• Title/Summary/Keyword: strain-hardening

Search Result 847, Processing Time 0.025 seconds

A Study on the Suitability of the Mohr-Coulomb Model for Numerical Analysis of Ground Excavation (지반굴착 시 Mohr-Coulomb 모델 적합성에 관한 수치해석적 분석)

  • Lee, Jonghyun;Jin, Hyunsik;An, Joonsang;Baek, Yong;Yoon, Hyeongsuk
    • The Journal of Engineering Geology
    • /
    • v.30 no.1
    • /
    • pp.1-15
    • /
    • 2020
  • The Mohr-Coulomb model is mainly used in evaluating the behavior of the ground in numerical analyses of domestic ground excavation. This study analyzes its limitations and compares its numerical results with the hyperbolic model, a model that closely follows actual ground behavior during excavation. Recent applications of the Mohr-Coulomb model in Korea have tended to impose arbitrary special boundary conditions to control the problem of excessive heaving of the ground excavation surface. This adjustment only controls the size of the heaving of the excavation surface, implying that the ground behavior is distorted from the actual behavior. This study compares results from the hyperbolic model (hardening soil model) and the Mohr-Coulomb model, and confirms that the hyperbolic model provides both a more-suitable solution to the problem of heaving during excavation and the actual stress-strain behavior. In numerical analyses of ground excavation, the hyperbolic model is expected to give results consistent with the actual ground behavior.

A Study on the Precipitation Behavior of Carbide Particle in L12-type Intermetallic Compound Ni3Al (L12형 금속간화합물 Ni3Al중에 탄화물입자의 석출거동에 관한 연구)

  • Han, Chang-Suk;Koo, Kyung-Wan;Oh, Dong-Cheol
    • Korean Journal of Materials Research
    • /
    • v.16 no.4
    • /
    • pp.241-247
    • /
    • 2006
  • Structural studies have been performed on precipitation hardening discovered in $L1_2-ordered\;Ni_3(Al,Cr)$ containing 0.2 to 3.0 mol% of carbon using transmission electron microscopy (TEM). Fine octahedral precipitates of $M_{23}C_6$ appeared in the matrix by aging at temperatures around 973 K after solution treatment at 1423 K. TEM examination revealed that the $M_{23}C_6$ phase and the matrix lattices have a cube-cube orientation relationship and keep partial atomic matching at the {111} interface. After prolonged aging or by aging at higher temperatures, the $M_{23}C_6$ precipitates then adopt a rod-like morphology elongated parallel to the <100> directions. Deformation at temperature below 973 K, typical Orowan loops were observed surrounding the $M_{23}C_6$ particles. At higher deformation temperatures, the Orowan loops disappeared and the morphology of dislocations at the particle-matrix interfaces suggested the existence of attractive interaction between dislocations and particles. The change of the interaction modes between dislocation and particles with increasing deformation temperature can be considered as a result of strain relaxation at the interface between matrix and particles.

Characterization of Aluminum Coated Layer in Hot Press Forming of Boron Steel (고온 프레스성형시 보론강 알루미늄 코팅층 거동특성)

  • Jang, Jeong-Hwan;Joo, Byeong-Don;Lee, Jae-Ho;Moo, Young-Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.21 no.4
    • /
    • pp.183-188
    • /
    • 2008
  • Hot press forming allows geometrically complicated parts to be formed from sheet and the rapid cooling hardens them to extremely high strength. The main purpose of this research is to characterize Al coated layer in Al coated boron steel during hot press forming. For the hot press hardening experiment, test specimens were heated up to $810{\sim}930^{\circ}C$ and held for 3, 6 and 9 minutes, respectively. And then, some specimens were press hardened and others were air-cooled without any pressing for the comparison purpose. Al coated layer shows four distinct micro-structural regions of interest; diffusion zone, Al-Fe zone(I) low-Al zone(LAZ) and Al-Fe zone(II). Band-like LAZ is clearly shown at temperature ranges of $810{\sim}870^{\circ}C$ and sparsely dispersed at temperature higher than 900oC. The micro-cracking behavior in the Al coated layer during forming were also analyzed by bending and deep drawing tests. The strain concentration in softer LAZ is found to be closely related with micro-cracking and exfoliation in coated layer during forming.

An Experimental Study on Tensile Properties of Steel Fiber-Reinforced Ultra High Strength Concrete (강섬유 보강 초고강도 콘크리트의 인장 특성 실험 연구)

  • Yang, In-Hwan;Park, Ji-Hun;Lee, Jae-Ho
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.3
    • /
    • pp.279-286
    • /
    • 2019
  • In this study, an experimental study on the tensile properties of steel fiber-reinforced ultra high strength concrete(UHSC) with a standard compressive strength of 180MPa was performed. Steel fibers with a volume ratio of 1% were mixed to prepare direct tensile strength specimens and prism specimens for the three-point bending test. The fabricated specimens were set up in the middle section of the specimen to induce cracks, and the test was carried out according to each evaluation method. First, the stress-strain curves were analyzed by performing direct tensile strength tests to investigate the behavior characteristics of concrete after cracking. In addition, the load-CMOD curve was obtained through the three-point bending test, and the inverse analysis was performed to evaluate the stress-strain curve. Tensile behavior characteristics of the direct tensile test and the three-point bending test of the indirect test were similar. In addition, the tensile stress-strain curve modeling presented in the SC structural design guidelines was performed, and the comparative analysis of the measured and predicted values was performed. When the material reduction factor of 1.0 was applied, the predicted value was similar to the measured value up to the strain of 0.02, but when the material reduction factor of 0.8 was applied, the predicted value was close to the lower limit of the measured value. In addition, when the strain was greater than 0.02, the predicted value by SC structural design guideline to underestimated the measured value.

Mechanical Properties of Strain-Hardening Cement Composites(SHCCs) according to the Water-Cement Ratio (물시멘트비에 따른 변형경화형 시멘트 복합체의 역학적 특성)

  • Kim, Yun-Su;Jang, Yong-Heon;Jang, Gwang-Su;Jeon, Esther;Yun, Hyun-Do;Kim, Keung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.11a
    • /
    • pp.465-468
    • /
    • 2008
  • SHCCs (Strain Hardening Cement Composites) show the high energy tolerance capacity due to the interfacial bonding of the fibers to the cement matrix. For effective material design and application of SHCCs, it is needed to investigate the compression, four-point bending, direct tensile response of SHCCs with different types of fibers and water-cement ratio. For these purposes, three kinds of fibers were used: PP(polypropylene, 2.0%), PVA(Polyvinyl alcohol, 2.0%), PE (Polyethylene, 1.0%). Also, effects of water-cement ratio(0.45, 0.60) on the SHCCs were evaluated in this paper. As the result of test, SHCCs with PVA and PE fiber were showed better overall behavior than specimens with PP fibers on bending and direct tensile test. Also, for the same type of fiber, SHCCs with water-cement ratio of 0.45 exhibited higher ultimate strength than specimen with water-cement ratio of 0.60 on compression strength, and showed the multiple cracking on bending and direct tensile test. Therefore, to improve of workability and dispersibility of SHCCs on water-cement ratio of 0.60, continual studies were needed.

  • PDF

A Study on the Cyclic Hardening Property and the Low Cycle Fatigue Behavior of Marine Materials (박용재료(舶用材料)의 반복경화(反復硬化) 및 저(低)싸이클 피로특성(疲勞特性)에 관한 연구)

  • S.M. Cho;K. Horikawa
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.28 no.1
    • /
    • pp.108-116
    • /
    • 1991
  • In the non-linear behavior of many materials, there is difference between the monotonic behavior by static load and the cyclic behavior by cyclic load. In particular, the short fatigue cracks to propagate in elasto-plastic stress concentrations(notches), are governed significantly by the cyclic behavior of materials. Accordingly, it is needed to investigate and compare the monotonic and cyclic behavior of materials. In the pressent study, the stress-strain relations of materials by monotonic and cyclic load tests were examined for 2 kinds of steels(SS41, HT80) and 5 kinds of Al-alloys(A5083-O, A6N01-T5, A7N01-T4, A7016-T6, A7178-T6). And the constants for mechanical properties of the materials were determined by experimental results, Moreover, when a notch was subjected to cyclic load, the effect of cyclic hardening property of materials on the variation of stress-strain amplitude in the notch tip was discussed by the application of Neuber's rule and experiments for a center notched plate.

  • PDF

The Widening of Fault Gouge Zone: An Example from Yangbuk-myeon, Gyeongju city, Korea (단층비지대의 성장: 경주시 양북면 부근의 사례)

  • Chang, Tae-Woo;Jang, Yun-Deuk
    • The Journal of Engineering Geology
    • /
    • v.18 no.2
    • /
    • pp.145-152
    • /
    • 2008
  • A fault gouge zone which is about 25cm thick crops out along a small valley in Yangbuk-myeon, Gyeongju city. It is divided into greenish brown gouge and bluish gray gouge by color. Under the microscope, the gouges have a lot of porphyroclasts composed of old gouge fragments, quartz, feldspar and iron minerals. Clay minerals are abundant in matrix, defining strikingly P foliation by preferred orientation. Microstructural differences between bluish pay gouge and greenish brown gouge are as follows: greenish brown gouge compared to bluish gray gouge is (1) rich in clay minerals, (2) small in size and number of porphyroclasts, and (3) plentiful in iron minerals which are mostly hematites, while chiefly pyrites in bluish gray gouge. Hematites are considered to be altered from pyrites in the early-formed greenish brown gouge under the influence of hydrothermal fluids accompanied during the formation of bluish gray gouge that also precipitated pyrites. It is believed that the fault core including bluish gray gouge zone and greenish brown gouge zone was formed by progressive cataclastic flow. In the first stage the fault core initiates from damage zone of early faulting. In the second stage damage zone actively transforms into breccia zone by repeated fracturing. The third stage includes greenish brown (old) gouge formation in the center of the fault core mainly by particle grinding. In the third stage further deformation leads to the formation of new (bluish gray) gouge zone while old gouge zone undergoes strain hardening. Consequently, the whole gouge zone in the core widens.

Flexural Experiments on Reinforced Concrete Beams Strengthened with SHCC and Special Reinforcements (SHCC와 특수 보강근으로 보강된 철근콘크리트 보의 휨 성능 실험)

  • Chang-Jin Hyun;Ji-Seok Seo;Yun-Yong Kim
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.27 no.1
    • /
    • pp.46-53
    • /
    • 2023
  • In this paper, we evaluated the flexural performance of three types of reinforced concrete beams (SHCC-RB, SHCC-SB, SHCC-FRP) strengthened with ordinary steel rebar, very high strength (super strength) rebar, and FRP bars together with strain-hardening cement composite (SHCC). For this purpose, a series of beam specimens were manufactured and four-point load bending experiments were performed. As a result of the experiment, all specimens strengthened with SHCC exhibited tightly controlled flexural microcrakcs with the crack width of less than 100 ㎛. This is mostly due to the material properties of SHCC showing tensile strain hardening properties with multiple microcracks under uniaxial tension. The specimen SHCC-FRP showed lower initial cracking moment and yield flexural strength than SHCC-RB, whereas the maximum flexural strength of SHCC-FRP was superior to that of SHCC-RC. This is because the tensile strength of FRP bars is higher than that of ordinary steel reabr. The initial cracking moment of the beam specimen SHCC-SB was similar to that of SHCC-RB, but the yield flexural strength and maximum flexural strength of SHCC-SB were evaluated to be the highest.

Identification of Compliance Function for Early-Age Concrete Based on Measured Strain & Thermal Stress Histories (변형률 및 열응력 이력 계측을 통한 초기재령 콘크리트의 컴플라이언스 함수 추정)

  • Oh, Byung-Hwan;Shin, Joon-Ho;Choi, Seong-Cheol;Cha, Soo-Won
    • Journal of the Korea Concrete Institute
    • /
    • v.15 no.5
    • /
    • pp.662-669
    • /
    • 2003
  • Recently, the serviceability and durability of concrete structures under thermal load have received great attention. The thermal stress and clacking behavior of concrete at early ages are one of the important factors that affect such serviceability and durability of concrete structures. Nevertheless, most studies on the behavior of early-age concrete have been confined to the temperature and strain development itself in the laboratory. The desirable efforts to explore the material properties of concrete at early-ages have not been made extensively so far. The purpose of the present study is, therefore, to identify some important material properties that affect the stress behavior of concrete at early-ages. To this end, full-scale concrete base-restrained wall members have been fabricated, and many sensors including thermocouples, strain meters and stress meters were installed inside of the wall members. These sensors were to measure the development of temperatures, strains and stresses at several location in concrete walls during the hardening and curing phase of early-age concrete. By using these measured values of strain and stress, the compliance function at early-age was identified. The basic form of compliance function derived in this study follows the double-power law. However, the results of present study indicate that the values of existing compliance functions are much lower than actual values, especially at very early-ages. It can be seen that the prediction of stresses of early-age concrete based on the proposed compliance function agrees very well with test data. The present study allows more realistic evaluation of varying stresses in early-age concrete under thermal load.

Damage of Overlaid Concrete Structures Subjected to Humidity Changes in the Atmosphere (습도 변화에 따른 콘크리트 덧씌우기 보수체의 손상분석)

  • 윤우현
    • Journal of the Korea Concrete Institute
    • /
    • v.14 no.5
    • /
    • pp.766-773
    • /
    • 2002
  • The failure phenomenon of overlaid concrete structures, such as surface crack, and peel-off failure, shear bond failure in the end contact zone, was investigated due to humidity changes. To investigate this failure phenomenon, the surface tensile stress, and the shear stress, the vertical tensile stress in the contact zone were analysed using the non-linear stress-strain relationship of material such as strain-hardening- and strain-softening diagrams. Overlay thickness and overlay material were the main variables in the analyses. It is assumed that the initial surface humidity of overlaid concrete structures was 100% r.H. With a atmospheric humidity of 55% r.H. and two load cases for drying(LCI), curing and drying(LC2), the stress states of overlaid concrete structures were calculated. The result shows that only fictitious cracks occurred in the overlay surface of CM2O, ECM25, and no shear bond failure occurred in the contact zone without CM2O. The peel-off failure was proved to be the main cause of the damage in the overlaid concrete structures. Only for overlay thickness of 1cm occurred no peel-off failure in the case of drying after a long-term public use(LC1). In the case of curing and drying during overlay work(LC2) occurred the peel-off failure within 1.5days for all the overlaid concrete structures.