• 제목/요약/키워드: strength at short

검색결과 367건 처리시간 0.027초

플레이트거더 용접구조상세의 피로거동에 관한 연구 (A Study on the Fatigue Behavior of the Welded Structural Details in Plate Girder)

  • 이명구;이승용
    • 한국안전학회지
    • /
    • 제23권2호
    • /
    • pp.14-20
    • /
    • 2008
  • The objective of this study is to examine fatigue strength of the welded details. In order to attain the goal of this study, the bending fatigue tests was performed for four kinds of welded details used in steel bridges, such as in-plane gusset, out-of-plane gusset, cruciform, and cover plate. The effect of the length of welded attachment on fatigue strength was greater in out-of-plane gusset than in in-plane gusset. The fatigue strength of welded details with short attachment was superior to that with long attachment. Fatigue strength of welded details with transversely loaded welds was lower than that with longitudinally loaded welds, and those results were not satisfied with AASHTO specifications. For the fatigue strength of cover plate, cover plate with rectangular section was superior to that with tapered section. It was found that the fatigue crack initiates at the points of stress concentration which are the boundary between the base metal and the bead of weld in the part of the longitudinal edge of attachment, and propagates first along the boundary and along the perpendicular to the direction of the principle stress in the base metal of welded tip.

Zircaloy-4에서 산화가 기계적 성질에 미치는 영향에 대한 연구 (A Study of the Effect of Oxidation on the Mechanical Properties of Zircaloy-4)

  • 고진현;김상호;황용화
    • 한국표면공학회지
    • /
    • 제35권5호
    • /
    • pp.312-318
    • /
    • 2002
  • A study on the change of mechanical properties and oxidation behavior of Zircaloy-4 fuel cladding after exposing at 90$0^{\circ}C$ and $1000^{\circ}C$ for various periods of exposure time under the steam atmosphere was carried out. The growth of the $ZrO_2$ layer combined with an oxygen-rich-phase layer into the Zircaloy tube material can be described by an expression, E = 1.1√Dt + $2 $\times$ 10^{-4}$ . The tensile strength of Zircaloy tubes increased for a short period of exposure time and decreased rapidly with further exposure while the hoop strength was not decreased greatly. In the meantime, the axial and circumferential elongations of oxidized Zircaloy tubes were decreased drastically with increasing exposure time as a result of embrittlement phenomena.

저탄소 박판 강재의 Nd:YAG 레이저 용접부 형성에 미치는 공정변수의 영향 (Effect of Process Parameters on Bead Formation in Nd:YAG Laser Welding of Thin Steels)

  • 김기철;허재협
    • Journal of Welding and Joining
    • /
    • 제19권3호
    • /
    • pp.317-324
    • /
    • 2001
  • This study deals with high power Nd:YAG laser welding of thin steels for small pressure vessels. Full penetration welding at the overlap joint was performed so as to assure sufficient weld strength. Results showed that mid-depth weld size reduced drastically with increasing the travel speed. Position of focus had little effect on the bead formation even though short focal system was used. However, the shape factor and the bead width had closely related with the position of focus. Based on the microstructural inspection, acceptable weld was obtained when the overlap clearance was controlled up to 20% of the base metal thickness. In the case that the joint contained more clearance than the critical value, both the tensile shear strength and the tear strength were reduced. Results also demonstrated that shielding gases were proved to play a key role as far as the bead formation characteristics was taken into consideration. Blowing dry air through 5mm in diameter nozzle produced narrower bead cross-section than that of argon or nitrogen shielding.

  • PDF

Interaction of Tip Vortices Generated by a Split Wing

  • Youn, Won Suk;Han, Yong Oun;Lee, Dong Yeon
    • International Journal of Aeronautical and Space Sciences
    • /
    • 제2권2호
    • /
    • pp.39-45
    • /
    • 2001
  • To reduce the strength of tip vortex of the fixed wing, a horizontal wing-let splitted into two parts was utilized, and the interaction between vortices generated by these wing-lets was investigated by the hot-wire anemometry. The process of vortex forming and merging was clarified by measurements of velocity vectors and their contours at five downstream cross-sections; 0.05C(chord length), 0.2C, 0.5C, 1.0C and 2.0C. Both vortex-lets formed by each wing-lets rotate counterclockwise and merge into a larger single vortex within a short downstream distance, 0.5C in this case. The strength of the merged tip vortex turned out to become smaller than that of the plain wing tip near the vortex core.

  • PDF

Experimental and analytical investigation of the shear behavior of strain hardening cementitious composites

  • Georgiou, Antroula V.;Pantazopoulou, Stavroula J.
    • Structural Engineering and Mechanics
    • /
    • 제72권1호
    • /
    • pp.19-30
    • /
    • 2019
  • The mechanical behavior of Fiber Reinforced Cementitious Composites (FRCC) under direct shear is studied through experiment and analytical simulation. The cementitious composite considered contains 55% replacement of cement with fly ash and 2% (volume ratio) of short discontinuous synthetic fibers (in the form of mass reinforcement, comprising PVA - Polyvinyl Alcohol fibers). This class of cementitious materials exhibits ductility under tension with the formation of multiple fine cracks and significant delay of crack stabilization (i.e., localization of cracking at a single location). One of the behavioral parameters that concern structural design is the shear strength of this new type of fiber reinforced composites. This aspect was studied in the present work with the use of Push-off tests. The shear strength is then compared to the materials' tensile and splitting strength values.

Novel approach to improve nano green mortar behaviour using nano-paper waste with nano-metakaolin

  • Radwa Defalla Abdel, Hafez;Bassam A., Tayeh;Raghda Osama Abd-Al, Ftah;Khaled, Abdelsamie
    • Advances in concrete construction
    • /
    • 제14권5호
    • /
    • pp.341-354
    • /
    • 2022
  • Treatment of solid waste building materials is a crucial method of disposal and an area of ongoing research. New standards for the treatment of solid waste building materials are necessary due to multisource features, huge quantities, and complicated compositions of solid waste. In this research, sustainable nanomaterial mixtures containing nano-paper waste (NPW) and nano-metakaolin (NMK) were used as a substitute for Portland cement. Portland cement was replaced with different ratios of NPW and NMK (0%, 4%, 8%, and 12% by weight of cement) while the cement-to-water ratio remained constant at 0.4 in all mortar mixtures. The fresh properties had a positive effect on them, and with the increase in the percentage of replacement, the fresh properties decreased. The results of compressive strength at 7 and 28 days and flexural strength at 28 days show that the nanomaterials improved the strength, but the results of NMK were better than those of NPW. The best replacement rate was 8%, followed by 4%, and finally 12% for both materials. The combination of NMK and NPW as a replacement (12% NMK + 12% NPW) showed less shrinkage than the others because of the high pozzolanic reactivity of the nanomaterials. The combination of NMK and NPW improved the microstructure by increasing the hydration volume and lowering the water in the cement matrix, as clearly observed in the C-S-H decomposition.

시편 크기 및 시험속도가 단섬유 강화 클로로프렌 고무의 관통 특성에 미치는 영향 (Effects of Specimen Size and Testing Velocity on Puncture Properties of Short-fiber Reinforced Chloroprene Rubber)

  • 류상렬;이동주
    • Composites Research
    • /
    • 제20권6호
    • /
    • pp.28-33
    • /
    • 2007
  • 단섬유 강화고무의 관통 특성에 대해 섬유 종횡비(AR: 섬유 길이/섬유 직경), 섬유 함유량, 시편 크기 그리고 시험속도를 변수로 하여 연구하였다. 기지와 단섬유 강화고무의 관통 저항은 시편 크기의 증가에 따라 감소하였고, 동일한 시편 크기에서 시험 속도의 증가에 따라 관통 저항력은 증가하였다. 각각의 섬유 함유량에서 섬유 종횡비가 클수록 높은 관통응력 값을 보였다. 인장강도와 관통응력의 비교를 통해 시편 형상의 문제점에 대해 고찰하였다. 기지와 단섬유 강화고무의 막에 작용하는 힘은 시편의 크기에 관계없이 유사한 값을 보였고, 동일한 시편 크기에서 시험속도의 증가에 따라 증가하였다. 각각의 섬유함유량에서 섬유 종횡비가 클수록 막에 작용하는 힘은 크게 나타났다 전체적으로 시편 크기, 시험속도가 단섬유 강화고무의 관통 특성에 지대한 영향을 미침을 확인하였다.

페리이트의 총형 연삭에서 전착 다이아몬드 연삭숫돌의 최적 연삭조건 (Optimum Grinding Condition for Electroplated Diamond Wheel in Form Grinding of Ferrite)

  • 김성청;이재우;김관우;한상욱;황선희
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1996년도 춘계학술대회 논문집
    • /
    • pp.29-33
    • /
    • 1996
  • This paper aims to clatify the potimum grinding condition for the electroplated diamond wheel in form grinding of Sr-ferrite. The main conclusions obtained were as follows. (1) The flexural strength and surface roughness of ferrite became the highest at the peripheral wheel speed of 1700m/min. (2) In the case of depth of cut larger than 0.4mm, crack layers is induced in the ground surface, the fracture type of chips exhibits slight ductile mode in the depth of cut smaller than 0.2mm. (3) When the depth of cut exceed 0.6mm, the tool life becomes extermely short due to large chipping and brackage. However, at the depth of cut .geq. 0.05mm, the diamond grain shows abrasive wear. (4) The flexural strength and surface roughness increases in proportion to the feed rate.

  • PDF

Influence of strong ground motion duration on reinforced concrete walls

  • Flores, Camilo;Bazaez, Ramiro;Lopez, Alvaro
    • Earthquakes and Structures
    • /
    • 제21권5호
    • /
    • pp.477-487
    • /
    • 2021
  • This study focuses on the influence of strong ground motion duration on the response and collapse probability of reinforced concrete walls with a predominant response in flexure. Walls with different height and mass were used to account for a broad spectrum of configurations and fundamental periods. The walls were designed following the specifications of the Chilean design code. Non-linear models of the reinforced concrete walls using a distributed plasticity approach were performed in OpenSees and calibrated with experimental data. Special attention was put on modeling strength and stiffness degradation. The effect of duration was isolated using spectrally equivalent ground motions of long and short duration. In order to assess the behavior of the RC shear walls, incremental dynamic analyses (IDA) were performed, and fragility curves were obtained using cumulative and non-cumulative engineering demand parameters. The spectral acceleration at the fundamental period of the wall was used as the intensity measure (IM) for the IDAs. The results show that the long duration ground motion set decreases the average collapse capacity in walls of medium and long periods compared to the results using the short duration set. Also, it was found that a lower median intensity is required to achieve moderate damage states in the same medium and long period wall models. Finally, strength and stiffness degradation are important modelling parameters and if they are not included, the damage in reinforced concrete walls may be greatly underestimated.

고온을 받은 고강도 콘크리트의 강도특성 (Strength Properties of High-Strength Concrete Exposed at High Temperature)

  • 윤현도;김규용;한병찬
    • 콘크리트학회논문집
    • /
    • 제14권5호
    • /
    • pp.698-707
    • /
    • 2002
  • 본 연구에서는 건축물에 발생된 화재와 같이 단기간에 빠르게 가열되는 조건하에 고강도 콘크리트의 압축강도특성을 구명하기 위하여 기존의 내화실험결과를 수집 및 분석하며 아울러 현행 노출온도에 따른 압축강도의 상관관계 기준식의 고강도 콘크리트에 적용 가능성을 검토하고자 한다. 노출온도에 따른 고강도 콘크리트의 압축강도 변화 특성은 내화실험방법(재하, 비재하 및 비재하 잔여 강도실험) 및 골재종류(천연 및 경량골재)에 따라 다르게 나타나므로 실험방법 및 골재종류별로 나누어 비교 및 분석하였다. 고강도 콘크리트의 압축강도 특성은 보통강도와는 노출온도에 따라 다르게 나타났으며 노출온도 약 2$0^{\circ}C$에서 40$0^{\circ}C$범위에서 보통강도 콘크리트보다 급격하게 압축강토가 저하되었으며 40$0^{\circ}C$ 이상에서는 큰 차이를 보이지 않았다. 80$0^{\circ}C$에서 고강도 콘크리트의 압축강도는 상온 압축강도의 30%까지 감소되었다. 노출온도에 따른 압축강도 및 탄성계수 변화에 대한 실험결과와 유럽 기준을 비교하여 볼 때 현행 기준식은 안전측이지 못하므로 화재에 노출된 고강도 콘크리트의 압축강토 및 탄성계수 평가에 적응 가능성이 결여된 것으로 평가되었다.