Rf Magnetron Sputtering 방법으로 제조된 $Ba_{1-x}Sr_xTiO_3$ 박막의 구조적 특성에 대한 연구 (A Study on the Structural Properties of rf Magnetron Sputtered $Ba_{1-x}Sr_xTiO_3$ Thin Film)

  • 김태송;오명환;김종희
    • 한국세라믹학회지
    • /
    • 제30권6호
    • /
    • pp.441-448
    • /
    • 1993
  • The Ba1-xSrxTiO3 thin films deposited on ITO-coated glass substrate at 55$0^{\circ}C$ by rf magnetron sputtering method have individual preferential orientations as a function of composition (X=0, 0.25, 0.5, 0.75, 1) due to the stress relief interactions among the intrinsic compressive stress, thermal tensile stress adn extrinsic compressive stress (compressive stress in case of BaTiO3(Tc=12$0^{\circ}C$) and Ba0.75Sr0.25TiO3(Tc=57$^{\circ}C$)). This behavior also appears on the (BaSr)TiO3 thin films (X=0.5) deposited on ITO-coated glass substrate at deposition temperature between 35$0^{\circ}C$ and 55$0^{\circ}C$. The composition of Ba1-xSrxTiO3 thin films deposited on ITO-coated glass substrate at 55$0^{\circ}C$ is close to stoichiometry (1.009~1.089 in A/B ratio), but the compositional deviation from a stoichiometry is larger as SrTiO3 is added. The morphology of Ba1-xSrxTiO3 thin films is very similar for over all substrate temperatures, and the roughness due to the differences of cluster size is the smallest at X=0.25.

  • PDF

PTCR Characteristics of BaTiO$_3$Thin Films made by rf/dc Magnetron Sputter Technique

  • Song, Min-Jong;So, Byung-Moom;Kim, Tae-Wan
    • Transactions on Electrical and Electronic Materials
    • /
    • 제1권2호
    • /
    • pp.28-31
    • /
    • 2000
  • BaTiO$_3$cerameic thin films doped with Mn were manufactured by rf/dc magnetron sputter technique. We have investigated crystal structure, surface morphology and PRCR(positive-temperature coefficient of resistance) characteristics of the specimen depending on second heat-treatment temperature. Second heat treatment of the specimen were performed in the temperature range of 400 to 1350$\^{C}$ X-ray diffraction patterns of BaTiO$_3$ thin films show that the specimen heat treated below 600$\^{C}$ is an amorphous phase and the one heat treated above 1100$\^{C}$ forms a poly-crystallization . In this specimen heat-treated at 1300$\^{C}$, a lattice constant ratio(c/a) was 1.188. Scanning electron microscope(SEM) image of BaTiO$_3$ thin films of the specimen heat treated in between 900 and 1100$\^{C}$ shows a grain growth. At 1100$\^{C}$, the specimen stops grain-growing and becomes a poly-crystallization . A resistivity-temperature characteristics of the specimen depends on the doping concentrations of Mn. A resistivity ratio between the value at room temperature and the one above Curie temperature was 10$^4$ for pure BaTiO$_3$ thin films and 10$\^$5/ fo BaTiO$_3$ : additive 0.127mol% MnO

  • PDF

Ar/$O_2$비에 따른 (Bi,Ba,Sr)$TiO_3$[BBST] 박막의 구조적 특성 (The structural properties of the (Bi,Ba,Sr)$TiO_3$[BBST] thin films with Ar/$O_2$ rates)

  • 김정태;이상철;이성갑;배선기;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2002년도 하계학술대회 논문집 C
    • /
    • pp.1488-1490
    • /
    • 2002
  • The (Bi,Ba,Sr)$TiO_3$[BBST] thin films were fabricated on Pt/Ti/$SiO_2$/Si substrate by RF sputtering method. We investigated the effects of Ar/$O_2$ rates on the structural properties of BBST thin films. Decreasing the $O_2$ rates, the intensity of $BaBi_4Ti_4O_{15}$ and $Bi_4Ti_3O_{12}$ peaks were increased but the $(Ba_{0.5}Sr_{0.5})TiO_3$ peak was decreased. In the case of BBST thin films deposited with condition of 90/10 (Ar/$O_2$) ratio, the composition of Ba/Sr/Bi was 0.35/0.4/0.25. Also, in the BBST thin films deposited with condition of 80/20(Ar/$O_2$) ratio, the composition of Br,Sr and Ti were relatively uniform. But the component of Bi and Ti were diffused into the Pt layers.

  • PDF

고용량 캐패시터로의 응용을 위한 (Ba,Bi,Sr)TiO3세라믹스의 제조 및 특성에 관한 연구 (A Study on the Properties and fabrication to the (Ba,Bi,Sr)TiO3 Ceramics for the Application of High Capacitance)

  • 이상철;최의선;배선기;이영희
    • 한국전기전자재료학회논문지
    • /
    • 제16권3호
    • /
    • pp.195-201
    • /
    • 2003
  • The (Ba,Bi,Sr)TiO$_3$[BBST] thin films were fabricated on Pt/Ti/SiO$_2$ /Si substrate by RF sputtering method. The effects of Ar/O$_2$ ratio on the structural and dielectric properties of BBST thin films were investigated. Increasing the Ar/O$_2$ ratio, the intensity of BaBi$_4$Ti$_4$O$_{15}$ and Bi$_4$Ti$_3$O$_{12}$ peaks were increased but (Ba$_{0.5}$Sr$_{0.5}$)TiO$_3$ peak was decreased. In the BBST thin films deposited with condition of Ar/O$_2$(90/10) ratio, the composition ratio of the Ba, Bi and Sr atoms were 0.35, 0.25 and 0.4 respectively. The Bi and Ti atoms were diffused into the Pt layers. Increasing the Ar/O$_2$ ratio, the dielectric constant of the BBST thin films were increased but the dielectric loss of the BBST thin films were decreased. The dielectric constant and dielectric loss of the BBST deposited at 90/10 of Ar/O$_2$ ratio were 319 and 2.2%. respectively . Increasing the applied voltage, the capacitance of the BBST thin films were decreased.reased.

코딩-열분해법에 의해 제조한 BaTiO$_3 $ 박막의 결정 성장을 위한 낮은 산소 분압에서의 열처리 (Annealing under low oxygen partial pressure for crystal growth of BaTiO$_3 $thin films prepared by coating-pyrolysis process)

  • 김승원
    • 한국결정성장학회지
    • /
    • 제10권2호
    • /
    • pp.111-115
    • /
    • 2000
  • Ba과 Ti의 금속 유기 화합물을 이용하여 (100) $SrTiO_3$ 기판 위에 $BaTIO_3$ 박막을 코팅-열분해법으로 제조하였다. $450^{\circ}C$에서 사전 열처리한 비정질상의 박막은 $2\times 10^{-4}$ atm으로 조정된 산소 분압 하에서 $700^{\circ}C$ 이상의 온도로 열처리함으로써 결정화되었다. $800^{\circ}C$ 이하에서 제조한 박막의 기판에 수직한 면의 격자상수는 cubic $BaTIO_3$의 a 값에 가까우면 $800^{\circ}C$ 이하에서 제조한 박막의 tetragonal $BaTIO_3$ 의 a 값에 가까 웠다. 박막과 기판의 정렬상태를 XRD $\beta$ scan과 pole-figure로 분석한 결과 $BaTIO_3$ 박막은 $SrTiO_3$ 기판과 에피택시 관계가 있었다. $800^{\circ}C$에서 열처리한 박막의 표면은 0.4${\mu}m$ 정도의 섬 형태의 입자로 구성되어 있었고 약 0.8$\mu\textrm{m}$의 두께를 가진 단면은 구형의 입자가 층을 이루고 있었다.

  • PDF

졸-겔법을 이용한 $(Ba_{1-x}Sr_x)TiO_3$ 박막의 제조 및 특성 (Preparation and Characteristics of $(Ba_{1-x}Sr_x)TiO_3$ Thin Films by the Sol-gel Process)

  • 황규석;김병훈
    • 한국세라믹학회지
    • /
    • 제32권4호
    • /
    • pp.516-524
    • /
    • 1995
  • In this study, to prepare the dielectric (Ba, Sr)TiO3 thin films by the sol-gel process, Titaminum (IV) sio-propoxide (Ti[OCH(CH3)2]4), Ba and Sr acetate were used for sol and thin films were prepared by dip-coating process. Stability of sol decreased with the increase of Sr, and thickness of thin films were obtained 0.13~0.17${\mu}{\textrm}{m}$ by 1 coating cycle. Transmittance of amorphous thin films heated at 500 and 55$0^{\circ}C$ was very good, and crystallization tendency of thin films according to heat-treatment temperature and crystallization characteristics of thin films heated at 11$0^{\circ}C$ for 3 hrs were analysed. As a result, good perovskite structure was obtained higher than 100$0^{\circ}C$, and tetragonality of thin film was decreased but pyrochlore was formed with increasing Sr. In case of addition to substitute 0.4mol% Sr for Ba, dielectric constant was 288 and loss factor (tan $\delta$) was 0.04.

  • PDF

강유전체$Ba_{1-x}Sr_xTiO_3$ 박막의 제조 및 상부전극재료에 따른 전기적 특성 (Deposition $Ba_{1-x}Sr_xTiO_3$Thin Films and Electrical Properties with Various Materials Top Electrodes)

  • 박춘배;김덕규;전장배
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제48권6호
    • /
    • pp.410-415
    • /
    • 1999
  • $Ba_{1-x}Sr_xTiO_3$ thin films with various ratio of Sr (X = 0.4, 0.5, 0.6) were grown $Pt/TiN/SiO_2/Si$ subastrate by RF magnetron sputtering deposition. As, Ag, and Cu films were deposited on $Ba_{1-x}Sr_xTiO_3$ thin films as top electrodes by using a thermal evaporator. The electrical properties of $Ba_{1-x}Sr_xTiO_3$ thin films for various compositions were characterized and the physical properties at interface between $Ba_{1-x}Sr_xTiO_3$ thin films and top electrodes were evaluated in terms of the work function difference. At x =0.5, the degradation of capacitance is lower to the other compositions. As negative biasapplied, the specimen with Cu top electrode has board saturation region and low leakage current since work function of Cu is bigger than other electrodes.$ Ba_{0.5}Sr_{0.5}TiO_3$ thin films with Cu top electrode, the dielectric constant was measured to the value of 354 at 1 kHz and the leakage current was obtained to the value of $5.26\times10^{-6}A/cm2$ at the forward bias of 2 V.

  • PDF

$BCl_3/Cl_2$/Ar 고밀도 플라즈마에서 (Ba,Sr)$TiO_3$ 박막의 식각 특성에 관한 연구 (The Characteristics of (Ba,Sr)$TiO_3$ Thin Films Etched With The high Density $BCl_3/Cl_2$/Ar Plasma)

  • 김승범;김창일
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1999년도 추계학술대회 논문집 학회본부 C
    • /
    • pp.863-866
    • /
    • 1999
  • (Ba,Sr)$TiO_3$ thin films have attracted groat interest as new dielectric materials of capacitors for ultra-large-scale integrated dynamic random access memories (ULSI-DRAMs) such as 1 Gbit or 4 Gbit. In this study, inductively coupled $BCl_3/Cl_2$/Ar plasmas was used to etch (Ba,Sr)$TiO_3$ thin films. RF power/dc bias voltage = 600 W/-250 V and chamber pressure was 10 mTorr. The $Cl_2/(Cl_2+Ar)$ was fixed at 0.2, the (Ba,Sr)$TiO_3$ thin films were etched adding $BCl_3$. The highest (Ba,Sr)$TiO_3$ etch rate is 480$\AA/min$ at 10 % $BCl_3$ adding to $Cl_2$/Ar. The characteristics of the plasmas were estimated using optical emission spectroscopy (OES). The change of Cl, B radical density measured by OES as a function of $BCl_3$ percentage in $Cl_2$/Ar. The highest Cl radical density was shown at the addition of 10% $BCl_3$ to $Cl_2$/Ar. To study on the surface reaction of (Ba,Sr)$TiO_3$ thin films was investigated by XPS analysis. Ion enhancement etching is necessary to break Ba-O bond and to remove $BaCl_2$. There is a little chemical reaction between Sr and Cl, but Sr is removed by physical sputtering. There is a chemical reaction between Ti and Cl, and Tic14 is removed with ease. The cross-sectional of (Ba,Sr)$TiO_3$ thin film was investigated by scanning electron microscopy (SEM), the etch slope is about $65\;{\sim}\;70$.

  • PDF

기판온도에 따른 (Ba,Sr)TiO$_3$ 박막의 구조적 특성 (Structural Properties of (Ba,Sr)TiO$_3$ Thin Films with Substrate Temperature)

  • 이상철;임성수;정장호;배선기;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.649-652
    • /
    • 1999
  • The (Ba, Sr)TiO$_3$(BST) thin films were fabricated on Pt/Ti/SiO$_2$/Si substrate by RF sputtering technique. The structural properties of the BST thin films were investigated with substrate temperature by XRD, SEM, EDS and AES depth profils. Increasing the substrate temperature, barium multi titanate phases were decreased. The BST thin film had a structure of perovskite type, and had peaks of (100), (200) at the substrate temperature of 50$0^{\circ}C$. When the BST thin films were deposited at the substrate temperature of 50$0^{\circ}C$, the composition ratio of Ba/sr was 52/48.

  • PDF

새로운 방법으로 제조된 적층구조 $BaTiO_3$ 박막의 전기적 특성에 관한 연구 (Study on the electric properties of layered $BaTiO_3$ films prepared new stacking method)

  • 송만호;이윤희;한택상;오명환;윤기현
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1995년도 하계학술대회 논문집 C
    • /
    • pp.1129-1132
    • /
    • 1995
  • In the preparation of the layered $BaTiO_3$ thin films with high performance, the new stacking method using the continuous cooling of the substrate was introduced. Amorphous/polycrystalline $BaTiO_3$ layered structure was confirmed by SEM and index of refraction. The layered $BaTiO_3$ thin films formed by the new stacking method showed such a high dielectric constant that the layered structure could not be explained by a stacking structure of the two defined layers but could only be explained by multi-layered structure, i.e. amorphous/micro crystalline/polycrystalline structure. The layered $BaTiO_3$ thin film with a thickness of 240 nm showed higher capacitance per unit area and breakdown strength than the double layered $BaTiO_3$ thin film prepared by the conventional stacking method. And well defined ferroelectric hysteresis leer was observed in the layered $BaTiO_3$ thin film with a thickness of 200 nm.