• Title/Summary/Keyword: strength reduction technology

검색결과 788건 처리시간 0.037초

1.2GPa급 초고강도강판의 단면 형태에 따른 스프링백에 관한 해석적 평가 및 연구 (Analytical evaluation and study on the springback according to the cross sectional form of 1.2GPa ultra high strength steel plate)

  • 이동환;한성렬;이춘규
    • Design & Manufacturing
    • /
    • 제13권4호
    • /
    • pp.17-22
    • /
    • 2019
  • Currently, studies on weight reduction and fuel efficiency increase are the most important topics in the automotive industry and many studies are under way. Among them, weight reduction is the best way to raise fuel efficiency and solve environmental pollution and resource depletion. Materials such as aluminum, magnesium and carbon curing materials can be found in lightweight materials. Among these, research on improvement of bonding technology and manufacturing method of materials and improvement of material properties through study of ultrahigh strength steel sheet is expected to be the biggest part of material weight reduction. As the strength of the ultra hight strength steel sheet increases during forming, it is difficult to obtain the dimensional accuracy as the elastic restoring force increases compared to the hardness or high strength steel sheet. It is known that the spring back phenomenon is affected by various factors depending on the raw material and processing process. We have conducted analytical evaluations and studies to analyze the springback that occurs according to the cross-sectional shape of the ultra high tensile steel sheet.

초기(初期) 갈색부후(褐色腐朽)에 따른 라디에타소나무의 역학적(力學的) 성질(性質) 감소(減少) (Reduction in Mechanical Properties of Radiata Pine Wood Associated with Incipient Brown-Rot Decay)

  • 김규혁;지우근;나종범
    • Journal of the Korean Wood Science and Technology
    • /
    • 제24권1호
    • /
    • pp.81-86
    • /
    • 1996
  • This study was performed to evaluate the reduction in bending properties of radiata pine sapwood associated with incipient brown-rot decay. Decayed bending specimens by Tyromyces palustris and Gloeophyllum trabeum for varoious periods were tested destructively. Brown-rot decay by T. palustris and G. trabeum caused serious reduction in bending properties at very early stages of decay, with about 30 percent decrease in bending strength observed for only 1~2 percent weight loss. In general, the reduction in bending properties caused by T. palustris was somewhat greater than that by G. trabeum. Work to maximum load was reduced most severely and rapidly from the onset of decay, while modulus of elasticity showed a much more moderate rate of reduction. Modulus of rupture was affected by decay to a greater extent than was modulus of elasticity. Since a relatively strong correlation between weight loss and bending strength was observed, the residual strength of decayed wood can be predicted by weight loss due to decay. The results of this study indicate that very early stages of brown-rot decay reduce the bending strength significantly. Thus, it is recommended that all load-bearing members in wooden structures, especially those that are periodically wetted, should be inspected regularly to prevent a sudden failure even though there are no definite signs of decay.

  • PDF

Seismic structural demands and inelastic deformation ratios: a theoretical approach

  • Chikh, Benazouz;Mebarki, Ahmed;Laouami, Nacer;Leblouba, Moussa;Mehani, Youcef;Hadid, Mohamed;Kibboua, Abderrahmane;Benouar, Djilali
    • Earthquakes and Structures
    • /
    • 제12권4호
    • /
    • pp.397-407
    • /
    • 2017
  • To estimate the structural seismic demand, some methods are based on an equivalent linear system such as the Capacity Spectrum Method, the N2 method and the Equivalent Linearization method. Another category, widely investigated, is based on displacement correction such as the Displacement Coefficient Method and the Coefficient Method. Its basic concept consists in converting the elastic linear displacement of an equivalent Single Degree of Freedom system (SDOF) into a corresponding inelastic displacement. It relies on adequate modifying or reduction coefficient such as the inelastic deformation ratio which is usually developed for systems with known ductility factors ($C_{\mu}$) and ($C_R$) for known yield-strength reduction factor. The present paper proposes a rational approach which estimates this inelastic deformation ratio for SDOF bilinear systems by rigorous nonlinear analysis. It proposes a new inelastic deformation ratio which unifies and combines both $C_{\mu}$ and $C_R$ effects. It is defined by the ratio between the inelastic and elastic maximum lateral displacement demands. Three options are investigated in order to express the inelastic response spectra in terms of: ductility demand, yield strength reduction factor, and inelastic deformation ratio which depends on the period, the post-to-preyield stiffness ratio, the yield strength and the peak ground acceleration. This new inelastic deformation ratio ($C_{\eta}$) is describes the response spectra and is related to the capacity curve (pushover curve): normalized yield strength coefficient (${\eta}$), post-to-preyield stiffness ratio (${\alpha}$), natural period (T), peak ductility factor (${\mu}$), and the yield strength reduction factor ($R_y$). For illustrative purposes, instantaneous ductility demand and yield strength reduction factor for a SDOF system subject to various recorded motions (El-Centro 1940 (N/S), Boumerdes: Algeria 2003). The method accuracy is investigated and compared to classical formulations, for various hysteretic models and values of the normalized yield strength coefficient (${\eta}$), post-to-preyield stiffness ratio (${\alpha}$), and natural period (T). Though the ductility demand and yield strength reduction factor differ greatly for some given T and ${\eta}$ ranges, they remain take close when ${\eta}>1$, whereas they are equal to 1 for periods $T{\geq}1s$.

Research on the mechanical properties of membrane connections in tensioned membrane structures

  • Zhang, Yingying;Zhang, Qilin;Li, Yang;Chen, Lu
    • Structural Engineering and Mechanics
    • /
    • 제49권6호
    • /
    • pp.745-762
    • /
    • 2014
  • As an important part, the connections generally are important for the overall behavior of the structure and the strength and serviceability of the connection should be ensured. This paper presents the mechanical properties of membrane connections in tensioned membrane structure. First, the details of common connections used in the membrane structure are introduced. Then, the common connections including membrane seam, membrane-flexible edge connection and membrane-rigid edge connection are tested and the corresponding failure mechanisms are discussed. Finally, the effects of connection parameters on the connection strength are investigated and proper connection parameters are proposed. The strength reduction factors corresponding to different connection types are proposed, which can be references for the design and analysis of membrane structures.

철강 압연제품의 제조기술 및 응용 (Manufacturing Technologies and Applications of Steel Strip Products)

  • 권오준
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 제3회 압연심포지엄 논문집 압연기술의 미래개척 (Exploitation of Future Rolling Technologies)
    • /
    • pp.10-21
    • /
    • 1999
  • Recent progress in manufacture of hot and cold rolled steel strip products and their applications were reviewed. The main trend in the technological development has been to meet the customers' requests for quality improvement and cost reduction. The weight reduction to reduce the fuel consumption is the main issue in the automotive industry and, therefore, various steels have been developed to improve formability as well as strength. The steels include super-EDDQ steels, bainitic steels, TRIP steels, etc. In the oil industry, efforts have been focused to improve strength together with either low temperature toughness or HIC/SSCC resistance. The packaging industry is also a highly competitive market, and steel and canmaking companies have worked cooperatively to develop cost-effective canmaking processes as well as high performance steels. This type of cooperation has also been found important in other industries such as the appliance and electronic industries for the benefits of both steelmakers and customers.

  • PDF

띠형 섬유보강재의 장기성능 평가를 위한 실험적 연구 (Experimental Study on Long-Term Performance Evaluation of Geosynthetic Strip Reinforcement)

  • 이광우;김주형;조삼덕;한중근;윤원일;홍기권
    • 한국지반신소재학회논문집
    • /
    • 제9권4호
    • /
    • pp.75-84
    • /
    • 2010
  • 본 연구에서는 띠형 섬유보강재의 인장특성, 크리프 변형, 내시공성 및 내구성을 평가하기 위한 일련의 장기성능 평가시험을 수행하였다. 또한 시험결과를 바탕으로 장기설계인장강도 산정을 위한 강도감소계수를 평가하였다. 먼저, 크리프 변형 특성을 평가하기 위해 단계 등온법과 시간-온도 중첩법을 이용하였으며, 크리프 감소계수는 1.6을 적용하는 것이 바람직한 것으로 평가되었다. 다음으로 입도 조정된 화강풍화토를 성토재로 사용하여 수행한 내시공성 시험 결과, 보강재의 강도특성에 영향을 미치는 원사의 손상이 거의 없는 것으로 확인되어, 장기설계인장강도에 큰 영향을 미치지 않을 것으로 분석되었다. 마지막으로 내구성 평가 결과, 내화학성, 내미생물 및 내후성을 고려한 강도감소계수는 1.1을 적용하는 것이 합리적인 것으로 평가되었다.

  • PDF

감수제의 감수 효율에 따른 다성분계 결합재를 사용한 콘크리트의 물리적 특성에 관한 기초적 연구 (A Study on the Physical Characteristics of Concrete using Multi-Component Blended Binder According to Warter Reduction Efficiency of Warter Reduction Agent)

  • 김경환;오성록;최병걸;최연왕
    • 콘크리트학회논문집
    • /
    • 제27권5호
    • /
    • pp.559-568
    • /
    • 2015
  • 본 연구에서는 감수제의 감수 효율에 따른 다성분계 결합재를 사용한 콘크리트의 물리적 특성에 대한 영향을 평가하기 위하여 고성능 감수제의 종류 3수준(0%, 8% 및 16%) 및 물-결합재비 3수준(40%, 45% 및 50%)에 따른 플라이애시 및 고로슬래그 미분말을 사용한 다성분계 콘크리트 배합을 제조하였다. 또한, 신뢰성 확보를 위하여 콘크리트 배합은 3회 반복실험을 실시하였다. 실험결과, 감수제 종류에 따른 압축강도는 약 20% 이상의 압축강도 차이가 발생하였으며, 감수제의 감수 효율이 콘크리트의 품질에 크게 영향을 미치는 것으로 나타났다. 따라서 감수제의 감수 효율을 반영한 다성분계 콘크리트의 압축강도 예측 모델식을 도출하였으며, 90% 이상의 높은 상관성이 있는 것으로 나타났다.

Using scratch test to evaluate cohesive bond strength of Mo composite coating

  • Koiprasert, Hathaipat;Thaiwatthana, Sirinee;Sheppard, Panadda
    • International Journal of Advanced Culture Technology
    • /
    • 제3권2호
    • /
    • pp.34-41
    • /
    • 2015
  • Bonding strength of a thermal sprayed coating is difficult to measure using a conventional pull-off test method. Scratch test is a potential alternative testing method. An adhesive and a cohesive bond strength of the coating can be measured by the pull-off test while the scratch test performed on the cross-section of the thermal sprayed coating can only demonstrate the cohesive bond strength of the coating. Nevertheless, it is still beneficial to perform the scratch testing on the cross-section of the coating for the sake of comparison thus providing an alternative to the pull-off test. The scratch test method can reduce testing time and cost in the long run due to a significant cost reduction in consumables and energy and time saving from the curing step of the glue used in the pull-off test. This research investigates the possibility of using the scratch test to measure the cohesive bond strength of Mo/NiCrBSi composite coating. The results from the pull-off test and the scratch test indicate that the cohesive bond strengths of the Mo composite coating show similar trend and that the cohesive bond strength are increased when increasing NiCrBSi content.

Performance of eco-friendly mortar mixes against aggressive environments

  • Saha, Suman;Rajasekaran, Chandrasekaran;Gupta, Prateek
    • Advances in concrete construction
    • /
    • 제10권3호
    • /
    • pp.237-245
    • /
    • 2020
  • Past research efforts already established geopolymer as an environment-friendly alternative binder system for ordinary Portland cement (OPC) and recycled aggregate is also one of the promising alternative for natural aggregates. In this study, an effort was made to produce eco-friendly mortar mixes using geopolymer as binder and recycled fine aggregate (RFA) partially and study the resistance ability of these mortar mixes against the aggressive environments. To form the geopolymer binder, 70% fly ash, 30% ground granulated blast furnace slag (GGBS) and alkaline solution comprising of sodium silicate solution and 14M sodium hydroxide solution with a ratio of 1.5 were used. The ratio of alkaline liquid to binder (AL/B) was also considered as 0.4 and 0.6. In order to determine the resistance ability against aggressive environmental conditions, acid attack test, sulphate attack test and rapid chloride permeability test were conducted. Change in mass, change in compressive strength of the specimens after the immersion in acid/sulphate solution for a period of 28, 56, 90 and 120 days has been presented and discussed in this study. Results indicated that the incorporation of RFA leads to the reduction in compressive strength. Even though strength reduction was observed, eco-friendly mortar mixes containing geopolymer as binder and RFA as fine aggregate performed better when it was produced with AL/B ratio of 0.6.

Assessment of lightweight recycled crumb rubber-cement composite produced by preplaced method

  • Shah, Syed Nasir;Mo, Kim Hung;Yap, Soon Poh;Putra, Azma;Othman, Muhammad Nur
    • Advances in concrete construction
    • /
    • 제11권5호
    • /
    • pp.409-417
    • /
    • 2021
  • The incorporation of non-biodegradable tyre waste in cement-based material has gained more interest towards sustainable construction these days. Crumb rubber (CR) from waste tyre is an alternative for sand replacement in low strength applications. Many researchers have studied CR cement-based materials produced by normal mixing (NM) method and reported a significant decrease in compressive strength due to CR. To compensate this strength loss, this research aims to study the innovative incorporation of CR in cement composite via the preplaced mixing (PM) method. In this investigation, cement composite was produced with NM and PM methods by replacing sand with 0%, 50%, and 100% CR by volume. The test results showed no significant difference in terms of densities of cement composite prepared with both mixing methods. However, cement composite prepared with PM method had lower strength reduction (about 10%) and lowered drying shrinkage (about 20%). In addition, the sound absorption coefficient and noise reduction coefficient of CR cement composite prepared by PM method were in similar range as those prepared with NM method. Overall, the results demonstrate that the PM method is promising, and the maximum replacement level of 50% is recommended for CR in the cement composite.