Investigation of Adhesion Mechanism at the Metal-Organic Interface Modified by Plasma - Part I

  • Sun, Yong-Bin
    • Proceedings of the Korean Society Of Semiconductor Equipment Technology
    • /
    • 2002.11a
    • /
    • pp.123-126
    • /
    • 2002
  • For the mold die sticking mechanism, the major explanation is that EMC filler of silica wears die surface roughened, which results in increase of adhesion strength. As big differences in experimental results from semiconductor manufacturers are dependent on EMC models, however, chemisorptions or acid-base interaction is apt to be also functioning as major mechanisms. In this investigation, the plasma source ion implantation (PSII) using $O_2$, $N_2$, and $CF_4$ modifies sample surface to form a new dense layer and improve surface hardness, and change metal surface condition from hydrophilic to hydrophobic and vice versa. Through surface energy quantification by measuring contact angle and surface ion coupling state analysis by Auger, major governing mechanism for sticking issue was figured out to be a complex of mechanical and chemical factors.

  • PDF

Deposition and Characterization of Electrophoretic Paint on AZ31 Magnesium Alloy

  • Nguyen, Van Phuong;Moon, Sungmo
    • Journal of the Korean institute of surface engineering
    • /
    • v.49 no.2
    • /
    • pp.141-146
    • /
    • 2016
  • In this study, electrophoretic paint (E-paint) was deposited on the knife-abraded surface of AZ31 magnesium alloy (AZ31), and its adhesion and corrosion resistance were examined by tape peel-test and salt spray test, respectively. E-paint started to deposit on AZ31 Mg alloy after an inductance time and pores were found in the E-paint layer which is ascribed to hydrogen bubbles generated on the surface during the painting process. The pores disappeared after curing for 15 min at $160^{\circ}C$. The E-paint on AZ31 exhibited good adhesion after immersion in deionized water for 500 h at $40^{\circ}C$. The E-paint sample without scratch showed no corrosion after 1500 h of salt spray test. However, on the scratched sample, blisters were visible adjacent to the scratched sites after 500 h of salt spray test.

Effect of Surface Treatment of Polycarbonate Film on the Adhesion Characteristic of Deposited SiOx Barrier Layer (폴리카보네이트 필름 표면 처리가 증착 SiOx 베리어층 접착에 미치는 영향)

  • Kim, Gwan Hoon;Hwang, Hee Nam;Kim, Yang Kook;Kang, Ho-Jong
    • Polymer(Korea)
    • /
    • v.37 no.3
    • /
    • pp.373-378
    • /
    • 2013
  • The interfacial adhesion strength is very important in $SiO_x$ deposited PC film for the barrier enhanced polycarbonate (PC) flexible substrate. In this study, PC films were treated by undercoating, UV/$O_3$ and low temperature plasma and then the effect of physical and chemical surface modifications on the interfacial adhesion strength between PC film and $SiO_x$ barrier layer were studied. It was found that untreated PC film shows significantly low interfacial adhesion strength due to the smooth surface and low surface free energy of PC. Low temperature plasma treatments resulted in the increase of both surface roughness and surface free energy due to etching and the appearance of polar molecules on the PC surface. However, UV/$O_3$ treatment only shows the increase of surface free energy by developed polar molecules on the surface. These surface modifications caused the enhancement of surface interfacial strength between PC film and $SiO_x$ barrier. In the case of undercoating, it was found that the increase of surface interfacial strength was achieved by adhesion between various acrylic acid on acrylate coated surface and $SiO_x$ without increase of polar surface energy. In addition, the barrier property is also improved by organic-inorganic hybrid multilayer structure.

Comparative Analysis of Substrate Wet Surface Adhesion and Substrate Movement Response Performance Testing Methods for Injection Type Repair Materials Used in Leakage Cracks of Concrete Structure in Underground Environment (지하 습윤 환경에서 콘크리트 구조물 균열 누수에 사용되는 주입형 보수재료의 부착 성능과 거동 대응 성능 평가의 상관성 분석 연구)

  • Kim, Soo-Yeon;Oh, Kyu Hwan;Oh, Snag-Keun
    • Journal of the Architectural Institute of Korea Structure & Construction
    • /
    • v.34 no.9
    • /
    • pp.19-26
    • /
    • 2018
  • The focus of this study was centered around 15 common injection type water leakage repair materials (3 different types for each; synthetic polymer, cementitious, acrylic, epoxy, urethane) used in concrete structures of Korea and analyzing their wet surface adhesion performance in accordance to the ISO TS 16774 Test Method for Repair Materials for Water-leakage Cracks in Underground Concrete Structures, Part 4: Test Method for Adhesion on Wet Concrete Surface, and the results of this study was taken to be place under a comparative analysis with the results of the preceeding study on response to substrate movement performance study. The results of this comparative study showed that other than 1 specimen of 1 type of the acrylic and 3 specimens of 1 type of the synthetic polymer type materials, all of the 93% of the specimens used in this study showed stable adhesion on wet substrate surface, and we were able to determine that materials that have proper response properties against substrate movement are highly flexible and have high adhesion properties, but their adhesion properties on wet substrate would change based on their viscosity.

Analysis of anti-adhesion property in replication of patterns of sub-micrometers (Sub-micrometer 크기의 패턴의 복제시 발생되는 이형 특성의 분석)

  • Lee, Nam-Seok;Kang, Shin-Ill
    • Proceedings of the KSME Conference
    • /
    • 2003.04a
    • /
    • pp.940-944
    • /
    • 2003
  • With the increasing demand for plastic micro components, micro-/nano-molding using the mother stamper has received much attention. If the replication temperature is too high, the adhesion between the stamper and the polymer melt may deteriorate the surface quality of the replicated part, excessively wearing down the stamper. In this paper, an experimental method analyzes the temperature dependency of the anti-adhesion property between the actual stamper with patterns of sub-micrometer and the polymer melt. As a practical example, a correlation between the contact angle of the stamper and the surface quality of the molded substrates as a function of the replication temperature, respectively, was obtained quantitatively.

  • PDF

The Study on the Safety Adhesion Test of Wet Surface for Waterproofing and Anti Corrosion Materials of Water Supply Facility (수처리 시설물에 적용되는 방수·방식재의 습윤면 부착 안정 성능평가방법에 대한 연구)

  • Choi, Su-Young;Kim, Dong-Bum;Park, Jin-Sang;Park, Wan-Goo;Kim, Byoung-Il;Oh, Sang-Keun
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2017.05a
    • /
    • pp.137-138
    • /
    • 2017
  • The Waterproofing and Anti corrosion materials applied to the water supply facility did not consider environment of water supply facility, thus defects occurred consistently on the site. In this study, it suggests safety adhesion test of wet surface and have a test for safety adhesion performance.

  • PDF

Influence of Surface Treatment of Polyimide Film on Adhesion Enhancement between Polyimide and Metal Films

  • Park, Soo-Jin;Lee, Eun-Jung;Kwon, Soo-Han
    • Bulletin of the Korean Chemical Society
    • /
    • v.28 no.2
    • /
    • pp.188-192
    • /
    • 2007
  • In this work, the effects of chemical treatment of polyimide films were studied by FT-IR, X-ray photoelectron spectroscopy (XPS), atomic force microscopy (AFM) and contact angles. The adhesion characteristics of the films were also investigated in the peel strengths of polyimide/aluminum films. The increases of surface functional groups of KOH-treated polyimide films were greatly correlated with the polar component of surface free energy. The peel strength of polyimides to metal substrate was also greatly enhanced by increasing the KOH treatment time, which can be attributed to the formation of polar functional groups on the polyimide surfaces, resulting in enhancement of the work of adhesion between polymer film and metal plate.

Anti-freezing effect of mortar surface with superhydrophobic water repellent (초소수성 발수제를 사용한 모르타르 표면의 결빙 방지 효과)

  • Kim, Sang-Jin;In, Byung-Eun;Kang, Suk-Pyo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2022.04a
    • /
    • pp.15-16
    • /
    • 2022
  • In order to examine the adhesion characteristics of road pavement according to environmental conditions, the freezing time of cement mortar and the adhesion performance between ice and pavement were evaluated depending on the presence or absence of polymer and water repellent. As a result of measuring the ice formation time, it was found that there was no delay when a polymer was added, but the complete freezing time was delayed when a water repellent was added. As a result of measuring the strength of ice adhesion, it was found that the bonding force between ice and the surface of the test body was greatly generated in the test body without water repellent. In the case of a test specimen to which a water repellent was added, it was found that the bonding strength between the test specimen surface and ice was reduced.

  • PDF

Nanotribological Characteristics of Silicon Surfaces Modified by IBAD (IBAD로 표면개질된 실리콘 표면의 나노 트라이볼로지적 특성)

  • Park, Ji-Hyun;Yang, Seung-Ho;Kong, Ho-Seung;Jhang, Kyung-Young;Yoon, Eui-Sung
    • Tribology and Lubricants
    • /
    • v.18 no.1
    • /
    • pp.1-8
    • /
    • 2002
  • Nano adhesion and friction between a $Si_{3}N_{4}$ AFM(atomic force microscope) tip and thin silver films were experimentally studied. Tests were performed to measure the nano adhesion and friction in both AFM and LFM(lateral force microscope) modes in various range of normal loads. Thin silver films deposited by IBAD (ion beam assisted deposition) on Si-wafer (100) and other Si-wafers of different surface roughness were used. Results showed that nano adhesion and friction decreased with the surface roughness. When the Si surfaces were coated by pure silver, the adhesion and friction decreased. But the adhesion and friction were not affected by the thickness of IBAD silver coating. As the normal force increased, the adhesion forces of bare Si-wafer and IBAD silver coating film remained constant, but the friction forces increased linearly. Test results suggested that the friction was mainly governed by the adhesion as long as the load was low.

Study on the Adhesion of Diamond Like Carbon Films Using the Linear Ion Source with Nitriding Layers (Linear Ion Source에 의해 증착된 Diamond-Like Carbon(DLC) 박막의 질화층 형성에 따른 밀착력 특성 연구)

  • Shin, Chang-Seouk;Park, Min-Seok;Kwon, Ah-Ram;Kim, Seung-Jin;Chung, Won-Sub
    • Journal of the Korean institute of surface engineering
    • /
    • v.44 no.5
    • /
    • pp.190-195
    • /
    • 2011
  • Diamond-like carbon (DLC) has many outstanding properties such as low friction, high wear resistance and corrosion resistance. However, it is difficult to achieve enough adhesion on the metal substrates because of weak bonding between DLC film and the metal substrate. The purpose of this study is to enhance an adhesion of DLC film. For improving adhesion, the substrate was treated by active screen plasma nitriding before DLC film deposing. Nitrided substrates were investigated by Glow Discharge Spectrometer (GDS), Micro-Vickers Hardness. DLC films were deposited on several metals by linear ion source, and characteristics of the films were investigated using nano-indentation, Field Emission Scanning Electron Microscope (FESEM). The adhesion was measured by scratch tester. The adhesion of DLC films was increased when nitriding layer was formed before DLC deposition. Therefore, the adhesion of DLC film can be enhanced as increasing the hardness of materials.