  • The electrical properties and stability of ZPCE varistors consisted of $ZnO-Pr_6O_{11}-CoO-Er_2O_3$ ceramics were investigated. $ZnO-Pr_6O_{11}-CoO-Er_2O_3$ based ceramics were sintered at $1300^{\circ}C$ and $1350^{\circ}C$, respectively, without and with 0.5 mol% $Er_2O_3$. The varistors sintered at $1300^{\circ}C$ exhibited a better nonlinearity than that $1350^{\circ}C$. The varistors with $Er_2O_3$ of 0.5 mol% exhibited a high nonlinear exponent of 52.8. However, they easily degraded due to the low density below 85% of TD. On the other hand, the varistors sintered at $1350^{\circ}C$ without $Er_2O_3$ exhibited an extremely poor nonlinearity, but the varistors with $Er_2O_3$ of 0.5 mol% exhibited a relatively good nonlinearity, which the nonlinear exponent is 34.8 and the leakage current is $7.4\;{\mu}A$ Morever, they exhibited a very high stability, which the variation rate of varistor voltage, nonlinear exponent, and leakage current are -0.9%, -2.9%, and +2.7%, respectively, under the third stress $(0.80 V_{1mA}/90^{\circ}C/12h)$ + $(0.85 V_{1mA}/115^{\circ}C/12h)$ + $(0.90 V_{1mA}/120^{\circ}C/12h)$. Consequently, it was estimated that $ZnO-Pr_6O_{11}-CoO-Er_2O_3$ ceramics will be usefully applied to develop the advanced $Pr_6O_{11}$-based ZnO varistors.

  • PDF

A Numerical Study to Analyze Safety of Pressure Leakage Monitoring System of Gas Extinguishing Agent (가스소화약제 압력누기감시장치의 안전성 분석을 위한 수치적 연구)

  • Go, A-Ra;Lim, Dong-Oh;Son, Bong-Sei
    • Fire Science and Engineering
    • /
    • v.30 no.4
    • /
    • pp.103-110
    • /
    • 2016
  • While the demand for the gas system fire extinguishers increases every year, there are insufficient safety measures for assessing the extinguishing performance, such as system safety and reliability in the preparation of increasing demand, which has emerged as a social problem. One of the most critical causes of accidents occurring with the gas extinguishing system is pressure leakage from the extinguishing agent storage container. This is considered to be one of the critical factors on which the success of fire suppression depends. In this study, its safety measure was studied, Because it was deemed urgently necessary. The newly developed pressure leakage monitoring system is a system monitoring storage condition, pressure, leakage and discharge of the storage container related to agent concentration, which is one of the critical factors for fire suppression. This was developed to be applicable to the $CO_2$ and HFC-23 systems. Therefore, for structural safety analysis, the safety performance was verified by the fluid structure coupling analysis of the safety problems that may occur when the pressure leakage monitoring system is applied to the gas fire extinguisher. For analysis programs, the FloEFD program from Mentor Graphics was used for computational fluid dynamics analysis and ABAQUS from Dassault Systems was used for structural analysis. From the result of numerical analysis, the structure of $CO_2$ did not develop plastic deformation and its safety was verified. However, plastic deformation and deviation issue occurred with the HFC-23 monitoring system and therefore verified the structural safety of pressure leakage monitoring system by data obtained from redesigning and adjusting the condition of numerical interpretation three times.

A Phenomenological Review on the Damage of Hot Gas Parts caused by Explosion of Gas Turbine Cooling System (가스터빈 내부 냉각계통 발화에 의한 고온부품 손상의 현상학적 고찰)

  • Yu, Won-Ju;Lee, Seong-Hyun
    • Journal of the Korea Safety Management & Science
    • /
    • v.12 no.2
    • /
    • pp.75-82
    • /
    • 2010
  • Gas turbines for power generating operate in a very high temperature condition and use natural gas for fuel. For this reason, many cases of damage happen at hot gas parts which are severely affected by high temperature gas and many cases of explosion occur by fuel gas. So a lot of efforts should be made to prevent hot gas parts damage and gas explosion accidents. Though there are many damage cases and explosion accidents, it is very difficult to find out the root causes of hot gas parts damage caused by gas explosion due to gas leakage in the heat exchanger for air cooling and gas heating. To prevent gas turbine from damage caused by gas explosion, removal of leakage gas from gas turbine is inevitably required before firing the gas turbine and installing alarm systems is also required for detecting gas leakage at stop valve to turbine while shut down.

The Transient Analysis of Instant Short-Circuit Test Equipment For Earth Leakage Circuit Breaker (IEC60947-2에 따른 누전차단기의 순시단락시험 과도현상에 대한 연구)

  • Ryu, Haeng-Soo;Kim, Myeong-Seok;Han, Gyu-Hwan
    • Proceedings of the KIEE Conference
    • /
    • 2003.07a
    • /
    • pp.357-359
    • /
    • 2003
  • This paper is for the transient analysis of instant short-circuit test equipment according to the test of tripping limits and characteristics under IEC 60947-2. The in-rush current is harmful to almost equipments and the exact testing is not made because of it. LGIS has a instant short-circuit test equipment, but it is not suitable for carrying out instant short-circuit test on ELB(Earth Leakage Circuit breaker) by reason of that. Now, I am going to show a solution for that problem. After applying this method, manufacturer is going to acquire the exact testing result according to the IEC standard. Moreover, Testing laboratory will be trusted by clients.

  • PDF

Microstructure and Electrical Properties of Zn-Pr-Co-Y-M(M=Ni, Mg, Cr) Oxide-Based Varistors (Zn-Pr-Co-Y-M(M=Ni, Mg, Cr) 산화물계 바리스터의 미세구조 및 전기적 특성)

  • Nahm Choon-Woo;Park Jong-Ah
    • Korean Journal of Materials Research
    • /
    • v.14 no.6
    • /
    • pp.420-424
    • /
    • 2004
  • The microstructure and electrical properties of $ZnO-Pr_{6}$$O_{11}$ $-CoO-Y_2$$O_3$-based varistors were investigated with and without various metal oxide additives (NiO, MgO, and $Cr_2$$O_3$). The addition of NiO promoted the grain growth while that of Cr$_2$O$_3$ decreased average grain size. Thereby, the varistor voltage was higher in $Cr_2$$O_3$-added composition. Among $ZnO-Pr_{6}$ $O_{11}$ /$-CoO-Y_2$$O_3$-based varistors, the$ Cr_2$$O_3$-added varistor exhibited the highest nonlinear exponent (51.2), the lowest leakage current (1.3 $\mu$A), and the lowest dielectric dissipation factor (0.0433).

A Study on the Ventilation Schemes for Gas Leakage and Dispersion Controlling at the Backfilled Working Face in Large-Opening Underground Mine (대단면 지하광산 갱도내 뒷채움 작업장 가스유출 및 확산제어 통기방안 연구)

  • Nguyen, Vanduc;Lee, Changwoo
    • Tunnel and Underground Space
    • /
    • v.28 no.4
    • /
    • pp.372-386
    • /
    • 2018
  • The air quality near the backfilled site area is significantly deteriorated during and even after the curing period of the backfill materials. Hazardous gases such as NH3 and CO2 may leak out prolongedly from the mined-out sites backfilled with the composite carbonate-based material; leakage can be observed at the underground working sites as well as on the surface. At operating mines, underground gas leakage will severely aggravate the workplace environment. The ventilation schemes should supply sufficient air to dilute the contaminated air, and control the toxic gas leakage and dispersion. This study shows the applicability of pressurization ventilation system to control gas leakage and dispersion at the backfilled underground mine site.

Influence of Sintering Temperature and Electrical Properties on ZPCCE Based Varistors (ZPCCE계 바리스터의 전기적 성질에 소결온도가 미치는 영향)

  • 류정선;윤한수;남춘우
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.242-245
    • /
    • 2000
  • The electrical properties of ZPCCE (ZnO-Pr$_{6}$O$_{11}$-CoO-Cr$_2$O$_3$-Er$_2$O$_3$) based varistors were investigated with sintering temperature in range of 1335 to 135$0^{\circ}C$ for 1h. As the sintering temperature increases, the nonlinear exponent decreased, but was high beyond 40 except for 1.0 mol% Er$_2$O$_3$. Among all ZPCCE varistors, the varistor having the highest nonlinear exponent was obtained by sintering at 1335$^{\circ}C$, containing 2.0 mol% Er$_2$O$_3$ and then the nonlinear exponent was 78.05, and the varistors with 0.5 mol% Er$_2$O$_3$ exhibited the lowest leakage current of 1.92 $\mu$A.A.A.

  • PDF

Co2O3 Doping Effects on the Electrical Properties of ZnO Varistor (Co2O3 의첨가량이 산화아연 바리스터의 전기적 특성에 미치는 효과)

  • 김명식;오명환
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.34 no.5
    • /
    • pp.186-192
    • /
    • 1985
  • Co2O3 additive effects on the electrical properties in ZnO varistor are investigated. As the Co Cations being substituted and ionized normally to a divalent state for Zn in the lattice site increase, the leakage current in the prebreakdown region decreases and the so-called

  • PDF

Output characteristics of ac excited $CO_2$ laser as a adjusting a phase angle and frequency (위상각와 주파수 제어에 따른 상용주파 AC 여기 방식의 펄스형 $CO_2$ 레이저 전원장치 개발에 관한 연구)

  • Chung, Hyun-Ju;Kim, Do-Wan;Lee, Dong-Hoon;Kim, Joong-Mann;Kim, Mee-Je;Cho, Jung-Soo
    • Proceedings of the KIEE Conference
    • /
    • 2000.07c
    • /
    • pp.2098-2100
    • /
    • 2000
  • We propose pulsed $CO_2$ laser below 30W by the AC(60Hz) switching control of leakage transformer primary which has some advantage of cost and size compared to a typical pulsed power supply. Pulse repetition rate is adjusted from 5Hz to 60Hz to control laser output. In this laser, a low voltage open loop control for high voltage discharge circuit is employed to avoid the HV sampling or switching and high voltage leakage transformer is used to convert rectified low voltage pulse to high voltage one. A ZCS(Zero Cross Switch) circuit and a PIC one-chip microprocessor are used to control gate signal of SCR precisely. The pulse repetition rate is limited by 60Hz due to the frequency of AC line and a high leakage inductance. The maximum laser output was obtained about 23W at pulse repetition rate of 60Hz, total gas mixture of $CO_{2}/N_{2}$/He = 1/9/15, SCR gate trigger angle 90$^{\circ}$, and total pressure of 18Torr.

  • PDF

A Study On The Deformation Behavior of Post-Construction Crest Settlement, Face Slab Deformation, and Leakage of Concrete Faced Rockfill Dams (콘크리트 표면차수벽형 석괴댐의 준공 후 정부침하와 슬래브 변형 및 누수 거동에 관한 연구)

  • Kim, You-Seong;Choi, Jae-Seon;Won, Myoung-Soo;Lee, Hee-Hun
    • Journal of the Korean Geosynthetics Society
    • /
    • v.8 no.2
    • /
    • pp.31-39
    • /
    • 2009
  • The purpose of present study performed 27 CFRD cases analyses to predict and effectively use post-construction crest settlement, face slab deformation, and leakage as indexes for the maintenance and management of concrete faced rockfill dams(CFRD). The results showed that the range of post-construction crest settlement suggested by Sherard and Cooke (1987), and Clements (1984) had a good agreement in the case analyses using rockfills with very high intact strength, but it had a trend which underestimated crest settlement in the cases using rockfills with medium to high intact strength. The leakage case analyses showed that leakage is mainly caused by face slab deformation due to the water load, the maximum leakage in general was observed during the first reservoir filling, and leakage was rapidly increasing when the dam height exceeds 125m.

  • PDF