α-case Interfacial Reaction Behavior of Al2O3 Mold Containing Interstitial and Substitutional Compounds for Titanium Investment Casting (침입형 및 치환형 화합물을 함유한 Ti 정밀주조용 Al2O3 주형의 α-case 계면반응 거동)

  • Choi, Bong-Jae;Lee, Seul;Kim, Young-Jig
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.7
    • /
    • pp.577-582
    • /
    • 2011
  • The newly developed ${\alpha}-case$ controlled mold material for Ti investment castings was suggested in this research. The $Al_2O_3$ mold containing interstitial $TiO_2$ and substitutional $Ti_3Al$ was manufactured by the reaction between $Al_2O_3$ and Ti. It is obvious that as the $TiO_2$ and $Ti_3Al$ content in the mold surface were increased, the depth of the interfacial reaction was significantly reduced. In addition, substitutional $Ti_5Si_3$ in the mold surface owing to the reaction between Ti and $SiO_2$ from the binder was effective for ${\alpha}-case$ reduction. Therefore, the ${\alpha}-case$ reduction was accomplished by the diffusion barrier effect of interstitial $TiO_2$, substitutional $Ti_3Al$ and $Ti_5Si_3$.

Effect of Sintering Additives and Annealing Atmospheres on the Microwave Dielectric and Sintering Characteristics of $(1-x)CaTiO_3-xLaAlO_3$ System (소결조제와 열처리 분위기가 $(1-x)CaTiO_3-xLaAlO_3$ 계의 소결 및 마이크로파 유전특성에 미치는 영향)

  • 이경태;여동훈;문종하
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.6
    • /
    • pp.629-635
    • /
    • 1997
  • The effects of the annealing atmospheres(O2, N2) and sintering additives that Bi2O3 is a major composition on the microwave dielectric and sintering propertie of (1-x)CaTiO3-xLaAlO3 system were investigated. The annealing atmospheres and the increase of annealing time after sintering did not affect the relative dielectric constant($\varepsilon$r) and temperature coefficient of resonant frequency($\tau$f) of (1-x)CaTiO3-xLaAlO3 system. However, the Q.f0 values of (1-x)CaTiO3-xLaAlO3 were very sensitive to annealing atmospheres. As the annealing time increased under O2 atmosphere the Q.f0 values of (1-x)CaTiO3-xLaAlO3 enhanced untill 10 hrs in 0.3$\leq$x$\leq$0.6 region, but degraded over that time. The increasing rate of Q.f0 value increased wth increasing x. On the other hand, as the annealing time increased under N2 atmosphere the Q.f0 values were constant in x$\leq$0.6 region, increased gradually in x$\geq$0.7 region. When 0.97Bi2O3-0.03Al2O3 and 0.76Bi2O3-0.24NiO of 3wt% as sintering additives were added to (Ca0.5La0.5) (Ti0.5Al0.5)O3 (x=0.5) the sintering temperature of 1$600^{\circ}C$ was lowered to 140$0^{\circ}C$, and the relative dielectric constant($\varepsilon$r) and temperature coefficient of resonant frequency($\tau$f) were not nearly changed. The addition of 0.97Bi2O3-0.03Al2O3 and 0.76Bi2O3-0.24NiO of 3wt% to (Ca0.5La0.5)(Ti0.5Al0.5)O3 made the Q.f0 values to be lower about 15% and 34%, respectively.

  • PDF

Characteristic Evaluation of SCR catalyst using Aluminum dross (알루미늄 폐드로스를 활용한 SCR 탈질촉매 제조 및 특성평가)

  • Bae, Min A;Kim, Hong Dae;Lee, Man Sig
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.14 no.10
    • /
    • pp.4672-4678
    • /
    • 2013
  • Aluminum dross is formation at the surface of the molten metal as the latter reacts with the furnace atmosphere and it was an unavoidable by-product of the aluminum production process. However aluminum dross was usually landfilled or disposed without treatment, causing much environmental damage. The purpose of this study is to investigate the possibility of ceramic catalyst support using recycled Al dross. The recycled Al dross was made into SCR catalyst by mixing with $WO_3$, $V_2O_5$ and $TiO_2$. The $V_2O_5-WO_3/TiO_2-Al_2O_3$ SCR catalyst was observed with XRF, XRD and BET. $V_2O_5-WO_3/TiO_2-Al_2O_3$ SCR strength was measured by Universal Testing Machine(UTM). As the added $Al_2O_3$, streagth is increased. And the NOx removal activity was observed by MR(Micro-Reactor). The temperatures ranging from $350^{\circ}C$ and $400^{\circ}C$, $V_2O_5-WO_3/TiO_2-Al_2O_3$ SCR catalyst De-NOx performance result of showed excellent activity over 90% at application condition.

Synthesis of Metallic Gold Colored α-Al2O3 Nanoplate-TiO2 Core-Shell Pigments with Robust and Photo-Stable Smooth TiO2 Shell

  • Lee, Su Jin;You, Myoung Sang;Park, Jin Kyoung;Park, Bum Jun;Im, Sang Hyuk
    • Applied Chemistry for Engineering
    • /
    • v.31 no.4
    • /
    • pp.390-397
    • /
    • 2020
  • To synthesize non-corrosive metallic gold colored α-Al2O3 nanoplate-TiO2 core-shell pigments with controlled roughness, we systematically checked the morphological variation of the TiO2 shell with the mole ratio of TiCl4 and NaOH from 1 : 1 to 1 : 1.5, 1 : 2, 1 : 2.5, 1 : 3, 1 : 3.5, and 1 : 4. The more increased mole ratio of TiCl4 and NaOH resulted in the smoother TiO2 shell due to the promoted formation of anatase TiO2 than that of the rutile one. By the heat-treatment of pigments at 500 ℃, we could improve the adhesiveness between TiO2 shell and α-Al2O3 nanoplates without changing their topology and roughness. In addition, the α-Al2O3 nanoplate with the robust TiO2 by heat-treatment exhibited comparable photo-stability against photo-catalytic degradation by UV exposure compared with the commercially available α-Al2O3/TiO2 lustering pigment.

Effect of Al2O3 Addition and WO3 Modification on Catalytic Activity of NiO/Al2O3-TiO2/WO3 for Ethylene Dimerization

  • Pae, Young-Il;Sohn, Jong-Rack
    • Bulletin of the Korean Chemical Society
    • /
    • v.28 no.10
    • /
    • pp.1763-1770
    • /
    • 2007
  • Strong solid acid catalysts, NiO/Al2O3-TiO2/WO3 for ethylene dimerization were prepared by the addition of Al2O3 and the modification with WO3. The acid sites and acid strength were increased by the inductive effect of WO3 species bonded to the surface of catalysts. The larger the dispersed WO3 amount, the higher both the acidity and catalytic activity for ethylene dimerization. The addition of Al2O3 to TiO2 up to 5 mol% enhanced acidity and catalytic activity gradually due to the interaction between Al2O3 and TiO2 and consequent formation of Al-O-Ti bond.

A Study on the Fabrication of Reinforced Reaction Bonded Alumina Ceramics (반응결합 강화 알루미나세라믹스의 제조에 관한 연구)

  • 김일수;강민수;박정현
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.4
    • /
    • pp.311-318
    • /
    • 1998
  • The reaction bonded alumina ceramics with reinforced particles which have low shrinkage were pro-duced by blending of SiC or TiC or ZrO2 powders to the mixture of Al metal and Al2O3 powder. The powd-ers were attrition milled isostantically pressed and preheated tio 110$0^{\circ}C$ with a heating rate of $1.5^{\circ}C$/min The specimens were then sintered at the temperature range 1500 to 1$600^{\circ}C$ for 5 hours with a heating rate of 5$^{\circ}C$/min. The specimens showed 5-9% weight gain and 2-9% dimensional expansion through the complete oxidation of Al after preheating up to 11--$^{\circ}C$ the overall dimensional change of the specimens after the reaction sintering at 1500-1$600^{\circ}C$ was 6-12% The maximum densities were 92% theoretical. The fine grain-ed(average grain size :0.4 ${\mu}{\textrm}{m}$) microstructure were observed in the specimen with ZrO2 and SiC. But the microstructure of specimen with TiC was relatively coarse.(average grain size : 2.1 ${\mu}{\textrm}{m}$) The mullite phase was formed by the reaction of Al2O3 and SiO2 in a specimen with SiC. In the TiC contained specimen TiC was oxidized into TiO2 and finally reacted with Al2O3 to form Al2TiO5 during sintering.

  • PDF

Occurrence and Chemical Composition of Ti-bearing Minerals from Samgwang Au-ag Deposit, Republic of Korea (삼광 금-은 광상에서 산출되는 함 티타늄 광물들의 산상 및 화학조성)

  • Yoo, Bong Chul
    • Korean Journal of Mineralogy and Petrology
    • /
    • v.33 no.3
    • /
    • pp.195-214
    • /
    • 2020
  • The Samgwang Au-Ag deposit has been one of the largest deposits in Korea. The deposit consists of eight lens-shaped quartz veins which filled fractures along fault zones in Precambrian metasedimentary rock, which feature suggest that it is an orogenic-type deposit. The Ti-bearing minerals occur in wallrock (titanite, ilmenite and rutile) and laminated quartz vein (rutile). They occur minerals including biotite, muscovite, chlorite, white mica, monazite, zircon, apatite in wallrock and white mica, chlorite, arsenopyrite in laminated quartz vein. Chemical composition of titanite has maximum vaules of 3.94 wt.% (Al2O3), 0.49 wt.% (FeO), 0.52 wt.% (Nb2O5), 0.46 wt.% (Y2O3) and 0.43 wt.% (V2O5). Titanite with 0.06~0.14 (Fe/Al ratio) and 0.06~0.15 (XAl (=Al/Al+Fe3++Ti)) corresponds with metamorphic origin and low-Al variety. Chemical composition of ilmenite has maximum values of 0.07 wt.% (ZrO2), 0.12 wt.% (HfO2), 0.26 wt.% (Nb2O5), 0.04 wt.% (Sb2O5), 0.13 wt.% (Ta2O5), 2.62 wt.% (As2O5), 0.29 wt.% (V2O5), 0.12 wt.% (Al2O3) and 1.59 wt.% (ZnO). Chemical composition of rutile in wallrock and laminated quartz vein has maximum values of 0.35 wt.%, 0.65 wt.% (HfO2), 2.52 wt.%, 0.19 wt.% (WO3), 1.28 wt.%, 1.71 wt.% (Nb2O3), 0.03 wt.%, 0.07 wt.% (Sb2O3), 0.28 wt.%, 0.21 wt.% (As2O5), 0.68 wt.%, 0.70 wt.% (V2O3), 0.48 wt.%, 0.59 wt.% (Cr2O3), 0.70 wt.%, 1.90 wt.% (Al2O3) and 4.76 wt.%, 3.17 wt.% (FeO), respectively. Rutile in laminated quartz vein is higher contents (HfO2, Nb2O3, As2O5, Cr2O3, Al2O3 and FeO) and lower content (WO3) than rutile in wallrock. The substitutions of rutile in wallrock and laminated quatz vein are as followed : rutile in wallrock [(Fe3+, Al3+, Cr3+) + Hf4+ + (W5+, As5+, Nb5+) ⟵⟶ 2Ti4+ + V4+, 2Fe2+ + (Al3+, Cr3+) + Hf4+ + (W5+, As5+, Nb5+) ⟵⟶ 2Ti4+ + 2V4+], rutile in laminated quartz vein [(Fe3+, Al3+) + As5+ ⟵⟶ Ti4+ + V4+, (Fe3+, Al3+) + As5+ ⟵⟶ Ti4+ + Hf4+, 4(Fe3+, Al3+) ⟵⟶ Ti4+ + (W5+, Nb5+) + Cr3+], respectively. Based on these data, titanite, ilmenite and rutile in wallrock were formed by resolution and reconcentration of cations (W5+, Nb5+, As5+, Hf4+, V4+, Cr3+, Al3+, Fe3+, Fe2+) in minerals of wallrock during regional metamorphism. And then rutile in laminated quartz vein was formed by reconcentration of cations (Nb5+, As5+, Hf4+, Cr3+, Al3+, Fe3+, Fe2+) in alteration minerals (white mica, chlorite) and Ti-bearing minerals reaction between hydrothermal fluid originated during ductile shear and Ti-bearing minerals (titanite, ilmenite and rutile) in wallrock.

The Effect of $Y_2O_3$ Dispersoids on the High Temperature Oxidation of Ti-34wt%Al-1.5wt%Mn Alloys (Ti-34wt%Al-1.5wt%Mn 합금의 고온산화에 미치는 $Y_2O_3$ 분산입자 첨가효과)

  • Lee, Dong-Bok
    • Journal of the Korean institute of surface engineering
    • /
    • v.39 no.6
    • /
    • pp.288-294
    • /
    • 2006
  • Alloys of TiAl-Mn-(0, 5, 10)wt.% $Y_2O_3$ were prepared by a powder metallurgical route, and their oxidation behavior was studied at 800, 900 and $1000^{\circ}C$ in 1 atm of air. The scale formed on the alloys consisted of $TiO_2$ and $Al_2O_3$ oxides. During oxidation, Mn tended to diffuse outward, whereas oxygen diffused inward. The dispersoids of $T_2O_3$, which segregated at the matrix grain boundaries, acted as a diffusion channel for cations and oxygen ions, nucleation sites for oxides, and vacancy annihilation sites. $T_2O_3$ increased the scale thickness, but improved the scale adherence.

Effect of Additives and Cooling Rates on the Electrical Resistivity of BaTiO3 Ceramics (I) (BaTiO$_3$ 세라믹스의 전기저항에 미치는 첨가제와 냉각속도의 영향(I) - TiO$_2$, SiO$_2$ 및 Al2O$_3$ 단미첨가 -)

  • 염희남;하명수;이재춘;정윤중
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.9
    • /
    • pp.661-666
    • /
    • 1991
  • Microstructure, room temperature resistivity and temperature coefficient of resistance of BaTiO3 ceramics were studied by varying cooling rates and additives such as TiO2, SiO2 and Al2O3. The basic composition of the BaTiO3 ceramics was formed by adding 0.25 mol% Dy2O3 and 0.07 mol% MnO2 to the BaTiO3 composition. Unlike the additives of SiO2 and Al2O3, an addition of 2 mol% TiO2 to the basic composition was effective to control the grain size of the fired specimens. The room temperature resistivity and the temperature coefficient of resistance for the specimen of this particular compostion were measured as about 102 ohm.cm and 16.5%/$^{\circ}C$, respectively. The observed grain boundary phase of the sample with Al2O3 additive was BaTi3O7, while that of the samples with SiO2 additive was confirmed as BaTiSiO5.

  • PDF

Fabrication and Machinability of Mullite-ZrO2-Al2TiO5 Ceramics

  • Shin, Young Been;Lee, Won Jae;Kim, Il Soo
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.6
    • /
    • pp.423-428
    • /
    • 2015
  • The machinability of materials is an important factor in engineering applications. Many ceramic components that have complex shapes require machining, typically using diamond tools, which leads to high production cost. Machinable ceramics containing h-BN have recently been developed, but these materials are very expensive because of high cost of raw materials and machining. Therefore the development of low-cost machinable ceramics is desirable. In this study, mullite-$ZrO_2$ ceramics were prepared additions of $Al_2TiO_5$. $ZrSiO_4$, $Al_2O_3$, and $Al_2TiO_5$ powders mixed at various molar ratios with sintering at 1400, 1500, and $1600^{\circ}C$ for 1 hr. Phase formation and microstructure of the sintered ceramics were observed by XRD and SEM, respectively. The machinability of each specimen was tested using the micro-hole machining method. The machinability results show that the ceramics sintered at temperatures over $1500^{\circ}C$ can be used as good low-cost machinable mullite-$ZrO_2-Al_2TiO_5$ ceramics.