Hydroxyapatite (HA) and $\beta$-tricalcium phosphate ($\beta$-TCP) are bio-compatible materials with bones and teeth. HA has been widely applied as bone substitutes because of chemical stability in vivo, while $\beta$-TCP has higher resorbability than HA when the material is implanted in a bone defect. In the present study, both HA and $\beta$-TCP porous ceramics were soaked in the simulated body fluid in order to investigate the reaction between the materials and the fluid. After the soaking test, carbonate hydroxyapatite was formed on HA surface at 1 week, and then the amount of precipitates increased with increasing period of the soaking test. While $\beta$-TCP was not dissolved in the fluid, carbonate hydroxyaopatite was also formed on $\beta$-TCP surface after 12 weeks, and the amount of precipitates was less than that on HA. In vitro behavior of HA was similar to that in vivo, but in vitro behavior of $\beta$-TCP was not similar to that in vivo.
연구 목적: $\beta$-Tricalcium phosphate/Hydroxyapatite ($\beta$-TCP/HA) 입자가 혼합된 합성 골 이식재의 particle size가 토끼의 두개골에서 타이타늄 메쉬를 이용해 시행된 골유도 재생술의 결과에 미치는 영향을 평가하고자 하였다. 연구 재료 및 방법: 여섯 마리의 수컷 뉴질랜드 산 백토끼 (5 kg)를 이용하여 실험 하였다. 토끼 두개골의 정 중앙을 절개하고 전층 판막을 형성하여 박리하였다. 두개골의 네 부위에 6 mm 직경의 트레핀 바 (XTP 5406; Dentium, Seoul, Korea)로 원형의 홈을 형성한 후 blood supply를 위해 원형의 홈안에 1 mm 직경의 라운드 바로 다섯 개의 작은 구멍을 형성하였다. 형성된 네 개의 홈 위에 표준화되어 맞춤 제작된 반구형 타이타늄 메쉬 (높이 3 mm, 직경 6 mm; Dentium, Seoul, Korea)를 위치시키고 세 개의 2 mm 길이의 티타늄 핀 (Dentium, Seoul, Korea)을 이용하여 고정하였다. 대조군은 이식재를 포함시키지 않았고 나머지 타이타늄 메쉬들은 실험군으로서 서로 다른 세 가지 크기의 이식재를 각각 담아서 고정하였다. 이식재 ($Osteon^{(R)}$, Dentium, Seoul, Korea)의 성분은 HA와 $\beta$-TCP ($\beta$-TCP/HA)가 혼합되어 있는 합성골 이식재이며 실험군으로 사용한 이식재의 크기는 각각 small (0.3 - 0.5 mm), medium (0.5 - 1.0 mm), large (1.0 - 2.0 mm) size 였다. 8주의 치유기간 후에 토끼를 희생시킨 후 조직 표본을 제작하고 CCD 카메라 (Polaroid DMC2 digital Microscope Camera (Polaroid Corporation, Cambridge, MA 02139, USA))가 부착되어 있는 광학 현미경 (Olympus BX, Tokyo, Japan)을 이용하여 두 가지 배율 (12.5배, 40배)로 조직학적 소견을 관찰하였다. 신생 골부위와 남은 골이식재 부위의 넓이를 측정하여 타이타늄 메쉬 내부 공간에서 차지하는 면적의 비율(%)을 구하였다. 그 수치들을 Mann-Whitney U-test와 Wilcoxon signed rank-test를 이용하여 통계 분석하였다 ($\alpha$ = .05). 결과: 대조군과 $\beta$-TCP/HA를 이식한 나머지 세 군의 신생골 형성을 비교하면 통계적으로 유의하게 $\beta$-TCP/HA를 이식한 군에서 신생골 형성이 더 많았다 (P = .003). 서로 다른 particle size 간 비교에서는 신생골 형성에 있어서 통계적으로 유의한 차이는 없었다. 하지만 형성된 수직골 총량 (신생골과 이식골의 면적의 합)을 각 그룹 간에 비교해 보면 대조군보다 $\beta$-TCP/HA를 이식한 군이 통계적으로 더 많은 비율을 나타내었고 (P = .001), 특히 $\beta$-TCP/HA 이식 군간 비교에서는 medium size 군이 large particle size 군보다 통계적으로 더 큰 면적을 나타내었다 (P = .039). 그러나 large particle size 군과 small particle size 군 사이 그리고 medium size 군과 small particle size 군 사이에는 통계적으로 유의한 차이를 보이지 않았다 (P> .05). 결론: 티타늄 메쉬를 이용한 수직골 증대술에서 $\beta$-TCP/HA 합성골을 사용하는 경우 수직골 형성에 기여하며 특히 medium size (0.5 - 1.0 mm)의 $\beta$-TCP/HA 이식재가 large size 이식재 보다 더 우수한 수직골 형성의 결과를 보였다.
Ceramics biomaterials are useful as implant materials in orthopedic surgery. In this study, porous HA(hydroxyapatite)/${\beta}$-TCP(tricalcium phosphate) composite biomaterials were successfully fabricated using HA/${\beta}$-TCP powders with 10-30 wt% $NH_4HCO_3$ as a space holder(SH) and $TiH_2$ as a foaming agent, and MgO powder as a binder. The HA/${\beta}$-TCP powders were consolidated by spark plasma sintering(SPS) process at $1000^{\circ}C$ under 20 MPa conditions. The effect of SH content on the pore size and distribution of the HA/${\beta}$-TCP composite was observed by scanning electron microscopy(SEM) and a microfocus X-ray computer tomography system(SMX-225CT). These microstructure observations revealed that the volume fraction of the pores increased with increasing SH content. The pore size of the HA/${\beta}$-TCP composites is about $400-500{\mu}m$. The relative density of the porous HA/${\beta}$-TCP composite increased with decreasing SH content. The porous HA/${\beta}$-TCP composite fabricated with 30%SH exhibited an elastic modulus similar to that of cortical bone; however, the compression strength of this composite is higher than that of cortical bone.
침전법 및 솔젤법에 의하여 10- l5 nm 및 500 nm 크기의 구형 TiO$_2$ 분말을 제조하고 수열합성법으로 50-70 nm 및 120-250 nm 크기의 침상 hydroxyapatite(이하 HA라 표기) 입자를 각각 제조한 다음, 두 분말의 조성비를 달리한 세 종류(HA/TiO$_2$비; 75/25, 50/50, 25/75wt%)의 HA/TiO$_2$ 복합분말을 planetary 볼밀로 혼합하여 각각 제조하였다. 복합분말을 탄소몰드에 넣고 hot-press를 사용하여 가압소결로 치밀체를 제조하였는데, 가압도중 대부분의 HA가 tricalcium phosphate(이하 TCP라 표기)로 분해되면서 $\beta$-TCP/TiO$_2$ 복합체가 제조되었다. 제조된 복합체의 미세구조와 소결밀도는 복합분말의 형태와 조성에 따라 변화하였는데, 입자가 균질하게 분산되어 있는 미세구조를 갖는 복합분말을 소결한 경우, 치밀한 소결체를 얻을 수 있었으며, 소결온도가 증가할수록 균질한 미세구조를 나타내었다. 또한 복합분말 내 HA 함량이 증가하면서 소결체의 입자크기가 증가한 반면, 소결밀도가 감소하고, 미세구조는 불균질하였다. 반대로 HA분말에 비하여 TiO$_2$분말의 함량이 큰 시편은 전체적으로 작은 입자크기와 균질한 미세구조를 나타냈으며, 소결밀도 또한 증가하였다.
Park, Jung-Chul;Lim, Hyun-Chang;Sohn, Joo-Yeon;Yun, Jeong-Ho;Jung, Ui-Won;Kim, Chang-Sung;Cho, Kyoo-Sung;Kim, Chong-Kwan;Choi, Seong-Ho
Journal of Periodontal and Implant Science
/
제39권sup2호
/
pp.223-230
/
2009
Purpose: Synthetic bone products such as biphasic calcium phosphate (BCP) are mixtures of hydroxyapatite (HA) and ${\beta}$-tricalcium phosphate (${\beta}$- TCP). In periodontal therapies and implant treatments, BCP provides to be a good bone reconstructive material since it has a similar chemical composition to biological bone apatites. The purpose of this study was to compare bone regeneration capacity of two commercially available BCP. Methods: Calvarial defects were prepared in sixteen 9-20 months old New Zealand White male rabbits. BCP with HA and ${\beta}$- TCP (70:30) and BCP with Silicon-substituted hydroxyapatite (Si-HA) and ${\beta}$-TCP (60:40) particles were filled in each defect. Control defects were filled with only blood clots. Animals were sacrificed at 4 and 8 week postoperatively. Histomorphometric analysis was performed. Results: BCP with HAand ${\beta}$- TCP 8 weeks group and BCP with Si-HA and ${\beta}$- TCP 4 and 8 weeks groups showed statistically significant in crease (P <0.05) in augmented area than control group. Newly formed bone area after 4 and 8 weeks was similar among all the groups. Residual materials were slightly more evident in BCP with HA and ${\beta}$- TCP 8 weeks group. Conclusions: Based on histological results, BCP with HA and ${\beta}$- TCP and BCP with Si-HA and ${\beta}$- TCP appears to demonstrate acceptable space maintaining capacity and elicit significant new bone formation when compared to natural bone healing in 4 and 8 week periods.
Abstract Scaffold used as a carrier of the cell has been actively conducted using plenty of technology in tissue engineering. ${\beta}$-tricalcium phosphate (${\beta}$-TCP) material has shown good biocompatibility and osteoconductive ability when it was implanted as a bone graft substitute in osseous defect in human and animal studies for bone regeneration. In this study, we fabricated the blended polycaprolactone (PCL) and ${\beta}$-TCP scaffold by the polymer deposition system (PDS). The PCL/${\beta}$-TCP scaffold was fabricated at a temperature of $110^{\circ}C$, pressure of 650 kPa, and scan velocity of 100 mm/sec. The Overall geometry and size of the scaffold were fixed circle type with a diameter of 10 mm and a height of 4 mm. PCL/${\beta}$-TCP scaffold was observed by scanning electron microscopy. Cell attachment and proliferation of the scaffold containing 30 wt% ${\beta}$-TCP was superior to those containing 10 wt% and 20 wt% ${\beta}$-TCP.
PURPOSE. The purpose of this study was to evaluate the properties of a porous zirconia scaffold coated with bioactive materials and compare the in vitro cellular behavior of MC3T3-E1 preosteoblastic cells to titanium and zirconia disks and porous zirconia scaffolds. MATERIALS AND METHODS. Titanium and zirconia disks were prepared. A porous zirconia scaffold was fabricated with an open cell polyurethane disk foam template. The porous zirconia scaffolds were coated with ${\beta}$-TCP, HA and a compound of ${\beta}$-TCP and HA (BCP). The characteristics of the specimens were evaluated using scanning electron microscopy (SEM), energy dispersive x-ray spectrometer (EDX), and x-ray diffractometry (XRD). The dissolution tests were analyzed by an inductively coupled plasma spectrometer (ICP). The osteogenic effect of MC3T3-E1 cells was assessed via cell counting and reverse transcriptase-polymerase chain reaction (RT-PCR). RESULTS. The EDX profiles showed the substrate of zirconia, which was surrounded by the Ca-P layer. In the dissolution test, dissolved $Ca^{2+}$ ions were observed in the following decreasing order; ${\beta}$-TCP > BCP > HA (P<.05). In the cellular experiments, the cell proliferation on titanium disks appeared significantly lower in comparison to the other groups after 5 days (P<.05). The zirconia scaffolds had greater values than the zirconia disks (P<.05). The mRNA level of osteocalcin was highest on the non-coated zirconia scaffolds after 7 days. CONCLUSION. Zirconia had greater osteoblast cell activity than titanium. The interconnecting pores of the zirconia scaffolds showed enhanced proliferation and cell differentiation. The activity of osteoblast was more affected by microstructure than by coating materials.
PURPOSE. This randomized clinical trial was conducted to assess the safety and effectiveness of the ErhBMP-2 in alveolar bone regeneration as well as preservation of the ${\beta}$-TCP bone graft material that contains ErhBMP-2. MATERIALS AND METHODS. This study involved 72 patients at the 3 study centers. The patients, who were divided into 2 groups: the experiment group who had ErhBMP-2 coated TCP/HA and the control group who had TCP/HA graft material alone transplanted immediately after tooth extraction. CT was taken before and 3 months after the transplantation and healing status was compared between the two groups. The efficacy endpoints that were used to measure the degree of bone induction included alveolar bone height and 3 measurements of bone width. The paired t test was used to determine the significance of the changes (P<.05). RESULTS. Changes in alveolar bone height were $-1.087{\pm}1.413$ mm in the control group and $-.059{\pm}0.960$ mm in the experimental group (P<.01). At 25% extraction socket length [ESL], the changes were $0.006{\pm}1.149$ mm in the control group and $1.279{\pm}1.387$ mm in the experimental group. At 50% ESL, the changes were $0.542{\pm}1.157$ mm and $1.239{\pm}1.249$ mm, respectively (P<.01 for 25% ESL, and P<.05 for 50% ESL). During the experiment, no adverse reactions to the graft material were observed. CONCLUSION. ErhBMP-2 coated ${\beta}$-TCP/HA were found to be more effective in preserving alveolar bone than conventional ${\beta}$-TCP/HA alloplastic bone graft materials.
인산칼슘(hydroxyapatite(HAp), ${\beta}$-tricalcium phosphate(${\beta}$-TCP) 및 HAp와 ${\beta}$-TCP가 혼합된 2상 인산칼슘(BCP, HA/${\beta}$-TCP))들을 수열합성법을 통해 합성하였다. 여러 수열합성 조건(최고온도 $150^{\circ}C$ 및 pH 12 이하)에서 수산화칼슘($Ca(OH)_2$) 수용액과 인산($H_3PO_4$) 용액을 반응시켜 얻은 침전물을 수열합성에 이용하였다. 초기 전구체 Ca/P 비율을 1.30, 1.50 및 1.67로 조절하였으며 이 조성비와 합성 후 열처리가 분말 및 소결체의 상합성에 미치는 영향에 대해 조사하였다. 초기 전구체 Ca/P 비율을 조절함으로써 분말 및 소결체의 상의 조절이 가능하였다. Ca/P 비율이 1.67일 경우 모든 열처리 온도에서 분말 및 소결체 모두에서 HAp 단일 상이 합성되었다. Ca/P 비율이 1.30과 1.50에서 $900^{\circ}C$ 이상 열처리 할 경우 각각 순수한 ${\beta}$-TCP와 BCP(HAp/${\beta}$-TCP)가 합성되었다. 반응성 높은 미세한 분말을 이용하여 소결함으로써 미세한 입경을 가지며 투광성을 가지는 소결체들을 저온에서 얻을 수 있었다.
Purpose: The aim of this pilot study was to determine the osteoconductivity and dimensional stability of augmented sinuses using different ratios of biphasic calcium phosphate (BCP) in a rabbit sinus model. Methods: Each sinus of New Zealand white rabbits (2.5-3.5 kg) was assigned to one of two groups: BCP with a hydroxyapatite to ${\beta}$-tricalcium phosphate (HA:${\beta}$-TCP) ratio of 70:30 (group TCP30) and BCP with an HA:${\beta}$-TCP ratio of 30:70 (group TCP70). After preparing a window in the antral wall of a sinus, the Schneiderian membrane was elevated, and the applicable material was grafted. A fluorochrome calcein green was injected five days before euthanizing the animals at four months post-surgery. The specimens were analyzed histologically, histomorphometrically, and by using micro-computed tomography (micro-CT). Results: Micro-CT analysis revealed that the total augmented volume and the new bone volume did not differ significantly between the two groups whereas the resorption of materials was greater in the TCP70 group. The trabecular thickness, number, and separation also did not differ significantly between the two groups. Histomorphometrically, the areas of total augmentation, new bone, and residual material, as well as the ratio of new-bone-material contact did not differ significantly between the groups. Histologically, the residual particles were more scattered in the TCP70 group than in the TCP30 group. The fluorescence of the calcein green did not differ notably between the two groups. Conclusions: The osteoconductivity and dimensional stability of the two BCPs with different ratios tested in this study were comparable after four months of healing. Therefore, we conclude that both BCPs show promise as a bone substitute for sinus augmentation.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.