• Title/Summary/Keyword: synthetic rubber

Search Result 90, Processing Time 0.028 seconds

Properties of Silicone and its Suitability as a Synthetic Leather Coating Agent (실리콘의 특성 이해와 합성피혁 코팅제로서의 적합성)

  • Suhong Kim;Doohyun Baik
    • Textile Coloration and Finishing
    • /
    • v.35 no.1
    • /
    • pp.42-65
    • /
    • 2023
  • Leather is widely used in human lives and many industries, and the market size continues to grow. In terms of quality and durability, natural leather is still being used as the most luxurious product. And synthetic leather, made of polyvinyl chloride (PVC) and polyurethane (PU), were developed and being widely have been used as alternative materials for natural leather. Processes, properties and issues of these leather were reviewed. Then silicone leather was reviewed why they can be good candidates for leather. Properties of general silicone polymers and silicone rubber coating agents were reviewed such as eco-friendliness, human-friendliness, stain resistances, resistance to uv light and ozone, heat stability and so on. Papers and patents related to silicone leather were studied to understand current status of development and commercialization of silicone leather. Finally direction of development was described how to improve deficient performances of current silicone leather, such as formulation of silicone, combination with organic materials and manufacturing processes.

Properties of CB/SBR Rubber Composites Filled by Carbon Blacks Used as Catalysts for Hydrogen Production through Hydrocarbon Decomposition

  • Dai, Shuangye;Ao, Gyeou;Kim, Myung-Soo
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2006.11a
    • /
    • pp.392-395
    • /
    • 2006
  • In this work, the reinforcing action of carbon blacks in rubber was investigated by SEM and UTM measurements which at low a testing of the surface and mechanical properties. In order to gain an insight into the different properties between carbon blacks before and after methane/propane decomposition, various composites were prepared with SBR synthetic rubber and different carbon blacks with four loading ratios. The results were analyzed with the aim of finding suitable conditions for decomposition reaction to cut down the net cost for hydrogen production through hydrocarbon decomposition.

  • PDF

The Study of Optimized Compounds Containing Silica and Coupling Agent to Improve the Physical Properties of Rubber Compounds (고무물성 향상을 위한 실리카 및 실란 커플링제의 최적배합에 관한 연구)

  • Oh, Sae-Chul;Go, Jin-Hwan;Lee, Seag;Park, Nam-Cook
    • Elastomers and Composites
    • /
    • v.30 no.2
    • /
    • pp.112-121
    • /
    • 1995
  • The physical properties of rubber compounds containing silica and siliane coupling agent in order to replace the carbon black and prepare for environmental regulation showed improved dynamic properties(rebound, heat build-up, $60^{\circ}C\;tan\;{\delta}$), but the abrasion resistance did not improve compared with the compounds containing carbon black. Also, curing retardation because of coherent structure of silica improved by the addition of DEG, but the mixing step change of activators did not so much improve the static and dynamic properties of the compounds containing high synthetic rubber, the status of mixing and dispersion showed that the compounds containing carbon black was much better than the compounds containing silica by TEM investigation.

  • PDF

On the Pyrolysis of Polymers III. Identification of Gases from Rubber Pyrolysis by Gas Chromatography (高分子物質의 熱分解에 關한 硏究 (第3報) 合成고무類의 熱分解生成物의 Gas Chromatography에 의한 檢索과 合成고무 確認에의 利用)

  • Chwa-Kyung Sung
    • Journal of the Korean Chemical Society
    • /
    • v.7 no.2
    • /
    • pp.115-121
    • /
    • 1963
  • Aliphatic hydrocarbon gases from rubber pyrolysis have been identified by gas chromatography with tetraethyleneglycol dimethylether column. Rubbers used in this work are polyisoprene, SBR, NBR, polybutadiene, buthyl rubber, polychloroprene and polyurethane rubber. The chromatogram is characteristic for each polymer. Author proposes a method of identification of synthetic rubbers by gas chromatograph of pyrolyzed gas. Sample is pyrolyzed at $450^{\circ}C$ under nitrogen or more effectively helium and gaseous portion, which eliminated liquid condensate, is passed to the column. The appearance of exclusively large peak of isoprene, isobutylene and carbon dioxide shows the presence of polyisoprene, polyisobutylene and polyurethane, respectively. Large peak of butadiene will appear in case of polybutadiene, SBR and NBR, but SBR can be identified through the styrene peak in gas chromatogram of liquid pyrolyzate and NBR can be identified by the evolution of hydrogen cyanide during pyrolysis. Polychloroprene is identified by the evolution of hydrogen chloride. This method could be applied to the identification of copolymer or polymer blend.

  • PDF

Studies on the Physical Properties of Synthetic Rubber Blends Containing Rein-forcing Fillers (보강성 충전제를 함유한 합성고무 블렌드의 물리적 특성에 관한 연구)

  • Go, Jin-Hwan;Lee, Seog
    • Elastomers and Composites
    • /
    • v.33 no.4
    • /
    • pp.231-237
    • /
    • 1998
  • In order to investigate the physical properties of rubber blend compound, this experiment was carried out on the cure rate, loss tangent, reinforcement and abrasion properties of S-SBR (solution styrene-butadiene rubber) blends containing silane coupled silica and E-SBR (emulsion styrene-butadiene rubber) blends containing carbon black as a model compound. E-SBR blend showed the highest total bound rubber(TBR), while S-SBR blends showed constant TBR level regardless of rubber type. Rapid cure rate was achieved when the styrene and vinyl content of rubber microstructure decreased and TBR content of rubber compounds increased. The modulus as the index of rubber reinforcement showed the linear relation with TBR content. The large amount of PICO loss was observed when the styrene and vinyl content of rubber microstructure increased, while the small amount of PICO loss was observed when the ratio of bu-tadiene increased in the S-SBR blends with silane copuled silica. The high loss tangent at $0^{\circ}C$, the low loss tangent at $60^{\circ}C$, and the large difference of loss tangent were shown in the S-SBR blends with high styrene content compared to E-SBR blend.

  • PDF

Evaluation of Chemical Resistance Performance of Synthetic Rubber and Cement Based Injection Repair Materials Used in Underground Concrete Structures (지하 콘크리트 구조물에 적용되는 합성고무계 및 시멘트계 주입형 보수재료의 화학 저항성능평가)

  • Kim, Soo-Yeon;Lee, Yeon-Sil;Song, Je-Young;Kim, Byoungil;Oh, Sang-Keun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.21 no.5
    • /
    • pp.148-155
    • /
    • 2017
  • In this study, by using the international standards ISO TS 16774, Part 2 Test method for chemical resistance as a quality control method of injection type repair material used for leakage crack of underground concrete structure, the performance requirement against of chemical environment of underground concrete structures for repair materials was tested. For this testing 3 types for each of the 2 classes of repair materials(synthetic rubber, cement), with a total of 9 types repair materials, were selected and examined. As a result, the test results showed that the smallest performance deterioration by the change in the mass was with the synthetic rubber(RG) type as opposed to the cement type system, showing that the synthetic rubber type had the strongest relative resistance to chemical exposure. Furthermore, it is necessary to investigate the material with high resistance to chemical substances and to examine the material which can increase resistance to sodium hydroxide and sodium chloride in cement system. These results can be used as a basic index for the selection of repair materials with the strongest resistance to chemical environment found in concrete structures. In addition, it is expected that the test results derived in this study can be used as reference data that can be reflected in the quality improvement of the maintenance material to be developed later.

Effect of Thermal Aging on the Change of Interfacial Adhesion between Polyketone Cord and Rubber by RFL Primer Treatment (RFL 프라이머 처리에 따른 폴리케톤 코드사와 고무 간의 계면접착성 변화에 열노화가 미치는 영향)

  • Jo, Hani;Oh, Woo Jin;Kang, Song Hee;Lee, Seung Goo
    • Textile Coloration and Finishing
    • /
    • v.30 no.2
    • /
    • pp.77-89
    • /
    • 2018
  • In the case of fiber/rubber composites for tire applications, the interfacial adhesion between fiber and rubber significantly affects the physical properties of the finished products. Generally, organic synthetic fibers used for tire cords are treated with resorcinol formaldehyde latex(RFL) primer on the surface of the fiber to improve the adhesion to rubber. Changes of adhesion between rubber and tire cords might weaken as temperature rises due to overheating of car engine and friction with road. In this study, the effects of temperature on the primer treated polyketone cord/rubber composites and the changes in interfacial adhesion were investigated. Polyketone cord/rubber composites were prepared after RFL solution treatment on the surface of polyketone fibers. After that, composites was thermally aged at different temperature conditions(60, 80, 100, $120^{\circ}C$) and times(1, 5, 10, 15days). The adhesion strength of polyketone cord/rubber composite treated with RFL primer was higher than untreated composite by more than 3 times. After heat aging, the adhesion strength of untreated polyketone cord/rubber composites increased while the RFL treated polyketone cord/rubber composites decreased somewhat.

Effects of Intermeshing Rotor for Dispersion of Silica Agglomerates in SBR/BR Compound (Intermeshing Rotor의 구조가 SBR/BR 합성고무 복합소재의 실리카 분산에 미치는 영향의 비교)

  • Kim, Sung-Min;Kim, Kwang-Jea
    • Polymer(Korea)
    • /
    • v.36 no.5
    • /
    • pp.637-642
    • /
    • 2012
  • The effects of mixing geometry (intermeshing vs. tangential rotor) for the dispersion and distribution of silica agglomerates in SBR/BR compound were investigated. Silica dispersion and distribution were found to be better with the intermeshing rotor compared to the tangential rotor. It was concluded that the intermeshing rotor compared to the tangential rotor delivered a higher shear stress due to interlocked rotor geometry to silica agglomerates leading to better dispersity and distribution of silica in the agglomerates.

Degradation of cis-Polyisoprene in Supercritical Tetrahydrofuran (Tetrahydrofuran의 초임계 상에서 cis-Polyisoprene의 분해)

  • Kim, H.J.;Hong, I.K.
    • Elastomers and Composites
    • /
    • v.32 no.5
    • /
    • pp.302-308
    • /
    • 1997
  • Over 1953/54 Karl Ziegler and Giulio Natta independently discovered new types of catalyst. Thus it was able to produce synthetic cis-polyisoprene rubber which has same properties like natural rubber, since then the amount of consumption was increased rapidly. The problem of disposing of used rubbers has become acute in recent years. cis-Polyisoprene was degraded in supercritical tetrahydrofuran and degree of degradation and product were observed by GPC, FT-IR, GC-MS analyses. As a result, degradation of cis-polyisoprene had small dependency upon the operating pressure, and was inhibited in concentration increase. And cis-polyisoprene was degraded into narrow molecular weight distribution oligomer in 3 hours, and more than 10 organic compounds were produced.

  • PDF

Comparison of SBR/BR Blend Compound and ESBR Copolymer Having Same Butadiene Contents

  • Hwang, Kiwon;Lee, Jongyeop;Kim, Woong;Ahn, Byungkyu;Mun, Hyunsung;Yu, Eunho;Kim, Donghyuk;Ryu, Gyeongchan;Kim, Wonho
    • Elastomers and Composites
    • /
    • v.54 no.1
    • /
    • pp.54-60
    • /
    • 2019
  • The rapid development of the automobile industry is an important factor that led to the dramatic development of synthetic rubber. The tread part of tire that comes in direct contact with the road surface is related to the service life of the tire. Rubber compounds used in tire treads are often blended with SBR (styrene-butadiene rubber) and BR (butadiene rubber) to satisfy physical property requirements. However, when two or more kinds of rubber are blended, phase separation and silica dispersion problems may occur due to non-uniform mixing of the rubber. Therefore, in this study, we synthesized an SBR copolymer with the same composition as that of a typical SBR/BR blend compound by controlling butadiene content during ESBR (emulsion styrene-butadiene rubber) synthesis. Subsequently, silica filled compounds were manufactured using the synthesized ESBR, and their mechanical properties, dynamic viscoelasticity, and crosslinking density were compared with those of the SBR/BR blended compound. When the content of butadiene was increased in the silica filled compound, the cure rate accelerated due to an increased number of allylic positions, which typically exhibit higher reactivity. However, the T-2 compound with increased butadiene content by synthesis less likely to show an increase in crosslink density due to poor silica dispersion. In addition, the T-3 compound containing high cis BR content showed high crosslink density due to its monosulfide crosslinking structure. Because of the phase separation, SBR/BR blend compounds were easily broken and showed similar $M_{100%}$ and $M_{300%}$ values as those of other compounds despite their high crosslink density. However, the developed blend showed excellent abrasion resistance due to the high cis-1,4 butadiene content and low rolling resistance due to the high crosslink density.