A Study on the Silk Degumming(1) - Degumming of Silk on Package - (견의 정련 방법에 관한 연구(1) - 패키지 정련 -)

  • Kim Moon-Sik;Kim Yong-Hak
    • Textile Coloration and Finishing
    • /
    • v.18 no.3 s.88
    • /
    • pp.16-22
    • /
    • 2006
  • Process contract has received considerable attention in silk degumming processes because of its critical role in quality assurance. In degumming, process exhibits shrinkage of high twisted yarn and lot-varying behavior, thus increasing the difficulties of reduction by conventional means. This necessitates the application of a package that adapts to changing degumming process, and a new approach involving package degumming is proposed. The gains of this process are prevent of shrinkage by package winding, which is simplified by reduced soft-winding or re-twisting process. The approach is expected to achieve high quality results in conventional process due to its feature of demage by tension and rubbing. Therefore package degumming has many merits such as reduce of pilling and shrinkage, production expenses saving by process contract are expected of the simplified degumming process.

The Study on Mechanical Properties and Handle of the Micro-Fiber Fabrics(I) (신합섬직물의 역학적특성과 태에 관한 연구(I))

  • 박명수;최영미
    • Textile Coloration and Finishing
    • /
    • v.11 no.2
    • /
    • pp.9-18
    • /
    • 1999
  • In order to establish fundamental data for the betterment of Polyester microfiber fabric handle, a study by using fixed warp of ITY yarn samples with P/F, DTY, and ITY weft yarns was performed. For this purpose the samples of total 27 kinds were prepared. That is, each sample yarn was twisted in three ways and for each twisted yarn the fabric structures were modified in three ways, plain, twill, and satin. The examination was done by focusing on the point of the change of handles and the characteristics of the mechanical properties of the samples with the change of yarn and the fabric structure. The handles and the mechanical properties were examined with the KES-F system suggested by Kawabata. The results were as follows : 1. WT and MIU increased with increasing the twist. By comparing WT and MIU by yarn, DTY was higher than P/F. It appeared that twill and satin were higher than plain. 2. The bending rigidity change in DTY with increasing the twist was not significant, however in P/F it appeared apparently decreased with increasing the tlvist. Also, it appeared that when using P/F as weft the bending rigidity was higher than when using DTY and the twill structure appeared higher than the satin structure. 3. In shear force the increasing rates of plain and the twill were higher than satin. When DTY and P/F were used as weft, the shear force was higher in ITY and DTY than in P/F case. 4. Koshi appeared higher in the order of plain, twill and satin. When DTY and P/F were used as the weft Koshi increased with increasing the twist in plain, however in twill and satin it appeared to decrease. In hand value ITY(=7.5) appea.ed to be highe. than DTY and P/F(=6.5). 5. In all cases Shinayakasa decreased with increasing the twist. The hand values observed that satin was =4, twill was =3, and plain was =1.5. 6. Fukurami showed no significant change with increasing the twist in DTY, however in P/F and ITY it decreased.

  • PDF

Dyeing Properties of Acetate/Functional Polyester Composite Yarn in Different Yarn Twisting Processes (연사방법에 따른 아세테이트/기능성 폴리에스터 복합사의 염색성에 관한 연구)

  • Kim, So-Jin;Jeon, Dong-Won;Park, Young-Hwan
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.30 no.2 s.150
    • /
    • pp.255-265
    • /
    • 2006
  • The purpose of this study was to examine the dyeing properties of four kinds of composite yams that were twisted in different processes. The composite yarns consist of acetate and functional polyester in ratio of 70 : 30. The composite yams were dyed at 100$^{circ}C$ and 125$^{circ}C$ using three types of dyes, disperse dyes for acetate fiber, PET fiber and PET-acetate blended fiber, in the three primary colors. The exhaustion($\%$) and K/S value were observed for each case. Also the effects of four different twisting processes to dyeing properties and physical properties were examined. Regardless of twisting methods, the composite yarns that were dyed at 125$^{circ}C$ had higher exhaustion($\%$) than those were dyed at 100$^{circ}C$ with all three types of dyes; However, tendency of the K/S value after reduction cleaning process was measured at 100$^{circ}C$ and the value measured 125$^{circ}C$ had a great difference with disperse dyes for acetate and dyes for PET. The difference of the K/S values of composite yarns, when dyed at 100$^{circ}C$ and 125$^{circ}C$ with disperse dyes for PET-acetate blended fiber, was almost negligible. According to twisting methods K/S values were in the following order: AP1 > AP3 > AP4> AP2. This means that AP1, treated at 220$^{circ}C$, had the highest K/S value and K/S value becomes higher as the yam is higher twisted and becomes lower as lower twisted. On the other hand, the dry shrinkage and wet shrinkage showed low shrinkage rate when the twist was high and steam setting temperature was high.

The Physical Properties of Filling Batt Using Polyester Yarn (Polyester사를 이용한 충전용 솜사의 물성)

  • Park, Myung-Soo
    • Fashion & Textile Research Journal
    • /
    • v.9 no.3
    • /
    • pp.347-350
    • /
    • 2007
  • To analyse basic properties for making packing batt according to doubling condition, packing batt yarn, of $300^D$, $900^D$, $3600^D$ made from DTY yarn $150^D$/48 were produced from KTDI. The results are as follows: The birefringence of the sample yarn increased with increasing the annealing temperature and denier. The initial modulus of the sample yarn decreased with increasing the annealing temperature and denier. The higher than annealing temperature of $160^{\circ}C$, initial modulus of the sample are equilibrated. The strain recovery ratio of samples decreased with increasing the annealing temperature and denier. The lower than annealing temperature of $140^{\circ}C$, strain recovery ratio of the sample are decreased Where the $900^D$, $3600^D$ yarns are at $100^{\circ}C$ the specific bending rigidity value obtained is 0.65kgf/d but the twisted yarn (3,600) obtained 0.006 ($gfcm^2/tex^2$). However, where the heat temperature is $160^{\circ}C$, specific bending rigidity value obtained 0.003($gfcm^2/tex^2$).

Durability Enhancement of Textile Materials for Thermotherapy Massager (온열안마기용 섬유재료의 내구성 향상)

  • Lee, Joo-Young;Kim, Ho-Dong
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.11 no.6
    • /
    • pp.2292-2299
    • /
    • 2010
  • The wear and abrasion mechanism of conventional PET/Cotton fabric which is used as a lining layer for thermotherapy massager was elaborately investigated in order to increase the life-span of the fabrics for Thermotherapy Massager. Based on the destruction mechanism, the feasible PET fabrics were prepared and its anti-wearing performance was evaluated. It is revealed that the wearing destruction is mainly caused by the repeat abrasion on a specific part of folded fabric as well as abrasion itself. Therefore, it is necessary that the prevention of fabric folding while massager is running is essential and the recovery from the crease on a fabric is also necessary to solve this problem. Covered elastic yarn, high twisted yarn, change of fabric structure or different fiber were utilized to prepare the possible alternatives. As a result, the anti-wearing performance of the fabrics are greatly improved to have about 2 times and 1.5 times longer life-span for the fabric with covered elastic yarn and high twisted yarn, respectively.

Effect of treatment temperature on mechanical properties of silk textiles made with silk/polyurethane core-spun yarn

  • Bae, Yeon Su;Um, In Chul
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.33 no.2
    • /
    • pp.108-112
    • /
    • 2016
  • Silk has been used extensively in textile applications because of its good luster and feel. However, the low elongation and elastic recovery of silk has limited its use in a wider variety of textile applications. In this study, silk textile samples were made with a highly twisted silk/polyurethane core-spun yarn. They were immersed in water and dried at different temperatures, and the effect of treatment temperature on the mechanical properties of the silk textile was examined. It was found that the water temperature strongly affected the morphology and mechanical properties of the silk textile, whereas the drying temperature did not. As the water temperature was increased, the weft silk yarn became tangled and the interval between warp yarns decreased, resulting in shrinkage of the silk textile. When the silk textile was immersed in water at high temperature (i.e., $100^{\circ}C$), the elongation of the textile increased eight-fold as compared to an untreated silk textile. The maximum elastic recovery ratio of the silk textile was 96.7%.

Physical and Hand Properties of the Knitted Fabrics From Machine Knitting Fancy Yarns (기계편용 장식사 니트소재의 물성 및 감성 평가)

  • Park, Key-Yoon;Park, Myung-Ja
    • Journal of the Korea Fashion and Costume Design Association
    • /
    • v.10 no.2
    • /
    • pp.125-138
    • /
    • 2008
  • For physical and hand property evaluation of fabrics, the knitted fabrics from 11 types of machines knitting fancy yarns, boucle (M1), knot (M2), snarl (M3), and slub (M4), tamtam (M5), tubular (M6), fur 1 (M7), bead (M8), fur 2 (M9), fur 3 (M10), and ladder (M11) yarns, were prepared with 7-10 G plain stitch. Washing test and pilling test had also been carried out. For hand properties by objective sensibility evaluation, 17 items of sir mechanical properties using KES-FB (Kawabata Evaluation System) had been measured. Then hand values of knitted fabrics were calculated with a calculation formula, namely KN-402-KT. Finally the total hand values were obtained through KN-301-WINTER. As a result of physical properties and objective evaluation for machines knitting fancy fabrics, most of them shrank in the direction of wale and course after the washing test, in which their shrinkage rate had a maximum of 3.5%. Therefore, the washing test indicated that the shrinkage ratio of knitted fabrics had a minor change. The results of the pilling test are mostly 4-5th grade, and all of the machines knitting fancy fabrics showed good results in the pilling resistance. In hand properties and objective sensibility evaluation, twisted fancy yarns, such as boucle (M1), knot (M2), snarl (M3), and slub (M4), were superior to bonding rigidity (B) and shear rigidity (G). The surface property between course and wale differs in all samples and course direction is tougher than wale direction. FUKURAMI (fullness and softness) of all samples have high values, besides NUMERI (smoothness) of tamtam (M5) and boucle (M1), which were rather good. Most samples except fur 1 (M7) had low KOSHI (stiffness) value. The total hand value (THV) of twisted yarns was low. This study proves that manufacturers, who plan knitting yarn products and knit fashion, can apply these data to develop machines knitting yarns and knits that fit the consumers' demands.

  • PDF

A Study on Dynamic Characteristics Analysis of Spindle Unit for Two-for-One Twister (투포원 연사기용 스핀들 유니트의 동특성 해석에 관한 연구)

  • Kim, Gwang-Yeong;Kim, Jong-Su
    • 연구논문집
    • /
    • s.27
    • /
    • pp.127-139
    • /
    • 1997
  • Two-for-one twister is a kind of textile machine and makes special fancy yarn which is twisted two times per one revolution in order to increase tensile strength and wear resis-tance of yarn. Spindle mechanism has to be stable and continuous motion in high speed revolution, and then optimal design is necessary to analyze dynamic characteristics of spindle unit. Spindle unit is consist of blade and rotary disc that are cylindrical body of revolution. For analysis of the dynamic characteristics of spindle unit, transfer matrix method is used and a numerical code SPINDLE also. Torsion and natural bending frequency of the spindle unit are examined. Its displacement mode is studied in function of variable revolutions.

  • PDF