Axial compressive behavior of concrete-encased CFST stub columns with open composite stirrups

  • Ke, Xiaojun;Ding, Wen;Liao, Dingguo
    • Advances in concrete construction
    • /
    • 제12권5호
    • /
    • pp.399-409
    • /
    • 2021
  • The existing method to improve the coordination performance of the inner and outer parts of concrete-encased concrete-filled steel tube (CFST) composite columns by increasing the volume-stirrup ratio causes difficulties in construction due to over-dense stirrups. Thus, this paper proposes an open polygonal composite stirrup with high strength and high ductility CRB600H reinforced rebar, and seventeen specimens were constructed, and their axial compressive performance was tested. The main parameters considered were the volume-stirrup ratio, the steel tube size, the stirrup type and the stirrup strength. The test results indicated: For the specimens restrained by open octagonal composite stirrups, compared with the specimen of 0.5% volume-stirrup ratio, the compressive bearing capacity increased by 14.6%, 15.7% and 21.5% for volume-stirrup ratio of 0.73%, 1.07% and 1.61%, respectively. For the specimens restrained by open composite rectangle stirrups, compared with the specimen of 0.79% volume-stirrup ratio, the compressive bearing capacity increased by 7.5%, 6.1%, and -1.4% for volume-stirrup ratio of 1.12%, 1.58% and 2.24%, respectively. The restraint ability and the bearing capacity of the octagonal composite stirrup are better than other stirrup types. The specimens equipped with open polygonal composite stirrup not only had a higher ductility than those with the traditional closed-loop stirrup, but they also had a higher axial bearing capacity than those with an HPB300 strength grades stirrup. Therefore, the open composite stirrup can be used in practical engineering. A new calculation method was proposed based on the stress-strain models for confined concrete under different restrain conditions, and the predicted value was close to the experimental value.

승마 속보 시 등자 길이에 따른 체간기울기와 양측 하지의 협응성 비교분석 : 비대칭 지수 및 전체이동지수 알고리즘 개발 (Analysis of the Coordination of the Trunk Tilting Angle and Bilateral Lower Limbs According to the Stirrups Length during Trot in Equestrian: Asymmetric Index Development of Overall Movement Index Algorithm)

  • 현승현;류재청
    • 한국운동역학회지
    • /
    • 제25권1호
    • /
    • pp.131-140
    • /
    • 2015
  • Purpose : The purpose of this study was to analyze the coordination of the trunk tilting angle and bilateral lower limbs according to the stirrups length during trot in equestrian. Methods : Participants selected as subject were consisted of adult male(n=7, mean age: $45.00{\pm}3.78yrs$, mean height: $172.50{\pm}2.44cm$, mean body mass: $76.95{\pm}4.40kg$, mean, mean leg length: $97.30{\pm}2.60cm$). They were divided into 3-types of stirrups lengths(67 cm, 72 cm, 77 cm) during trot. The variables analyzed were consisted of the trunk front-rear angle, lower limb joint(Right Left hip, knee, ankle), overall movement index(OMI) of the lower limbs(thigh, shank, foot) and asymmetry index(AI%) during trot. Results : The average angle in hip and knee joint showed more extended posture according to the increase of stirrups lengths and ankle angle showed more plantarflexion posture according to increase of stirrups length during 1 stride in trot. Also, average angle showed more extended posture in right hip and ankle joint than that of left. The angle of knee joint didn't show significant difference statistically between right and left. Also asymmetric index in average angle of hip, knee and ankle joint didn't show significant difference statistically in between lower limbs, but hip joint showed higher asymmetric index in stirrup length of 77 cm and ankle joint showed higher asymmetric index in stirrup length of 67 cm than that of the others respectively. The FR angle in trunk of horse-rider showed relative backward leaning motions at stirrup length of 67 cm and 77 cm than that of stirrup length of 72 cm during stance and swing phase. OMI in thigh, shank, and foot limbs didn't show significant difference statistically according to the stirrups length of right and left lower limbs, but left lower limbs showed higher index than that of right lower limb. Stirrup length of 72 cm in shank and foot limbs showed higher index than that of stirrup length of 67 cm and 77 cm. But stirrup length of 72 cm showed higher asymmetric index than that of stirrups length of 67 cm and 77 cm. Conclusions : When considering the above, 72 cm(ratio of lower limb 74.04%) stirrup lengths could be useful in posture correction and stabilization than 67cm(ratio of lower limb 68.69%) and 77 cm(ratio of lower limb 79.18%) stirrup lengths during trot in horse back riding.

Seismic behaviour of concrete columns with high-strength stirrups

  • Wang, Peng;Shi, Qingxuan;Wang, Feng;Wang, Qiuwei
    • Earthquakes and Structures
    • /
    • 제18권1호
    • /
    • pp.15-25
    • /
    • 2020
  • The seismic behaviour of reinforced concrete (RC) columns made from high-strength materials was investigated experimentally. Six high-strength concrete specimen columns (1:4 scale), which included three with high-strength stirrups (HSSs) and three with normal-strength stirrups (NSSs), were tested under a combination of high axial and reversed cyclic loads. The effects of stirrup strength and the ratio of transverse reinforcement on the cracking patterns, hysteretic response, strength, stiffness, ductility, energy dissipation and strain of transverse reinforcement were studied. The results indicate that good seismic behaviour of an RC column subjected to high axial compression can be obtained by using a well-shaped stirrup. Stirrup strength had little effect on the lateral bearing capacity. However, the ductility was significantly modified by improving the stirrup strength. When loaded with a large lateral displacement, the strength reduction of NSS specimens was more severe than that of those with HSSs, and increasing the stirrup strength had little effect on the stiffness reduction. The ductility and energy dissipation of specimens with HSSs were superior to those with NSSs. When the ultimate displacement was reached, the core concrete could be effectively restrained by HSSs.

전단보강철근이 있는 기존 전단실험 자료를 이용한 전단특성에 관한 연구 (A Study of Shear Resistance Characteristics using Shear Test Data with Stirrup)

  • 신근옥;이창신;정제평;김우
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 봄학술 발표회 논문집(I)
    • /
    • pp.403-406
    • /
    • 2005
  • This paper deals with the propriety of the shear test data with stirrup reported in ACI and ASCE structural journal and the shear resistance characteristics affected by compressive strength of concrere($f_{ck}$), shear span-to-depth ratio (a/d), tensile reinforcement ratio($\rho$), and shear reinforcement ratio($rho_{v}$). The analysis was accomplished by the 242 shear test data. The test data include the flexural failure data around 40$\%$.

  • PDF

GFRP 스터럽으로 보강된 콘크리트 보의 전단성능에 관한 실험적 연구 (An Experimental Study for Shear-Carrying Capacity of Reinforced Concrete Beam with GFRP Stirrup)

  • 심종성;오홍섭;박철우;주민관;강태성
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2005년도 추계 학술발표회 제17권2호
    • /
    • pp.263-266
    • /
    • 2005
  • Recently, many researches for high-strength and high-durability concrete structure have remarkably been studied by adopting new construction material, fiber reinforced polymer (FRP). In connection with these research trend, the shearing capacity of concrete beams reinforced by GFRP stirrup which is developed in this study was evaluated. Experimental variables are span to depth ratio and spacing of shear reinforcement for test. In the result of test, the crack pattern, failure mode and shear load between shear steel reinforcement specimen and GFRP stirrup reinforcement specimen showed similar structural tendency. Therefore, it was investigated that the adaptability of shear-reinforced concrete structure with GFRP stirrup will be improved with further researches of shear design variables.

  • PDF

Analysis of the dynamic confining effect of CRAC short column under monotonic loadings

  • Wang, Changqing;Xiao, Jianzhuang
    • Structural Engineering and Mechanics
    • /
    • 제74권3호
    • /
    • pp.351-363
    • /
    • 2020
  • Based on the dynamic tests of recycled aggregate concrete (RAC) short columns confined by the hoop reinforcement, the dynamic failure mechanism and the mechanical parameters related to the constitutive relation of confined recycled aggregate concrete (CRAC) were investigated thoroughly. The fracturing sections were relatively flat and smooth at higher strain rates rather than those at a quasi-static strain rate. With the increasing stirrup volume ratio, the crack mode is transited from splitting crack to slipping crack constrained with large transverse confinement. The compressive peak stress, peak strain, and ultimate strain increase with the increase of stirrup volume ratio, as well as the increasing strain rate. The dynamic confining increase factors of the compressive peak stress, peak strain, and ultimate strain increase by about 33%, 39%, and 103% when the volume ratio of hoop reinforcement is increased from 0 to 2%, but decrease by about 3.7%, 4.2%, and 9.1% when the stirrup spacing is increased from 20mm to 60mm, respectively. This sentence is rephrased as follows: When the stirrup volume ratios are up to 0.675%, and 2%, the contributions of the hoop confinement effect to the dynamic confining increase factors of the compressive peak strain and the compressive peak stress are greater than those of the strain rate effect, respectively. The dynamic confining increase factor (DCIF) models of the compressive peak stress, peak strain, and ultimate strain of CRAC are proposed in the paper. Through the confinement of the hoop reinforcement, the ductility of RAC, which is generally slightly lower than that of NAC, is significantly improved.

Seismic performance and damage evaluation of concrete-encased CFST composite columns subjected to different loading systems

  • Xiaojun Ke;Haibin Wei;Linjie Yang;Jin An
    • Steel and Composite Structures
    • /
    • 제47권1호
    • /
    • pp.121-134
    • /
    • 2023
  • This paper tested 11 concrete-encased concrete-filled steel tube (CFST) composite columns and one reinforced concrete column under combined axial compression and lateral loads. The primary parameters, including the loading system, axial compression ratio, volume stirrup ratio, diameter-to-thickness ratio of the steel tube, and stirrup form, were varied. The influence of the parameters on the failure mode, strength, ductility, energy dissipation, strength degradation, and damage evolution of the composite columns were revealed. Moreover, a two-parameter nonlinear seismic damage model for composite columns was established, which can reflect the degree and development process of the seismic damage. In addition, the relationships among the inter-story drift ratio, damage index and seismic performance level of composite columns were established to provide a theoretical basis for seismic performance design and damage assessments.

전단보강된 고강도경량콘크리트 보의 휨거동에 관한 연구 (A Study on the Flexural Behavior of Reinforced High Strength Lightweight Concrete Beams With Web Reinforcement)

  • 오창륜;김재식;곽윤근
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1998년도 봄 학술발표회논문집(II)
    • /
    • pp.513-518
    • /
    • 1998
  • In general, flexural strength and ductility of reinforced concrete beam with stirrup depend on the compressive strength of concrete and longitudinal steel ratio. In this study, nine reinforced high strength lightweight concrete beams and three reinforced normalweight concrete beams with stirrup were tested to investigate their behavior and to determine their ultimate moment capacity. The variable were strength of concrete (400, 500kg/$\textrm{cm}^2$) and the ratio of tensile steel content to the ratio of the balanced steel content(0.22<$\rho$/$$\rho$_b$<0.56). Test results are presented in terms of load-deflection behavior, ductility index, and cracking patterns.

  • PDF

Seismic analysis of RC tubular columns in air-cooled supporting structure of TPP

  • Wang, Bo;Yang, Ke;Dai, Huijuan;Bai, Guoliang;Qin, Chaogang
    • Earthquakes and Structures
    • /
    • 제18권5호
    • /
    • pp.581-598
    • /
    • 2020
  • This paper aims to investigate the seismic behavior and influence parameters of the large-scaled thin-walled reinforced concrete (RC) tubular columns in air-cooled supporting structures of thermal power plants (TPPs). Cyclic loading tests and finite element analysis were performed on 1/8-scaled specimens considering the influence of wall diameter ratio, axial compression ratio, longitudinal reinforcement ratio, stirrup reinforcement ratio and adding steel diagonal braces (SDBs). The research results showed that the cracks mainly occurred on the lower half part of RC tubular columns during the cyclic loading test; the specimen with the minimum wall diameter ratio presented the earlier cracking and had the most cracks; the failure mode of RC tubular columns was large bias compression failure; increasing the axial compression ratio could increase the lateral bearing capacity and energy dissipation capacity, but also weaken the ductility and aggravate the lateral stiffness deterioration; increasing the longitudinal reinforcement ratio could efficiently enhance the seismic behavior; increasing the stirrup reinforcement ratio was favorable to the ductility; RC tubular columns with SDBs had a much higher bearing capacity and lateral stiffness than those without SDBs, and with the decrease of the angle between columns and SDBs, both bearing capacity and lateral stiffness increased significantly.

보의 전단거동에서 콘크리트 압축강도가 스터럽 유효성에 미치는 영향 (Effect of Concrete Strength on Stirrup Effectiveness in Shear Behavior of Concrete Beams)

  • 이영재;서원명;김진근;박찬규
    • 콘크리트학회지
    • /
    • 제8권6호
    • /
    • pp.173-182
    • /
    • 1996
  • 이 연구에서는 콘크리트 보의 전단거동에서 콘크리트 압축강도가 스터럽 유효성에 미치는 영향을 실험적으로 연구하였다. 이를 위하여 단며이 $300{\times}600mm$ 인 수직 스터럽이 배근되지 않은 콘크리트 보 4개와 수직 스터럽이 배근된 콘크리트 보 20개에 대하여 실험을 수행하였다. 주요 실험변수는 2종류(보통강도, 고강도)의 콘크리트 압축강도 수준과 6종류의 전단철근비이다. 실험에 앞서 주어진 단면과 가정된 재료 상수에 대하여 ACI Building Code를 사용하여 휨파괴가 유발되는 전단철근비( ${\rho}_vACI$)를 산정하였으며, 이 값을 기준으로 6종류의 전단철근비를 선택하였다. 실험결과, 스터럽이 배근되지 않은 콘크리트 보에 있어서 ACI 전단강도식의 안전율은 콘크리트의 압축강도가 증가함에 따라 감소하는 것으로 나타났다. 그러나 스터럽이 많이 배근된 고강도 콘크리트 보에서는 보통강도 콘크리트 보 이상의 안전율이 확보되는 것으로 나타나 스터럽 유효성은 고강도 콘크리트 보에서 더 큰 것으로 나타났다.