Thermal Shock Resistance and Thermal Expansion Behavior of $Al_2TiO_5$ Ceramics

  • Kim, Ik-Jin
    • 한국결정성장학회:학술대회논문집
    • /
    • 한국결정성장학회 2000년도 Proceedings of 2000 International Nano Crystals/Ceramics Forum and International Symposium on Intermaterials
    • /
    • pp.179-193
    • /
    • 2000
  • Aluminium titanate (Al₂TiO5) with an excellent thermal shock resistant and a low the expansion coefficient was obtained by solid solution with MgO, SiO₂, and ZrO₂ in the Al₂TiO5 lattice or in the grain boundary solution through electrofusion in an arc furnace. However, these materials have low mechanical strength due to the presence of microcracks developed by a large difference in thermal expansion coefficients along crystallographic axes. Pure Al₂TiO5 tends to decompose into α-Al₂O₃ and TiO₂-rutile in the temperature range of 750-1300℃ that rendered it apparently useless for industrial applications. Several thermal shock tests were performed: Long therm thermal annealing test at 1100℃ for 100h; and water quenching from 950 to room temperature (RT). Cyclic thermal expansion coefficients up to 1500℃ before and after decomposition tests was also measured using a dilatometer, changes in the microstructure, thermal expansion coefficients, Young's modulus and strengths were determined. The role of microcracks in relation to thermal shock resistance and thermal expansion coefficient is discussed.

  • PDF

비평형 극음속 유동에서 구에 대한 충격파 이탈거리 계산 (CALCULATION OF SHOCK STAND-OFF DISTANCE FOR A SPHERE IN NONEQUILIBRIUM HYPERSONIC FLOW)

  • Furudate, M. Ahn
    • 한국전산유체공학회지
    • /
    • 제17권4호
    • /
    • pp.69-74
    • /
    • 2012
  • Hypersonic flowfields over a sphere is calculated by using a nonequilibrium flow solver. The flow solver features a two-temperature model and finite rate chemical reaction models to describe nonequilibrium thermochemical processes. For the purpose of validation, the calculated shock stand-off distance is compared with the experimental data which is measured in a ballistic range facility. The present nonequilibrium calculation well reproduced the experimental shock stand-off distance in the cases where the experimental flowfields are expected to be nearly equilibrium, as well as in the cases to be nonequilibrium flowfields in the velocity range 4000 to 5500 m/s.

금강모치(Rhynchocypris kumgangensis)에서 heat shock protein 70의 클로닝과 수온상승에 의한 발현 변화 분석 (Cloning of Heat Shock Protein 70 and Its Expression Profile under an Increase of Water Temperature in Rhynchocypris kumgangensis)

  • 임지수;길성호
    • 한국물환경학회지
    • /
    • 제29권2호
    • /
    • pp.232-238
    • /
    • 2013
  • Water temperature is key factor influencing growth and reproduction of fish and its increase give rise to various physiological changes including gene expression. Heat shock protein (Hsp), one of the molecular chaperones, is highly conserved throughout evolution and its expression is induced by various stressors such as temperature, oxidative, physical and chemical stresses. Here, we isolated partial cDNA clones encoding 70-kDa Hsp (Hsp70) and $\beta$-actin using reverse transcriptase-PCR (RT-PCR) from gut of Rhynchocypris kumgangensis, a Korean indigenous species and cold-water fish, and investigated expression profiles of Hsp70 under an increase of water temperature using $\beta$-actin as an internal control for RT-PCR. Cloned Hsp70 cDNA of R. kumgangensis showed homology to Ctenopharyngodon idella (96%), Hypophthalmichthys molitrix (96%), Danio rerio (93%) and Oncorhynchus mykiss (81%) Hsp70. Cloned $\beta$-actin cDNA of R. kumgangensis showed homology to D. rerio (98%), H. molitrix (97%), C. idella (97%) and O. mykiss (90%) $\beta$-actin. Both mRNA of Hsp70 and $\beta$-actin were expressed in gut, brain, and liver in R. kumgangensis. Futhermore, expression of Hsp70, in brain, was highly augmented by an increase of water temperature. These results suggest that Hsp70 mRNA expression level in brain can be used as a biological molecular marker to represent physiological stress against an increase of water temperature.

Shock Tube and Modeling Study of the Monomethylamine Oxidation at High Temperature

  • Shin, Kuan-Soo;Yoo, Sang-Jo
    • Bulletin of the Korean Chemical Society
    • /
    • 제25권2호
    • /
    • pp.293-297
    • /
    • 2004
  • The ignition of monomethylamine was studied in reflected shock waves over the temperature range of 1255- 1579 K and the pressure range of 1.04-1.51 bar. The ignition delay time was measured by the sudden increase of pressure profile and the radiation emitted by OH radicals. The relationship between the ignition delay time and the concentrations of monomethylamine and oxygen was determined in the form of mass-action expressions with an Arrhenius temperature dependence. In contrast to the behavior observed in hydrocarbons, monomethylamine acts to accelerate rather than inhibit its own ignition. And numerical modeling of the ignition of $CH_3NH_2$ has also been carried out to test the several kinetic mechanisms.

LOW CYCLE THERMAL FATIGUE OF THE ENGINE EXHAUST MANIFOLD

  • Choi, B.L.;Chang, H.;Park, K.H.
    • International Journal of Automotive Technology
    • /
    • 제5권4호
    • /
    • pp.297-302
    • /
    • 2004
  • This paper presents the low cycle thermal fatigue of the engine exhaust manifold subject to thermo-mechanical cyclic loading. As a failure of the exhaust manifold is mainly caused by geometric constraints of the less expanded inlet flange and cylinder head, the analysis is based on the exhaust system model with three-dimensional temperature distribution and temperature dependent material properties. The result show that large compressive plastic deformations are generated at an elevated temperature of the exhaust manifold and tensile stresses are remained in several critical zones at a cold condition. From the repetition of these thermal shock cycles, maximum plastic strain range (0.454%) could be estimated by the stabilized stress-strain hysteresis loops. It is used to predict the low cycle thermal fatigue life of the exhaust manifold for the thermal shock test.

Multiscale modeling of the anisotropic shock response of β-HMX molecular polycrystals

  • Zamiri, Amir R.;De, Suvranu
    • Interaction and multiscale mechanics
    • /
    • 제4권2호
    • /
    • pp.139-153
    • /
    • 2011
  • In this paper we develop a fully anisotropic pressure and temperature dependent model to investigate the effect of the microstructure on the shock response of ${\beta}$-HMX molecular single and polycrystals. This micromechanics-based model can account for crystal orientation as well as crystallographic twinning and slip during deformation and has been calibrated using existing gas gun data. We observe that due to the high degree of anisotropy of these polycrystals, certain orientations are more favorable for plastic deformation - and therefore defect and dislocation generation - than others. Loading along these directions results in highly localized deformation and temperature fields. This observation confirms that most of the temperature rise during high rates of loading is due to plastic deformation or dislocation pile up at microscale and not due to volumetric changes.

열초음파 접합 공정과 접합부의 신뢰성 평가에 관한 연구 (A Study on Thermosonic Bonding Process and Its Reliability Evaluation of Joints)

  • 신영의;박진석;손선익
    • 한국전기전자재료학회논문지
    • /
    • 제22권8호
    • /
    • pp.625-631
    • /
    • 2009
  • In this thesis, lateral thermosonic bonding with ACFs was investigated as a process to make high reliability joints for FPD fabrication. Conditions for thermosonic and thermocompression bonding with ACFs were determined and used to make specimens in a driving test jig for testing of bond reliability by thermal shock. The results showed that thermosonic bonding temperature of $199\;^{\circ}C$ and bonding time of 1s produced bonds with good reliability. Additionally, thermosonic bonding temperature and time were reduced and thermal shock test results compared to this proposed curing condition. It is concluded that theromosonic bonding with ACFs can be effectively applied to reduce bonding temperature and time compared with that of thermocompression bonding.

가압열충격 사고에 대한 원자로 용기의 최대 허용 기준무연성천이온도 (Maximum Allowable $RT_{NDT}$ of Nuclear Reactor Vessel for Pressurized Thermal Shock Accident)

  • 정명조;박윤원;송선호
    • 전산구조공학
    • /
    • 제11권1호
    • /
    • pp.153-160
    • /
    • 1998
  • 본 연구에서는 가압열충격 사고로 소형 냉각재 상실사고를 가정하여 냉각재의 온도와 압력의 이력으로 부터 용기 벽의 온도분포를 구하고, 이로 부터 열응력과 압응력을 해석적으로 구하였다. 또 균열 선단에서의 응력강도계수와 파괴인성치를 ASME코드의 방법을 이용하여 구하였고, 이들을 시간에 따라 비교하여 균열의 진전여부를 평가하였다. 원자로 용기 벽에 존재하는 여러 형태의 균열이 견딜 수 있는 최대 기준무연성천이온도를 결정하였으며 평가 결과에 대하여 고찰하였다.

  • PDF

어류 CHSE-214와 인간 HeLa 세포에서의 열충격에 의한 Heat Shock Protein의 발현 (Expression of the Heat Shock Proteins in HeLa and Fish CHSE-214 Cells Exposed to Heat Shock)

  • 공회정;강호성김한도
    • 한국동물학회지
    • /
    • 제39권2호
    • /
    • pp.123-131
    • /
    • 1996
  • In this study, we examined the expression of heat shock proteins (HSPs) in fish cell line CHSE-2lnl and human HeLa cells exposed to heat shock. In fish CHSE-214 cells HSP70 was the major polvpeptide induced by an elevated temperature or an amino acid analog, while in HeLa cells HSP90 as well as HSP70 were prominently enhanced in response to these stresses. Pretreatment of actinomvcin D prior to heat shock completely inhibited the induction of fish HSP70, indicating the transcriptional regulation of fish HSP70 gene expression. In HeLa and CHSE-214 cells either recovering from heat shock or experiencing prolonged heat shock, attenuation in the HSP90 a'nd HSP70 induction occurred but both induction and repression of HSP70 synthesis appear 19 precede those of HSP90. Moreover, attenuation did not occur in the syntheses of 40 kDa and 42 kOto proteins which were only induced in CHSE-214 cells. The enhanced syntheses of these he proteins continued as long as CHSE-214 cells were Siven heat shock. These results suggest that down-regulation of HSP syntheses during prolonged heat shock may be controlled by several different. as vet undefined, mechanisms.

  • PDF

자동차용 충격 흡수기의 동특성 연구 (A Study on Dynamic Characteristics of Automotive Shock Absorber)

  • 남경탁;황성원;신귀수
    • 한국안전학회지
    • /
    • 제17권3호
    • /
    • pp.1-6
    • /
    • 2002
  • A dynamic characteristics of shock absorber in the various excitation is investigated experimentally. Work diagrams and characteristic curves are used as a experimental standard. The various excitation conditions temperature and noise are very important factors in associated with the reduction of damping force. It is found that the heat occurrence from shock absorber, the gas shock absorber is much higher than oil shock absorber and increased in high speed. As to the variation of damping force, there are no change when the speed is low but we fixed amount of variation by increasing speed and change of new and old decrease. The sound pressure of the swash noise from cycle of shock absorber, we compared with theory sound pressure by experiment.