Performance of self-compacting geopolymer concrete with and without GGBFS and steel fiber

  • Al-Rawi, Saad;Taysi, Nildem
    • Advances in concrete construction
    • /
    • v.6 no.4
    • /
    • pp.323-344
    • /
    • 2018
  • The study herein reports the impact of Steel Fiber (SF) and Ground Granulated Blast Furnaces slag (GGBFS) content on the fresh and hardened properties of fly ash (FA) based Self-Compacting Geopolymer Concrete (SCGC). Two series of self-compacting geopolymer concrete (SCGC) were formulated with a constant binder content of $450kg/m^3$ and at an alkaline-to-binder (a/b) ratio of 0.50. Fly ash (FA) was substituted with GGBFS with the replacement levels being 0%, 25%, 50%, 75%, and 100% by weight in each SCGC series. Steel fiber (SF) wasn't employed in the assembly of the initial concrete series whereas, within the second concrete series, an SF combination was achieved by a constant additional level of 1% by volume. Fresh properties of mixtures were through an experiment investigated in terms of slump flow diameter, T50 slump flow time, V-funnel flow time, and L-box height ratio. Moreover, the mechanical performance of the SCGCs was evaluated in terms of compressive strength, splitting tensile strength, and fracture toughness. Furthermore, a statistical analysis was applied in order to judge the importance of the experimental parameters, like GGBFS and SF contents. The experimental results indicated that the incorporation of SF had no vital impact on the fresh characteristics of the SCGC mixtures whereas GGBFS aggravated them. However, the incorporation of GGBFS was considerably improved the mechanical properties of SCGCs. Moreover, the incorporation of SF with the total different quantity of GGBFS replacement has considerably increased the mechanical properties of SCGCs, by close to (65%) for the splitting strength and (200%) for compressive strength.

Strength Characteristics of Concrete Subjected In Horizontal Continuous Vibration During Initial Curing (초기양생중에 수평연속진동을 받은 콘크리트의 강도특성)

  • 장희석;김명식;김종수;한중기
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.5
    • /
    • pp.423-429
    • /
    • 2001
  • In this study, strength characteristics of concrete specimens subjected to horizontal continuous vibration during initial curing were investigated. As experimental variables, vibration velocity(0.25, 0.5, 1.0, 2.0, 4.0 kine) and vibration time(3, 6, 12, 24 hrs) were used. Density and segregation of the specimens were also investigated. Vibrating was started soon after placing, and strengths investigated consist of compressive strength, splitting tensile strength, and bond strength. Strengths decrease were hardly occurred at 0.25 kine vibration velocity regardless of vibration times and all strengths were increased for 3 hrs vibration at 0.5 kine vibration velocity. Density was increased for all specimens due to the vibration and there was no serious segregation under even 4 kine vibration velocity.

A Study on the Strength and Mechanical Characteristics of Normal and High-Strength Fly-Ash Concretes (플라이애쉬 콘크리트의 강도 및 역학적 특성에 관한 연구)

  • 오병환;고재군
    • Magazine of the Korea Concrete Institute
    • /
    • v.3 no.2
    • /
    • pp.87-95
    • /
    • 1991
  • Presented is a study on the strength and mechanical characteristics of various fly ash concrete mixes. To this end, a comprehensive experimental study was conducted for normal and high-strength fly ash concretes. The fly-asb contents were varied from 0% to 30% of cement weight to explore the effects of fly ash addition. The op timum fly-ash amounts reqUIred to obtain the desired strengths were established from the present study. ThE prediction equations for the flexural -strength. splitting tensile strength and elastic modulus of lly-ash concrete were also proposed.

Effect of waste glass as powder and aggregate on strength and shrinkage of fiber reinforced foam concrete

  • Mayada A. Kareem;Ameer A. Hilal
    • Advances in materials Research
    • /
    • v.12 no.4
    • /
    • pp.331-349
    • /
    • 2023
  • Foam concrete can be considered as environmental friendly material due to its low weight, its minimal cost and a possibility to add waste materials in its production. This paper investigates the possibility of producing foam concrete with waste glass as powder and aggregate. Then, the effect of using waste glass on strength and drying shrinkage of foam concrete was examined. Also, the effect of incorporating polypropylene fibers (12 mm length and proportion of 0.5% of a mix volume) on distribution of waste glass as coarse particles within 1200 kg/m3 foam concrete mixes was evaluated. Waste glass was used as powder (20% of cement weight), as coarse particles (25%, 50% and 100% instead of sand volume) and as fine particles (25% instead of sand volume). From the results, the problem of non-uniform distribution of coarse glass particles was successfully solved by adding polypropylene fibers. It was found that using of waste glass as coarse aggregate led to reduce the strength of foam concrete mixes. However, using it with polypropylene fibers in combination helped in increasing the strength by about 29- 50% for compressive and 55- 71% for splitting tensile and reducing the drying shrinkage by about (31- 40%). In general, not only the fibers role but also the uniformly distributed coarse glass particles helped in improving and enhancing the strength and shrinkage of the investigated foam concrete mixes.

Properties of Concrete Mixed with Waste Incinerated Bottom Ash (쓰레기 소각재를 혼입한 콘크리트의 재료특성 및 강도특성)

  • 어석홍;홍기호;최덕진;김희성
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.10a
    • /
    • pp.217-222
    • /
    • 2002
  • The purposes of this study are to investigate the material characteristics and strength properties of concrete mixed with waste incinerated bottom ash(BA), and to evaluate the leaching of environmentally harmful heavy metals from the bottom ash itself and from hardened concrete mixed with bottom ash. For this purpose, two reference mixes with W/C ratios of 0.45 and 0.55 were used, and the replacement proportion of BA was varied with the ratios of 0%, 30%, 50%, 70%, and 100% by volume of fine aggregate in the reference mixes. The variation of compressive and splitting tensile strength, workability and unit weight of concrete were considered. Test results showed that the strengths, workability and unit weight decreased with increase in proportion of BA replaced. Leaching test results showed that there would be no environmentally harmful problem from using BA as the substitutes of fine aggregates in concrete.

  • PDF

Recycled Concrete Aggregates: A Review

  • McNeil, Katrina;Kang, Thomas H.K.
    • International Journal of Concrete Structures and Materials
    • /
    • v.7 no.1
    • /
    • pp.61-69
    • /
    • 2013
  • This paper discusses the properties of RCA, the effects of RCA use on concrete material properties, and the large scale impact of RCA on structural members. The review study yielded the following findings in regards to concrete material properties: (1) replacing NA in concrete with RCA decreases the compressive strength, but yields comparable splitting tensile strength; (2) the modulus of rupture for RCA concrete was slightly less than that of conventional concrete, likely due to the weakened the interfacial transition zone from residual mortar; and (3) the modulus of elasticity is also lower than expected, caused by the more ductile aggregate. As far as the structural performance is concerned, beams with RCA did experience greater midspan deflections under a service load and smaller cracking moments. However, structural beams did not seem to be as affected by RCA content as materials tests. Most of all, the ultimate moment was moderately affected by RCA content. All in all, it is confirmed that the use of RCA is likely a viable option for structural use.

Fracture Behavior of Concrete Beam Subjected to Dynamic Loading (동적하중을 받는 콘크리트보의 파괴거동)

  • Kang, Sung-Hoo;Kim, Woo;Park, Sun-Joon
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1995.04a
    • /
    • pp.257-262
    • /
    • 1995
  • In this study, after concrete cylinders were made on the condition of varying water-to -cement ratio, and cured 80 days compressive strength and splitting tensile strength were performed and moduls of elasticy is obtained. The fracture energy was obtained by acting three point bending on the 80cm in length. This test involved static loading test and dynamic loading test. In this work, the new interrelation of the material constants was obtained clearly and the property of the mixture was inspected, including the relation between the fracture energy and all kind of the material constants.

  • PDF

Mechanical Behavior of Steel Fiber Reinforced Lightweight Polymer Concretese (강섬유보강 경량 폴리머 콘크리트의 역학적 거동)

  • Youn, Joon-No;Sung, Chan-Yong
    • Journal of The Korean Society of Agricultural Engineers
    • /
    • v.47 no.2
    • /
    • pp.63-72
    • /
    • 2005
  • In this study, the physical and mechanical properties of steel fiber reinforced lightweight polymer concrete were investigated experimentally with various steel fiber contents. All tests were performed at room temperature, and stress-strain curve and load-deflection curve were plotted up to failure. The unit weight of steel fiber reinforced lightweight polymer concrete was in the range of $1,020{\sim}1,160\;kg/m^3$, which was approximately $50\%$ of that of the ordinary polymer concrete, The compressive strength, splitting tensile strength, flexural toughness and flexural load-deflection curves after maximum load were shown with increase of steel fiber content. The stress-strain curves of steel fiber reinforced lightweight polymer concrete were bilinear in nature with a small transition zone, Based on these results, steel fiber reinforced lightweight polymer concrete can be widely applied to the polymer composite products.

An Experimental Research on the Material Properties of Super Flowing Concrete (초유동 콘크리트의 재료특성에 관한 실험적 연구)

  • 김진근;한상훈;박연동;노재호
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1995.10a
    • /
    • pp.56-62
    • /
    • 1995
  • In this study, the properties of super flowing cocrete containing gly ash were experimentally investigated and compared with those of ordinary concrete. Tests were carried out on five types of super flowing concrete mixes containing fly ash and three types of ordinary concrete mixes without fly ash. Flow test, O-funnel test, box test, Ltype thest and slump test were carried out to obtain the properties for the workability of fresh concrete. Compressime strength, splitting tensile strength, modulus of elasticity. creep and shrinkage test were also obtained as the mechanical properties of hardened concrete. In fresh concrete, it was found that super flowing concrete had excellent workability and flowability compared with ordinary concrete, and the volume ratio of coarse aggregate to concrete volume greatly influenced flowability. Super flowing concrete also had good mechanical properties at both early and late ages with compressive strengths reaching as high as 40 MPa at 28 days. The creep deformation of super flowing concrete investigated were relatively lower than that of ordinary concrete.

  • PDF

Effect of quartz powder, quartz sand and water curing regimes on mechanical properties of UHPC using response surface modelling

  • Mosaberpanah, Mohammad A.;Eren, Ozgur
    • Advances in concrete construction
    • /
    • v.5 no.5
    • /
    • pp.481-492
    • /
    • 2017
  • The aim of this paper is to investigate the effect of quartz powder (Qp), quartz sand (Qs), and different water curing temperature on mechanical properties including 7, 14, 28-day compressive strength and 28-day splitting tensile strength of Ultra High Performance Concrete and also finding the correlation between these variables on mechanical properties of UHPC. The response surface methodology was monitored to show the influences of variables and their interactions on mechanical properties of UHPC, then, mathematical models in terms of coded variables were established by ANOVA. The offered models are valid for the variables between: quartz powder 0 to 20% of cement substitution by cement weight, quartz sand 0 to 50% of aggregate substitution by crushed limestone weight, and water curing temperature 25 to $95^{\circ}C$.