The pure Ti is taken annealing process for one hour at 90$0^{\circ}C$. The pure Ti is sufficient for ASTM B348 Grade2. The rolling mill roll the Ti-8Ta-3Nb(wt%) which became vacuum melting in arc furnace until the length is about 45mm and the thickness is about 6.05mm. Then it is made 6mm$\times$6mm$\times$44mm by wire cutting with EDM and it is made ∮ 6mm by rough cutting with the general purpose lathe. The machining accuracy of implant parts in the dental and medical science are decided by dimension, shpe, straightness, surface roughness. It is difficult to cut for the Ti alloy. It is caused problems of straight degree and surface roughness to the Ti alloy have many cases which length is smaller than diameter in cutting. Total 24 specimens different kind of 4 alloies are used in experiment to gain a cutting property. According to the cutting velocity, cutting depth, cutting temperature, feed and clearance angle experiments are performed. Conclusively it is expected that cutting depth of 0.5mm, feed velocity of 0.07mm/rev and cutting velocity of 80m/min could make a suitable result.

키워드