Abstract
The purpose of this study was to design the self-compaction concrete mixture, having not only high strength but also compensation of shrinkage without thermal crack under 4 sides outer restraint of the member. In the experimental mix, replacement ratio of limestone Powder, CSA expansive additives, and unit water were selected as parameters, using portland blast-furnace slag cement. And, bleeding test, expansibility test, hydration heat analysis were performed. As a results, when 35% of limestone Powder, 6% CSA expansive additives are replaced at unit water 175kg/$\textrm{m}^3$, demanded performances of fresh and hardened self-compaction concrete are accomplished.