• Title/Summary/Keyword: $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$

Search Result 13, Processing Time 0.029 seconds

Fabrication and Characterization of$(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$ Thin Films by Pulsed Laser Deposition (펄스 레이저 증착법에 의한 $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$ 박막의 제작 및 특성)

  • Shim, Kyung-Suk;Lee, Sang-Yeol
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.48 no.5
    • /
    • pp.303-308
    • /
    • 1999
  • Dielectric thin films of PLT(28) ($(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$) have been deposited on $Pt/Ti/SiO_2/Si$ substrates in situ by a laser ablation. We have systematically changed the laser fluence from 0.4 J/$cm^2$ to 3 J/$cm^2$, and deposition temperature from $450^{\circ}C\; to\; 700^{\circ}C$. The surface morphology was changed from planar grain structure to columnar structure as the nucleation energy was increased. The PLT thin film with columnar structure showed good dielectric properties. The deposition temperature influenced on nucleation energy much stronger than the laser energy density did.

  • PDF

Growth of $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$ thin film by pulsed laser deposition (펄스 레이저 증착법에 의한 $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$ 박막의 증착)

  • Eun, Dong-Seog;Park, Jeong-Heum;Lee, Sang-Yeol;Park, Chang-Yub
    • Proceedings of the KIEE Conference
    • /
    • 1997.07d
    • /
    • pp.1236-1238
    • /
    • 1997
  • 유전체 PLT(28) ($Pb_{0.72}La_{0.28}Ti_{0.93}O_3$) 박막을 레이저 어블레이션 기법으로 Pt/Ti/$SiO_3$/Si기판을 $500^{\circ}C{\sim}700^{\circ}C$까지 가열한 상태에서 $O_2$분위기에서 증착시켰다. 증착된 박막은 SEM, XRD 등의 구조적 분석을 통하여 $600^{\circ}C$이상에서 증착된 경우, (111)방향으로 우세하게 성장한, 결정성이 양호한 박막임을 확인하였다. 박막의 전기적 특성은, 증착 온도가 $650^{\circ}C$일 때 약 1400정도의 높은 비유전율을 얻었으며, 전하저장밀도는 100[KV/cm]에서 약 9[${\mu}C/cm^2$]이었다.

  • PDF

Enhancement of Dielectric Properties of Pb(La,Ti)$O_3$ Thin Films Using Two-step Process (Two-Step Process를 이용한 Pb(La,Ti)$O_3$ 박막의 유전특성 향상 연구)

  • Hur, Chang-Hoi;Lee, Sang-Yeol
    • Proceedings of the KIEE Conference
    • /
    • 2000.11c
    • /
    • pp.416-418
    • /
    • 2000
  • Thin films of phase-pure perovskite $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$ (PLT) were deposited in-situ onto Pt/Ti/$SiO_2$/Si substrates by pulsed laser deposition. We have systematically investigated the variation of grain sizes depending on the process condition. Both in-situ annealing and ex-situ annealing treatments have been compared depending on the annealing time. The grain sizes of PLT thin films were successfully controlled 260 to 350 nm by changing process parameters. Microstructural and electrical properties of the film were investigated by C-V measurement, leakage current measurement and SEM. Two-step process to grow $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$ (PLT) films was adopted and verified to be useful to enlarge the grain size of the film and to enhance the leakage current characteristics.

  • PDF

Effect of the Hydrogen Annealing on the Pb(Zr0.52Ti0.48)O3 Film using (Pb0.72La0.28)Ti0.94O3 Buffers ((Pb0.72La0.28)Ti0.94O3 Buffer를 사용한 Pb(Zr0.52Ti0.48)O3 박막의 수소 후열처리 효과)

  • Lee, Eun-Sun;Li, Dong-Hua;Chung, Hyun-Woo;Lim, Sung-Hoon;Lee, Sang-Yeol
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.18 no.4
    • /
    • pp.327-329
    • /
    • 2005
  • Pb(Zr/sub 0.52/Ti/sub 0.48/)O₃(PZT) thin films were deposited by using a pulsed laser deposition method on a Pt/Ti/SiO₂/Si substrate with (Pb/sub 0.72/La/sub 0.28/)Ti/sub 0.93/O₃ (PLT) buffer and on a Pt/Ti/SiO₂/Si substrate without buffer. These films were annealed in H₂-contained ambient for 30 minutes at the substrate temperature of 400。C to evaluate the forming gas annealing effects. The comparative studies on the ferroelectric properties of these two films were carried out, which are shown that ferroelectric properties, such as remanent polarization didn't change in the case of PLT buffered PZT film while remanent polarization value of PZT film degraded from 20.8 C/㎠ to 7.3 C/㎠. The leakage current became higher in both cases, but that of the more-oriented PZT film had the moderate value of the 10/sup -6/ order of A/㎠. This is mainly because the hydrogen atoms which make the degradation of PZT films cannot infiltrate into the more -oriented PZT film as well as the less-oriented PZT film.

Hydrogen Annealing effect on the dielectric properties of $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$ thin film

  • Lee, Eun-Sun;Chung, Hyun-Woo;Lim, Sung-Hoon;Lee, Sang-Yeol
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.07a
    • /
    • pp.41-43
    • /
    • 2004
  • Dielectric thin films of $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3$ were deposited on $Pt(111)/Ti/SiO_2/Si$ substrates in situ by pulsed laser deposition(PLD) and annealed with different gases which are forming gas and oxygen gas, respectively. The diffusion of hydrogen into the ferroelectric film was caused by annealing process and resulted in the destruction of polarization. The dielectric properties of forming gas annealed PLT thin films, which are dielectric constant, ferroelectric characteristic, and leakage current characteristics, were degraded

  • PDF

Effect Of Variation Of Laser Wavelength OH Properties of ($Pb_{0.72}La_{0.28}$)$Ti_{0.93}O_{3}$Thin Films Fabricated by Pulsed Laser Deposition (펄스레이저 증착법으로 제작된 ($Pb_{0.72}La_{0.28}$)$Ti_{0.93}O_{3}$박막의 레이저 파장 변화에 따른 특성 연구)

  • 한경보;허창회;이상렬
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.170-173
    • /
    • 2001
  • Thin films of phase-pure perovskite (P $b_{0.72}$L $a_{0.28}$) $Ti_{0.93}$ $O_3$(PLT) were deposited in-situ onto Pt/Ti/ $SiO_2$/Si substrates by pulsed laser deposition. We have systematically investigated the variation of grain sizes depending on the process condition. Both in-situ annealing and ex-situ annealing treatments have been compared depending on the annealing time. Two-step process to grow (P $b_{0.72}$L $a_{0.28}$) $Ti_{0.93}$ $O_3$(PLT) films was adopted and verified to be useful to enlarge the grain size of the film and to enhance the leakage current characteristics. The grain sizes of PLT thin films were successfully controlled 260 to 350 nm by changing process parameters. Electrical properties including dielectric constant, ferroelectric characteristics, crystallization and leakage current of PLT thin films were shown to be strongly inf1uenced by grain size. Also PLT thin films on p-type(100) Si substrate will be fabricated by pulsed laser deposition technique using a Nd:YAG laser with different wavelengths of 355, 532 and 1064 nm. Effect of the variation of laser wavelength on dielectric properties will be discussed. Microstructural and electrical properties of the film were investigated by C-V measurement leakage current measurement and SEM.ent and SEM.

  • PDF

Effect of grain size of Pb(La,Ti)O$_3$thin films grown by pulsed laser deposition for memory device application (메모리 소자 응용을 위한 펄스 레이저 증착법으로 제작된 PLT박막의 열처리 효과 연구)

  • 허창회;심경석;이상렬
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.07a
    • /
    • pp.861-864
    • /
    • 2000
  • Ferroelectric thin film capacitors with high dielectric constant are important for the application of memory devices. In this work, thin films of PLT(28)(Pb$\sub$0.72/La$\sub$0.28/Ti$\sub$0.93/O$_3$) were fabricated on Pt/Ti/SiO$_2$/Si substrates in-situ annealing and ex-situ annealing have been compared depending on the annealing time. We have systematically investigated the variation of grain sizes depending on the condition of post-annealing and the variation of deposition rate. C-V measurement, ferroelectric properties, leakage current and SEM were performed to investigate the electrical properties and the microstructural properties of Pb(La,Ti)O$_3$.

  • PDF

Hydrogen Post-annealing Effect of (Pb0.72,La0.28)Ti0.93O3 Films Fabricated by Pulsed Laser Deposition (펄스레이저 증착법으로 제작된(Pb0.72,La0.28)Ti0.93O3박막의 수소후열처리에 관한 전기적 특성 연구)

  • 한경보;전창훈;전희석;이상렬
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.16 no.3
    • /
    • pp.190-194
    • /
    • 2003
  • Dielectric thin films of (P $b_{0.72}$,L $a_{0.28}$) $Ti_{0.93}$ $O_3$ (PLT(28)) have been deposited on Pt(111)/Ti/ $SiO_2$/Si(100) substrates in-situ by pulsed laser deposition using different annealing and deposition Processes. We have investigated the effect of hydrogen annealing on the ferroelectric properties of PLT thin films and found that the annealing process causes the diffusion of hydrogen into the ferroelectric film resulting in the destruction of polarization. We have tried to form the film by a two-step deposition process In order to improve electrical property. Two-step process to grow PLT films was adopted and verified to be useful to enlarge the grain size of the film and to reduce the leakage current characteristics. Structural properties and electrical properties including dielectric constant, ferroelectric characteristics, and leakage current of PLT thin films were shown to be strongly influenced by grain size. The film deposited by using two-step Process including pre-annealing treatment has a strongly(111) orientation. However, the films deposited by using single -step process with hydrogen annealing process show the smallest grain size. The film deposited by using two-step process including pre-annealing treatment shows the leakage current density of below 10$^{-7}$ A/c $m^2$ for the field of smaller than 100 kV/cm. However, the films deposited by using single-step process with hydrogen annealing process and pre-annealing process show worse leakage current density than the film deposited by using two-step process including pre-annealing treatment.tment.

Fabrication of $(Pb,La)TiO_3$ Thin Films by Pulsed Laser Ablation (레이저 어블레이션에 의한 $(Pb,La)TiO_3$ 박막의 제작)

  • Park, Jeong-Heum;Kim, Joon-Han;Lee, Sang-Yeol;Park, Chong-Woo;Park, Chang-Yub
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.2
    • /
    • pp.133-137
    • /
    • 1998
  • $(Pb_{0.72}La_{0.28})Ti_{0.93}O_3(PLT(28))$ thin films were fabricated by pulsed laser deposition. PLT films deposited on $Pt/Ti/SiO_2/Si$ at $600^{\circ}C$ had a preferred orientation in (111) plane and at $550^{\circ}C$ had a (100) preferred orientation. We found that (111) preferred oriented films had well grown normal to substrate surface. This PLT(28) thin films of $1{\mu}m$ thickness had dielectric properties of ${\varepsilon}_r$=1300, dielectric $loss{\fallingdotseq}0.03 $. and had charge storage density of 10 [${\mu}C/cm^2$] and leakage current density of less than $10^{-6}[A/cm^2]$ at 100[kV/cm]. These results indicated that the PLT(28) thin films fabricated by pulsed laser deposition are suitable for DRAM capacitor application.

  • PDF

Development of high dielectric PLT thin films by laser processing for high power applications (레이저 공정을 이용한 전력용 고유전율 PLT 박막 개발)

  • Lee, Sang-Yeol
    • Proceedings of the KIEE Conference
    • /
    • 1998.11c
    • /
    • pp.1046-1049
    • /
    • 1998
  • PLT(28) ($Pb_{0.72}La_{0.28}Ti_{0.93}O_3$) dielectric thin films have been deposited on Pt/Ti/$SiO_2$/Si substrates in situ by a laser ablation. We have systematically changed the laser fluence from $0.5\;J/cm^2$ to $3\;J/cm^2$, and deposition temperature from $450^{\circ}C$ to $700^{\circ}C$. The surface morphology was changed from planar grain structure to columnar structure as the nucleation energy was increased. The PLT thin film with columnar structure showed good dielectric properties. It is shown that the deposition temperature strongly affect the film nucleation compared with the laser fluence.

  • PDF