Structural properties of Pd-barium zirconate dense membrane synthesized by dual sputtering method (동시 증착 스퍼터링 공정에 의해 증착된 Pd-barium zirconate membrane의 구조분석)

  • Byeon, Myeong-Seop;Kang, Eun-Tae;Cho, Woo-Seok;Kim, Jin-Ho;Hwang, Kwang-Taek
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.22 no.1
    • /
    • pp.19-24
    • /
    • 2012
  • Barium zirconate exhibits good thermo-chemical stability and proton conduction at high temperatures, but shows poor electron conductivity. Therefore, for high efficiency of hydrogen separation, a very thin and dense Pd-Barium zirconate membrane has to be coated on a porous substrate. A thin and dense Pd-Barium zirconate membrane was successfully synthesized on a porous substrate by means of dual sputtering method. The structural and chemical features of the $BaZr_{0.85}Y_{0.15}O_{3-{\delta}}$ membranes sputtered at $300^{\circ}C$ and $400^{\circ}C$ were investigated by X-ray diffractometry, and it was found that a well-crystallized membrane, Pm-3m space group of $BaZrO_3$, was synthesized. The surface and cross-sectional morphologies of membrane were assessed by SEM (scanning electron microscopy) and TEM(transmission electron microscopy) of the surface and of cross sections. The cross sectional observation of Pd-$BaZr_{0.85}Y_{0.15}O_{3-{\delta}}$ membrane by dual sputtering shows that the coating is quite dense with columnar structure.

A Thermal Study of the Harmful Chemical Species of Charcoal and Their Transformation during Combustion (숯의 유해물질과 이들의 연소 중 상변화에 대한 열분석 연구)

  • Yoon, Hye-On;Kim, Ki-Hyun
    • Journal of the Mineralogical Society of Korea
    • /
    • v.24 no.2
    • /
    • pp.101-110
    • /
    • 2011
  • Charcoal burning in the process of manufacture and ordinary use often release many constituent chemical species. As a result of open burning, the chemical composition as well as the physical properties of original material changes through the modification of surface properties of charcoal. Surface modification could be more responsible toward the outside elements for surface adsorption, it becomes easy to adsorb more toxic elements through surface adsorption. In this study, four kinds of commercially available charcoal were studied against the chemical and thermal stability along with the heavy metals and organic hazardous substances. Thermo gravimetric analysis (TGA) and differential scanning calorimetry, from room temperature to $400^{\circ}C$, were performed to study the weight loss and the changes in the behavior of those substances. According to TGA analysis, about 10% of weight loss was happened before $200^{\circ}C$. It was found that related weight loss of this temperature region may responsible to the gas phase organic matter. Natural charcoal, K1 and C1 show 15% of loss during the reaction heated to $400^{\circ}C$, while the artificial charcoal K2, C2 show the weight loss of about 20% was found. This is consistent with the main organic matter and VOC analysis results shown. Chemical composition based on the x-ray diffraction analysis was carried out. X-ray diffraction analysis reveals the existence of chemical additive in the forms of $Ba(NO_3)_2$, $BaCO_3$, and $NaNO_3$.

Comparision of Ca- and Na- Based Dry Sorbent in Desulfurization Characteristics (Ca계 및 Na계 흡수제의 건식 탈황 특성 비교)

  • Moon, Seung-Hyun;Hyun, Ju-Soo
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.31 no.1
    • /
    • pp.21-28
    • /
    • 2009
  • Physico-chemical characteristics of the Ca-based and Na-based dry sorbents were compared using thermo-gravimetric analysis (TGA) and temperature programmed desorption (TPD) methods. The studied characteristics were thermal stability, sulfur dioxide ($SO_2$) absorption capacity and absorption rate at $250^{\circ}C$ which is a typical temperature before a fabric filter, and $SO_2$ absorption capacity at an ambient temperature. Calcium hydroxide ($Ca(OH)_2$) started to decompose into calcium oxide (CaO) at $390^{\circ}C$ and completed at 480~$500^{\circ}C$, showing 76% of an original $Ca(OH)_2$ weight. Sodium bicarbonate ($NaHCO_3$) also converted to sodium carbonate ($Na_2CO_3$) between $95^{\circ}C$ and $190^{\circ}C$, decreasing the weight to 63% of its initial weight. Among four sorbents tested at $250^{\circ}C$, sodium carbonate had the highest capacity, absorbing 0.35 g $SO_2$/g sorbent. Calcium oxide and calcium hydroxide followed that showing 0.156 g and 0.065 g $SO_2$ absorption per absorbent respectively. Ca-based absorbents showed slower rate than sodium carbonate because of initial stagnant step. However, calcium hydroxide caught more $SO_2$ than sodium carbonate at ambient temperature. From this work, it can be concluded that Ca-based absorbent is a proper sorbent for $SO_2$ treatment at low temperature and sodium carbonate, at high temperature.

Thermal Stability of Israeli Carp Actomyosin and Its Protection by Chemical Additives (이스라엘 잉어 Actomyosin의 열안정성과 그 보호)

  • NAM Taek-Jeong;CHOI Yeung-Joon;PYEUN Jae-Hyeung
    • Korean Journal of Fisheries and Aquatic Sciences
    • /
    • v.17 no.4
    • /
    • pp.271-279
    • /
    • 1984
  • Effects of temperature and additives on the stability of actomyosin extracted from skeletal muscle of Israeli carp, Cyprinus carpio nudus, were studied by analyzing free SH-group, ATP-sensitivity and Ca-ATPase activity. The used additives were sucrose, sorbitol, Na-glutamate and L-cysteine. Furthermore, the denaturation constant($K_D$), protective effect(${\Delta}E/M$) and the other thermo-dynamic parameters on protein denaturation are systematically discussed. The actomyosin showed $4.12{\sim}4.68 mg/ml$ in protein concentration, $2.63{\sim}2.93\%$ in ribonucleic acid to the protein, $1:2.20{\sim}2.63$ in the binding ratio of myosin and actin, $4.33{\sim}5.26\%$ in fat content, 109.78 in ATP-sonsitivity, $0.159{\sim}0.201\;{\mu}M-Pi/min/mg-protein$ in Ca-ATPase activity and $3.3{\sim}3.4M/10^5$g-protein in free SH-group content. The first-order rate plots were obtained on the decrease of Ca-ATPase activity and ATP-sensitivity with an increase in temperature, while the free SH-group was increased to $60^{\circ}C$ and decreased rapidly above the temperature. The half-life of Ca-ATPase activity on the actomyosin Ca-ATPase was 280 min at $12^{\circ}C$, 125 min at $20^{\circ}C$, 55 min at $30^{\circ}C$ and 13 min at $40^{\circ}C$, and activation energy, activation enthalpy, activation entropy and free energy of the proteins at $20^{\circ}C$ wene 5,395 cal/mole, 4,814 cal/mole, -40.42 e.u. and 17,626 cal/mole, respectively. The protective effect of the additives on the actomyosin Ca-ATPase showed that the most effective material is $3\%$ sorbitol and followed in the order of $8\%$ Na-glutamate, $1\%$ sucrose and $1\%$ L-cysteine. The actomyosin was more stable at $-30^{\circ}C$ than at $0^{\circ}C$ and $-20^{\circ}C$. and when the additives were used in the low temperature storage, $8\%$ Na-glutamate was the most effective. $3\%$ sorbitol, $1\%$ sucrose and $1\%$ L-cysteine was to become lower in the order.

  • PDF

Stabilization of Radioactive Molten Salt Waste by Using Silica-Based Inorganic Material (실리카 함유 무기매질에 의한 폐용융염의 안정화)

  • Park, Hwan-Seo;Kim, In-Tae;Kim, Hwan-Young;Kim, Joon-Hyung
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.5 no.3
    • /
    • pp.171-177
    • /
    • 2007
  • This study suggested a new method to stabilize molten salt wastes generated from the pyre-process for the spent fuel treatment. Using conventional sol-gel process, $SiO_2-Al_2O_3-P_2O_5$ (SAP) inorganic material that is reactive to metal chlorides were prepared. In this paper, the reactivity of SAP with the metal chlorides at $650{\sim}850$, the thermal stability of reaction products and their leach-resistance under the PCT-A test method were investigated. Alkali metal chlorides were converted into metal aluminosilicate($LixAlxSi1-_xO_{2-x}$) and metal phosphate($Li_3PO_4\;and\;Cs_2AlP_3O_{10}$) While alkali earth and rare earth chlorides were changed into only metal phosphates ($Sr_5(PO_4)_3Cl\;and\;CePO_4$). The conversion rate was about $96{\sim}99%$ at a salt waste/SAP weight ratio of 0.5 and a weight loss up to $1100^{\circ}C$ measured by thermogravimetric analysis were below 1wt%. The leach rates of Cs and Sr under the PCT-A test condition were about $10^{-2}g/m^2\;day\;and\;10^{-4}g/m^2\;day$. From these results, it could be concluded that SAP can be considered as an effective stabilizer for metal chlorides and the method using SAP will give a chance to reduce the volume of salt wasteform for the final disposal through further researches.

  • PDF