrx)MnO_3$ system was obtained at x=0∼0.2 and the particle size of the synthesized powder was about 40 nm. The unit cell was prepared by firing at $1200^{\circ}$ for 1h with $(La_{0.9}Sr_{0.1})MnO_3$ cathode and 0.9NiO-0.1YSZ anode screen-printed on surfaces of $(La_{0.8}Sr_{0.2})(Ga_{0.8}Mg_{0.2})O_{3-\delta}$ electrolyte. The grain size of the electrode was close to $1{\mu}m$ and the electrode had porous structure. The maximum power density of unit cell showed $0.3W/cm^2$ at $800^{\circ}$.

Crystal growth and dielectric properties of $La_{1/3}MO_3$ (M=Nb, Ta) by infrared floating zone method (적외선 용융대역법에 의한 $La_{1/3}MO_3$ (M=Nb, Ta) 단결정 성장 및 유전 특성)

  • Mitisuru Itoh
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.5 no.3
    • /
    • pp.233-239
    • /
    • 1995
  • $La_{1/3}NbO_3$ and $La_{1/3}TaO_3$ large single crystal was prepared by the infrared floating zone method and their crystal structure and dielectric properties were investigated from the viewpoint of A - site vacancy. In $La_{1/3}TaO_3$ crystal, the crystal symmetry and approximate lattice constants was tetragonal and a $\approx$ 0.397, b $\approx$ 0.397 and c $\approx$ 0.775 from the nonextinction and the reciprocal lattice point length seen on Weissenberg and Precession photographs. The jump of some $2/3La^{3+}$ ions leads to increase the moving paths due to the generation of new vacancies at middle empty sites and thus this result is confirmed to provoke the dielectric anomaly.

  • PDF

The Study on Optical Properties by Adding $La_2O_3$ in Multicomponent Glass Fiber (다성분계 Glass Fiber의 $La_2O_3$ 첨가에 따른 광학적 특성에 관한 연구)

  • 김용호;강원호
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1994.11a
    • /
    • pp.21-23
    • /
    • 1994
  • By adding La₂O₃ to optical multicomponent glass composition, after making mother glass and core fiber that enable to enlarge the infrared transmittance region, then surveyed the optical properties. Through thermal analysis of the glass abstained by melt-quenching after selecting stable basic composition on devitrification and replace SiO₂ by 4-12wt% La₂O₃. As La₂O₃ increases up to l2wt% transition temperature, refractive index, density, deformation temperature increased, whereas thermal expansion coefficient decreased. As a result of inspectig transmittance in UV/VIS/IR region, visable region indicated the decrease of transmittance by increasing the La₂O₃ and transmittance region was enlarged by increasing the La₂O₃ in IR region. Also, fabricate core fiber at 820℃ and severy the optical loss we could fact that La₂O₃ composition added 12wt% showed the minimum optical loss.

Dependence of LaAlO3/SrTiO3 Interfacial Conductivity on the Thickness of LaAlO3 Layer Investigated by Current-voltage Characteristics (LaAlO3 두께에 따른 LaAlO3/SrTiO3 계면에서의 전류-전압 특성을 이용한 전도성 변화 연구)

  • Moon, Seon-Young;Baek, Seung-Hyub;Kang, Chong-Yun;Choi, Ji-Won;Choi, Heon-Jin;Kim, Jin-Sang;Jang, Ho-Won
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.25 no.8
    • /
    • pp.616-619
    • /
    • 2012
  • Oxides possess several interesting properties, such as ferroelectricity, magnetism, superconductivity, and multiferroic behavior, which can effectively be used oxide electronics based on epitaxially grown heterostructures. The microscopic properties of oxide interfaces may have a strong impact on the electrical transport properties of these heterostructures. It was recently demonstrated that high electrical conductivity and mobility can be achieved in the system of an ultrathin $LaAlO_3$ film deposited on a $TiO_2$-terminated $SrTiO_3$ substrate, which was a remarkable result because the conducting layer was at the interface between two insulators. In this study, we observe that the current-voltage characteristics exhibit $LaAlO_3$ thickness dependence of electrical conductivity in $TiO_2$-terminated $SrTiO_3$. We find that the $LaAlO_3$ layers with a thickness of up 3 unit cells, result in highly insulating interfaces, whereas those with thickness of 4 unit cells and above result in conducting interfaces.

Electrical Properties and Stability of La2O3 Doped ZnO-Pr6O11-Based Varistor Ceramics (La2O3 Doped ZnO-Pr6O11계 바리스터 세라믹스의 전기적 성질 및 안정성)

  • Nahm, Choon-Woo
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.6 s.289
    • /
    • pp.383-388
    • /
    • 2006
  • The varistor properties and DC accelerated aging characteristics of $ZnO-Pr_{6}O_{11}-CoO-Cr_{2}O_{3}$-based varistors were investigated at different $La_{2}O_3$ contents in the range of $0{\sim}2.0mol%$. The varistors doped with 0.5 mol% $La_{2}O_3$ exhibited good nonlinearity, with 81.6 in nonlinear coefficient. Increasing the $La_{2}O_3$ content further to 2.0 mol% caused the sintered density to increase, and the breakdown voltage and nonlinearity to decrease abruptly. The varistors with 0.5 mol% $La_{2}O_3$ exhibited the high electrical stability, with -1.14% in variation rate of breakdown voltage, -3.7% in variation rate of nonlinear coefficient, and +100% in variation rate of leakage current for specified DC accelerated aging stress condition (95% of breakdown voltage/$150^{\circ}C$/24 h).

Characteristics of $LaCrO_3$-Dispersed Cr Alloy for Metallic Interconnector of Solid Oxide Fuel Cell (고체 산화물 연료전지 금속 연결재용 $LaCrO_3$가 분산된 Cr 합금의 특성 연구)

  • Jeon, Kwang-Sun;Song, Rak-Hyun;Shin, Dong-Ryul
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.48 no.8
    • /
    • pp.570-576
    • /
    • 1999
  • $LaCrO_3$-dispersed Cr alloys for metallic interconnector of solid oxide fuel cell have been studied as function of $LaCrO_3$ content in the range of 5 to 25 vol.% in order to examine the electric conductivity, the oxidation property and the thermal expansion behavior of these alloys. The $LaCrO_3$-dispersed Cr alloys showed high electrical conductivities of $3~5\times10^4$ S/cm at room temperature, and as the $LaCrO_3$content increased the conductivity decreased slightly. During the cyclic oxidation test at $1100^{\circ}C$, the weight change of the Cr alloys decreased with increasing number of oxidation cycle except first cycle, which is attributed to the vaporization of the oxide scale. More addition of the $LaCrO_3$ content reduced also the weight change of the Cr alloys. These mean that the oxide scale formed at the surface of the Cr alloy becomes stable with increasing number of oxidation cycle and$LaCrO_3$ content. The measured thermal expansion of the Cr alloy was well fitted to that of 8 mol% $Y_2O_3$-stabilized $ZrO_2$ electrolyte. These results demonstrate that $LaCrO_3$-dispersed Cr alloy is a useful material for metallic interconnector of solid oxide fuel cell.

  • PDF

Stoichiometry, Thermal Stability and Reducibility of Perovskite-Type Mixed Oxide LaBO$_3$ (B = Fe, Co, Ni)

  • Park, Il-Hyun;Lee, Hyung-Pyo
    • Bulletin of the Korean Chemical Society
    • /
    • v.9 no.5
    • /
    • pp.283-288
    • /
    • 1988
  • The titled properties on reduction of the perovskite $LaBO_3$ (B = Fe, Co, Ni) have been investigated by means of temperature-programmed reduction, isothermal reduction and X-ray diffraction methods. Nominal composition of $LaFeO_{3.18},\;LaCoO_{3.00}\;and\;LaNiO_{2.92}$ are determined. Reduction reaction of these mixed oxides differed according to B-site transition metal and thermal stability on reduction decreased as following order: $LaFeO_{3.18}$ > $LaCoO_{3.00}$ > $LaNiO_{2.92}$. From the results of isothermal reaction, kinetics on reduction of the perovskite has been discussed in detail.

Sintering behavior and characterization of Ln0.7Ca0.3MnO3 (Ln=Nd, Sm, La) (Ln0.7Ca0.3MnO3 (Ln=Nd, Sm, La)의 소결 거동 및 특성)

  • Chon, Gom-Bai;Koo, Bon-Heun;Lee, Chan-Gyu
    • Korean Journal of Materials Research
    • /
    • v.16 no.1
    • /
    • pp.44-49
    • /
    • 2006
  • Effects of doping rare earth element on Ln site of $Ln_{0.7}Ca_{0.3}MnO_3$ (Ln=Nd, Sm and La) were examined from sintering behavior, structure and magnetic properties. Sintering reactions proceeded rapidly in order of $La_{0.7}Ca_{0.3}MnO_3>Nd_{0.7}Ca_{0.3}MnO_3>Sm_{0.7}Ca_{0.3}MnO_3$. This result can be explained by diffusivity of metal cation. Size of a-axis increased as following order of La$Nd_{0.7}Ca_{0.3}MnO_3$, 93K for $Sm_{0.7}Ca_{0.3}MnO_3$ and 225K for $La_{0.7}Ca_{0.3}MnO_3$ were obtained. This result coincides with change of Mn-O bond length causing by a-axis lattice constant.

Hydrothermal Synthesis of LaCO3OH and Ln3+-doped LaCO3OH Powders under Ambient Pressure and Their Transformation to La2O2CO3 and La2O3

  • Lee, Min-Ho;Jung, Woo-Sik
    • Bulletin of the Korean Chemical Society
    • /
    • v.34 no.12
    • /
    • pp.3609-3614
    • /
    • 2013
  • Orthorhombic and hexagonal lanthanum(III) hydroxycarbonate ($LaCO_3OH$) and $Ln^{3+}$-doped $LaCO_3OH$ ($LaCO_3OH:Ln^{3+}$, where Ln = Ce, Eu, Tb, and Ho) powders were prepared by a hydrothermal reaction under ambient pressure and characterized by thermogravimetry, powder X-ray diffraction, infrared and luminescence spectroscopy, and field-emission scanning electron microscopy. The polymorph of $LaCO_3OH$ depended on the reaction temperature, inorganic salt additive, species of $Ln^{3+}$ dopant, and solvent. The calcination of orthorhombic $LaCO_3OH:Ln^{3+}$ (2 mol %) powers at $600^{\circ}C$ yielded a mixture of hexagonal and monoclinic $La_2O_2CO_3:Ln^{3+}$ powders. The relative quantity of the latter increased with decreasing ionic radius of the $Ln^{3+}$ dopant ion and increasing doping concentrations. On the other hand, the calcination of hexagonal $LaCO_3OH:Ln^{3+}$ (2 mol %) powders at $600^{\circ}C$ resulted in a pure hexagonal $La_2O_2CO_3:Ln^{3+}$ powder, regardless of the species of $Ln^{3+}$ ions (Ln = Ce, Eu, and Tb). The luminescence spectra of $LaCO_3OH:Ln^{3+}$ and $La_2O_2CO_3:Ln^{3+}$ were measured to examine the effect of their polymorph on the spectra.

Preparation of dielectric Bi4-xLaxTi3O12 (x~2) from K2La2Ti3O10 via exfoliation and restacking routes (박리화와 재적층법을 통한 K2La2Ti3O10부터 유전성 Bi4-xLaxTi3O12(x~2)의 합성)

  • Jeon, A Young;Ko, Jieun;Kim, Jong-Young
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.23 no.1
    • /
    • pp.14-19
    • /
    • 2013
  • We have successfully synthesized $Bi_{4-x}La_xTi_3O_{12}$ (x~2) having Aurivillius-type layered perovskite structure from exfoliated layered perovskite oxide of $K_2La_2Ti_3O_{10}$ with Ruddlesden-Popper structure. The reaction between the exfoliated lanthanum titanate nanosheets and BiOCl nanocrystal resulted in the formation of polycrystalline $Bi_{4-x}La_xTi_3O_{12}$ (x~2) after heating above $700^{\circ}C$. Colloidal suspension of the nanosheets could be obtained by intercalating ethylamine (EA) into the protonated lanthanum titanate, $H_2La_2Ti_3O_{10}$, derived from $K_2La_2Ti_3O_{10}$. Transmission electron microscopic (TEM) analysis show that the exfoliated lanthanium titanate nanosheets have a thickness of a few nano meters. According to X-ray diffraction (XRD) analysis, the exfoliated lanthanium titanate was found to be transformed into $Bi_{4-x}La_xTi_3O_{12}$ (x~2) after restacking with BiOCl and subsequent thermal treatment at > $700^{\circ}C$.