Studies on the Technical Development of Traditional Korean Golden Varnish (Hwangchil)(II) - Chemical Composition and Coatings-oil Characteristics of the Exudates and Bark-extractives of Hwangchil-namu(Dendrogapax morbifera Lev.) - (전통 황칠 도료 개발에 관한 연구 (II) - 황칠나무 수피 추출물 및 삼출액의 화학적 조성과 도료용 오일특성 -)

  • Lim, Kie-Pye;Jung, Woo-Yang
    • Journal of the Korean Wood Science and Technology
    • /
    • v.26 no.1
    • /
    • pp.7-13
    • /
    • 1998
  • In order to reconstruct the traditional technology of Korean golden varnish(Hwangchil) made from the exudates of D. morbifera, this study in the second step was carried out to analyze the chemical composition and oil properties of the exudates for coatings and bark extractives made from the trees of D. morbifera more than 20 years old grown in Wando and Jejudo islands in the southwestern part of Korean peninsula according to the physiological seasons. The results obtained are as follows: 1. The exudates appeared to be a phytoalexin because it exudated after several days in tapping only in summer season. 2. Both the exudates and bark-extracts with acetone contained 50~60% unsaponifiables and 30~50% saponifiables 3. A major component of essential oil in bark-extractives was ${\beta}$-cubebene and reached to 60~80%, while that of exudates included only 34% ${\beta}$-cubebene and some other compounds such as ${\beta}$-cadinene of 12%, aromadendrene of 9%, ${\beta}$-selinene of 9%, CAS030021-74-0 of 10%, etc. in GC-MS spectrometer. 4. A mjor component of fatty oil fraction in bark-extractives was linoleic acid and reached to more than 60%, while the exudates had mostly other components such as terpenes and phenolics instead of fatty acids accordint to GC-MS spectrometer. 5. Iodine value of samples after oil refining had 214mg/g in the exudates and more than than 150mg/g in bark-extractives, so the latter belonged to a drying oil.. 6. Therefore, the exudates from D. morbifera for traditional Korean golden varnish seems to have beeen used to a good varnish because it has some specific compounds different from its bark-extractives or general varnishes.

  • PDF

The preventive effect of fluoride materials on the dental caries by dental polishing prior to fluoride application (불화물 도포 전 치면연마 시행여부에 따른 우식예방효과)

  • Cho, Min-Jung;Ha, Myung-Ok;Oh, Han-Na
    • Journal of Korean society of Dental Hygiene
    • /
    • v.12 no.1
    • /
    • pp.113-122
    • /
    • 2012
  • Objectives : This study was carried out to investigate the caries resistant effect of fluoride by dental polishing prior to fluoride application in vitro. Methods : Artificial caries lesion was made on the surface of specimen enamel taken from cow's permanent cuspid on the part of labial surface after resin embedding and polishing. Artificial dental plaque was formed on the 72 dental specimen 25~45 VHN(Vickers Hardness Number) which were divided into three groups(fluoride varnish, APF gel, control) with dental polishing and without polishing respectively. Fluoride varnish and APF gel group with 20 second polishing or without polishing were immersed in the artificial saliva respectively. Control group with or without polishing were immersed in the artificial saliva. Results : 1. Significant difference was not found by fluoride varnish between polishing group and non polishing group (p>0.01). 1) polishing group. The changes of Vickers Hardness Number(VHN) were $14.49{\pm}13.73$. 2) non-polishing group. The changes of VHN were $11.67{\pm}5.39$. 2. Significant difference was not found by APF gel between polishing group and non polishing group (p>0.01). 1) polishing group. The changes of VHN were $8.48{\pm}8.37$. 2) non-polishing group. The changes of VHN were $5.32{\pm}2.59$. Conclusions : Showed no significant difference between polishing group and non-polishing group regardless of fluoride materials (fluoride varnish, APF gel).

Heat-resistant Enamel Varinish (내열성 에나멜 바니쉬)

  • Kim, Yang-Kook;Bae, Hun-Jai
    • Applied Chemistry for Engineering
    • /
    • v.4 no.2
    • /
    • pp.264-272
    • /
    • 1993
  • Current research aimed at investigating of heat-resistance of magnet wire to endow miniaturizing electronic equipment with a high efficiency or reliability. Thermal stability of magnet wire has a close relationship with physical properties of polymeric coating that is formed from enamel varnish. Design of heat-resistant enamel varnish and coating technology of varnish solution were briefly described. Some factors which have a thermal effect on wire were discussed through the evaluation method of the wire properties.

  • PDF

Application of optimized time domain reflectometry probe for estimating contaminants in saline soil

  • Dongsoo Lee;Jong-Sub Lee;Yong-Hoon Byun;Sang Yeob Kim
    • Geomechanics and Engineering
    • /
    • v.33 no.3
    • /
    • pp.291-299
    • /
    • 2023
  • Monitoring contaminants in waste landfills on a seabed is important because the leachate affects the marine ecosystem and facility stability. The objective of this study is to optimize a time-domain reflectometry (TDR) probe using different coating materials and several electrodes to estimate contaminants in saline soil. Copper concentrations ranging from 0 mg/L to 10 mg/L were mixed in 3% salinity water to simulate contaminants in the ocean environment. Epoxy, top-coat, and varnish were used as coating materials, and two to seven electrodes were prepared to vary the number and arrangement of the electrodes. Test results showed that the varnish stably captured the increase in copper concentration, while the other coating materials became insensitive or caused leakage current. In addition, a TDR probe with more electrodes exhibited stable and distinct electromagnetic signals. Thus, the TDR probe with seven electrodes coated with varnish was effectively used to estimate contaminants in saline soil.

Development of Surface Improvement Technique of Japanese Larch Flooring Board(II) (낙엽송 마루판재의 표면강화 처리기술 개발(II))

  • Park, Sang-Bum
    • Journal of the Korean Wood Science and Technology
    • /
    • v.28 no.1
    • /
    • pp.28-35
    • /
    • 2000
  • This paper deals with a coating technique for hardening surface layer of softwood(Larix leptolepis) flooring board to improve its surface properties such as hardness and abrasion resistance, Two coating methods were applied for surface hardening of the wood in this study. First, several functional monomers were added in UV-curing epoxy acrylate varnish. Secondly, unsaturated polyester varnish was used as under coat and acryl varnish including anti-abrasive agent was used as top coat. The hardness of the treated wood was similar to that of high density hardwood such as keruing by the first coating method. The abrasion resistance of the coated wood was greatly improved by the second method. Adhesion properties and impact resistance of the coated wood surface were also good. It was suggested that the well-coated softwood could be used as interior flooring board for heavy walking as substitute for hardwood.

  • PDF

Durability and Properties of Coating Film on Lumbers Coated with Hwangchil (황칠처리재의 도막 물성 및 내구성)

  • 조종수;김종인
    • Journal of the Korea Furniture Society
    • /
    • v.12 no.1
    • /
    • pp.11-20
    • /
    • 2001
  • To investigate weathering and surface characteristics of coating film on lumbers coated with Hwangchil(varnish of Dendropanax morbifera), we carried out to investigate the resistance against discoloration, value of crack and surface characteristics of coating films on seven domestic lumbers and those of four introduced tropical lumbers. There was investigated to evaluate the properties of coating films by the varnish of Dendropanax morbifera. There was insignificant correlations between the hardness and moisture contents of each lumber treated by the varnish. There was no significant correlations between the thickness of coating film and the hardness, either. Although we investigated 11 wood species, we found only three species as resistance wood species against discoloration; Diospysos spp., Abies holophylla and Ulmus davidiana. The crack of coaing films was the largest on Zelkova serrata followed by Juglans sinensis, Cercidiphum japonicum, Tectona grands, Ulmus davidiana, Guibourtia tessmannii, Diospysos spp. and Dalbergia latifolia. However, there was no crack of coating films on the lumbers of Juniperus rigida, Prunus serrulata var. spontanea and Abies holophylla. The crack of coating film showed positive correlations with the thickness of coating film and hardness. The surface characteristics of the coating films evaluated on the basis of $R_{a}$ values indicated the lumbers of Ulmus davidiana($0.14{\;}{\mu}m$), Juniperus rigida($0.1 5{\;}{\mu}m$), Guibourtia tessmannii($0.19{\;}{\mu}m$), Dalvergia latifolia($0.20{\;}{\mu}m$) and Diospysos spp.($0.20{\;}{\mu}m$), Cercidiphum japonicum($0.24{\;}{\mu}m$) as good species while there was insignificant differences between softwoods and hardwoods. Tectona grands, Prunus serrulata var. spontanea and Abies holophylla showed rough surface with $1.53~2.63{\;}{\mu}m$ of $R_a$ values. The four kinds of rough indices($R_a,{\;}R_z,{\;}R_{max}{\;}and{\;}R_q$) showed very low correlations with moisture contents with the correlation coefficients. The $R_a{\;}and{\;}R_{max}$ also showed slight relationship with hardness.

  • PDF

AN EXPERIMENTAL STUDY ON THE CHANGES OF FLEXURAL STRENGTH OF GLASS IONOMER CEMENT FOLLOWING SURFACE TREATMENT (시간경과 및 표면처리에 따른 Glass ionomer cement의 flexual strength의 변화에 관한 실험적 연구)

  • Kim, Byung-Wooh;Min, Byung-Soon
    • Restorative Dentistry and Endodontics
    • /
    • v.15 no.1
    • /
    • pp.120-128
    • /
    • 1990
  • The purpose of this study was to examine the effect of surface treatment on the flexural strength of glass ionomer cement with time elapsed. Glass ionomer cement (Fuji ionomer type II, (GC Co.) was used as experimental materials. Glass ionomer cement was placed in a beam-shaped teflon mold (3mm ${\times}$ 3mm ${\times}$ 25mm) that was rest on a glass plate. Another flat glass was placed on the top of the mold with pressure. After the cement was set, the specimens were divided into three groups and thirty two specimens in each group were surface-treated as follows: No treatment group: Specimens were no surface-treated and stored at $35.6^{\circ}C$ in distilled water. Fuji varnish application (FA) group: Specimens were surface-treated with Fuji varnish (GC Co.) and stored at $35.6^{\circ}C$ in distilled water. Vaseline storage (VS) group: Specimens were no surface-treated and stored at $35.6^{\circ}C$ in vaseline. The flexural strength was measured after I day, 1 week, 2 weeks, 4 weeks from the start of mixing using Instron Universal Testing Instruments. Results were as follows: 1. After 4 weeks, vaseline storage group exhibited the maximum flexural strength (p <0.0005). 2. The flexural strengths in no treatment group were slightly increased with time elapsed, but its difference was not significant, statistically. 3. The flexural strengths in Fuji varnish application group were increased with time elapsed (p <0.05). 4. The flexural strengths in Fuji varnish application group and vaseline storage group were greater than that in no treatment group (p <0.0005).

  • PDF

Development of fluoride varnish with sustained fluoride release and biocompatibility (불소 지속방출 및 생체적합성을 가진 불소 바니쉬의 개발)

  • Shin, Kyung-Su;Kim, Ah-Jin;Oh, Seunghan;Bae, Ji-Myung
    • Korean Journal of Dental Materials
    • /
    • v.44 no.1
    • /
    • pp.21-31
    • /
    • 2017
  • The purpose of this study was to fabricate a biocompatible fluoride varnish with sustained fluoride release, and to compare it with commercial fluoride varnishes. For the experimental fluoride varnish, bis-GMA (BG) or two types of rosin (KR-610: K0, KR-612: K2) were used as bases. Either ethyl acetate or ethanol was added as solvent and 5 wt% NaF was used. 5 mg of experimental F- varnishes and 2 commercial products, Cavity shield (CS) and Flor-opal (FO), were applied on a labial surface of bovine teeth ($10mm{\times}7mm$). The amount of fluoride release was measured at 1 hr, 2 hrs, 3 hrs, 4 hrs, 8 hrs, 12 hrs, 1 day, 3 days, 5 days, 10 days, 15 days, 20 days and 30 days. MTT test was done with diluted F- varnishes using ethanol. Statistical analysis was done with one-way ANOVA and Duncan multiple range test (${\alpha}=0.05$). BG showed the highest fluoride release at 1 hr (P<0.05), while that of K0 was highest at 2 hrs (P<0.05). From 1 day to 5 days, experimental fluoride varnishes showed higher fluoride release than the commercial products (P<0.05), and there were no significant differences after 5 days (P>0.05). For MTT test, K0 and FO showed higher cell viability than other experimental groups (P<0.05), with no significant differences with K2 (P>0.05). Considering the sustained fluoride release and cell viability of the experimental rosin-based fluoride varnishes compared with commercial products, it will be appropriate for clinical application.

THE EFFECT OF FLUORIDE VARNISH AND ACIDULATED PHOSPHATE FLUORIDE GEL ON ARTIFICIAL CARIES LESION (Fluoride varnish와 acidulated phosphate fluoride gel이 인공우식 병소에 미치는 영향)

  • Kim, Kwang-Hyon;Hahn, Se-Hyun;Kim, Chong-Chul
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.28 no.1
    • /
    • pp.159-165
    • /
    • 2001
  • Fluoride has been used widely for the prevention of dental caries. Many dental professionals applicated acidulated phosphate fluoride(APF) gel for the purpose of prevention of dental caries in recent years. However, the topical application of fluoride varnish is growing and getting much recognition in many parts of Europe and Scandinavia. The main purpose of this study was to compare the effect of fluoride varnish and acidulated phosphate fluoride gel on artificial caries lesion. The artificial caries lesion was caused on the sound bovine enamel and divided 60 specimens into three groups each containing twenty for the purpose of study. No application was done on group 1, which acted as control group. Group 2 was treated with the topical application of fluoride varnish and removed after 1 hour Group 3 was treated with APF gel and removed after a minute. The cycle of remineralization/demineralization went on in vitro and the microhardness was measured for the each group after 5 and 15days. The following results were obtained : 1. According to the results after 5 days, the microhardness of groups 2 and 3 were significantly higher than group 1, the control group(p<0.05) Similar results was also noticed after 15 days(p<0.05) 2. In comparison of microhardness between groups 2 and 3 after 5days, there were no significant differences between them. The results after 15 days was also similar 3. Much difference in microhardness wasn't present in groups 2 and 3 after 5 and 15days. However, the microhardness of the group 1 dropped significantly in the result of 15 days and 5 days(p<0.05).

  • PDF

Elemental analysis of the fluoride varnish effects on root caries initiation (불소 바니쉬 도포 후 초기 치근 우식 발현에 대한 정량원소분석)

  • Park, Se-Eun;Yi, Kee-Wook;Kim, Hae-Young;Son, Ho-Hyun;Chang, Ju-Hea
    • Restorative Dentistry and Endodontics
    • /
    • v.36 no.4
    • /
    • pp.290-299
    • /
    • 2011
  • Objectives: The usage of fluoride varnish for a moderate to low caries-risk group has not been well validated. This study aimed to evaluate the preventive and therapeutic efficacies of fluoride varnish on the initiated root caries. Materials and Methods: Ten premolars were sectioned into quarters, further divided into two windows, one of which was painted with Fluor Protector (1,000 ppm fluoride, Ivoclar Vivadent). An initial lesion with a well-preserved surface layer was produced by pH cycling. Scanned line analysis using energy dispersive spectrometry determined the weight percentages of Ca and P in the demineralized layer. Scanning Electron microscopy and confocal laser scanning microscopy (CLSM) evaluated the varnish-applied root surfaces. Results: The mean lesion depth (SD) was 12.3 (2.6) ${\mu}m$ (single cycling) and 19.6 (3.8) ${\mu}m$ (double cycling). Double cycling extended the lesion depth, but induced no more mineral loss than single cycling (p < 0.05). The mean weight percentages of Ca and P between groups with and without varnish were not significantly different (p < 0.05). A CLSM showed varnish remained within 15 ${\mu}m$ of the surface layer. Conclusions: When a mild acid challenge initiated root tissue demineralization, the application of low-concentration fluoride varnish did not influence the lesion depth or the mineral composition of the subsurface lesion.