• Title/Summary/Keyword: styrene butadiene rubber (SBR)

Search Result 116, Processing Time 0.02 seconds

Wear Behavior of Silica filled Styrene-Butadiene Rubber: A Comparative Study Between the Blade-Type and Akron-Type Abrader

  • Gi-Bbeum Lee;Dongwon Kim;Seowon Lee;Seonhong Kim;Myung-Su Ahn;Bismark Mensah;Changwoon Nah
    • Elastomers and Composites
    • /
    • v.58 no.4
    • /
    • pp.179-190
    • /
    • 2023
  • The effect of the particle size and silica structure on the wear behavior of Silica/Styrene-Butadiene Rubber (SBR) compounds was investigated using a blade-type abrader and the findings were compared with those obtained with an Akron abrader. The compensated characteristic parameter (Ψc), which was the contributory factor of the combined effect of the particle size and filler structure, was introduced. This parameter was found to exhibit a linear relationship with the Young's modulus. The Young's modulus correlated more with Ψc than the uncompensated characteristic parameter (Ψ) modeled for carbon black. The wear rate and volume loss measured using a blade-type abrader and Akron abrader were respectively observed to be inversely proportional to Ψc, that is, the wear resistance of Silica/SBR compound improved as the particle size became smaller and the silica structure became intricate. The coefficient of determination (R2) obtained from the linear relationship between Ψc and wear rate was higher than those between Ψc and volume loss for the Silica/SBR compound. Thus, the blade-type abrader exhibited high potential to be used for accurately evaluating the effect of particle size and structural properties of silica on the wear behavior of SBR compounds.

Influence of SBR Type and Blend Ratio on Dynamic Mechanical Properties of SBR/SBR Biblend Composites

  • Sung-Seen Choi
    • Elastomers and Composites
    • /
    • v.59 no.1
    • /
    • pp.17-21
    • /
    • 2024
  • Solution styrene-butadiene rubber (S-SBR) is used to improve the wet grip and rolling resistance properties of tire treads. As blending of SBRs can improve the physical properties of tire treads, we investigated the effects of SBR type and blending ratio on the physical properties. Twelve SBR/SBR biblend composites were prepared using four SBRs with different microstructures. The glass transition temperature (Tg), tanδ at 0℃ (wet grip predictor), and tanδ at 60℃ (rolling resistance predictor) were obtained from dynamic mechanical analysis, and were compared to the expected values obtained from the results of single SBR samples. Most of the SBR/SBR biblend composites exhibited crosslink densities lower than the expected values. The tanδ values at 0℃ and 60℃ of the SBR/SBR blend composites deviated from the expected values, with many of the deviations being disadvantageous. Of the twelve composites, six samples had higher 0℃ tanδ values than the corresponding expected values, and four exhibited superior wet grip properties to those of the SBR single samples. In addition, two of the twelve samples exhibited improved rolling resistance properties as compared with the single SBR samples. Finally, four samples exhibited lower Tg values than expected, and the Tg of one composite was lower than those of the single SBR samples.

Development of Polymer-Concrete Composite(I) - Physical Properties of Polymer-Cement Concrete Composites - (폴리머-콘크리트 복합재료 개발(I) - 폴리머-시멘트 콘크리트의 물성 -)

  • Hwang, Eui-Hwan;Kil, Deog-Soo;Oh, In-Seok
    • Applied Chemistry for Engineering
    • /
    • v.8 no.6
    • /
    • pp.979-984
    • /
    • 1997
  • Test specimens of polymer-cement concrete composites were prepared using styrene-butadiene rubber(SBR) latex, ethylenevinyl acetate(EVA) and polyacrylic ester(PAE) emulsions as polymer dispersions in cement modified system at constant slump($10{\pm}0.5cm$), then compressive and flexural strengths water absorption, pore size distribution, and microstructures were investigated. Compressive and flexural strengths of these composites were remarkably improved with an increase of polymer-cement ratio. These composites had a desirable pore size distribution against frost damage due to a small capillary pore volume. Continuous polymer film was able to form in higher than 15% of polymer cement ratio.

  • PDF

Properties of Polymer-Modified Mortars Containing FPR Wastes (FRP 폐기물을 첨가한 폴리머-시멘트 모르타르의 특성)

  • 이병기;김승문;황의환;노재성
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1996.10a
    • /
    • pp.84-92
    • /
    • 1996
  • The flexural and compressive strengths of polymer-modified mortars containing FRP wastes were investigated. The specimens of polymer-modified mortars containing FRP mortat were perpared by using styrene-butadiene rubber(SBR) latex, ethylene-vinyl acetate(EVA) emulsion and polyacrylic ester(PAE) emulsion with various FRP-sand ratios(10, 20, 30, 40, 50wt%). The compressive and flexural strengths of polymer-mokified mortars containing FRP wastes were decreased with an increase of FRP-sand ratio. But the compressive and flexural strengths of PAE polymer-modified mortar were more improved than OPC, whereas those of SBR and EVA polymer-modified mortars containing FRP wastes were decreased than OPC.

  • PDF

Influence of Nano-Cellulose Dispersant on the Vulcanization Characteristics, Viscoelastic Properties, and Mechanical Properties of Silica-SBR Compounds

  • Kim, Jung Soo;Kim, Dong Hyun
    • Elastomers and Composites
    • /
    • v.55 no.3
    • /
    • pp.215-221
    • /
    • 2020
  • Silica/SBR (styrene-butadiene rubber) compounds are the primary constituents of tire treads. Furthermore, the excellent dynamic viscoelastic properties of silica lead to good fuel efficiencies. However, the silanol group on the surface of silica does not mix well with non-polar rubber because of its polarity. This incompatibility causes aggregation due to the occurrence of hydrogen bonding between the hydroxyl groups, thereby reducing the dispersibility of silica. Recently, the wet master batch (WMB) process has been applied to overcome these disadvantages, and research on silica dispersants that can be used in the WMB process has been increasing. In this study, we prepared silica/SBR compounds by using three types of eco-friendly cellulose-based dispersants in the WMB process, namely: cellulose-, sodium carboxymethyl cellulose, and nanocellulose-based dispersants. Subsequently, we compared the vulcanization characteristics, viscoelastic properties, and mechanical properties of the compounds. The silica dispersibility in the rubber compounds was improved with the addition of the nano-cellulose dispersant, resulting in the enhancement of the workability, hardness, tensile strength, and wear resistance of the SBR compound.

Synthesis and Properties of New Polymeric Photostabilizers Containing HALS Groups (HALS 그룹을 가진 새로운 고분자형 자외선 안정제의 합성 및 특성)

  • 김한식;채규호
    • Polymer(Korea)
    • /
    • v.25 no.5
    • /
    • pp.625-634
    • /
    • 2001
  • New polymeric photostabilizers containing hindered amine light stabilizer (HALS) were prepared by the reaction of liquid polyisoprene rubber grafted maleic anhydride (MAH) and 2,2,5,6-tetramethyl-4-piperidinol (TMPO). Their chemical composition and physical properties were characterized by titration, GPC and TGA analysis. The effects of polymeric HALS on the photooxidation of the styrene-butadiene rubber were studied from the UV, IR spectral changes, and photo-crosslinking was examined by the measurement of the insoluble fraction. The photooxidation of SBR upon irradiation was inhibited by addition of the new polymeric HALS. The extraction resistance of new polymeric photostabilizer was much better than that of the low molecular weight compound which is prepared by the reaction of MAH and TMPO. The new polymeric HALS ate fairly compatible with the SBR.

  • PDF

A Study in Application and Manufacture Technique of Cold-Mix Cold-Laid Type Asphalt Concrete Using of Polymer Modified Asphal (개질 아스팔트를 이용한 상온아스콘 제조 및 실용화 연구)

  • 김영근;남궁연;박유신
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1997.04a
    • /
    • pp.627-634
    • /
    • 1997
  • This is the Study on Application and Manufacture Technique of Cold-Mix, Cold-Laid type Asphalt Concrete using of Polymer modified asphalt the could be constructed easily and economically on damaged road repaireless for seasons. The modified materials for this study are SBS(Styrene-Butadiene-Styrene). SBR (Styrene-Butadiene-Rubber) and PUR(Polyurethane). The Marshall stability and the value of flow and resistance in water stability degree according to the alternation types and weight percent of modified materials were compared and evaluated on this study. The results of the study show that PUR modified asphalt have improvement of over 150% Marshall stability in AI MS-14 standard and they are evaluated to have the easiness of storage and better working efficiency compared with other types of modified asphalt compound.

  • PDF

Properties of Activated Carbon Blacks Filled SBR Rubber Composites

  • Ao, Geyou;Hu, Quanli;Kim, Myung-Soo
    • Carbon letters
    • /
    • v.9 no.2
    • /
    • pp.115-120
    • /
    • 2008
  • Rubber reinforcing carbon black N330 was treated by physical activation under $CO_2$ to different degrees of burn-off. The mechanical properties indicating the reinforcement of SBR (Styrene-Butadiene Rubber) vulcanizates filled by activated carbon blacks, such as tensile strength, modulus at 300% strain and elongation at break were determined. During $CO_2$ activation of fresh carbon blacks, the development of microporous structure caused an increase of extremely large specific surface area and the porosity turned out to be an increasing function of the degree of burn-off. The tensile strength and modulus at 300% of activated carbon blacks filled rubber composites were improved at lower loading ratios of 20 and 30 phr, but decreased drastically after 30 phr, which is considered that it might be difficult to get a fully dispersed rubber mixture at higher loading ratios for fillers having very large specific surface areas. However, the Electromagnetic Interference (EMI) shielding effectiveness of SBR rubber composites having activated carbon black at 74% yield were improved at a large extent when compared to those having raw carbon black and increased significantly as a function of increasing loading ratio.

Development of the Novel Cosmetics Impregnation Material and Study on Makeup W/O Emulsions using It (새로운 화장료 함침재의 개발과 이를 활용한 메이크업 유중수형 에멀전에 관한 연구)

  • Kang, Sungsoo;Kim, Hyeon Jeong;Oh, Se Woong;Park, Sang Wook;Kim, Kyung Seob
    • Journal of the Society of Cosmetic Scientists of Korea
    • /
    • v.43 no.1
    • /
    • pp.27-33
    • /
    • 2017
  • Up to now, better convenience and portability were important factors in the development of the cosmetics and achieved by immersing low viscosity makeup water-in-oil (W/O) emulsion into the impregnation material. Conventionally, polyurethane sponges having porous network structures and hard textures have been dominantly used. It has an advantage of easy to manufacture because of its good impregnation property due to its structural characteristics. However, it releases emulsion too much at first use, and shows unexpected dramatic decline during the period of usage. In this study, we studied on makeup W/O emulsion with various features and developed the new foaming sponge, which showed excellent formability and proper absorption and discharge ability of cosmetic composition through the combination of natural rubber (NR) and styrene butadiene rubber (SBR). This impregnation material is characterized by the softness of elasticity like a rubber, high elongation and uniform output. We confirmed that this material can be used to develop makeup products using various oils depending on polarity and controlling the viscosity of the makeup W/O emulsion. Thus, it is concluded that these results provide valuable information in developing new cosmetics impregnation materials.

Modified Silica with Cellulose/Starch by Gel-Adsorption Method as Reinforcing Materials for SBR Latex

  • Li, Xiang Xu;Cho, Ur Ryong
    • Elastomers and Composites
    • /
    • v.53 no.1
    • /
    • pp.6-12
    • /
    • 2018
  • Styrene-butadiene Rubber (SBR) Latex composites, incorporated with cellulose/starch-silica hybrids synthesized by gel-adsorption method, were filled into rubber by the latex compounding method. The structure morphology, mechanical properties, and thermodynamic properties of gel-silica hybrids were characterized. The states of hybrids which used as fillers were also characterized by SEM. As the fillers ratio increased, the difference for storage modulus of samples had been morphology by rubber process analyzer (RPA). Then, as more fillers ratio was filled into the matrix, the best tensile strength result, and the largest modulus value were also proved by UTM and RPA. As for thermal stability, increase in the ratio of fillers led to higher initial decomposition temperature, which was also proved by TGA. The swelling ratio of samples has also been characterized. From the results of all the tests, cellulose-silica hybrid showed the best results as a filler, and the best filling ratio of this hybrid is about 10 phr, which has the best storage modulus and great tensile strength.