Abstract

High fluid concrete unlike OPC concrete is made with various material, and the phase of fresh concrete is considerably different. In order to understand fluidity phase and mix properties of high fluid concrete, concrete is required to access as suspension structure which consists of aggregate and paste. The focus of this paper is to analyze the test results and quantify the effect of mix proportions of mortar and fineness modulus of sand on the properties of fresh mortar. The effect of water-binder ratio. sand-binder ration. contents of ggbs (by mass of total cementitious materials). and various contents of water reducing agent on the yield stress and plastic viscosity of the mix is studied. Based on the experimental results, the fellowing conclusions can be drawn: (1) The mixing time needed for high fluid mortar was approximately two times more than that of ordinary portland mortar. (2) The fluidity phase of mortar could be explained by yield stress of mix and the fluidity of mortar. (3) As the content of ggbs increased, yield stress of mortar was decreased and plastic viscosity of it was increased. (4) For the high fluid mortar, it was appeared that sand-binder ratio should be below 1.5.

Keywords

References

  1. 岡村甫, 前川宏一, 小澤一雅, "ハイパフオ一マンスコンクりート", 技報堂, 1993. 9
  2. 村田二郞 "まだ固まらないコンクリ一トのレオロジーに關する基礎的硏究", コンクリート工學, Vol.15, No. 1, Jan. 1977, pp. 25-34
  3. 김재훈 외 3 인, "플라이애쉬 및 고로슬래그를 사용한 시멘트페이스트의 레올로지 특성에 관한 연구", 대한건축학회 논문집, Vol14., No.6 구조계, 1998. 6, pp.105-115
  4. P.C.Aitcin, "High Performance Concrete", 1998, pp.269
  5. ACI Committee 233, "Ground Granulated Blast Furnace Slag as a Cementitious Constituent in Concrete", 1995.
  6. 김재훈 외 2 인, "문헌조사를 통한 한.일간의 고유동 콘크리트 사용 재료의 구성에 관한 비교 연구", 대한건축학회 논문집, 제 14권 12호, 1998.12, pp.111-118
  7. 平田隆祥, 竹田宣典, "高流動コンクートのフレッシュ性狀に及ぼす骨材粒度の影響", コンクリート工學年次論文報告集, Vol. 17, No.1, 1995, pp.81-86
  8. 須藤榮治, 五味信治, "細骨材の粗粒率ガ高流動コンクリートのフレッシュ時の性狀におよぼす影響", コンクリート工學年次論文報告集, Vol. 18, No.1, 1996, pp.123-128
  9. 竹內博幸, 吉井一郞 "高流動コンクリートの配合設計および製造に關する硏究", コンクリート工學年次論文報告集, Vol. 18, No.1, 1996, pp.39-44

Cited by

  1. Utilization of power plant bottom ash as aggregates in fiber-reinforced cellular concrete vol.30, pp.2, 2010, https://doi.org/10.1016/j.wasman.2009.09.043