• Title/Summary/Keyword: structural wood member

Search Result 33, Processing Time 0.016 seconds

A study on the Bending Property of Structural Size Skin-Timber (대단면 스킨팀버의 휨 성질에 관한 연구)

  • Kim, Gwang-Chul
    • Journal of the Korean Wood Science and Technology
    • /
    • v.40 no.1
    • /
    • pp.26-37
    • /
    • 2012
  • Recently, the demand and supply on the Hanok have been increased. However, Hanok should be requested larger section of structural members because of excessive roof weight. So, structural skin-timber was manufactured to get a lightweight structural member. The structural skin-timber has exterior shape with larger section but a great volume of wood be removed. The reduced strength of structural skin-timber can be supplemented by hybridizaion of structural member. Japanese larch and Domestic pine were used to manufacture the structural skin-timber. Structural skin-timbers of rectangular shape and cylinder shape were manufactured and tested to evaluate the bending properties. The intended strength property could not be obtained because member had been suffered severe damage by precision deficiency of manufacturing machine. However, if precision of manufacturing machine would be improved and additional hybridizaion of structural skin-timber would be done, lightweight structural member will be able to be manufactured. Structural skin-timber did not showed statistical significancy between two species, so it is possible to use pine mixed with larch. Only MOR of larch showed statistical significancy between rectangular shape and cylinder shape, so it is necessary to use of those as separate things. However, the rest of skin-timber can be judged mixed using because of non statistical significancy. The objective of this study was the development of lightweight larger structural member with relatively strength. If hybrid member of skin-timber could be developed with wood-ceramics, lightweight steel and more, it can be possible to be used as a building material of Hanok, interior material, post & beam construction material and more.

Difference of Deterioration According to Exposed Condition of Column in Wooden Traditional Building (노출 환경에 따른 목조 고건축물 기둥의 열화 차이)

  • Kim, Gwang-Chul;Bae, Mun-Sung;Lee, Jun-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.2
    • /
    • pp.58-68
    • /
    • 2003
  • Capacity assessment of structural member must be ahead of the safety assessment of wooden traditional building. Capacity assessment of structural member has been dependent on empirical method with visual inspection even now. Safety assessment of building, however, can be more correct and reasonable provided non-destructive evaluation technique that scientific and logic would be used to evaluate the capacity of structural member. For that purpose, non-destructive evaluation technique was applied to column among many structural members of wooden traditional building to examine the possibility of capacity assessment of structural member. And then, those data will be used as a basic data for capacity assessment of structural member in a following study. Specially, deterioration progress levels of column according to exposed condition were measured. Similar results were obtained as compared with results of visual inspection, so there was a good possibility of application for non-destructive evaluation technique.

Evalulation of Specific Gravity in Post Member by Drilling Resistance Test

  • Park, Chun-Young;Kim, Se-Jong;Lee, Jun-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.34 no.2
    • /
    • pp.1-9
    • /
    • 2006
  • The structural wooden members of the ancient building are deteriorated by fungi and termite over time. The deteriorate of the members causes the decrease of the specific gravity and the strength of it, so the stability of the building is threatened. Therefore, in this study, the evaluation of the specific gravity, which is correlated with the strength of the wood, was conducted in the post member using Nondestructive Evaluation (NDE) - Drilling Resistance Test (DRT). For the purpose of it, the specific gravity and drilling resistance of small specimens was measured to obtain the correlation between the specific gravity and the drilling resistance. And then, the drilling resistance test of the post members, which were expected to have the deteriorated parts, was performed. Consequently, the correlation between the specific gravity and the drilling resistance was very high ($R^2=0.89$) and the distributions of the specific gravity were evaluated for the each member. Also, the results were verified by the visual inspection of the cross section of it. Especially, the various variations of the wood member such as the deteriorated parts with termite or fungi and the crack could be detected exactly but the knot couldn't because the drill could pass by or could not penetrate the knot.

A Study of Modular Dome Structural Modeling with Highly Filled Extrusion Wood-Plastic Composite Member (고충진 압출성형 합성목재를 이용한 모듈러 돔의 구조모델링에 관한 연구)

  • Shon, Su-Deok;Kwak, Eui-Shin;Lee, Seung-Jae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.2
    • /
    • pp.76-83
    • /
    • 2015
  • This paper aims at developing an environmentally friendly modular dome structure system with highly filled extrusion wood-plastic composite (WPC) member, and manufacturing a real-size specimen by modularizing members and nodes. The member used in the model is the WPC member with 70% wooden fiber contests, which is higher then previous WPC one. Its members and nodes are modularized by analyzing geometric characteristics of icosahedral-based geodetic dome. Applicapability of the 6ea prototype nodes and 3ea prototype members to the modular dome is examined with the results of the modulaization and the making process for the real-size specimen. Besides, from the analysis results, the lowest buckling mode is expected to be a nodal buckling on a node near the boundary.

Investigation of Transmission Process for Ultrasonic Wave in Wood (목재 내 초음파 전달 경로 구명)

  • Lee, Jun-Jae;Kim, Gwang-Mo;Bae, Mun-Sung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.2
    • /
    • pp.31-37
    • /
    • 2003
  • Among the nondestructive evaluation (NDE) methods for wood defect detection, ultrasonic wave has been considered as competitive technique in terms of economics and workability. Until now, researches on application of NDE methods for wood have focused mainly on standing tree and logs. Recently, some attempts have been conducted with NDE technique, for evaluation of wooden structural members. However, wooden structural members are different from others (standing tree or log) in various aspects. Expecially when some parts or whole member are covered with other materials, they can't be evaluated appropriately on general NDE methods. For the purpose of development of proper NDE technique for the wooden structural members, the ultrasonic wave transmission process investigated on artificial defect in wood. First, various types of transmission process were assumed, and then the transmission times were predicted respectively. Predicted times were compared with the measured time of ultrasonic wave and then a suitable type of transmission process is determined. In case of the ultrasonic wave doesn't transmit directly due to defect, it is reflected once only at the opposite surface of member, and the path is accord with the line of shortest length.

A Study on the Estimation for the Compressive Strength of Member According to the Knot Types (옹이 형태별 소재의 압축강도 예측에 관한 연구)

  • Kim, Gwang-Chul
    • Journal of the Korean Wood Science and Technology
    • /
    • v.38 no.3
    • /
    • pp.170-177
    • /
    • 2010
  • Finite element numerical analysis was conducted with using the knot data which has a strong influence on the prediction of capacity for the structural wood member. Wood is a orthotropic property unlike other structural materials, so orthotropic property was applied. Knot was modelled as a cylinder shape, cone shape, and cubic shape. Compressive test was carried out to investigate the failure types and to calculate ultimate strengths for the wood members. Numerical model which can reflect the member size, number of knot, location of knot, size of knot was created and analyzed. By the numerical analysis using the ultimate compressive strength, numerical stress distribution types of each specimen was compared to real failure types for the test specimen. Cylinder shape modelling might be most reasonable, according to the necessary time for the analysis, the difficulty of element meshing, and the similarity of stress transfer around knot. Moreover, according to the stress and deformation distribution for the numerical analysis, failures or cracks of real specimen were developed in the vicinity of stress concentrated section and most transformed section. Based on the those results, numerical analysis could be utilized as a useful method to analyze the performance of bending member and tensile member, if only orthotropic property and knot modelling were properly applied.

A Structural Characteristics of Hwatong-Connections in Traditional Mindori Type of Wood Structures (전통 민도리식 목구조 화통맞춤의 구조적 특성)

  • Yu, Hye-Ran;Kwon, Ki-Hyuk
    • Journal of architectural history
    • /
    • v.21 no.3
    • /
    • pp.7-28
    • /
    • 2012
  • This study is intended to Mindori structure which is general private houses' structural type among traditional types and is a basic study to confirm structural characteristics of Hwatong connection which is general connection type of column-beam-cross beam. It is aimed to analyze how main member, column, such as size, figure, thickness of Sungetuk and Dugeup affect on structure. Following conclusions are drawn. 1. According to connection conditions, models with big coefficient of friction show stable hysteretic behavior until the angle rotation of member reaches 1/60 and models with small coefficient of friction show dramatical increase in load after the angle rotation of member reaches 1/24. After the angle rotation of member reaches 1/30, separation distance of members is identified physically and cracks are not observed. 2. Specimens with big coefficient of friction show similar inner force regardless of column size(except column size 150mm) and models with small coefficient of friction show increasing inner force as the column size increases. Specimens with same sectional area have similar inner force even though the column figures are different. The thickness of Sungetuk and Dugeup doesn't affect inner force greatly, however, when the thickness of Sungetuk is thin, it could lead to failure of structure as it breaks. 3. The bigger the size of column and the coefficient of friction are, the smaller Bending stiffness depreciation ratio is. 4. Energy Dissipation Efficiency differs from the coefficient of friction. When the coefficient of friction is big, square column shows bigger than round one and it is bigger when the thickness of Sungetuk and Dugeup is thicker. When the coefficient of friction is small, round column shows bigger than square one.

Determination of Ratio of Wood Deterioration Using NDT Technique

  • Lee, Jun-Jae;Bae, Mun-Sung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.32 no.3
    • /
    • pp.33-41
    • /
    • 2004
  • In ancient wooden structures, the mechanical properties of the structural members have been reduced by time-dependent degradations such as fatigue or creep. Also, the external and internal deterioration was caused by environmental condition, fungi, bacteria, or insect, and then reduced the quality of structural members. However, the previous methods for evaluating the deterioration have been mainly depended on the visual inspection. In this study, therefore, ultrasonic stress wave test, accelerometer stress wave test were used to evaluate the deterioration of structural wood members in ancient wooden structures. Based on the results, the quantitative criteria of stress wave transmitted velocity were proposed to evaluate the deterioration of structural member. The proposed criteria were related to the degree of deterioration. In accelerometer stress wave, the criteria of deterioration of wave reciprocal velocity was below 1800 ㎲/m at incipient deterioration (below 12% ratio of deterioration), between 1800 and 2200 ㎲/m at moderate deterioration (12~17%) and above 2200 ㎲/m at severe deterioration (above 17%). The ultrasonic stress wave, the criteria of deterioration were 800 and 950 ㎲/m at below 8% and above 15% of the degree of deterioration respectively.

Wood Quality and Strength Properties of Old Structural Members (목조건축 해체 고목재의 재질특성 및 강도성능)

  • Hwang, Kweonhwan;Park, Byeongsu;Park, Moon-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.36 no.1
    • /
    • pp.36-44
    • /
    • 2008
  • It is necessary to assess wood quality and strength of the clear specimens from used members in old wooden structures for the reuse of old members on the same structure or a new structure. Wood species classification by microscope observation of each wood member that was used in truss cord and temple, and several physical and strength tests by the specification of present KS standards were conducted to compare with some references. From the comparison of strengths with references, Korean larch gives relatively better wood quality and mechanical properties than other wood species. No significant deterioration of cell wall was found by microscopic observation for the sound wood part that was selected visually. Tensile specimens with 3 mm in thickness on the middle span showed greater strength than 5 mm thick specimens, which explains that dimension of tensile specimen should be examined for evaluating precise tensile strength properties. Other tests, compression, shear, and bending, are adoptable for each strength properties. Test methods for the evaluation of basic strengths and fastener connections for old wood species should be further examined.

Effect of Cross-Sectional Dimension on the Shrinkage Property of Korean Red-Pine Wood (소나무재의 단면치수에 따른 수축률 특성)

  • Hwang, Kweonhwan;Park, Beyung-Su
    • Journal of the Korean Wood Science and Technology
    • /
    • v.37 no.3
    • /
    • pp.231-238
    • /
    • 2009
  • Red pine (Pinus densiflora) has been used for structural wood members of Korean traditional residence (HANOK) and historic wooden structures. For these constructions, generally, natural drying has conducted for long time; however, unless drying is conducted sufficiently, it could cause several drying defects such as check or warping. Shrinkage changes of red pine species for small clear specimens and big-size specimens according to the conditions of moisture contents, were examined. For the estimation of volumetric shrinkage at a special moisture content, it was more precise to divide the range of moisture contents into two groups, green to air-dry and air-dry to oven-dry. The volumetric shrinkage had no difference with specimen sizes in sapwood, but decreased as specimen size increased in heartwood.