Crystal Structure of Ca1.29Bi0.14VO4

  • Kim, Myung-Seab;Lah, Myoung-Soo;Kim, Ho-Kun
    • Bulletin of the Korean Chemical Society
    • /
    • 제23권1호
    • /
    • pp.98-102
    • /
    • 2002
  • The structure of a single crystal, grown by a slow cooling a melt of $Ca_{1.29}Bi_{0.14}VO_4$ composition, was analyzed. The crystals belong to the rhombohedral space group R3c and the dimensions of the unit cells are a = 10.848(1)${\AA}$, c = 38.048(6)${\AA}$, V = 3877.6(8)${\AA}^3$ for the pale yellow crystal, and a = 10.857(1), c = 38.063(6)${\AA}$, V = 3885.6(8)${\AA}^3$ for the yellow crystal, respectively. Unit cell dimensions of the crystal were larger than those of the host crystal, $Ca_3(VO_4)_2$, owing to the Bi that replaced Ca in the unit cell. Ca in the unit cell formed six, eight and nine coordinated polyhedra with O atoms and Bi replacing Ca entered the eight or nine coordinated Ca sites with different crystallographic environments in the unit cell. All the V in the unit cell formed four coordinated tetrahedra with O atoms, however V-O bond lengths in the tetrahedra were different from one another.

ZnO-Zn2BiVO6-Co3O4-Cr2O3-CaCO3 바리스터 내의 결정결함과 입계특성 (Crystal Defects and Grain Boundary Properties in ZnO-Zn2BiVO6-Co3O4-Cr2O3-CaCO3 Varistor)

  • 홍연우;하만진
    • 한국전기전자재료학회논문지
    • /
    • 제32권4호
    • /
    • pp.276-280
    • /
    • 2019
  • In this study, we investigated the crystal defects and grain boundary properties in a ZZCCC ($ZnO-Zn_2BiVO_6-Co_3O_4-Cr_2O_3-CaCO_3$) varistor, with the liquid-phase sintering aid $Zn_2BiVO_6$ developed by our laboratory. The ZZCCC varistor sintered at $1,200^{\circ}C$ exhibited excellent nonlinear current-voltage characteristics (${\alpha}=63$), with oxygen vacancy ($V_o^*$ ; 0.35 eV) as a main defect, and an apparent activation energy of 1.1 eV with an electrically single grain boundary. Therefore, among the various additives to improve the electrical properties of ZnO varistors, if $Zn_2BiVO_6$ is used as a liquid phase sintering aid, it will be ideal to use Co for the oxygen vacancy and Ca for the electrically single grain boundary. This will allow the good properties of ZnO varistors to be maintained up to high sintering temperatures.

침전 반응에 의한 가시광 광촉매 Bismuth Vanadate 합성 (Synthesis of Bismuth Vanadate as Visible-light Photocatalyst by Precipitation Reaction)

  • 김상문;이재용;문추연;이헌수
    • 한국세라믹학회지
    • /
    • 제48권6호
    • /
    • pp.630-635
    • /
    • 2011
  • Bismuth vanadate($BiVO_4$) with monoclinic phase as photocatalyst under visible light is synthesized by precipitation reaction in hot water. Properties such as crystal phase, particle morphology and visual light absorbance as well as the effects of thermal treatment for $BiVO_4$ powders are investigated. $BiVO_4$ powders with both single monoclinic phase and 0.2 ${\mu}m$ in particle size are synthesized when precipitate is stirred in water for 5 h at 95$^{\circ}C$. Well-developed monoclinic phase and light absorption property under 535 nm are observed as a result of thermal treatment for 1 h at 300$^{\circ}C$ after precipitation reaction in water for 5 h at 95$^{\circ}C$. Degradation of monoclinic crystal is found in firing above 350$^{\circ}C$, and particle growth is occurred in firing above 550$^{\circ}C$.

Bi 치환에 따른 $Ca_{1.5-1.5x}Bi_xVO_4$ 조성 화합물의 결정상에 관한 연구 (Study on the Crystal Phases of $Ca_{1.5-1.5x}Bi_xVO_4$ Compositions by Bi Substitution)

  • 김명섭;박선민;김호건
    • 대한화학회지
    • /
    • 제43권5호
    • /
    • pp.547-551
    • /
    • 1999
  • $Ca_{1.5-1.5x}Bi_xVO_4$계 화합물에 대하여 Bi 치환량(x)에 따른 결정상을 조사한 결과, 치환량이 x=0.14까지 다른 상의 생성없이 단일상으로 존재하였으나, 치환량이 0.18 이상인 경우 새로운 화합물인 $BiV_{1.025}O_{4+x}$가 함께 석출되었다. $BiV_{1.025}O_{4+x}$의 양은 x=0.18인 경우 16%, x=0.22인 경우 21%임이 확인되었다. Bi의 치환량이 0.02인 경우 구조의 변화가 거의 없었으나, 치환량이 0.06∼0.14일 때 치환량에 따른 면간거리(d)의 변화량은 0.01 mole% Bi당 (214)면은 $1.7417{\times}10^{-3}{\AA}$,(300)면은 $1.7417{\times}10^{-3}{\AA}$을 나타내었다. 단일상으로 존재하는 최대 치환량이 x=0.14인 $Ca_{1.29}Bi_{0.14}VO_4$ 조성 화합물은 합치용융조성(congruent melting composition)이 아니며, 이 조성이 용융을 시작하는 고상선 온도(solidus temperature)는 1182$^{\circ}C$임을 알 수있었다.

  • PDF

LiTaO3 단결정 내의 Fe3+ 상자성 불순물 이온에 대한 에너지 준위 계산 (Energy Level Calculation of Fe3+ Paramagnetic Impurity Ion in a LiTaO3 Single Crystal)

  • 염태호;윤달호;이수형
    • 한국자기학회지
    • /
    • 제24권3호
    • /
    • pp.71-75
    • /
    • 2014
  • 정비조성으로 성장시킨 $LiTaO_3$ 단결정 및 비정비조성으로 성장시킨 $LiTaO_3$ 단결정 내에 불순물로 도핑된 $Fe^{3+}$ 상자성 불순물 이온의 바닥 상태에서의 에너지 준위를 계산하였다. $LiTaO_3$ 단결정 내에서 육방정계 대칭성을 갖는 $Fe^{3+}$ 이온의 전자 상자성 공명 상수인 분광학적 분리인자 g 및 영자기장 갈라지기 D 값을 이용하여 6개의 에너지 준위 사이의 에너지 준위를 계산하였다. 자기장을 결정학적 주축 ([100], [001], [111])과 나란하게 가하여 자기장을 증가시켜 감에 따라 얻은 에너지 준위 갈라지기는 자기장을 가한 방향에 따라서 서로 다른 값을 나타내었다. ${\mid}{\pm}5/2$ > ${\leftrightarrow}{\mid}{\pm}3/2$ >및 ${\mid}{\pm}3/2$ > ${\leftrightarrow}{\mid}{\pm}1/2$ > 사이의 전이에서 계산한 영자기장 갈라지기 값은 정비조성으로 성장시킨 $LiTaO_3$ 단결정과 비정비조성으로 성장시킨 단결정의 경우에 각각 12.300 GHz, 6.150 GHz와 59.358 GHz, 29.679 GHz이다. 결정성장 조건에 따라 에너지 준위가 상당히 다른 것으로 나타났다.