• 제목/요약/키워드: wood density

검색결과 594건 처리시간 0.025초

Characteristics of Magnetic Sengon Wood Impregnated with Nano Fe3O4 and Furfuryl Alcohol

  • Gilang Dwi LAKSONO;Istie Sekartining RAHAYU;Lina KARLINASARI;Wayan DARMAWAN;Esti PRIHATINI
    • Journal of the Korean Wood Science and Technology
    • /
    • 제51권1호
    • /
    • pp.1-13
    • /
    • 2023
  • Sengon (Falcataria moluccana Miq.) tree offers a wood of low quality and durability owing to its low density and thin cell walls. This study aimed to improve the properties of sengon wood by making the wood magnetic, producing new functions, and characterizing magnetic sengon wood. Each wood sample was treated using one of the following impregnation solutions: Untreated, 7.5% nano magnetite-furfuryl alcohol (Fe3O4-FA), 10% nano Fe3O4-FA, and 12.5% nano Fe3O4-FA. The impregnation process began with vacuum treatment at 0.5 bar for 2 h, followed by applying a pressure of 1 bar for 2 h. The samples were then tested for dimensional stability and density and characterized using scanning electron microscopy and energy-dispersive X-ray spectroscopy (SEM-EDX), Fourier transform infrared spectrometry (FTIR), X-ray diffraction (XRD) analysis, and vibrating sample magnetometry (VSM) analysis. The results showed that the Fe3O4-FA impregnation treatment considerable affected the dimensional stability, measured in terms of weight percent gain, anti-swelling efficiency, water uptake, and bulking effect, as well as the density of sengon wood. Changes in wood morphology were detected by the presence of Fe deposits in the cell walls and cell cavities of the wood using SEM-EDX analysis. XRD and FTIR analyses showed the appearance of magnetite peaks in the diffractogram and Fe-O functional groups. Based on the VSM analysis, treated sengon wood is classified as a superparamagnetic material with soft magnetic properties. Overall, 10% Fe3O4-FA treatment led to the highest increase in dimensional stability and density of sengon wood.

목분의 첨가량에 따른 산화마그네슘 경화체의 밀도 및 흡수율 특성 (Density and Water Absorption Ratio Property of the Magnesium Oxide Matrix According to Wood flour Addition Ratio)

  • 정병열;김헌태;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.236-237
    • /
    • 2014
  • Recently, it changes to the frame construction in the wall type structure for the life span improvement of the apartment house of our country. The execution of the light panel increased while the execution of the frame construction increased. Therefore, the density and absorption ratio of the magnesium oxide matrix according to the wood flour amount of addition ratio property try to be analyze for the lightweight of the surface material of the light panel. The test result, the density has been declined as the addition ratio increase of the wood flour. In the case of the water absorption ratio, water absorption ratio has been increased as addition ratio increase of wood flour. However, wood flour addition ratio 15% determined the most appropriate when considering the density and water absorption ratio.

  • PDF

열압밀화를 이용한 낙엽송의 표면경도 개선 (Surface Hardness Improvement of Larch Wood Using Thermal-Compression)

  • 황성욱;박상범;서진석;김종인;홍성철;이원희
    • 한국가구학회지
    • /
    • 제23권4호
    • /
    • pp.460-466
    • /
    • 2012
  • This study was conducted to investigate the surface hardness of thermally-compressed larch wood by compression set and temperature. The surface hardness of thermally-compressed larch wood increased with increasing compression set and temperature. For compression set 60%, the specific gravity was increased as 0.93. However, the surface hardness was lower value as 31.1 N/$mm^2$ compared with a similar specific gravity of the tropical timber. For density profile, less than compression set 40%, compression was observed mainly surface area. On the other hand, more than 50%, density profile variation was reduced by compression of central part. Results of this study indicate that thermally-compressed larch wood can be replace some imported hardwoods such as oak or cherry. However, thermally-compressed larch wood was difficult to replace the tropical timber being imported in terms of surface hardness.

  • PDF

Determination of Air-dry Density of Wood with Polychromatic X-ray and Digital Detector

  • Kim, Chul-Ki;Kim, Kwang-Mo;Lee, Sang-Joon;Lee, Jun-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • 제45권6호
    • /
    • pp.836-845
    • /
    • 2017
  • Gravimetric method is usually used to evaluate air-dry density, which is governing physical or mechanical properties of wood. Although it had high evaluation accuracy, the method is time consuming process. Thus, this study was conducted to estimate air-dry density of wood with high accuracy by using polychromatic X-ray and digital detector as alternative of gravimetric method. To quantify polychromatic X-ray projection for evaluating air-dry density, Lambert-Beer's law with the integral value of probability function was used. The integral value was used as weighting factor in the law, and it was determined by conducting simple test at various penetration depths and tube voltage. Mass attenuation coefficient (MAC) of wood also calculated by investigating polychromatic X-ray projection according to species, penetration depth and tube voltage. The species had not an effect on change of MAC. Finally, an air-dry density of wood was estimated by applying the integral value, MAC and Lambert-Beer's law to polychromatic X-ray projection. As an example, the relation of the integral value (${\alpha}$) according to penetration depth (t, cm) at tube voltage of 35 kV was ${\alpha}=-0.00091t{\times}0.0184$ while the regression of the MAC (${\mu}$, $cm^2/g$) was ${\mu}=0.5414{\exp}(-0.0734t)$. When calculation of root mean squared error (RMSE) was performed to check the estimation accuracy, RMSE at 35, 45 and 55 kV was 0.010, 0.013 and $0.009g/cm^3$, respectively. However, partial RMSE in relation to air-dry density was varied according to tube voltage. The partial RMSE below air-dry density of $0.41g/cm^3$ was $0.008g/cm^3$ when tube voltage of 35 kV was used. Meanwhile, the partial RMSE above air-dry density of $0.41g/cm^3$ decreased as tube voltage increased. It was conclude that the accuracy of estimation with polychromatic X-ray and digital detector was quite high if the integral value and MAC of wood were determined precisely or a condition of examination was chosen properly. It was seemed that the estimation of air-dry density by using polychromatic X-ray system can supplant the gravimetric method.

바이올린 브릿지의 음향적 특성 및 SDM 시뮬레이션에 관한 연구 (Studies on the Acoustical Characteristics of Violin Bridges and SDM Simulation)

  • 정우양
    • 한국가구학회지
    • /
    • 제12권1호
    • /
    • pp.47-55
    • /
    • 2001
  • Violin bridge blank cut from maple wood with good quality has typical pattern of the radial direction in the side edge with minimal dispersion. This experimental study was designed and carried out to examine the effect of the physical and macroscopical characteristics on the compressive creep of violin bridge blank which had been imported from European manufacturer. This research arose from the idea that the maple solid wood with heterogeneous wood density and ray direction in the side edge would have uneven rheological property of violin bridge blank which is supposed to be pressed by the tension of strings. Experimentally, the compressive creep of bridge blank became smaller with the higher density of imported maple wood and showed clear density-dependence for the duration of load under the string tension of 5 kgf. Every bridge blank showed the behavior of primary creep stage(stress stabilization) having logarithmic regression creep curve with high correlation coefficient under the designed stress level. Even though the relationship between compressive creep and ray direction on the side edge of bridge was not so clear contrary to expectation, we could conclude that wood density and ray direction should be the quality decisive factors affecting the acoustical characteristics and performance of the bridge, the core member of violin-family bow instruments.

  • PDF

Effect of Heat Treatment on the Bending Strength and Hardness of Wood

  • Won, Kyung-Rok;Kim, Tae-Hong;Hwang, Kyo-Kil;Chong, Song-Ho;Hong, Nam-Euy;Byeon, Hee-Seop
    • Journal of the Korean Wood Science and Technology
    • /
    • 제40권5호
    • /
    • pp.303-310
    • /
    • 2012
  • Heat treatment improves dimensional stability and sound absorption properties of wood. However, mechanical properties of wood can be deteriorated during the heat treatment. The effect of heat treatment on the bending strength and hardness of wood for Korean paulownia, Pinus densiflora, Lidiodendron tulipifera and Betula costata were measured. The heat treatment temperature has been investigated at $175^{\circ}C$ and $200^{\circ}C$, respectively. The results showed that the weight and density of wood decreased after heat treatment. It was found that the density by heat treatment was lower at $200^{\circ}C$ than that at $175^{\circ}C$. And, MOE increased with the reduced density. On the contrary, MOR and hardness decreased. In all conditions, It was found that there was a high correlation of 1% level between bending modulus of elasticity and modulus of rupture.

Microscopic Interpretation on Thickness Swelling Mechanism of Nonwoven Web Composites from Wood Particles and Polypropylene Fibers

  • Chae, Shoo-Geun;Eom, Young-Geun
    • 한국가구학회지
    • /
    • 제17권2호
    • /
    • pp.9-23
    • /
    • 2006
  • Control particleboards were significantly higher in thickness swelling than wood particle-polypropylene fiber composites and their thickness swelling increased with the increase of target density. In the composites, thickness swelling did not vary significantly with the increase of target density but increased with the increase of wood particle content. And the composites with fine wood particles were significantly lower in thickness swelling than those with coarse wood particles irrespective of target density and formulation. In the scanning electron microscopy, significantly higher thickness swelling in the composites with coarse wood particles was thought to be the result of more interfacial separations by higher swelling stresses.

  • PDF

Study on the Estimation of Proper Compression Ratios for Korean Domestic Wood Species by Single Pellet Press

  • LEE, Hyoung-Woo;KIM, Soon-Bae
    • Journal of the Korean Wood Science and Technology
    • /
    • 제48권4호
    • /
    • pp.450-457
    • /
    • 2020
  • Single pellet press technology allows for fast, low-cost, and small-scale tests to investigate pelletizing characteristics. We estimated proper compression ratios for five Korean domestic wood species through predicted relationships between pelletizing pressure Px and compression ratio based on experimental data obtained from a single pellet press unit. The pressures required to obtain a 6-mm-diam pellet of density 1200 kg/㎥ were estimated as 111 MPa for Populus davidiana, 133 MPa for Robinia pseudoacacia, 136 MPa for Quercus mongolica, 97 MPa for Pinus densiflora, and 127 MPa for Pinus rigida. On the basis of these pressures, we estimated proper compression ratios to be within the range 7.676-8.410 for these species, and we found the compression ratios needed for hardwood species to be somewhat higher than those needed for softwood species to obtain the pellet density of 1200 kg/㎥.

대나무 탄소계정을 위한 목재기본밀도 개발 (Development of a Basic Wood Density for Carbon Accounting in Bamboo Forests)

  • 배은지;정재엽;이선정;노혜정;손영모
    • 한국산림과학회지
    • /
    • 제112권2호
    • /
    • pp.188-194
    • /
    • 2023
  • 본 연구는 우리나라의 대나무림에 대한 탄소계정을 위하여 탄소배출계수 중 하나인 목재기본밀도를 도출하기 위하여 수행되어 졌다. 대나무는 전라남도와 경상남도에 주로 분포해 있으며, 계수 도출을 위한 표준목은 솜대, 왕대, 맹종죽 등 3수종별로 각각 101본씩을 선정하여 활용하였다. 목재기본밀도 도출은 KS F 2098 방법을 따랐다. 측정결과, 솜대의 목재기본밀도는 0.83 g/cm3, 왕대는 0.81 g/cm3, 맹종죽은 0.72 g/cm3로 각각 나타났다. 그렇지만, 우리나라는 대나무 분포 면적이 많지 않고, 맹종죽의 경우 일정 지역에 국한되어 생육하고 있다. 따라서 대나무에 적용할 수 있는 목재기본밀도는 하나로 통합하여 0.79 g/cm3로 확정하였다. 그리고 도출된 목재기본밀도에 대한 불확도를 평가한 결과, 1.61%로 낮은 불확도 값을 가져, 본 분석에서의 측정값에 대한 신뢰도를 확인할 수 있었다. 본 연구에서는 이번에 개발한 목재기본밀도와 기존의 바이오매스확장계수, 뿌리함량비 등을 이용하여 대나무 표준목에 대한 탄소저장량을 계산하고, 이를 확장시켜 ha단위까지 계산해 보았다. 이번 연구로 대나무의 재적을 이용하여 목재기본밀도 등 탄소배출계수 적용으로 탄소저장 및 흡수량 계산이 가능하게 되었다. 본 결과가 우리나라 탄소중립 정책 및 산림관리 방향에 도움이 되기를 기대한다.

Density Profile and Sound Absorption Capability of Ceramics Manufactured from Sawdust, Chaff and Charcoal: Effect of Carbonization Temperature and Mixing Ratio

  • Jung-Woo HWANG;Seung-Won OH
    • Journal of the Korean Wood Science and Technology
    • /
    • 제52권3호
    • /
    • pp.234-242
    • /
    • 2024
  • In this study, the effect of carbonization temperature and mixing ratio of ceramics manufactured from sawdust, chaff and charcoal on sound absorption performance and density profile was investigated. The density profile of ceramics prepared by the addition rates of sawdust, chaff and charcoal showed the highest value at 91.00% when the ratio of sawdust, chaff and charcoal was 50:25:15. However, the difference in density profile according to the addition rate was insignificant. The density profile of ceramics manufactured according to the carbonization temperature showed the highest value of 88.06% when manufactured at 800℃. However, it does not show any particular trend, so it is understood that the effect of the carbonization temperature on the density gradient is small. On the other hand, the sound absorption coefficients of ceramics prepared by the addition rates of sawdust, chaff and charcoal is between 0.3 and 0.4 at almost all frequencies when the addition rates of sawdust, chaff and charcoal are 50:30:10 and 50:35:5, respectively. Therefore, as the chaff particles increased, the sound absorption performance was improved. In addition, the sound absorption coefficients of the ceramics manufactured at each carbonization temperature showed the highest value in the ceramics manufactured at 1,200℃.